Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “radiation defect”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Damage induced by electronic excitation in ion-irradiated yttria-stabilized zirconia

This article presents a study of the damage production in yttria-stabilized cubic zirconia single crystals irradiated with swift heavy ions. The combination of techniques which probe the material at different spatial scales (Rutherford backscattering spectrometry in channeling geometry, x-ray diffraction, transmission electron microscopy, and atomic force microscopy) was used in order to gain information about the damage depth distribution, the disordering buildup, the nature of radiation defects, and the occurrence of microstructural modifications. The damage results from the formation of tracks, due to the huge electronic excitations induced in the wake of incident ions. The melting of the material in the core of tracks, via a thermal spike mechanism, leads to the creation of large hillocks at the surface of the crystals. The overlapping of ion tracks at high fluence (above {approx}10{sup 12} cm{sup -2}) induces a severe transformation of the microstructure of the material. Nanodomains slightly disoriented from the main crystallographic direction are formed, with a size decreasing with increasing irradiation fluence. These results may be used to predict the damage evolution in other nonamorphizable ceramics irradiated with swift heavy ions.

36 MATERIALS SCIENCE↗

Carriers mobility of InAs- and InP- rich InAs-InP solid solutions irradiated by fast neutrons

We have studied the low temperature charge carriers mobility in bulk single crystals of InAs- and InP- rich InAs-InP solid solutions irradiated with maximum integral flux 2⋅10{sup 18} n/cm{sup 2} of fast neutrons. Influence of minor component small addition in InAs-InP solid solutions has been revealed. There are also presented data of radiation defects thermal stability.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Hydrogen plasma induced modification of photoluminescence from a-SiN{sub x}:H thin films

Low temperature (250–350 °C) hydrogen plasma annealing (HPA) treatments have been performed on amorphous hydrogenated silicon nitride (a-SiN{sub x}:H) thin films having a range of compositions and subsequent modification of photoluminescence (PL) is investigated. The PL spectral shape and peak positions for the as deposited films could be tuned with composition and excitation energies. HPA induced modification of PL of these films is found to depend on the N/Si ratio (x). Upon HPA, the PL spectra show an emergence of a red emission band for x ≤ 1, whereas an overall increase of intensity without change in the spectral shape is observed for x > 1. The emission observed in the Si rich films is attributed to nanoscale a-Si:H inclusions. The enhancement is maximum for off-stoichiometric films (x ∼ 1) and decreases as the compositions of a-Si (x = 0) and a-Si{sub 3}N{sub 4} (x = 1.33) are approached, implying high density of non-radiative defects around x = 1. The diffusion of hydrogen in these films is also analyzed by Elastic Recoil Detection Analysis technique.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Cascade phonon-assisted trapping of positrons by divacancies in n-FZ-Si(P) single crystals irradiated with 15 MeV protons

The trapping of positrons by the radiation defects in moderately doped oxygen-lean n-FZ-Si(P) single crystal irradiated with 15 MeV protons has been investigated in a comparative way using the positron lifetime spectroscopy and Hall effect measurements. The experiments were carried out within a wide temperature interval ranging from 25 K – 29 K to 300 K. The positron trapping rate for divacancies was reconstructed in the course of many-stage isochronal annealing. The concentration and the charged states of divacancies (V{sub 2}{sup −} and V{sub 2}{sup −−}) were estimated. The temperature dependency of the trapping cross section of positrons by the negatively charged divacancies is in a good agreement with the data of calculations based on the assumptions of the cascade phonon-assisted mechanism of exchange of the energy between the positron and acoustic long-wave phonons. Obeying ∼ T{sup −3} law, the cross-section of the trapping of positrons by divacancies changes considerably ranging from ∼1.7×10{sup −12} cm{sup 2} (66 – 100 K) to ∼2×10{sup −14} cm{sup 2} (≈ 250 K). The characteristic length of trapping of the positron by V{sub 2}{sup −−} divacancy was estimated to be l{sub 0}(V{sub 2}{sup −−})≈(3.4±0.2)×10{sup −8} cm.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural evolution and photoluminescence of annealed Si-rich nitride with Si quantum dots prepared by plasma enhanced chemical vapor deposition

