Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “WELDING, ARC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Pulsed-Current Welding Of Nickel-Based Alloy

Joints as strong (or stronger than) joints made with constant current. Report based on study of pulsed-current versus constant-current gas/tungsten arc welding of butt joints between panels of nickel-based alloy 718. In pulsed-current welding, arc current alternated between high and low value. Enables greater control of freezing and depth of penetration of weld puddle at given heat input. Thicker sections joined. Readily incorporated into automated welding system, with resultant greater uniformity and reproducibility of welds than attained in manual welding.

Gamwell, W. R.↗

Vacuum Deposition From A Welding Torch

Process derived from arc welding produces films of high quality. Modified gas/tungsten-arc welding process developed for use in outer space. Welding apparatus in process includes hollow tungsten electrode through which inert gas flows so arc struck between electrode and workpiece in vacuum of space. Offers advantages of fast deposition, possibility of applying directional impetus to flow of materials, very low pressure at surface being coated, and inert environment.

Poorman, R. M.↗

Time-Dependent 600 °C Post-Weld Heat Treatment Response of Laser-Wire-Directed Energy Deposited Austenitic Stainless Steel Claddings on Carbon Steel

Austenitic stainless steel overlay claddings are often used to protect nuclear reactor pressure vessels from corrosion. Arc welding processes are traditionally employed, which require a high heat input to bond the dissimilar metals, creating a large heat-affected zone and high residual stress that demands a lengthy stress-relieving post-weld heat treatment, up to 48 hours. High energy beam (e.g., laser, electron beam) directed energy deposition-based overlay cladding processes show promise for fabricating claddings with superior performance compared to arc welded ones because of their localized heat input; however, their necessity and time of post-weld heat treatment are currently unclear. In this research, we investigate the time dependence of a 600 C stress-relieving post-weld heat treatment of austenitic stainless steel clad on low carbon steel by laser-wire-directed energy deposition, comparing the microstructure and mechanical properties of the as-fabricated condition to 2-, 10-, and 48-hour heat treatment times. Diffusion simulations and microscopy show a gradual carburization of the stainless steel cladding and decarburization of the heat-affected zone/base metal. Nanoindentation testing shows up to a 1.8–2.69 embrittlement in the cladding and a 0.33 to 0.69 softening in the heat-affected zone after the 48-hour post-weld heat treatment. Tensile testing of the cladding composites reveals that increasing post-weld heat treatment time raises clad cracking susceptibility due to intergranular carbide formation and shows that laser-wire-directed energy deposition claddings may not require post-weld heat treatment.

Coating↗

Exploring the Cooling Process for Residual Stress Reduction in Dissimilar Welds

Dissimilar metal welds are currently used in various industry applications; however, a significant number of failures have been reported in these joints due to the existence of large tensile residual stresses induced by arc welding processes. Hence, it is crucial to reduce or eliminate such residual stresses in dissimilar metal welds. Recently, modern techniques such as CO 2 rapid cooling have received attention by scholars to reduce residual stress in similar metal welds. Nevertheless, the effectivity of this technique has not been explored in dissimilar metal welds. In this paper, the impact of in-situ rapid local cooling in dissimilar metal welds is studied experimentally. The residual stresses of CO 2 -cooled welds were measured using the neutron diffraction technique. The effect of rapid cooling on the microstructure of the weld and heat-affected zones were examined. Finally, it is shown that for certain cases, in-situ rapid cooling during the arc welding process can minimize tensile residual stresses in dissimilar metal welds.

42 ENGINEERING↗

Process-Information Display Panel For Welder's Visor

Head-up display (HUD) unit mounted in welder's visor or helmet provides process information in real time. Display enables welder to gain greater awareness of effects of welding while controlling welding process in usual way(s) by use of foot pedal, voice command, and/or manipulation of welding torch. Possible to avoid need for every new welder on job to solve same problems solved by other welders. Graphical display presented to welder, adjacent to normal field of view through visor. Beneficial in supporting and enhancing continued practice of manual arc welding. Valuable in industries that invest millions of technician-hours each year in manual arc welding for variety of products.

Russell, Carolyn↗

The effect of shielding gases on the geometrical features in metal big area additive manufacturing (mBAAM)

The purpose of this 2018 Visiting Faculty Program (VFP) award is to understand the effect of shielding gas on the geometric features in metal big area additive manufacturing (mBAAM) using arc welding. The selection of shielding gases in mBAAM comes from experiences in the welding community. However, there is a little to no information on how shielding gas affects different geometrical features in large-scale AM. It is desirable to have different melting characteristics and fluidity for different geometrical features in mBAAM, which cannot be fulfilled by established arc welding practices. During the 10 weeks appointment, a variation of reactive and non-reactive shielding gases (binary and ternary) have been used to deposit three different geometric shapes using two metallic alloys: C-Mn steel and 410 Stainless steel. These distinct as-deposited geometric shapes are 3-d scanned and compared. The fluidity, wetting characteristics, thermal effect is experimentally analyzed. The mechanical properties are investigated and the microstructure is analyzed.

