216 records · Page 12

Corrosion behavior of mesoporous transition metal nitrides

Transition metal nitrides (TMN) have many desirable characteristics such as high hardness and good thermal stability under reducing conditions. This work reports an initial survey of the chemical stability of mesoporous TMNs (TM=Nb, V, Cr and Ti) in water at 80 °C at neutral, acidic and alkaline pH. The mesoporous TMNs had specific surface areas of 25–60 m{sup 2}/g with average pore sizes ranging from 10 to 50 nm. The high surface areas of these materials enhance the rate of corrosion per unit mass over that of a bulk material, making detection of corrosion much easier. The products were characterized by Rietveld refinement of powder X-ray diffraction (PXRD) patterns and by scanning electron microscopy (SEM). Several nitrides have corrosion rates that are, within error, not distinguishable from zero (±1 Å/day). Of the nitrides examined, CrN appears to be the most corrosion resistant under acidic conditions. None of the nitrides studied are corrosion resistant under alkaline conditions. - Graphical abstract: Corrosion behavior of mesoporous transition metal nitrides (TM=Nb, V, Cr and Ti) in acidic and alkaline solutions at 80 °C for 2 weeks. Display Omitted - highlights: • Corrosion rates of mesoporous transition metal nitrides in aqueous solution is reported. • The mesoporous TMNs had surface areas of 25–60 m{sup 2}/g. • CrN is the most corrosion resistant under the conditions studied.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Development of LWR Fuels with Enhanced Accident Tolerance ATF Feasibility Analysis Report Deliverable for the Westinghouse Accident Tolerant Fuel Program

The Westinghouse Electric Company LLC (Westinghouse) accident tolerant fuel (ATF) program utilizes chromium (Cr) coated zirconium alloy cladding with uranium silicide (U 3 Si 2 ) high density/high thermal conductivity fuel for its lead test rod (LTR) program with irradiation beginning in 2019. The lead test assembly (LTA) program will use both SiC/SiC composites and Cr coated zirconium alloy claddings with the high density/high thermal conductivity U 3 Si 2 pellet which will begin in 2022. Over the past several years, Westinghouse has tested the Cr coated zirconium (Zr) and silicon carbide (SiC) claddings in autoclaves and in the Massachusetts Institute of Technology (MIT) reactor and the U 3 Si 2 pellets have been tested in the Advanced Test Reactor (ATR) at Idaho National Laboratory (INL). High temperature tests at the state-of-the-art Westinghouse facilities in Churchill, PA have been carried out to determine the time and temperature limits for the SiC and Cr coated zirconium claddings. Fuel rod and assembly design in preparation for the LTR and LTA programs is underway as well as licensing efforts with the Nuclear Regulatory Commission (NRC). Finally, accident analyses coupled with economic evaluations for both operating savings as well as fuel savings have been initiated. Cr coated zirconium alloy claddings showed low corrosion rates in both autoclave and in-reactor tests and will be fabricated using commercial processes for the first LTRs for insertion in 2019. Current autoclave results for SiC composite claddings indicate that a corrosion rate of fewer than 2 micrometers per year which meets corrosion requirements may be achieved under normal operating conditions. Modular Accident Analysis Program 5 (MAAP5) calculations indicate that solid fission products can be contained within SiC cladding for up to two hours longer than current Zr based cladding in a station blackout scenario. This additional time is due to the much higher temperature capability of SiC (~2000°C). These two hours can be used to implement additional response options instituted through the FLEX program by reactor operators. While the Cr coated Zr alloy option offers more modest ATF gains (~200°C higher than bare Zr) in similar situations, the coatings do delay the runaway oxidation encountered by uncoated zirconium cladding. Both ATF cladding options also reduce hydrogen production which dramatically reduces primary system and containment pressure and the risk of fission product release beyond containment in the unlikely event of an accident. The lower pressure in the system allows more time to feed cooling water to the core, resulting in the avoidance of fuel melting. The coping time is extended indefinitely as long as the water flow continues. SiC exhibits the highest accident tolerance of any cladding and significant advances in understanding the design, manufacture and accident behavior of SiC cladding have been made. Department of Energy support is needed to continue the on-going experimental work addressing the interaction between U 3 Si 2 and SiC at temperatures >1200°C, the effect of SiC manufacturing methods and manufacturing variability on physical properties, and the ability to predict the mechanical properties of SiC composites based on the composite design. Additionally, experimental work on methods to rapidly fabricate SiC composite structures with high density and reduce the fabrication price of SiC fibers while maintaining a high level of performance is needed. Minimal (<1%) swelling of U 3 Si 2 and subsequent fission gas release has been demonstrated up to 20 MWd/kgU. Irradiation experiments with U 3 Si 2 fuel in ATR to determine these properties at 40 to 50 MWd/kgU are underway. These experiments will provide the data needed to license fuel rod design codes. Research is continuing on production methods for making U 3 Si 2 from UF 6 without going through the U metal step. Oxidation tests of fuel pellets and powder in steam and synthetic air indicate that U 3 Si 2 has a lower oxidation reaction initiation temperature than UO 2 . Options to reduce the U 3 Si 2 oxidation rate are being explored. A hybrid fuel design using pellets with the weight ratio of 30%/70% U 3 Si 2 /UN is currently undergoing testing in the ATR. This approach is being explored to further increase the positive economics of the U 3 Si 2 fuel. In addition to the work supported by the USDOE, research and testing activities are being carried on in a world-wide effort funded by many countries such as Sweden, United Kingdom, Belgium, Netherlands, Spain, Germany, Japan and France. This work is being facilitated through the Westinghouse led Collaboration for Advanced Research on Accident Tolerant Fuel (CARAT) program. Annual meetings are organized by Westinghouse as a venue for presentation of this work and to provide for the cross-fertilization of ideas among the many outstanding researchers in the ATF area. Since SiC, coated cladding and high density fuel options are not currently used in the nuclear industry, support from the government and industry members is needed to further the significant effort of setting new standards. The same is true for the Nuclear Regulatory Commission (NRC) which must review and approve the commercial use of these new fuels since all current regulations are oriented toward Zr/ UO 2 fuel. There are no showstoppers for accident tolerant fuel technologies when considering supply chain, fabrication, enrichment suppliers, production, and licensing. Due to the cost savings from higher density fuel and the accident tolerance of coated claddings, Exelon has identified potential commercial plants to host the LTRs and LTAs. Planning is underway to implement this schedule.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of annealing treatment on the electrical characteristics of Pt/Cr-embedded ZnO/Pt resistance random access memory devices