Silicon-rich nitride films were deposited by plasma enhanced chemical vapor deposition. Silicon quantum dots (Si QDs) were formed by post-thermal annealing processing verified using the High-Resolution Transmission Electron Microscope. The 1100 °C thermal annealing leads to the nucleation of silicon atoms, the growth of Si QDs, and the rearrangement of Si 2p and N 1s elements. The structural evolution of silicon-rich nitride thin film with post annealing promotes the formation of Si QDs and Si{sub 3}N{sub 4} matrix. We also investigated the effect of the NH{sub 3}-to-SiH{sub 4} ratio R on the photoluminescence (PL) of SiN{sub x} with Si QDs. We found that the broad blue luminescence originates from both quantum confined effect and radiative defects. The intensity of the PL was changed by adjusting the NH{sub 3} flow rate. The increase of R could limit the transformation of Si QDs from amorphous to crystalline status, meanwhile lead to the alteration of distribution of defect states. These can help to understand the annealing-dependent characteristics, the PL mechanisms of silicon-rich nitride and to optimize the fabrication process of Si QDs embedded in nitride.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Absence of quantum confinement effects in the photoluminescence of Si{sub 3}N{sub 4}–embedded Si nanocrystals

Superlattices of Si-rich silicon nitride and Si{sub 3}N{sub 4} are prepared by plasma-enhanced chemical vapor deposition and, subsequently, annealed at 1150 °C to form size-controlled Si nanocrystals (Si NCs) embedded in amorphous Si{sub 3}N{sub 4}. Despite well defined structural properties, photoluminescence spectroscopy (PL) reveals inconsistencies with the typically applied model of quantum confined excitons in nitride-embedded Si NCs. Time-resolved PL measurements demonstrate 10{sup 5} times faster time-constants than typical for the indirect band structure of Si NCs. Furthermore, a pure Si{sub 3}N{sub 4} reference sample exhibits a similar PL peak as the Si NC samples. The origin of this luminescence is discussed in detail on the basis of radiative defects and Si{sub 3}N{sub 4} band tail states in combination with optical absorption measurements. The apparent absence of PL from the Si NCs is explained conclusively using electron spin resonance data from the Si/Si{sub 3}N{sub 4} interface defect literature. In addition, the role of Si{sub 3}N{sub 4} valence band tail states as potential hole traps is discussed. Most strikingly, the PL peak blueshift with decreasing NC size, which is often observed in literature and typically attributed to quantum confinement (QC), is identified as optical artifact by transfer matrix method simulations of the PL spectra. Finally, criteria for a critical examination of a potential QC-related origin of the PL from Si{sub 3}N{sub 4}-embedded Si NCs are suggested.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Spectra of surface plasmon polariton enhanced electroluminescence from electroformed Al-Al{sub 2}O{sub 3}-Ag diodes

