Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “property”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Magnetic properties of KNaMSi{sub 4}O{sub 10} compounds (M=Mn,Fe,Cu)

In the present work the synthesis and magnetic properties of three compounds with formula KNaMSi{sub 4}O{sub 10}(M=Mn,Fe,Cu) are described. These compounds are synthetic analogs to natural occurring minerals: fenaksite-Fe{sup 2+}, litidionite-Cu{sup 2+} and manaksite-Mn{sup 2+}. The crystal structure consists of complex silicate chains interconnected by edge-sharing MO{sub 5} square pyramids dimerized in M{sub 2}O{sub 8} units. This charged metal-silicate framework is compensated by monovalent alkali metals (K{sup +}, Na{sup +}). Despite the isostructural nature of these compounds, and the consequent similarity of the M-O topology, that rules the magnetic properties, these are quite different. While there are antiferromagnetic (AF) interactions within the Mn and Cu dimers (exchange interaction J=-3.83(1) and -2.86(3)K, respectively) with no long range order, a ferromagnetic interaction within Fe dimers (J=+7.6(1)K) is observed with a three-dimensional transition at 9 K to an AF ground state. The magnetic behavior is analyzed using the HDVV (Heisenberg-Dirac-Van Vleck) formalism and discussed in the light of the crystal structure. - Magnetic susceptibility times temperature. The antiferromagnetic arrangement within Mn and Cu dimers is evident (due to the positive derivative at lower temperatures). For the Fe-counterpart a three-dimensional transition to an antiferromagnetic (AF) inter-dimer interaction is found upon cooling. Above this transition the drop in {chi}T is a signature of ferromagnetic intra-dimer interactions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Material properties of perovskites in the quasi-ternary system LaFeO{sub 3}–LaCoO{sub 3}–LaNiO{sub 3}

An overview is presented on the variation of electrical conductivity, oxygen permeation, and thermal expansion coefficient as a function of the composition of perovskites in the quasi-ternary system LaFeO{sub 3}–LaCoO{sub 3}–LaNiO{sub 3}. Powders of thirteen nominal perovskite compositions were synthesized under identical conditions by the Pechini method. The powder X-ray diffraction data of two series, namely La(Ni{sub 0.5}Fe{sub 0.5}){sub 1−x}Co{sub x}O{sub 3} and LaNi{sub 0.5-x}Fe{sub x}Co{sub 0.5}O{sub 3}, are presented after the powders had been sintered at 1100 °C for 6 h in air. The measurements revealed a rhombohedral structure for all compositions except LaNi{sub 0.5}Fe{sub 0.5}O{sub 3} for which 60% rhombohedral and 40% orthorhombic phase was found. The maximum DC electrical conductivity value of the perovskites at 800 °C was 1229 S cm{sup −1} for the composition LaCoO{sub 3} and the minimum was 91 S cm{sup −1} for the composition LaCo{sub 0.5}Fe{sub 0.5}O{sub 3}. The oxygen permeation of samples with promising conductivities at 800 °C was one order of magnitude lower than that of La{sub 0.6}Sr{sub 0.4}Co{sub 0.8}Fe{sub 0.2}O{sub 3} (LSCF). The highest value of 0.017 ml cm{sup −2} min{sup −1} at 950 °C was obtained with LaNi{sub 0.5}Co{sub 0.5}O{sub 3}. The coefficients of thermal expansion varied in the range of 13.2×10{sup −6} K{sup −1} and 21.9×10{sup −6} K{sup −1} for LaNi{sub 0.5}Fe{sub 0.5}O{sub 3} and LaCoO{sub 3}, respectively. {sup 57}Fe Mössbauer spectroscopy was used as probe for the oxidation states, local environment and magnetic properties of iron ions as a function of chemical composition. The substitution had a great influence on the chemical properties of the materials. - Graphical abstract: Compositional dependence of isothermal electrical conductivity at 800 °C and thermal expansion coefficient in the series La(Fe{sub 0.5}Ni{sub 0.5}){sub (1−x)}Co{sub x}O{sub 3} and LaNi{sub 0.5−x}Fe{sub x}Co{sub 0.5}O{sub 3}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Structure and magnetic properties of Co-W clusters produced by inert gas condensation

In this article, inert-gas condensation was used to synthesize Co-W clusters. The formation, structure, and magnetic properties of the clusters were investigated. Sub-10-nm clusters were obtained, and the structures and average sizes were strongly dependent on sputtering power. At low sputtering powers, the clusters were predominantly amorphous, while, at high sputtering power, the clusters were crystalline. X ray diffraction and transmission electron microscopy revealed clusters with hcp structure at high sputtering power. The magnetic properties were dependent on the sputtering power and temperature, with the highest coercivity of 810 Oe at 10 K for high sputtering power.