ZnO/Cr/ZnO trilayer films sandwiched with Pt electrodes were prepared for nonvolatile resistive memory applications. The threshold voltage of a ZnO device embedded with a 3-nm Cr interlayer was approximately 50% lower than that of a ZnO monolayer device. This study investigated threshold voltage as a function of Cr thickness. Both the ZnO monolayer device and the Cr-embedded ZnO device structures exhibited resistance switching under electrical bias both before and after rapid thermal annealing (RTA) treatment, but resistive switching effects in the two cases exhibited distinct characteristics. Compared with the as-fabricated device, the memory cell after RTA demonstrated remarkable device parameter improvements, including a lower threshold voltage, a lower write current, and a higher R{sub off}/R{sub on} ratio. Both transmission electron microscope observations and Auger electron spectroscopy revealed that the Cr charge trapping layer in Cr-embedded ZnO dispersed uniformly into the storage medium after RTA, and x-ray diffraction and x-ray photoelectron spectroscopy analyses demonstrated that the Cr atoms lost electrons to become Cr{sup 3+} ions after dispersion. These results indicated that the altered status of Cr in ZnO/Cr/ZnO trilayer films during RTA treatment was responsible for the switching mechanism transition.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic properties of CuFe{sub 1−x}Cr{sub x}O{sub 2} nanoparticles surrounded by amorphous SiO{sub 2}

CuFe{sub 1−x}Cr{sub x}O{sub 2} (0 ≤ x ≤ 1.0) nanoparticles surrounded by amorphous SiO{sub 2} with an average diameter of 30–50 nm were synthesized using a wet chemical method. The annealing temperatures were controlled to yield various sizes of single-phase CuFe{sub 1−x}Cr{sub x}O{sub 2} nanoparticles. CuFeO{sub 2} bulk crystal is known to have a multiferroic delafossite structure with two Néel temperatures of 11 and 14 K; however, the transition temperature shifted higher as the Cr–ion doping level increased. In addition, the lattice constants decreased in accordance with increased Cr-ion doping, which was confirmed by X-ray diffraction measurements. The magnetization curves showed weak ferromagnetic behavior and no coercivity was observed. Hence, frustration in the triangular lattice of the delafossite structure can be released by Cr–ion doping and higher magnetization can be expected. A fine structure analysis through X-ray absorption fine structure measurements was also conducted. It was found that the structure of the Cu ion is similar to that of Cu{sub 2}O, and the c axis of the CuFe{sub 1−x}Cr{sub x}O{sub 2} should be shortened by the Cr–ion doping.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Highly (002) textured large grain bcc Cr{sub 80}Mn{sub 20} seed layer on Cr{sub 50}Ti{sub 50} amorphous layer for FePt-C granular film

Effect of bcc Cr{sub 80}Mn{sub 20} seed layer and Cr{sub 50}Ti{sub 50} amorphous texture inducing layer on the heteroepitaxy system in FePt-C granular film was studied by introducing a new concept of the layered structure. The concept suggested that the large grain seed layer in which the crystallographic texture was initially formed on an amorphous layer in the layered structure can reduce the angular distribution of (002) c-axis crystal orientation in the FePt-C granular film owing to heteroepitaxial growth. Structure analysis by X-ray diffraction revealed that (1) when the substrate heating temperature was elevated from 300 °C to 500 °C, grain size in the seed layer increased from 9.8 nm to 11.6 nm, and then decreased with further increasing the substrate temperature. The reduction of the grain size over 500 °C corresponds to the crystallization of the amorphous texture inducing layer, (2) when the grain size increased from 9.8 nm to 11.6 nm, the angular distribution of the (002) orientation in the seed layer dramatically decreased from 13.7° to 4.1°. It was shown that the large grain seed layer increased the perpendicular hysteresis in FePt-C granular film.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of high temperature treatment on microstructure and mechanical properties of laser-clad NiCrBSi/WC coatings on titanium alloy substrate

Laser-clad composite coatings on the Ti6Al4V substrate were heat-treated at 700, 800, and 900 °C for 1 h. The effects of post-heat treatment on the microstructure, microhardness, and fracture toughness of the coatings were investigated by scanning electron microscopy, X-ray diffractometry, energy dispersive spectroscopy, and optical microscopy. The wear resistance of the coatings was evaluated under dry reciprocating sliding friction at room temperature. The coatings mainly comprised some coarse gray blocky (W,Ti)C particles accompanied by the fine white WC particles, a large number of black TiC cellular/dendrites, and the matrix composed of NiTi and Ni{sub 3}Ti; some unknown rich Ni- and Ti-rich particles with sizes ranging from 10 nm to 50 nm were precipitated and uniformly distributed in the Ni{sub 3}Ti phase to form a thin granular layer after heat treatment at 700 °C. The granular layer spread from the edge toward the center of the Ni{sub 3}Ti phase with increasing temperature. A large number of fine equiaxed Cr{sub 23}C{sub 6} particles with 0.2–0.5 μm sizes were observed around the edges of the NiTi supersaturated solid solution when the temperature was further increased to 900 °C. The microhardness and fracture toughness of the coatings were improved with increased temperature due to the dispersion-strengthening effect of the precipitates. Dominant wear mechanisms for all the coatings included abrasive and delamination wear. The post-heat treatment not only reduced wear volume and friction coefficient, but also decreased cracking susceptibility during sliding friction. Comparatively speaking, the heat-treated coating at 900 °C presented the most excellent wear resistance. - Highlights: • TiC + WC reinforced intermetallic compound matrix composite coatings were produced. • The formation mechanism of the reinforcements was analyzed. • Two precipitates were generated at elevated temperature. • Cracking susceptibility and microhardness of the coatings were improved. • Post-heat treatment enhances wear resistance of the coatings.

