Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “laser melting”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

A lightweight Fe–Mn–Al–C austenitic steel with ultra-high strength and ductility fabricated via laser powder bed fusion

Lightweight Fe–Mn–Al–C steels have become a topic of significant interest for the defense and automotive industries. These alloys can maintain high strength and ductility while also reducing weight in structural applications. Conventionally processed Fe–Mn–Al–C austenitic steels with high Al content (~9 wt%) demonstrate greater than 1.5 GPa strength with 35% elongation. Several recent studies have demonstrated success in fabricating steel parts using laser powder bed fusion (L-PBF) additive manufacturing (AM), which can generate near-net-shape components with complex geometries and is capable of local microstructural control. However, studies on L-PBF processing of Fe–Mn–Al–C alloys have focused on low Al content (<5 wt%) compositional regimes representing alloys that undergo transformation-induced plasticity (TRIP) and twinning-induced plasticity (TWIP). Here, in this study, we present the effects of L-PBF processing on the microstructure and mechanical properties of an Fe–30Mn–9Al–1Si-0.5Mo-0.9C austenitic steel. A process optimization framework is employed to determine an ideal L-PBF processing space that will result in >99% density parts. Implementing this framework resulted in near-fully dense specimens fabricated over a broad range of process parameters. Additionally, two bi-directional scan rotation strategies (90° and 67°) were applied to understand their effects on texture and anisotropy in this material. As-printed specimens displayed considerable work-hardening characteristics with average strengths of up to 1.3 GPa and 36% elongation in the build direction. However, solidification microcracks oriented in the build direction resulted in anisotropy in tensile strength and ductility resulting in average strengths of 1.1 GPa and 20% elongation perpendicular to the build direction. The successful L-PBF fabrication of Fe–30Mn–9Al–1Si-0.5Mo-0.9C presented here is expected to open new avenues for weight reduction in structural applications with a high degree of control over part topology.

36 MATERIALS SCIENCE↗

An efficient numerical model for predicting residual stress and strain in parts manufactured by laser powder bed fusion

Abstract Computational modeling of additively manufactured structures plays an increasingly important role in product design and optimization. For laser powder bed fusion processes, the accurate modeling of stress and distortion requires large amount of computational cost due to very localized heat input and evolving complex geometries. The current study takes advantage of a graphics processing unit accelerated explicit finite element analysis code and approximated heat conduction analysis to predict the macroscopic thermo-mechanical behavior in laser selective melting. Adjacent layers and tracks were lumped to reduce the number of time steps and elements in the finite element model. The effects of track and layer grouping on prediction accuracy and solution efficiency are investigated to provide a guidance for a cost-effective simulation. Thin-wall builds from Inconel alloy 625 (IN625) powders were simulated by applying the developed modeling approach to get the detailed residual stress and distortion at a computational speed 50 times higher than conventional approach. Under repeated heating and cooling cycles, a high tensile stress was produced near surfaces of a build due to a larger shrinkage on surface than that in central area. It is also shown that horizontal stresses concentrate near the root and top layers of the IN625 build. The predicted residual elastic strain distribution was validated by the experimental measurement using x-ray synchrotron diffraction.

36 MATERIALS SCIENCE↗

The structure of molten calcium ferrite under various redox conditions

Laser-heated melts based on the 43CaO–57Fe 2 O 3-x eutectic, close to the calcium ferrite (CF) composition, were measured with high-energy X-ray diffraction using aerodynamic levitation over a range of redox states controlled by CO/CO 2 gas atmospheres. The iron–oxygen coordination number was found to rise from 4.4 ± 0.3 at 15% Fe 3+ to 5.3 ± 0.3 at 87% Fe 3+ . Empirical potential structure refinement modelling was used to obtain the ferric and ferrous partial pair distribution functions. It was found that the Fe 2+ iron–oxygen coordination number is consistently approximately 10% higher in CF than in pure iron oxide, while Fe 3+ is essentially identical in all but the most oxygen-rich environments (where it is higher in CF compared with FeO x ). The model also shows calcium octahedra to be the dominant species across all redox environments, although the population of CaO 7 increases with the availability of oxygen at the expense of CaO 4 and CaO 5 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Evaluation of DED and LPBF Fe-based Alloys Process Application Envelopes based on Performance, Process Economics, Supply Chain Risks, and Reactor-specific Targeted Components