36 MATERIALS SCIENCE↗

Thermal Properties of Sodium Borosilicate Glasses as a Function of Sulfur Content

SO3 additions, up to 3.0 wt%, were systematically investigated for effects on the physical properties of sodium borosilicate glass melted in air, with a sulfur-free composition of 50SiO2-10Al2O3-12B2O3-21Na2O-7CaO (wt%). Solubility measurements, using electron microscopy chemical analysis, determined the maximum loading to be ~1.5 wt% SO3. It was found that sulfur (here as sulfate) in this glass increased the glass transition temperature, thermal diffusivity, heat capacity, and thermal conductivity, and decreased the mass density. Structural analysis, performed with Raman spectroscopy, indicated that the borosilicate network polymerized with sulfur additions, presumably due to Na2O being required to charge compensate the ionic SO42- additions, thus becoming unavailable to form non-bridging oxygen in the silicate network. It is postulated that this increased crosslinking of the borosilicate backbone lead to a structure with higher dimensionality and average bond energy. This increased the mean free paths and vibration frequency of the phonons, which resulted in the observed increase in thermal properties.

Thermal properties, Borosilicate glass, Sulfur sol↗

Catalyst design to direct high-octane gasoline fuel properties for improved engine efficiency

The paraffin-to-olefin (P/O) ratio in gasoline fuel is a critical metric affecting fuel properties and engine efficiency. In the conversion of dimethyl ether (DME) to high-octane hydrocarbons over BEA zeolite catalysts, the P/O ratio can be controlled through catalyst design. Here, we report bimetallic catalysts that balance the net hydrogenation and dehydrogenation activity during DME homologation. The Cu-Zn/BEA catalyst exhibited greater relative dehydrogenation activity attributed to higher ionic site density, resulting in a lower P/O ratio (6.6) versus the benchmark Cu/BEA (9.4). The Cu-Ni/BEA catalyst exhibited increased hydrogenation due to reduced Ni species, resulting in a higher P/O ratio (19). The product fuel properties were estimated with an efficiency merit function and compared against finished gasolines and a typical alkylate blendstock. Merit values for the hydrocarbon product from all three BEA catalysts exceeded those of the comparison fuels (0–5.3), with the product from Cu-Zn/BEA exhibiting the highest merit value (9.7).

Catalyst design↗

Characterization of concrete properties from dielectric properties using ground penetrating radar

This paper presents the experimental results of a study of the relationships between light-weight (LWAC) and normal aggregate concrete (NAC) properties, as well as radar wave properties that are derived by using ground penetrating radar (GPR). The former (LWAC) refers to compressive strength, apparent porosity and saturated density, while the latter (NAC) refers to real part of dielectric permittivity ({epsilon}' or real permittivity) and wave energy level (E). Throughout the test period of the newly cast concrete cured for 90 days, the above mentioned material properties gradually changed which can be attributed to the effects of cement hydration, different types of aggregates and initial water to binder ratios. A number of plots describing various properties of concrete such as dielectric, strength and porosity perspectives were established. From these plots, we compare the characteristics of how much and how fast free water was turned to absorbed water in LWAC and NAC. The underlying mechanisms and a mechanistic model are then developed.

36 MATERIALS SCIENCE↗

Production and Fuel properties of Iso-Olefins with Controlled Molecular Structure and Obtained from Butene Oligomerization

The ability to control the molecular structure (e.g., degree of branching) of iso-olefins produced from oligomerizing light olefins is a valuable tool for tuning the final compositions of hydrocarbon fuels and targeting specific fuel properties. In this study, we demonstrated that the degree of branching of iso-olefins obtained from butene(s) oligomerization can be controlled by tuning process conditions (i.e., temperature, weight hourly space velocity [WHSV], and nature of butene feedstock) and by choosing the proper catalyst (i.e., Amberlyst-36 vs. Y/ZSM-22). In this study, we produced three types of iso-olefin mixtures: 1) a methyl-heptenes rich (74 wt.%) mixture, 2) dimethyl-hexenes rich (80–96 wt.%) mixtures, and 3) highly branched (i.e., more than three methyl substitutions) iso-olefins rich (>50 wt.%) mixtures. While dimethyl-hexenes are preferentially formed at lower temperatures (60–100°C) and WHSV (i.e., 2 hr-1), methyl-heptenes are favorably produced at higher temperatures (>100°C) and WHSVs (i.e., 7 hr-1) over Amberlyst-36. The use of either 1-butene or 2-butene as feedstock resulted in liquid products with similar branching because facile intramolecular isomerization occurs prior to oligomerization. However, the use of isobutylene feedstock forms a significantly more branched olefin product. The formation of highly branched iso-olefins also is favored at higher temperature (140°C) over Amberlyst-36. Using Y/ZSM-22 instead of Amberlyst-36 allowed preferential formation of less-branched methyl-heptenes. For each type of iso-olefins mixture, we determined fuel properties including research octane number (RON), motor octane number (MON), and octane sensitivity (S), which is the difference between RON and MON. We found that not only RON and MON but also S values increased with the degree of branching of these complex mixtures of iso-olefins. The highest RON of 99.7 and S value of 9.3 were obtained for a mixture of highly branched iso-olefins.