Narrow band-pass filters have been used to measure the spectral distribution of electroluminescent photons with energies between 1.8 eV and 3.0 eV from electroformed Al-Al{sub 2}O{sub 3}-Ag diodes with anodic Al{sub 2}O{sub 3} thicknesses between 12 nm and 18 nm. Electroforming of metal-insulator-metal (MIM) diodes is a non-destructive dielectric breakdown that results in a conducting channel in the insulator and changes the initial high resistance of the MIM diode to a low resistance state. It is a critical step in the development of resistive-switching memories that utilize MIM diodes as the active element. Electroforming of Al-Al{sub 2}O{sub 3}-Ag diodes in vacuum results in voltage-controlled negative resistance (VCNR) in the current-voltage (I-V) characteristics. Electroluminescence (EL) and electron emission into vacuum (EM) develop simultaneously with the current increase that results in VCNR in the I-V characteristics. EL is due to recombination of electrons injected at the Al-Al{sub 2}O{sub 3} interface with radiative defect centers in Al{sub 2}O{sub 3}. Measurements of EL photons between 1.8 eV and 3.0 eV using a wide band-pass filter showed that EL intensity is exponentially dependent on Al{sub 2}O{sub 3} thickness for Al-Al{sub 2}O{sub 3}-Ag diodes between 12 nm and 20 nm thick. Enhanced El intensity in the thinnest diodes is attributed to an increase in the spontaneous emission rate of recombination centers due to high electromagnetic fields generated in Al{sub 2}O{sub 3} when EL photons interact with electrons in Ag or Al to form surface plasmon polaritons at the Al{sub 2}O{sub 3}-Ag or Al{sub 2}O{sub 3}-Al interface. El intensity is a maximum at 2.0–2.2 eV for Al-Al{sub 2}O{sub 3}-Ag diodes with Al{sub 2}O{sub 3} thicknesses between 12 nm and 18 nm. EL in diodes with 12 nm or 14 nm of Al{sub 2}O{sub 3} is enhanced by factors of 8–10 over EL from a diode with 18 nm of Al{sub 2}O{sub 3}. The extent of EL enhancement in the thinnest diodes can vary significantly between samples. A narrow band of recombination centers was found in one Al-Al{sub 2}O{sub 3}-Ag diode with 12 nm of Al{sub 2}O{sub 3}; it had EL intensity 100 times greater at 2.15 eV than the diode with 18 nm of Al{sub 2}O{sub 3}. EL intensity for photons with energies greater than 2.6 eV is nearly the same for all diodes.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Carrier quenching in InGaP/GaAs double heterostructures

Photoluminescence measurements on a series of GaAs double heterostructures demonstrate a rapid quenching of carriers in the GaAs layer at irradiance levels below 0.1 W/cm{sup 2} in samples with a GaAs-on-InGaP interface. These results indicate the existence of non-radiative defect centers at or near the GaAs-on-InGaP interface, consistent with previous reports showing the intermixing of In and P when free As impinges on the InGaP surface during growth. At low irradiance, these defect centers can lead to sub-ns carrier lifetimes. The defect centers involved in the rapid carrier quenching can be saturated at higher irradiance levels and allow carrier lifetimes to reach hundreds of nanoseconds. To our knowledge, this is the first report of a nearly three orders of magnitude decrease in carrier lifetime at low irradiance in a simple double heterostructure. Carrier quenching occurs at irradiance levels near the integrated Air Mass Zero (AM0) and Air Mass 1.5 (AM1.5) solar irradiance. Additionally, a lower energy photoluminescence band is observed both at room and cryogenic temperatures. The temperature and time dependence of the lower energy luminescence is consistent with the presence of an unintentional InGaAs or InGaAsP quantum well that forms due to compositional mixing at the GaAs-on-InGaP interface. Our results are of general interest to the photovoltaic community as InGaP is commonly used as a window layer in GaAs based solar cells.

14 SOLAR ENERGY↗

Enhanced quantum yield of photoluminescent porous silicon prepared by supercritical drying

The effect of supercritical drying (SCD) on the preparation of porous silicon (pSi) powders has been investigated in terms of photoluminescence (PL) efficiency. Since the pSi contains closely spaced and possibly interconnected Si nanocrystals (<5 nm), pore collapse and morphological changes within the nanocrystalline structure after common drying processes can affect PL efficiency. We report the highly beneficial effects of using SCD for preparation of photoluminescent pSi powders. Significantly higher surface areas and pore volumes have been realized by utilizing SCD (with CO{sub 2} solvent) instead of air-drying. Correspondingly, the pSi powders better retain the porous structure and the nano-sized silicon grains, thus minimizing the formation of non-radiative defects during liquid evaporation (air drying). The SCD process also minimizes capillary-stress induced contact of neighboring nanocrystals, resulting in lower exciton migration levels within the network. A significant enhancement of the PL quantum yield (>32% at room temperature) has been achieved, prompting the need for further detailed studies to establish the dominant causes of such an improvement.