The U.S. Department of Energy (DOE), Office of Nuclear Energy (NE), Advanced Materials and Manufacturing Technologies (AMMT) program aims to develop extreme-environment materials solutions for use in the deployment of advanced nuclear reactors and the sustainment of the current fleet. To achieve this objective, a combination of experiment, a computational tool, and machine learning (ML) for the design of materials is adopted for the maturation of materials for nuclear technology. Through advanced manufacturing techniques such as laser powder bed fusion (LPBF) and laser powder direct energy deposition (LP-DED), components with complex geometries can be fabricated with reduced time and effort. Such advanced manufacturing methods can also provide the opportunity to improve materials performance through optimized microstructures and mechanical properties. However, existing engineering alloys are not always well suited for fabrication with additive manufacturing (AM), as their compositions have been tuned to optimize fabrication via conventional methods. Thus, similar alloys with modified compositions that are better suited for AM can be studied for improved performance. Over the past three years, the AMMT teams from Argonne National Laboratory (ANL) and Pacific Northwest National Laboratory (PNNL) studied various known Fe-based alloys by evaluating their initial printability using LPBF, and an AMMT-developed down-selection and decision matrix reduced the number of alloys to be studied from six to three in fiscal year (FY) 2024. Additionally, in FY 2024, for parallel evaluation, these three alloys were studied using LPDED. While LPBF is better for small- to medium-sized components with high detail and internal features, LP-DED combines a material feed system to place the powder onto the exact spot where the laser will melt the material. This AM method can be easily scaled to extremely large components and provides high build rate speeds compared to those of conventional LPBF systems. Additionally, DED is a better choice for complex geometries and compositional gradients.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Low-cost and high-performance heat exchangers for CSP

This project aimed to design and manufacture a low-cost and high-performance, particle–to–sCO 2 heat exchanger (HX) for Concentrated Solar Power (CSP) using additive manufacturing (AM). Three enabling technologies will be integrated to achieve the targeted cost and performance. The first technology is the extreme high‐speed laser materials deposition (LMD) AM process known by its German acronym EHLA that was invented at the Fraunhofer Institute for Laser Technology. The EHLA process utilizes a specially designed powder-feeding nozzle that enables a laser to melt the powder particles above the melt pool, in contrast to the conventional LMD process where the powders are melted inside the melt pool. EHLA enables much faster deposition rate than conventional LMD without the need to wait for the powders to melt. The second technology is an innovative double-helical HX geometry that can be easily fabricated using the EHLA process by rotating a rod at a high-speed to take advantage of the high EHLA deposition rate. The double-helical fins separate the hot region (the hot particle side) and the cold region (the sCO 2 side) and provide large heat transfer surface area without a large pressure drop on the sCO 2 side. The particle side will have a larger gap to facilitate the particle flow. The outer rims of the double helixes can be sealed off using the same AM process. After sealing-off, additional double helixes can be built radially on top of the first set to improve HX performance. The HX can be installed vertically for gravity-driven flow of the hot particles if necessary. The third technology is a low-cost high-temperature alumina-forming austenitic (AFA) steel TMA-6350 that has creep and oxidation resistance up to 1100 °C. These technologies together will enable high-performance and low-cost HXs for particle–to–sCO 2 for CSP.