Dagle, Vanessa↗

Investigation of structural and magnetic properties of rapidly-solidified iron-silicon alloys at ambient and elevated temperatures

In this work, we investigated the ambient temperature structural properties (~300 K) and the ambient and high temperature (up to 900 K) direct current (DC) magnetic properties of melt-spun Fe-x wt.% Si (x = 3, 5, & 8) alloys. The wheel surface speeds selected for the study were 30 m/s and 40 m/s. The thickness, width, lattice parameter, saturation magnetization (MS), and intrinsic coercivity (HCI) of the melt spun ribbons are presented and compared with data in the literature. The ribbons produced at the lower wheel surface speed (30 m/s) were continuous having relatively uniform edges compared to the ribbons produced at the higher wheel surface speed. The thickness and the width of the melt-spun ribbons ranged between ~15-60 μm and 500-800 μm, respectively. The x-ray diffraction spectra of the melt-spun ribbons indicated the presence of disordered α-phase, irrespective of the composition, and the wheel-surface speed. The lattice parameter decreased gradually as a function of increasing silicon content from ~0.2862 nm (Fe-3 wt.% Si) to ~0.2847 nm (Fe-8 wt.% Si). Wheel surface speed was not shown to have a significant effect on the magnetization, but primarily impacted the ribbon structure. A decreasing trend in the saturation magnetization was observed as a function of increased silicon content. The intrinsic coercivity of the melt-spun alloys ranged between ~50 to 200 A/m. Elevated temperature evaluation of the magnetization in the case of Fe-3 & 5 wt.% Si alloy ribbons was distinctly different from the Fe-8 wt.% Si alloy ribbons. The curves of the as-prepared Fe-3 wt.% Si and Fe-5 wt.% Si alloy ribbons were irreversible while that of Fe-8 wt.% Si was reversible. The MS for any of the combinations of wheel surface speed and composition decreased monotonically with the increase in temperature (from 300 – 900 K). The percentage decrease in MS from 300 K to 900 K for the Fe-3 wt.% Si and Fe-5 wt.% Si alloys was ~19-22 %, while the percentage decrease in the same temperature range for Fe-8 wt.% Si alloy was ~26-30 %. It appears that Fe-3 wt.% Si and Fe-5 wt.% Si alloys ribbons are primarily comprised of the α phase (disordered phase) with any minor constituents being beyond the detection limits of the studies performed, while the Fe-8 wt.% Si alloy ribbons are comprised of disordered and regions of short-range ordering.

Elevated Temperature↗

Intrinsic magnetic properties of L1{sub 0} FeNi obtained from meteorite NWA 6259

FeNi having the tetragonal L1{sub 0} crystal structure is a promising new rare-earth-free permanent magnet material. Laboratory synthesis is challenging, however, tetragonal L1{sub 0} FeNi—the mineral “tetrataenite”—has been characterized using specimens found in nickel-iron meteorites. Most notably, the meteorite NWA 6259 recovered from Northwest Africa is 95 vol. % tetrataenite with a composition of 43 at. % Ni. Hysteresis loops were measured as a function of sample orientation on a specimen cut from NWA 6259 in order to rigorously deduce the intrinsic hard magnetic properties of its L1{sub 0} phase. Electron backscatter diffraction showed that NWA 6259 is strongly textured, containing L1{sub 0} grains oriented along any one of the three equivalent cubic directions of the parent fcc structure. The magnetic structure was modeled as a superposition of the three orthonormal uniaxial variants. By simultaneously fitting first-quadrant magnetization data for 13 different orientations of the sample with respect to the applied field direction, the intrinsic magnetic properties were estimated to be saturation magnetization 4πM{sub s} = 14.7 kG and anisotropy field H{sub a} = 14.4 kOe. The anisotropy constant K = 0.84 MJ/m{sup 3} is somewhat smaller than the value K = 1.3 MJ/m{sup 3} obtained by earlier researchers from nominally equiatomic FeNi prepared by neutron irradiation accompanied by annealing in a magnetic field, suggesting that higher Ni content (fewer Fe antisite defects) may improve the anisotropy. The fit also indicated that NWA 6259 contains one dominant variant (62% by volume), the remainder of the sample being a second variant, and the third variant being absent altogether.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The effects of oxygen pressure on disordering and magneto-transport properties of Ba{sub 2}FeMoO{sub 6} thin films grown via pulsed laser deposition