36 MATERIALS SCIENCE↗

Uranium–Molybdenum Alloy Critical Experiments for the Design of the Health Physics Research Reactor

Clean critical experiments with a uranium-molybdenum alloy (average of 10.1616 wt. % Mo with a density of 17.08 g/cm 3 ) were performed at the Oak Ridge Critical Experiments Facility in 1961 to support the design of the Health Physics Research Reactor (HPRR). The HPRR was similar to the Godiva burst reactor at Los Alamos National Laboratory and was designed to produce 50 microseconds burst of 10 17 fission pulses of radiation for dosimetry measurements, initially in support of the determination of the doses from the nuclear detonations in Japan during World War II. These experiments reported here were used to verify the calculational methods used to design the HPRR. These delayed critical measurements were:1) a solid unreflected and unmoderated 8-in.-dimeter U-Mo cylinder, 2) an unmoderated and unreflected annulus with 8-in.-outside diameter, 2-in.-inside diameter cylinder with a central void, 3) an unmoderated and unreflected annulus with 8-in.-outside diameter, 2-in.-inside diameter cylinder with a central void filled with stainless steel, 4) Same as 3) but with 3-in-thick Plexiglas reflector on top with and without cadmium between the reflector and the U-Mo alloy assembly with steel in the center, and 5) an unmoderated and unreflected annulus which was a modification of the second but with the lower 5 inches of the central hole enlarged to 3.5 in. with various reflector conditions. The reflector conditions were: 1-in.-thick Plexiglas on all outer surfaces-void in the center; 1-in.-thick Plexiglas on all outer surfaces-Plexiglas in the center; 2-in.- thick Plexiglas on radial surface-void in the center; 6-in.-thick Plexiglas on the bottom only-Plexiglas in the center; and 6-in.-thick Plexiglas on bottom, 1-in.-thick on top and on the lower 8.25-cm.-section of the radial surface-void in the center. For some of these reflector conditions 0.025-cm.thick cadmium was located between the reflector and the U-Mo alloy. The uranium contained 93.17 wt. % 235 U. Reflection was a safety concern for this unmoderated and unreflected reactor and reduction of reflection effects was also investigated by insertion of neutron absorber around the U-Mo alloy. The stainless steel 304 contained 18% nickel and 8% chromium and the rest iron. The reflector material was a methacrylate plastic (Plexiglas) containing 5.8 x 10 22 atoms/cm 3 of hydrogen and 3.6 x 10 22 atoms/cm 3 of carbon with a density of 1.20 g/cm 3 . The purpose of this report is to document the experimental information for the measurements performed so that at a later date researchers could perform the required uncertainty and calculational analyses and documentation to use these data for an International Nuclear Criticality Safety Benchmark Program (ICSBEP) or a EURATON Nuclear Energy Agency (NEA) benchmark. The data from the experiments described should be acceptable for use as criticality safety benchmark experiments for the ICSBEP and the NEA nuclear criticality safety benchmark program, once the uncertainty analysis is completed. Based on previous ICSBEP benchmarks with this enriched uranium metal at ORCEF, the uncertainties in k eff could be as low as ±0.0002 for some configurations.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Preparation, structural and magnetic characterization of DyCrMnO{sub 5}

The title compound has been first synthesized by a citrate technique followed by thermal treatments under moderate oxygen pressure conditions, and characterized by X-ray and neutron powder diffraction (NPD) and magnetization measurements. The crystal structure of DyCrMnO{sub 5} has been refined from NPD data in the space group Pbam; a=7.2617(6) A, b=8.5161(6) A, and c=5.7126(5) A at 295 K. This oxide is isostructural with RMn{sub 2}O{sub 5} oxides (R=rare earths) and it contains infinite chains of (Cr, Mn){sup 4+}O{sub 6} octahedra-sharing edges, linked together by (Mn, Cr){sup 3+}O{sub 5} pyramids and DyO{sub 8} units. The high degree of antisite disordering exhibited by DyCrMnO{sub 5} is noteworthy. The octahedral positions are occupied by roughly 50% of Mn and Cr cations, and the pyramidal groups contain two thirds of Mn and one third of Cr cations. We assume that Mn and Cr cations at the octahedral positions exhibit a tetravalent oxidation state, whereas the metals at the pyramidal positions are trivalent, in order to preserve the electroneutrality of this oxide. The susceptibility vs temperature curve of DyCrMnO{sub 5} does not suggest the establishment of a long-range magnetic structure even at low temperatures; the NPD technique does not provide any signal of magnetic ordering, since the reflections do not show any magnetic contribution. - Graphical abstract: DyCrMnO{sub 5} is isostructural with DyMn{sub 2}O{sub 5}, belonging to the Pbam space group. The crystal structure contains infinite chains of edge-sharing Mn{sup 4+}O{sub 6} octahedra, interconnected by dimer units of Cr{sup 3+}O{sub 5} square pyramids. The low-temperature neutron powder diffraction (NPD) patterns do not show any magnetic contribution, indicating that a full long-range magnetic ordering is not established down to low temperature, although the Dy{sup 3+} magnetic moments are susceptible to be polarized by an external magnetic field at the lowest temperature of 5 K.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Calcium Phosphate Constraints in HLW Glasses: Phosphate Liquidus Model