14 SOLAR ENERGY↗

Effects of Build Orientation and Heat Treatment on Neutron Irradiation Hardening in Inconel 625 Fabricated via Laser Powder Bed Fusion

Various Inconel 625 coupons fabricated via Laser Powder Bed Fusion (L-PBF) were neutron irradiated using the inside reflector of the reactor at the University of Missouri Research Reactor (MURR). Effects of build orientation and heat treatment on neutron-induced hardening were investigated by inspecting L-PBF samples built vertically or at a 45º angle in the following heat-treated conditions: as-built (no heat treatment), 700 ºC for 1 hour, 900 ºC for 1 hour, and 1050 ºC for 1 hour. The microhardness results of L-PBF samples before and after neutron irradiation were compared with traditional wrought Inconel 625. All samples underwent an irradiation flux of 6.61 x 1013 neutrons/cm²/s for 310 hours for an estimated damage of 0.012 dpa. Results indicate that as-built L-PBF specimens are less prone to radiation hardening relative to their wrought counterparts. As-printed diagonal specimens were shown to harden by 8% as compared to 1.2% hardening in as-printed vertical specimens.

36 MATERIALS SCIENCE↗

X-ray observation of individual Ti-6Al-4V spherical powder particle impact in an in-situ operando laser directed energy deposition system

Understanding the particle capture mechanism in the laser directed energy deposition additive manufacturing process provides a foundation for improving productivity and reducing material loss. Capturing this phenomenon is challenging due to its highly transient time interval. To analyze the impact behavior of spherical Ti-6Al-4V powder, a custom laser directed energy deposition system was designed to control the deposition of individual particles. Synchrotron X-ray imaging at 24 kHz monitored the impact dynamics of individual powder particles. A multi-physics model based on the Smoothed-Particle Hydrodynamics scheme supported the analysis by providing the temperature and velocity fields of the molten pool. Results revealed that in laser directed energy deposition, surface tension forces dominated the powder–molten pool interaction. Hydrophobic Ti-6Al-4V powder particles had an equilibrium contact angle of 121 degrees with their molten state. Furthermore, Ti-6Al-4V powder particles required a high impact velocity (6 to 12 m/s) to transition from oscillation to submergence behavior. Lastly, oscillating powder particles that impacted near the location of the laser beam exhibited faster melting, highlighting the contribution of the laser beam to the melting mechanism. This work lays the foundation for investigations of powder particle impact in laser directed deposition and supports the validation of numerical models of powder–molten pool interactions.

36 MATERIALS SCIENCE↗

Two-color high speed thermal imaging system for laser-based additive manufacturing process monitoring

Monitoring melt pool temperature in laser powder bed fusion by providing a build laser that produces a laser beam that is directed onto the melt pool and produces an incandescence that emanates from the melt pool, receiving the incandescence and producing a first image having a first spectral band and a second image having a second spectral band, and determining the ratio of said first image having a first spectral band and said second image having a second spectral band to monitor the melt pool temperature.

Calta, Nicholas P.↗

ADDITIVE MANUFACTURING OF REFRACTORY ALLOYS

Refractory alloys are known for their high temperature capabilities and are intended for use at ultra-high temperatures above even 1200°C, which exceeds the capabilities of conventional superalloys. Additive manufacturing (AM) is an attractive alternative processing route because refractory alloys are difficult to fabricate through traditional methods; AM can form a near net-shape part with a tailored microstructure. This work seeks to evaluate the solidification behavior of refractory alloys under AM conditions and establish corresponding solidification models. Two binary alloys, Mo30Nb and Nb7.5Ta, as well as the commercial Nb alloy, C103, and one refractory high entropy alloy (RHEA), MoNbTaTi, were subjected to single track melts in a laser powder bed fusion (LPBF) machine. Each melt track was evaluated in the scanning electron microscope (SEM), which determined that some AM conditions used led to non-ideal behavior. Electron backscatter diffraction (EBSD) revealed that the Nb7.5Ta, C103, and MoNbTaTi all exhibited new grain nucleation to various extents while the Mo30Nb exhibited primarily epitaxial growth. This was found to be inconsistent with solidification models that were developed for each alloy and each set of AM conditions to predict the columnar to equiaxed transition behavior (CET) of the experimental microstructures. This disparity was largely attributed to the input parameters for the solidification model, which were developed using Thermo-Calc and SYSWELD. These input parameters include the alloy specific Gibbs-Thomson coefficient and thermophysical properties, the solute specific liquidus slopes and partitioning coefficients, as well as the process specific thermal gradients. Each input parameter was evaluated to determine the likely changes required for the modeled values to generate solidification models that better correspond to what was observed experimentally.