36 MATERIALS SCIENCE↗

Microstructure Evolution, Structural Integrity, and Hot Corrosion Performance of Nitrogen-Enhanced Stainless Steel Welds

This work articulated the multi-pass, gas tungsten arc welding by adopting pulsating current for joining nitrogen-enhanced, low-carbon austenitic stainless steel, AISI 316L(N). An austeno-ferrite stainless steel (ER2594) and an over-alloyed (ERNiCrMo-3) fillers were employed to join 6-mm-thick plates of AISI 316L(N). Acicular and lathy ferrite in the weld zone of ER2594 and the occurrence of secondary phases in the fusion zone of over-alloyed filler were observed. The notch tensile strength data attested that the joint strength was greater for the welds employing an over-alloyed filler. This study also affirms that the welds obtained with ER2594 filler resulted in better impact toughness (144 J) compared with ERNiCrMo-3 filler and base metal. Also the notch impact toughness of ER2594 weldment is increased to 60% in comparison with that of candidate metal. Corrosion studies were also performed by exposing the coupons in a eutectic salt mixture comprising of 40%K{sub 2}SO{sub 4}-60%NaCl for 50 cycles at 650 °C. It is observed that the weld zone employing over-alloyed filler experienced better high-temperature corrosion resistance compared to the base metal. The specific results of this investigation will be of greater demand to the nuclear and marine applications utilizing these joints.

36 MATERIALS SCIENCE↗

Metal Big Area Additive Manufacturing: Process Modeling and Validation

Metal Big Area Additive Manufacturing (mBAAM) is a new additive manufacturing (AM) technology for printing large-scale 3D objects. mBAAM is based on the gas metal arc welding process and uses a continuous feed of welding wire to manufacture an object. An electric arc forms between the wire and the substrate, which melts the wire and deposits a bead of molten metal along the predetermined path. In general, the welding process parameters and local conditions determine the shape of the deposited bead. The sequence of the bead deposition and the corresponding thermal history of the manufactured object determine the long range effects, such as thermal-induced distortions and residual stresses. Therefore, the resulting performance or final properties of the manufactured object are dependent on its geometry and the deposition path, in addition to depending on the basic welding process parameters. Physical testing is critical for gaining the necessary knowledge for quality prints, but traversing the process parameter space in order to develop an optimized build strategy for each new design is impractical by pure experimental means. Computational modeling and optimization may accelerate development of a build process strategy and saves time and resources. Because computational modeling provides these opportunities, we have developed a physics-based Finite Element Method (FEM) simulation framework and numerical models to support the mBAAM process s development and design. In this paper, we performed a sequentially coupled heat transfer and stress analysis for predicting the final deformation of a small rectangular structure printed using the mild steel welding wire. Using the new simulation technologies, material was progressively added into the FEM simulation as the arc weld traversed the build path. In the sequentially coupled heat transfer and stress analysis, the heat transfer was performed to calculate the temperature evolution, which was used in a stress analysis to evaluate the residual stresses and distortions. In this formulation, we assume that physics is directionally coupled, i.e. the effect of stress of the component on the temperatures is negligible. The experiment instrumentation (measurement types, sensor types, sensor locations, sensor placements, measurement intervals) and the measurements are presented. The temperatures and distortions from the simulations show good correlation with experimental measurements. Ongoing modeling work is also briefly discussed.

Additive Manufacturing↗

Effect of Low-Temperature Sensitization on the Corrosion Behavior of AISI Type 304L SS Weld Metal in Simulated Groundwater

The manuscript presents the investigations carried out on the effect of low-temperature sensitization (LTS) of 304L SS weld metal on its corrosion behavior in simulated groundwater, for its application as a canister material for long-term storage of nuclear vitrified high-level waste in geological repositories. AISI type 304L SS weld pad was fabricated by multipass gas tungsten arc welding process using 308L SS filler wire. The as-welded specimens were subsequently subjected to carbide nucleation and further to LTS at 500 °C for 11 days to simulate a temperature of 300 °C for 100-year life of the canister in geological repositories. Delta ferrite (δ-ferrite) content of the 304L SS weld metal substantially decreased on carbide nucleation treatment and further only a marginal decrease occurred on LTS treatment. The microstructure of the as-welded consisted of δ-ferrite as a minor phase distributed in austenite matrix. The δ-ferrite appeared fragmented in the carbide-nucleated and LTS-treated weld metal. The degree of sensitization measured by double-loop electrochemical potentokinetic reactivation method indicated an increase in carbide nucleation treatment when compared to the as-welded specimens, and further increase occurred on LTS treatment. Potentiodynamic anodic polarization investigations in simulated groundwater indicated a substantial decrease in the localized corrosion resistance of the carbide-nucleated and LTS 304L SS weld metals, when compared to the as-welded specimens. Post-experimental micrographs indicated pitting as the primary mode of attack in the as-welded, while pitting and intergranular corrosion (IGC) occurred in the carbide-nucleated weld metal. LTS-treated weld metal predominantly underwent IGC attack. The decrease in the localized corrosion resistance of the weld metal after LTS treatment was found to have a direct correlation with the degree of sensitization and the weld microstructure. The results are detailed in the manuscript.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Three-Layer TIG-Welded 2219 Aluminum Alloys with Dissimilar Heat Treatments