About 50 million gallons of high-level mixed waste is currently stored in underground tanks at the United States Department of Energy’s (DOE’s) Hanford site in the State of Washington. The Hanford Tank Waste Treatment and Immobilization Plant (WTP) will provide DOE’s Office of River Protection (ORP) with a means of treating this waste by vitrification for subsequent disposal. The tank waste will be separated into low- and high-activity waste fractions, which will then be vitrified respectively into Immobilized Low Activity Waste (ILAW) and Immobilized High Level Waste (IHLW) products. The ILAW product will be disposed in an engineered facility on the Hanford site while the IHLW product is designed for acceptance into a national geological disposal facility for high-level nuclear waste. The ILAW and IHLW products must meet a variety of requirements before they can be accepted for disposal. Glass property-composition models will be used to control the vitrification process at the WTP to ensure that the glass meets product quality and processability requirements. The quality and the validity ranges of the property-composition models and the supporting database will greatly influence waste treatment operations, including the waste loading that is achievable in the glass for each waste composition. The current baseline models for operation of the WTP were developed under the Bechtel National, Inc. (BNI) WTP contract. These models were based on LAW and HLW glass property data over a range of compositions that was guided primarily by the WTP contract and the set of tanks specified therein. The HLW testing was directed towards waste streams from the then-planned early feed tanks for the WTP (i.e., AZ-101, AZ-102, C-106/AY-102, and C-104/AY-101). These wastes are high in iron (AZ-101, AZ-102, and C-106/AY-102) or thorium (C-104/AY-101). While the baseline models may be adequate for commissioning of the facility and processing of the specified tanks, refinements and extensions or augmentations of these models will be required to process the balance of the tank waste inventory. The overall mission of the WTP will require the immobilization of tank waste compositions that are variously dominated by mixtures of aluminum, chromium, bismuth, iron, phosphorous, zirconium, and sulfur compounds as waste-loading-limiting components. Further, the WTP contract includes minimum waste loading requirements that are generally rather modest while loadings significantly higher than those in the current baseline are likely achievable. In order to achieve these higher waste loadings and to expand the applicable composition regions, new models will be needed to support the optimized operation of the WTP. Since the development of the baseline WTP models, ORP directed a program of work at the Vitreous State Laboratory (VSL) to examine various approaches for optimization of the performance of the WTP, including increasing the waste loadings in the LAW and HLW glass products. That work involved HLW rich in Al, Al+Na, Cr, Bi, S, Zr, Sr, P and Fe, in contrast to old baseline models that were based mostly on HLW tanks that were high in Fe, with one other that was also high in Th. Glass property data collected under the ORP program were compiled and combined with data collected to develop the WTP models. The combined databases have been used to update pre-existing HLW composition models or to develop new models for properties such as Product Consistency Test (PCT) responses, spinel crystallization (one-percent crystal fraction temperature, T 1% ), melt viscosity, melt electrical conductivity, nepheline formation upon slow cooling (i.e., Canister Centerline Cooling [CCC]), and Toxicity Characteristic Leach Procedure (TCLP) Cd response. While spinel is typically the most commonly occurring phase in HLW glasses, other phases can be limiting depending on the waste and glass composition. For example, various phosphate phases can become important as the phosphorus content increases. Lithium phosphate crystallization can impact PCT releases of HLW glasses, while calcium phosphate phases forming in the cold-cap can deleteriously impact feed processing in the melter. At present, however, no models exist that relate glass composition and crystallization of phosphate phases in general and calcium phosphate in particular. The present work was therefore directed towards the initial development of such models. Future work may be directed at studying amorphous phase separation in high phosphate HLW glasses. Within the River Protection Project, feed compositions are projected using the Hanford Tank Waste Operations Simulator (HTWOS), a dynamic computer model that tracks the waste through storage, retrieval, feed staging, and treatment processes. A review of the HTWOS data shows that WTP will process 4106 batches of HLW glass for the overall mission (System Plan Rev. 6, ORP-11242), each with its own waste feed and glass composition. Some of the projected HTWOS feed batches are expected to have relatively high concentrations of phosphorous compared to typical HLW streams. In the 4106 batches of HLW for the overall WTP mission P 2 O 5 varies from 0.59 wt% to 13.00 wt%, with 95 batches containing at least 10 wt% P 2 O 5 . Occurrences of phosphate crystals have commonly been noted in glasses with high bismuth and phosphorus contents. In addition, recently collected data from a set of statistically designed HLW matrix glasses prepared and characterized to support enhancement of the HLW glass property-composition models identified apatite in a number of glass samples. However, the current HLW model for crystallization (one-percent crystal fraction temperature) is applicable only to spinel crystallization in glasses. Previous projections of waste loadings and glass volume (such as those in System Plan Rev. 6, ORP-11242) have used preliminary constraints for calcium phosphate crystallization that are based on the limited available data. Additional data and improved constraints or, preferably, models that relate glass composition to crystallization of phosphate-containing phases, are therefore needed to support HLW vitrification at the WTP. The present study focuses on the development of such a model based on data from previously characterized glasses and a set of newly fabricated glasses.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Dynamic observation of dual-beam irradiated Fe and Fe-10Cr alloys at 435 °C

The attractive mechanical properties and superior resistance to void-swelling make ferritic/martensitic alloys a promising structural material for advanced nuclear reactors. However, one anomaly that has intrigued researchers for more than 50 years is the proportion of two types of dislocation loops in Fe and Fe-Cr alloys with Burger vectors b=½<111> and b=<100>. Although the possible mechanisms responsible for the presence of <100> loops continue to be the subject of intense modeling studies, there remains incomplete experimental understanding of fundamental irradiation processes in Fe(Cr) alloys. Here, the dose dependence of the irradiation-induced microstructural evolution was examined from 0 to 20 displacement per atom (dpa) in high purity Fe and Fe-10Cr during simultaneous dual-beam (1 MeV Kr + 10 appm He/dpa) irradiation at 435 °C. We experimentally revealed that the mechanism for the formation of <100> loops may not follow the conventional simple dislocation reaction between two 1½<111> loops. Real-time dynamic formation and evolution of defects including black dot loops, loop coarsening, loop decoration, network dislocations, and cavities were demonstrated. Several results indicated that the addition of Cr and He could impede dislocation loop motion. The evolution of the defect size/density and relative fraction of ½<111> vs <100> loops were quantitatively summarized. With increasing dose, ½<111> loops became the dominant type of loop in both materials. Notably, <100> loops were predominantly observed near grain boundaries only for pure Fe, while arrays of nanoscale black dot defects composing the <100> loop strings were observed in plenty in Fe-10Cr.