Miklas, Abigail↗

Elucidating the effect of preheating temperature on melt pool morphology variation in Inconel 718 laser powder bed fusion via simulation and experiment

In laser powder bed fusion (L-PBF) additive manufacturing, the mechanical performance, microstructure and defects of fabricated parts are closely associated with the melt pool morphology, e.g., its dimension and shape through the building process. Past studies have largely focused on how the process parameters such as laser power and scan speed affect melt pool characteristics. In this study, the melt pool morphology variation as a function of preheating temperature in the conduction, transition, and keyhole regimes and the underlying mechanisms in each regime are investigated through ex-situ sample characterization and computation thermal fluid dynamics (CtFD) simulation. Single tracks with different combinations of laser power and scan speed are deposited on an Inconel 718 bare plate preheated to a temperature range of 100–500 °C in the experiment. Significant changes are observed in melt pool morphology as a function of preheating temperature from optical measurements of melt track cross sections. The depth of melt pool in the three regimes increases monotonically with preheating temperature, e.g., at 500 °C, the experimental melt pool depth is increased by 49% in conduction regime, 34% in transition regime and 33% in keyhole regime, respectively, while the variation of melt pool width in each regime does not all follow an increasing trend but depends on the melt pool regimes. Melt pool width variation in the conduction and transition regimes is found to depend on the enhanced heat conduction directly related to temperature dependent thermal properties. Through validated CtFD simulations, it is found that in the keyhole regime the evaporation mass, recoil pressure, and laser drilling effect is enhanced with higher preheating temperature, which gives rise to a deeper melt pool. The simulations also reveal that preheating temperature significantly elongates the melt track length due to the increased flow rate and strong recoil pressure that accelerates the backward flow.

36 MATERIALS SCIENCE↗

Melt pool temperature measurement and monitoring during laser powder bed fusion based additive manufacturing via single-camera two-wavelength imaging pyrometry (STWIP)

Melt pool (MP) temperature is one of the determining factors and a key signature for evaluating the properties of printed components in metal additive manufacturing (AM). The state-of-the-art measurement systems are hindered, primarily by the large-scale data acquisition and processing demands. In this work, we introduce a novel coaxial, high-speed, single-camera two-wavelength imaging pyrometer (STWIP) system as opposed to the typical utilization of multiple cameras for measuring MP temperature profiles in laser powder bed fusion (LPBF) processes. Developed on a commercial LPBF machine (EOS M290), the STWIP system demonstrated its ability to quantitatively monitor the MP temperature and its variation for 50 layers at high framerates (>30,000 fps) for a real-world application (standard fatigue specimens) print. High performance computing is employed to analyze the acquired big data (MP images), for determining each MP's average temperature and 2D temperature profile. The MP temperature evolution in the gage section of a fatigue specimen is also examined at a temporal resolution of 1 ms, by evaluating the MP temperatures in the samples' first, middle, and last layers. This report is the first of its kind on monitoring MP temperature distribution and evolution at such a large, detailed scale for longer durations in practical applications.