36 MATERIALS SCIENCE↗

High-Resolution Thermal Profiling of a High-Power Diode Laser Facet During Aging

Here, we study the facet temperature distribution of a high-power diode laser over its lifetime using a noncontact, high spatial resolution CCD-based thermoreflectance technique. Based on the known correlation between non-radiative defects and heating, thermal maps can provide valuable information regarding the formation and evolution of small point defects that are at or near the facet during aging. In the laser under study in this work we measure the appearance of local hot spots on the facet, including concentrated hot spots that appear just before or just after COD and are correlated with loss of local light emission. The locations of these hot spots do not exhibit morphology changes in high-resolution SEM imaging of the facet, indicating that the related defects are too small to be observable in SEM or are located at some depth under the facet. Prior to COD, we measure a gradual facet temperature increase accompanied by a gradual optical power decrease and gradual facet optical absorption increase, indicating gradual degradation of the laser.

47 OTHER INSTRUMENTATION↗

Analysis of GaInP Solar Cells Grown by Hydride Vapor Phase Epitaxy

We analyzed the performance of a simple n-on-p GaInP solar cell grown without surface passivation but with a back reflector by dynamic hydride vapor phase epitaxy (DHYPE). We employed a thin emitter because the lack of surface passivation limited collection in that layer. We obtained a maximum internal quantum efficiency of nearly 95% by using 1 x 10^16 cm^-3 base doping. This device exhibited an open circuit voltage (VOC) of 1.27 V, short circuit current (JSC) of 12.6 mA/cm^2 , a fill factor (FF) of 79.3%, and 12.8% efficiency. Limits on cell performance predominantly come from VOC and FF. A Suns-VOC analysis of this cell indicates that 5.5% (absolute) of the FF is lost to series resistance, which stems from a high contact resistance. Another 5.5% of FF loss results from elevated dark current, leading to non-ideal diode behavior. This behavior implies that improvement in bulk material quality through reduction in concentrations of non-radiative defects will improve cell performance.

14 SOLAR ENERGY↗

Effect of electron and proton irradiation on characteristics of SiC surface-barrier detectors of nuclear radiation

Structures with a Schottky barrier based on CVD-grown 4H-SiC films were irradiated with 8 MeV protons and 900 keV electrons. The maximum fluences were 10{sup 14} and 3 Multiplication-Sign 10{sup 16} cm{sup -2}, respectively. It was found that, in the case of electrons, the primarily introduced radiation defects are closely spaced Frenkel pairs. Changes in the electrical characteristics of the structures were compared. Capacitance methods and nuclear spectrometry were employed. The latter technique was used to determine the charge collection efficiency under pulsed ionization with {alpha}-particles. It was determined that, under proton irradiation, the charge collection efficiency steadily decreases as the fluence increases. For electrons, the efficiency remains unchanged in the fluence range (1-3) Multiplication-Sign 10{sup 16} cm{sup -2}. However, a fluence of 3 Multiplication-Sign 10{sup 16} cm{sup -2} leads to a pronounced increase in the non-uniformity of charge transport conditions throughout the sample volume.

36 MATERIALS SCIENCE↗

The effect of neutron irradiation and annealing temperature on the electrical properties and lattice constant of epitaxial gallium nitride layers

Effect of irradiation with high reactor-neutron fluences ({Phi} = 1.5 Multiplication-Sign 10{sup 17}-8 Multiplication-Sign 10{sup 19} cm{sup -2}) and subsequent heat treatments in the temperature range 100-1000 Degree-Sign C on the electrical properties and lattice constant of epitaxial GaN layers grown on an Al{sub 2}O{sub 3} substrate is considered. It is shown that, with the neutron fluence increasing to (1-2) Multiplication-Sign 10{sup 18} cm{sup -2}, the resistivity of the material grows to values of about 10{sup 10} {Omega} cm because of the formation of radiation defects, and, with the fluence raised further, the resistivity passes through a maximum and then decreases to 2 Multiplication-Sign 10{sup 6} {Omega} cm at 300 K, which is accounted for by the appearance of a hopping conductivity via deep defects in the overlapping outer parts of disordered regions. With the neutron fluence raised to 8 Multiplication-Sign 10{sup 19} cm{sup -2}, the lattice constant c increases by 0.38% at a nearly unchanged parameter a. Heat treatment of irradiated samples at temperatures as high as 1000 Degree-Sign C does not fully restore the lattice constant and the electrical parameters of the material.