36 MATERIALS SCIENCE↗

Dynamics of reactive high-power impulse magnetron sputtering discharge studied by time- and space-resolved optical emission spectroscopy and fast imaging

Time- and space-resolved optical emission spectroscopy and fast imaging were used for the investigation of the plasma dynamics of high-power impulse magnetron sputtering discharges. 200 {mu}s pulses with a 50 Hz repetition frequency were applied to a Cr target in Ar, N{sub 2}, and N{sub 2}/Ar mixtures and in a pressure range from 0.7 to 2.66 Pa. The power density peaked at 2.2-6 kW cm{sup -2}. Evidence of dominating self-sputtering was found for all investigated conditions. Up to four different discharge phases within each pulse were identified: (i) the ignition phase, (ii) the high-current metal-dominated phase, (iii) the transient phase, and (iv) the low-current gas-dominated phase. The emission of working gas excited by fast electrons penetrating the space in-between the electrodes during the ignition phase spread far outwards from the target at a speed of 24 km s{sup -1} in 1.3 Pa of Ar and at 7.5 km s{sup -1} in 1.3 Pa of N{sub 2}. The dense metal plasma created next to the target propagated in the reactor at a speed ranging from 0.7 to 3.5 km s{sup -1}, depending on the working gas composition and the pressure. In fact, it increased with higher N{sub 2} concentration and lower pressure. The form of the propagating plasma wave changed from a hemispherical shape in Ar, to a droplike shape extending far from the target in N{sub 2}. An important N{sub 2} emission rise in the latter case was detected during the transition at the end of the metal-dominated phase.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Phase relations and structural features in the system Ni-Zn-B

Phase relations for the system Ni-Zn-B have been established in the isothermal section at 800 Degree-Sign C based on X-ray powder diffraction and electron microprobe analyses of about 60 samples, which have been prepared by hot pressing of pre-annealed powder compacts of arc-melted master alloys Ni{sub x}B{sub y} and Zn-filings. Six ternary compounds (labeled {tau}{sub 1} to {tau}{sub 6}) were found to exist, which in some cases exhibit considerable mutual solid solubilities mostly as an exchange of Ni-Zn at constant B-content, but in the case of the so-called {tau}-phase {tau}{sub 1}-(Ni{sub 1-x}Zn{sub x}){sub 21}[Zn{sub 1-y-z}{open_square}{sub y}(B{sub 4}){sub z}]{sub 2}B{sub 6} (0.07{<=}x{<=}0.11, 0.07{<=}y{<=}0.53, 0{<=}z{<=}0.3) also with Zn/B substitution. Single crystal X-ray data analysis for the composition x=0.07, y=0.125, z=0.30, and a=1.05800(3) nm confirmed the Cr{sub 23}C{sub 6} type with space group Fm3{sup Macron }m, but revealed partial replacement of Zn-atoms by B{sub 4}-tetrahedra (R{sub F}=0.014). Whereas Ni/Zn exchange (at constant B-content) ranges at about 4-5 at% for {tau}{sub 4}-Ni{sub 3}ZnB{sub 2} and {tau}{sub 5}-Ni{sub 48}Zn{sub 32}B{sub 20}, it is below 3 at% for {tau}{sub 2}-Ni{sub 12}ZnB{sub 8-x} (x=0.43), {tau}{sub 3}-Ni{sub 21}Zn{sub 2}B{sub 20} and {tau}{sub 6}-Ni{sub 47}Zn{sub 23}B{sub 30}. The crystal structures of {tau}{sub 2}-Ni{sub 12}ZnB{sub 8-x} (x=0.43; Ni{sub 12}AlB{sub 8} type), {tau}{sub 3}-Ni{sub 21}Zn{sub 2}B{sub 20} (own type) and {tau}{sub 4}-Ni{sub 3}ZnB{sub 2} (own type) have been determined in our foregoing paper [8]. Due to the non-availability of suitable single crystals, the crystal structures of {tau}{sub 5}-Ni{sub 48}Zn{sub 32}B{sub 20} (body-centered orthorhombic; a=1.6(2) nm, b=0.63(7) nm, and c=0.27(0) nm, determined from TEM) and of {tau}{sub 6}-Ni{sub 47}Zn{sub 23}B{sub 30} have not been elucidated yet. Phase equilibria at 800 Degree-Sign C are dominated by a large three-phase field ({beta}B)+Ni{sub 2}Zn{sub 11}+{tau}{sub 3}, as practically all ternary compounds form at compositions with less than about 50 at% Ni. Furthermore, precise data on atom site distribution and positional parameters have been provided from X-ray single crystal refinements for Ni-borides, for which crystal structures hitherto have only been derived from X-ray diffraction photographs: o-Ni{sub 4}B{sub 3-x} (x=0.19; Pnma, a=1.9665(4) nm, b=0.29852(1) nm, c=0.65750(2) nm; R{sub F}=0.015) and m-Ni{sub 4}B{sub 3} (C2/c, a=0.64356(3) nm, b=0.48867(3) nm, c=0.78267(3) nm, {beta}=103.288(3) Degree-Sign , R{sub F}=0.021). - Graphical abstract: Ni-Zn-B isothermal section at 800 Degree-Sign C. Highlights: Black-Right-Pointing-Pointer Phase relations were determined for the system Ni-Zn-B at 800 Degree-Sign C. Black-Right-Pointing-Pointer Existence of six ternary compounds ({tau}{sub 1}-{tau}{sub 6}) has been confirmed at 800 Degree-Sign C. Black-Right-Pointing-Pointer Homogeneity range for {tau}{sub 1} with respect to Ni/Zn and Zn/B at 800 Degree-Sign C has been determined. Black-Right-Pointing-Pointer The crystal structures of {tau}{sub 5}-Ni{sub 48}Zn{sub 32}B{sub 20} from TEM (oI, a=1.6(2) nm, b=0.63(7) nm, and c=0.27(0) nm). Black-Right-Pointing-Pointer Precise data on {tau}{sub 1}-(Ni{sub 1-x}Zn{sub x}){sub 21}[Zn{sub 1-y-z{open_square}y}(B{sub 4}){sub z}]{sub 2}B{sub 6} (0.07{<=}x{<=}0.11, 0.07{<=}y{<=}0.53, 0{<=}z{<=}0.3), o-Ni{sub 4}B{sub 3-x} and m-Ni{sub 4}B{sub 3} have been presented.