42 ENGINEERING↗

Microstructure-Based Modeling of Laser Beam Shaping During Additive Manufacturing

Recent experimental studies suggest the use of spatially extended laser beam profiles as a strategy to control the melt pool during laser powder bed fusion (LPBF) additive manufacturing. However, linkages connecting laser beam profiles to thermal fields and resultant microstructures have not been established. Herein, we employ a coupled thermal transport-Monte Carlo model to predict the evolution of temperature fields and grain microstructures during LPBF using Gaussian, ring, and Bessel beam profiles. In addition, simulation results reveal that the ring-shaped beam yields lower temperatures compared with the Gaussian beam. Owing to the small melt pool size when using the Bessel beam, the grains are smaller in size and more equiaxed compared to those using the Gaussian and ring beams. Our approach provides future avenues to predict the impact of laser beam shaping on microstructure development during LPBF.

36 MATERIALS SCIENCE↗

In-Situ Characterization of Pore Formation Dynamics in Pulsed Wave Laser Powder Bed Fusion

Laser powder bed fusion (LPBF) is an additive manufacturing technology with the capability of printing complex metal parts directly from digital models. Between two available emission modes employed in LPBF printing systems, pulsed wave (PW) emission provides more control over the heat input compared to continuous wave (CW) emission, which is highly beneficial for printing parts with intricate features. However, parts printed with pulsed wave LPBF (PW-LPBF) commonly contain pores, which degrade their mechanical properties. In this study, we reveal pore formation mechanisms during PW-LPBF in real time by using an in-situ high-speed synchrotron x-ray imaging technique. We found that vapor depression collapse proceeds when the laser irradiation stops within one pulse, resulting in occasional pore formation during PW-LPBF. We also revealed that the melt ejection and rapid melt pool solidification during pulsed-wave laser melting resulted in cavity formation and subsequent formation of a pore pattern in the melted track. The pore formation dynamics revealed here may provide guidance on developing pore elimination approaches.

36 MATERIALS SCIENCE↗

Microstructural banding of directed energy deposition-additively manufactured 316L stainless steel

The microstructures of 316 L stainless steel created by rapid solidification are investigated here by comparing the similar microstructures of individual hatches of directed energy deposition additive manufacturing (DED-AM) and those of single, laser surface-melted tracks formed on a solid plate. High recoil pressure, which is exponentially dependent on the laser beam power density, induces convection of the melt pool, which causes formation of microstructural bands in the as-solidified microstructure. The microstructural bands are associated with changes in the chromium concentration and are a significant component of the inhomogeneous microstructure of DED-AM.

36 MATERIALS SCIENCE↗

Neutron Characterization of 3D Printed Gas Turbine Alloy With Internal Cooling Structure

The objective of this research work is to investigate the residual strains induced by the presence of a exit hole and internal hollow geometry present in a 3D printed IN718 similar to that seen in a gas turbine blade. The specimens were manufactured with an internal hollow structure that ended with an exit hole, and fabricated by direct metal laser sintering additive manufacturing technique. Using this technique, metal powder was melted by a laser source and rapidly cooled to form the part layer by layer. Rapid heating and cooling generate large thermal gradients and residual stresses in the 3D printed material. To be aligned with industry standards, specimens were heat-treated to relieve most of the residual stresses as well as to investigate whether IN718 still preserved a nonhomogeneous stress state after the thermal treatment. Roughness and microstructure analysis was performed to understand the heat-treated sample properties. To investigate the volumetric residual strain, the neutron diffraction technique was used with a definite neutron wavelength. Bragg’s law was used to determine lattice spacing. Interplanar lattice spacing and stress-free state lattice spacings were measured to calculate the strains. Residual strains were measured in the x and y direction to understand the impact of the presence of a exit hole and internal hollow geometry. The results of volumetric residual strain in the x and y directions showed no significant variations in the distribution of the strain due to the presence of a hollow structure as well as the exit hole. Overall, no significant stress concentration was observed in the heat treated sample. Sample geometry, instrumentation for neutron diffraction, and material properties are discussed in detail in this paper.

Raju, Nandhini↗