36 MATERIALS SCIENCE↗

Electronic properties and deep traps in electron-irradiated n-GaN

The study is concerned with the effect of electron irradiation (with the energies E = 7 and 10 MeV and doses D = 10{sup 16}-10{sup 18} cm{sup -2}) and subsequent heat treatments in the temperature range 100-1000 Degree-Sign C on the electrical properties and the spectrum of deep traps of undoped (concentration of electrons n = 1 Multiplication-Sign 10{sup 14}-1 Multiplication-Sign 10{sup 16} cm{sup -3}), moderately Si-doped (n = (1.2-2) Multiplication-Sign 10{sup 17} cm{sup -3}), and heavily Si-doped (n = (2-3.5) Multiplication-Sign 10{sup 18} cm{sup -3}) epitaxial n-GaN layers grown on Al{sub 2}O{sub 3} substrates by metal-organic chemical vapor deposition. It is found that, on electron irradiation, the resistivity of n-GaN increases, this is due to a shift of the Fermi level to the limiting position close to E{sub c} -0.91 eV. The spectrum of deep traps is studied for the initial and electron-irradiated n-GaN. It is shown that the initial properties of the irradiated material are restored in the temperature range 100-1000 Degree-Sign C, with the main stage of the annealing of radiation defects at about 400 Degree-Sign C.

36 MATERIALS SCIENCE↗

Effect of H{sup +} implantation on the optical properties of semi-insulating GaAs crystals in the IR spectral region

The optical properties of semi-insulating GaAs crystals subjected to multienergy hydrogen-ion implantation and treatment in a high-frequency electromagnetic field are studied in the infrared spectral region. It is established that such combined treatment provides a means for substantially increasing the transmittance of GaAs crystals to values characteristic of crystals of high optical quality. On the basis of analysis of the infrared transmittance and reflectance data, Raman spectroscopy data, and atomic-force microscopy data on the surface morphology of the crystals, a physical model is proposed to interpret the effects experimentally observed in the crystals. The model takes into account the interaction of radiation defects with the initial structural defects in the crystals as well as the effect of compensation of defect centers by hydrogen during high-frequency treatment.

36 MATERIALS SCIENCE↗

Effect of Annealing on Structural, Textural, Thermal, Magnetic, and Luminescence Properties of Calcium Fluoride Nanoparticles

Mesoporous nanocrystalline CaF{sub 2} powder was produced by pulsed electron beam evaporation (PEBE) in vacuum. The specific surface area (SSA) of CaF{sub 2} nanopowder (NP) reached 88.7 m{sup 2}/g. The effect of in-air thermal annealing in the temperature range of 200–900°C on the particle size, morphology, textural, thermal, magnetic, and luminescence properties of NPs is studied. A strong deviation from stoichiometry is observed in produced nanoparticles and a significant increase in the SSA after annealing at 200°C. The obtained CaF{sub 2} NP shows ferromagnetic (FM) behavior. The FM response appearance can be explained by the formation of structural and radiation defects. An analysis of pulsed cathodoluminescence (PCL) and magnetization curves of CaF{sub 2} NPs allows conclusions about their interrelation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Degradation and recovery mechanisms in lithium-doped solar cells

Several groups of lithium-doped solar cells have been evaluated under 1-MeV electron irradiation. Many of these groups indicated superior electrical output after irradiation and recovery as compared to similarly irradiated n/p solar cells. The superior cells are those with lithium concentrations of 2 to 5 x 10 to the 14th power atoms per cu cm at the junction. An irradiation of lithium-doped cells with 28-MeV electrons indicated a tenfold advantage of lithium-doped cells over n/p cells. Studies of the changes in the lithium concentration during recovery have shown the amounts of lithium reacting is highly nonlinear in regard to the electron fluence and varies greatly with distance from the junction. The results indicate that precipitation of lithium on radiation defects may be the cause of recovery rather than ion pairing.

Downing, R. G.↗