36 MATERIALS SCIENCE↗

Low Temperature Surface Carburization of Stainless Steels

Low-temperature colossal supersaturation (LTCSS) is a novel surface hardening method for carburization of austenitic stainless steels (SS) without the precipitation of carbides. The formation of carbides is kinetically suppressed, enabling extremely high or colossal carbon supersaturation. As a result, surface carbon concentrations in excess of 12 at. % are routinely achieved. This treatment increases the surface hardness by a factor of four to five, improving resistance to wear, corrosion, and fatigue, with significant retained ductility. LTCSS is a diffusional surface hardening process that provides a uniform and conformal hardened gradient surface with no risk of delamination or peeling. The treatment retains the austenitic phase and is completely non-magnetic. In addition, because parts are treated at low temperature, they do not distort or change dimensions. During this treatment, carbon diffusion proceeds into the metal at temperatures that constrain substitutional diffusion or mobility between the metal alloy elements. Though immobilized and unable to assemble to form carbides, chromium and similar alloying elements nonetheless draw enormous amounts of carbon into their interstitial spaces. The carbon in the interstitial spaces of the alloy crystals makes the surface harder than ever achieved before by more conventional heat treating or diffusion process. The carbon solid solution manifests a Vickers hardness often exceeding 1000 HV (equivalent to 70 HRC). This project objective was to extend the LTCSS treatment to other austenitic alloys, and to quantify improvements in fatigue, corrosion, and wear resistance. Highlights from the research include the following: • Extension of the applicability of the LTCSS process to a broad range of austenitic and duplex grades of steels • Demonstration of LTCSS ability for a variety of different component shapes and sizes • Detailed microstructural characterization of LTCSS-treated samples of 316L and other alloys • Thermodynamic modeling to explain the high degree of carbon solubility possible in austenitic grades under the LTCSS process and experimental validation of model results • Corrosion testing to determine the corrosion resistance improvement possible from the LTCSS process • Erosion testing to determine the erosion resistance improvement possible from the LTCSS process • Wear testing to quantify the wear resistance improvement possible from the LTCSS process • Fatigue testing for quantifying the extent of improvement from the LTCSS process • Component treating and testing under simulated and in-line commercial operations XRD verified expanded austenite lattice, with no evidence of carbide precipitation. Carbon concentration profiles via Auger and electron dispersion spectroscopy (EDS) showed carbon levels in excess of 12 at. % in treated, type 316 SS. Scanning electron microscopy (SEM) of pulled-to-failure treated tensile specimens showed slip bands and no de-cohesion of the treated layer, verifying that the layer remains ductile. Compressive stresses in excess of 2 GPa (300 ksi) have been calculated at the surface of the case. Phase diagram (CALPHAD) (ThermoCalc) and Wagner dilute solution thermodynamic models were developed that calculate the solubility of carbon in austenite as a function of alloying content for the process time and temperature. Several commercial alloys have been modeled, and the model has been used to design experimental alloys with enhanced affinity for carbon solubility at treatment temperatures. Four experimental alloys were melted, rolled, and manufactured into test specimens, and the LTCSS treatment indicated successfully enhanced results and validated the predictions based on thermodynamic modeling. Electrochemical polarization curves show a 600 to 800 mV increase in pitting potential in treated (900-1000 mV) versus non-treated (200-300 mV) type 316 in chloride solutions. Treated 316L showed crevice-corrosion behavior similar to that of Ti-6Al-4V and Hastelloy C22. Cavitation tests showed significant increases in cavitation resistance for treated materials as compared to the non-treated materials. Standard ASTM pin-on-disk sliding friction and reciprocating friction wear tests also indicate significant enhancement in wear properties. Fatigue testing showed an order of magnitude improvement for treated versus non-treated Type 316 at the same maximum stress level (R = -1). The maximum stress at 107 cycles and the endurance stress for infinite life, improved by approximately 50%, from 30 to 45 ksi. The energy savings from this project is estimated at 21.8 trillion Btu/year by 2020. This energy savings will be associated with a CO2 reduction of 1.3 million ton/year. One application of this technology in a sludge pump of a cardboard recycling plant during the course of this project has resulted in an energy savings of 84. 106 Btu and cost savings of $900.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Hydrogenation induced structure and property changes in GdGa

