X-ray absorption spectroscopic study of the alumina supported Fe and FeMo catalysts for methane dehydrogenation
Nanoscale Fe (5%Fe/Al 2 O 3 ) and FeMo (4.5%Fe-0.5%Mo/Al 2 O 3 ) catalysts are prepared by precipitating metal components onto alumina and then reducing in hydrogen at 700 °C for 2 hrs. Here, the catalysts are characterized before and after their exposures to methane at 700 °C, employing ex-situ X-ray absorption spectroscopy (XAS) and X-ray diffraction techniques. XAS data of the as-prepared catalysts shows that, iron precipitates onto alumina as 6L-ferrihydrite, and Mo is present as molybdate (Mo(VI)O 4 2- ). The molybdate, which binds the alumina in the as-prepared FeMo catalyst, is partially reduced to MoO 2 . The reduction of iron to metallic state is incomplete because the ferrous iron binds the alumina, forming hercynite. After several hrs of methane exposure to both the catalysts at 700 °C, a major Fe 3 C and a graphite phase are observed only in the FeMo catalyst. The observation confirms that the Mo promotes more iron to an active Fe metal, a part of that metal converts to Fe 3 C and austenite (Fe x C). Concurrently, the MoO 2 converts to Mo-oxycarbide (MoO x C y ), the latter then carburize to Mo 2 C in the FeMo catalyst. The Fe metal, Mo-oxycarbide and metal carbides are mainly responsible for the conversion of methane to H 2 and carbon. At reaction temperature > 900 °C, the Mo carbide particles agglomerate, and the excess carbon deposits on this agglomerate leading to catalyst deactivation. The deactivated catalyst is regenerated with CO 2 treatment at 1000 °C to restore its initial oxide structure.