Epitaxial Ba{sub 2}FeMoO{sub 6} thin films were grown via pulsed laser deposition under low oxygen pressure and their structural, chemical, and magnetic properties were examined, focusing on the effects of oxygen pressure. The chemical disorder, off-stoichiometry in B site cations (Fe and Mo) increased with increasing oxygen pressure and thus magnetic properties were degraded. Interestingly, in contrast, negative magneto-resistance, which is the characteristics of this double perovskite material, was enhanced with increasing oxygen pressure. It is believed that phase segregation of highly disordered thin films is responsible for the increased magneto-resistance of thin films grown at high oxygen pressure. The anomalous Hall effect, which behaves hole-like, was also observed due to spin-polarized itinerant electrons under low magnetic field below 1 T and the ordinary electron-like Hall effect was dominant at higher magnetic fields.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Engineering the mechanical properties of ultrabarrier films grown by atomic layer deposition for the encapsulation of printed electronics

Direct deposition of barrier films by atomic layer deposition (ALD) onto printed electronics presents a promising method for packaging devices. Films made by ALD have been shown to possess desired ultrabarrier properties, but face challenges when directly grown onto surfaces with varying composition and topography. Challenges include differing nucleation and growth rates across the surface, stress concentrations from topography and coefficient of thermal expansion mismatch, elastic constant mismatch, and particle contamination that may impact the performance of the ALD barrier. In such cases, a polymer smoothing layer may be needed to coat the surface prior to ALD barrier film deposition. We present the impact of architecture on the performance of aluminum oxide (Al{sub 2}O{sub 3})/hafnium oxide (HfO{sub 2}) ALD nanolaminate barrier films deposited on fluorinated polymer layer using an optical calcium (Ca) test under damp heat. It is found that with increasing polymer thickness, the barrier films with residual tensile stress are prone to cracking resulting in rapid failure of the Ca sensor at 50 °C/85% relative humidity. Inserting a SiN{sub x} layer with residual compressive stress between the polymer and ALD layers is found to prevent cracking over a range of polymer thicknesses with more than 95% of the Ca sensor remaining after 500 h of testing. These results suggest that controlling mechanical properties and film architecture play an important role in the performance of direct deposited ALD barriers.

36 MATERIALS SCIENCE↗

Magnetic and structural properties of ferromagnetic Fe{sub 5}PB{sub 2} and Fe{sub 5}SiB{sub 2} and effects of Co and Mn substitutions

Crystallographic and magnetic properties of Fe{sub 5}PB{sub 2}, Fe{sub 4}CoPB{sub 2}, Fe{sub 4}MnPB{sub 2}, Fe{sub 5}SiB{sub 2}, Fe{sub 4}CoSiB{sub 2}, and Fe{sub 4}MnSiB{sub 2} are reported. All adopt the tetragonal Cr{sub 5}B{sub 3} structure-type and are ferromagnetic at room temperature with easy axis of magnetization along the c-axis. The spin reorientation in Fe{sub 5}SiB{sub 2} is observed as an anomaly in the magnetization near 170 K and is suppressed by substitution of Co or Mn for Fe. The silicides are found to generally have larger magnetic moments than the phosphides, but the data suggest smaller magnetic anisotropy in the silicides. Cobalt substitution reduces the Curie temperatures by more than 100 K and ordered magnetic moments by 16%–20%, while manganese substitution has a much smaller effect. This suggests Mn moments align ferromagnetically with the Fe and that Co does not have an ordered moment in these structures. Anisotropic thermal expansion is observed in Fe{sub 5}PB{sub 2} and Fe{sub 5}SiB{sub 2}, with negative thermal expansion seen along the c-axis of Fe{sub 5}SiB{sub 2}. First principles calculations of the magnetic properties of Fe{sub 5}SiB{sub 2} and Fe{sub 4}MnSiB{sub 2} are reported. The results, including the magnetic moment and anisotropy, are in good agreement with experiment.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