Hydrides GdGaH{sub x} were obtained by exposing the Zintl phase GdGa with the CrB structure to a hydrogen atmosphere at pressures from 1.5 to 50 bar and temperatures from 50 to 500 °C. Structural analysis by powder X-ray diffraction suggests that conditions with hydrogen pressures in a range between 15 and 50 bar and temperatures below 500 °C afford a uniform hydride phase with the NdGaH{sub 1.66} structure (Cmcm, a=3.9867(7) Å, b=12.024(2) Å, c=4.1009(6) Å) which hosts H in two distinct positions, H1 and H2. H1 is coordinated in a tetrahedral fashion by Gd atoms, whereas H2 atoms are inserted between Ga atoms. The assignment of the NdGaH{sub 1.66} structure is corroborated by first principles DFT calculations. Modeling of phase and structure stability as a function of composition resulted in excellent agreement with experimental lattice parameters when x=1.66 and revealed the presence of five-atom moieties Ga-H2-Ga-H2-Ga in GdGaH{sub 1.66}. From in situ powder X-ray diffraction using synchrotron radiation it was established that hydrogenation at temperatures above 200 °C affords a hydride with x≈1.3, which is stable up to 500 °C, and that additional H absorption, yielding GdGaH{sub 1.66}, takes place at lower temperatures. Consequently, GdGaH{sub 1.66} desorbs H above T=200 °C. Without the presence of hydrogen, hydrides GdGaH{sub x} decompose at temperatures above 300 °C into GdH{sub 2} and an unidentified Gd-Ga intermetallics. Thus the hydrogenation of GdGa is not reversible. From magnetic measurements the Curie-Weiss constant and effective magnetic moment of GdGaH{sub 1.66} were obtained. The former indicates antiferromagnetic interactions, the latter attains a value of ~8 μ{sub B} which is typical for compounds containing Gd{sup 3+}ions. - Graphical abstract: Ferromagnetic GdGa absorbs hydrogen in two steps to yield antiferromagnetic GdGaH{sub 1.66}. Display Omitted - Highlights: • Elucidation of hydrogen uptake behavior of the rare earth gallide GdGa by in situ diffraction. • H-incorporation in GdGa leads to the formation of chain-like polyanions Ga-H-Ga-H-Ga. • H-incorporation in GdGa changes magnetism from ferromagnetic to antiferromagnetic.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Easy Controlled Properties of Quaternary FeNiCrCd Thin Films Deposited from a Single dc Magnetron Sputtering Under the Influence of Deposition Rate

The quaternary FeNiCrCd thin films were produced from a single FeNiCrCr source on a commercial flexible polymer substrate using one dc magnetron sputtering technique. For that, a series of the films with a thickness of 50 nm were produced at different deposition rates of 0.02, 0.04, 0.06, and 0.08 nm/s, separately. In this study, as far as concerned, this was the first time that structural and magnetic properties of FeNiCrCd thin films were investigated. According to compositional analysis, the Fe and Cr contents slightly decreased with increasing deposition rate while Ni was almost constant, whereas those of the amount of Cd atoms increased. However, the atomic amounts of Fe and Cd in the films are quite different from those of the source material. The change of the atomic contents in the films from the source may be attributed to the relatively different bond energy/melting point of metals which have different contents sputtered from source material since this physical parameter is very significant for the sputtering process. For crystal structural analysis, a combination of hexagonal close-packed (hcp) and body-centered cubic (bcc) were observed. The peak intensity of the bcc-dominated planes decreased while the hcp-dominant plane increased since the change in peak intensities is compatible with the compositional analysis with increasing deposition rate. And, the grain sizes decreased gradually from 40.1 to 23.4 nm, with increasing deposition rate from 0.02, to 0.08 nm/s. Also, the film surfaces transformed from a rough to smooth surfaces with decreasing grain sizes as deposition rate increased. For magnetic analysis, the saturation magnetization M{sub s} values decreased as 1030, 773, 730, and 217 emu/cm{sup 3} with increasing deposition rate as 0.02, 0.04, 0.06, and 0.08 nm/s, respectively. In the same manner, the coercivity H{sub c} values were found as 11, 7, 6, and 2 Oe with the deposition rate of 0.02, 0.04, 0.06, and 0.08 nm/s, respectively. The decrease of the H{sub c} may have primarily come from the transformation of rough to smooth surface of the films. It may also be said that the films showed soft magnetic properties due to their low H{sub c} values with increasing deposition rate. Thus, the magnetic properties of the quaternary FeNiCrCd alloy films were seen to be easily improved with the deposition rate parameter for potential use in different industrial applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Comparison of the sputter rates of oxide films relative to the sputter rate of SiO{sub 2}

There is a growing interest in knowing the sputter rates for a wide variety of oxides because of their increasing technological importance in many different applications. To support the needs of users of the Environmental Molecular Sciences Laboratory, a national scientific user facility, as well as our research programs, the authors made a series of measurements of the sputter rates from oxide films that have been grown by oxygen plasma-assisted molecular beam epitaxy, pulsed laser deposition, atomic layer deposition, electrochemical oxidation, or sputter deposition. The sputter rates for these oxide films were determined in comparison with those from thermally grown SiO{sub 2}, a common reference material for sputter rate determination. The film thicknesses and densities for most of these oxide films were measured using x-ray reflectivity. These oxide films were mounted in an x-ray photoelectron or Auger electron spectrometer for sputter rate measurements using argon ion sputtering. Although the primary objective of this work was to determine relative sputter rates at a fixed angle, the measurements also examined (i) the angle dependence of the relative sputter rates, (ii) the energy dependence of the relative sputter rates, and (iii) the extent of ion beam induced reduction for some oxides. Oxide films examined include SiO{sub 2}, Al{sub 2}O{sub 3}, CeO{sub 2}, Cr{sub 2}O{sub 3}, Fe{sub 2}O{sub 3}, HfO{sub 2}, In-Sn oxide, Ta{sub 2}O{sub 5}, TiO{sub 2} (anatase, rutile, and amorphous), and ZnO. The authors found that the sputter rates for the oxides can vary up to a factor of 2 (usually lower) from that observed for SiO{sub 2}. The ratios of sputter rates relative to those of SiO{sub 2} appear to be relatively independent of ion beam energy in the range of 1-4 kV and for incident angles <50 deg. As expected, the extent of ion beam induced reduction of the oxides varies with the sputter angle.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

TASK 2.5.5 NATURAL EXPOSURE TESTING IN CALIFORNIA

Airborne particulate matter that settles on a roof can either reflect or absorb incoming solar radiation, dependent on the chemical content and size of the particles. These light scattering and absorption processes occur within a few microns of the surface, and can affect the solar reflectance of the roof. Wilkes et al. (2000) tested 24 different roof coatings on a low-slope test stand and observed about a 25% decrease in the solar reflectance of white-coated and aluminum-coated surfaces as the time of exposure increased; however, the decrease leveled off after 2 years. SPRI Inc. and its affiliates studied the effect of climatic exposure on the surface properties of white thermoplastic single-ply membranes and determined that membranes lose from 30 to 50% of their reflectance over 3 years (Miller et al. 2002). The CMRC and its affiliates AISI, NamZAC, MBMA, MCA and NCCA exposed unpainted and painted metal roofing on both steep- and low-slope test roofs and found that after 3 years, the painted polyvinylidene fluoride (PVDF) metal roofs lost less than 5% of their original reflectance (Miller et al. 2004). The results of the three different weathering studies are very interesting in terms of their solar reflectance after 3 years of exposure. The white thermoplastic membrane and white ceramic coating with white topcoat had original reflectance measures that were about 20 percentage points higher than the painted metal; however, after 3-years of field exposure the solar reflectance of the painted metal exceeds that of the thermoplastic membrane and equals that of the coating. The long-term loss of reflectance appears driven by the ability of the particulate matter to cling to the roof and resist being washed off by wind and or rain. Miller et al. (2002) discovered that aerosol deposition introduced biomass of complex microbial consortia onto the test roofs and the combination of contaminants and biomass accelerated the loss of solar reflectance for the thermoplastic membranes and the roof coatings. Airborne contaminants and biomass were also detected on the painted metal roofs; however, the loss of solar reflectance was less than 5% for the painted metal roofs. The chemistry of the PVDF paint resin system uses similar organic film bonding to that responsible for Teflon , making it extremely chemical resistant and dirt shedding. Miller and Rudolph (2003) found the PVDF painted metals maintained solar reflectance even after 30 years of climatic exposure. Therefore the reduction of roof reflectance is closely related to the composition of the roof and to the chemical profile of the contaminants soiling the roof. Contaminants collected from samples of roof products exposed at seven California weathering sites were analyzed for elements and carbons to characterize the chemical profile of the particles soiling each roof sample and to identify those elements that degrade or enhance solar reflectance. The losses in solar reflectance varied from site to site and also varied at a give site based on the color of the coupon. The least drop in reflectance was observed in the alpine climate of McArthur while the largest drop occurred in sites near urban development. Light color samples were soiled after just one year of exposure. The darker color coupons did not show the same seasonal variations in solar reflectance as observed for the lighter colors. However, after an additional year of exposure the samples at all sites regained most of their solar reflectance due to rain and/or wind washing. The loss of reflectance appears cyclical with the onset of seasons having more rainfall. Solar reflectance of the cool pigmented coupons always exceeded that of the conventional pigmented coupons. Climatic soiling did not cause the cool pigmented roof coupons to lose any more solar reflectance than their conventional pigmented counterparts. The effect of roof slope appears to have more of an effect on lighter color roofs whose solar reflectance exceeds at least 0.5 and visually shows the accumulation of airborne contaminants. The thermal emittance remained invariant with time and location and was therefore not affected by climatic soiling. A thin-film deposition model was developed based on first principles, which simulates light interaction with a soiled substrate. This model was used in combination with the measured data to determine the solar absorptance and reflectance of particulate matter at each of the sites calculated using least squares fitting routines. Principal Component Analysis was used to determine the most important combinations of chemicals correlated with changes in solar absorption. Linear regression helped extract an approximate correlation using chromium, iron and elemental carbon concentrations. It appears that chromium ranks first, iron ranks second, and elemental carbon ranks third in importance to soil absorptance in the data

09 BIOMASS FUELS↗

Characterizations of Binary FeCr (AISI 430) Thin Films Deposited from a Single Magnetron Sputtering Under Easy Controllable Deposition Parameters

A series of 50-nm binary FeCr martensitic thin films were sputtered from a single source made of commercial AISI 430 ferritic stainless steel under the deposition rates gradually increased from 0.03 to 0.11 nm/s with 0.02 nm/s steps at stationary condition. And, under 0.09 nm/s deposition rate, a second series of the films were also deposited under the rotation speed of their substrates which was chosen at 0, 25, and 45 rpm. As far as we are concerned, this study is the first investigation of properties of the thin films produced from AISI 430. The atomic Fe content in the films increased from 79.3 to 98.6% while atomic Cr content decreased from 20.5 to 1.2% with the increase of deposition rate from 0.03 to 0.11 nm/s. According to compositional analysis, the Fe content increased while Cr content decreased with increasing deposition rate. The reason for this may be attributed to the relatively different bond energy/melting point of metals which have different contents sputtered from source material since this physical parameter is very significant for the sputtering process. And, the Fe content in the films decreased from 84.9 to 79.2 at. % while the Cr content increased from 14.9 to 20.6 at. % when the increase of rotation speed of substrate. The crystal structure of all films was observed to have a body-centered tetragonal phase and the intensity of (110) peak varied with the atomic Fe content. The surface observations of films performed by a scanning electron microscope exposed that the number of surface grains increased with the increase of deposition rate and decreased with the increase of rotation speed. According to surface roughness analysis done by an atomic force microscope, the roughness of the film surfaces increased as the deposition rate increased. And, the roughness of the film surfaces decreased as the rotation speed increased. This has been consistent with the grain size and roughness parameters. Thus, increasing deposition rate and decreasing rotation speed of the substrate caused an increase in grain size and roughness parameters. The magnetic measurements of the films achieved, by a vibrating sample magnetometer at room temperature, displayed that the saturation magnetization, M{sub s}, values increased from 820.1 to 1700.4 emu/cm{sup 3}, the remanence magnetization, M{sub r}, values increased from 293 to 817 emu/cm{sup 3}, and the coercivity, H{sub c}, value also increased from 38 to 107 Oe with the increasing of deposition rate. It is also seen that the magnetic easy axis are in the film plane due to the shape anisotropy. With the increase rotation speed, the values of M{sub s} and M{sub r} increased and the H{sub c} decreased. It was seen that variation of Fe content in the films influences the M{sub s} values and the H{sub c} values are consistent with the surface properties. It was concluded that the deposition rate and the rotation speed of the substrate play a considerable role on the structural and related magnetic properties of the sputtered FeCr thin films, and the properties of the films can be easily controlled by changing production parameters.

36 MATERIALS SCIENCE↗