2219-C10S and 2219-CYS aluminum alloys are 2219 aluminum alloys with different heat treatment processes, and they have been widely used in the aerospace industry. In the present study, 2219-C10S and 2219-CYS aluminum alloys were butt-welded by three-layer tungsten inert gas arc welding (with the welding center of the third layer shifted toward the CYS side), and the microstructure characteristics and mechanical properties of the welded joint were investigated. The lamellar θ′ phases, the bulk or rod θ phases, and the coarse rod-shaped or pancake-shaped Al-Cu-Fe-Mn phases coexisted in the two aluminum alloys. The Cu content of the α-Al matrix and the distribution of eutectic structures of different welding layers in the weld zone (WZ) were varied, implying that the segregation degrees of the Cu element were different due to the different welding thermal cycles in different welding layers. The microhardness values of the CYS side were much higher than those of the C10S side in each region on both sides of the joint. The tensile test deformation was concentrated mainly in the regions of WZ and the over aged zone (OAZ), where the microhardness values were relatively low. The main deformation concentrated region was transferred from the CYS side to the C10S side with the increase in the tensile load during the tensile test. The fracture behavior of the tensile test showed that the macroscopic crack initiated near the front weld toe had gone through the crack blunt region, the shear fracture region of the partially melted zone (PMZ), and the shear fracture region of OAZ. Meanwhile, the fracture characteristics gradually evolved from brittle to ductile. The concentrated stress and the dense eutectic structure in the region near the front weld toe of the C10S side contributed to the fracture of the joint. The shift of the welding center of the third layer to the CYS side resulted in two effects: (i) the microhardness values from the middle layer to the top layer in the PMZ of the CYS side were the most significantly increased and (ii) the distance between the front weld toe and the fusion line of the CYS side was significantly larger.

36 MATERIALS SCIENCE↗

Atom probe tomography characterization of neutron irradiated surveillance samples from the R. E. Ginna reactor pressure vessel

Surveillance samples of a low copper (nominally 0.05 wt.% Cu) forging and a higher copper (0.23 wt.% Cu) submerged arc weld from the R. E. Ginna reactor pressure vessel have been characterized by atom probe tomography (APT) after exposure to three levels of neutron irradiation, i.e., fluences of 1.7, 3.6 and 5.8 × 10 23 n.m –2 (E > 1 MeV), and inlet temperatures of ~289 °C (~552 °F). As no copper-enriched precipitates were observed in the low copper forging, and the measured copper content in the ferrite matrix was 0.04± <0.01 at.% Cu, after neutron irradiation to a fluence of 1.7 × 10 23 n.m –3 , this copper level was below the solubility limit. A number density of 2 × 10 22 m –3 of Ni–, Mn– Si-enriched precipitates with an equivalent radius of gyration of 1.7 ± 0.4 nm were detected in the sample. However, Cu-, Ni-, Mn-enriched precipitates were observed in specimens cut from different surveillance specimens from the same forging material in which the overall measured copper level was 0.08± <0.01 at.% (fluence of 3.6 × 10 23 n.m –3 ) and 0.09± <0.01 at.% Cu (fluence of 5.8 × 10 23 n.m –3 ). Therefore, these slightly higher copper contents were above the solubility limit of Cu under these irradiation conditions. A best fit of all the composition data indicated that the size and number density of the Cu-enriched precipitates increased slightly in both size and number density by additional exposure to neutron irradiation. High number densities of Cu-enriched precipitates were observed in the higher Cu submerged arc weld for all irradiated conditions. The size and number density of the precipitates in the welds were higher than in the same fluence forgings. Some Cu-enriched precipitates were found to have Ni-, Mn- Si-, and P-enriched regions on their surfaces suggesting a preferential nucleation site. Furthermore, atom maps revealed P, Ni, and Mn segregation to, and preferential precipitation of, Cu-enriched precipitates over the surface of a grain boundary in the low fluence weld.

36 MATERIALS SCIENCE↗

Effect of Weld Consumable Conditioning on the Diffusible Hydrogen and Subsequent Residual Stress and Flexural Strength of Multipass Welded P91 Steels

P91 steel weld joint was prepared using the shielded metal arc welding process and four different conditions of weld consumable that provide the different levels of diffusible hydrogen in deposited metal. In the present research, the effects of diffusible hydrogen content on the flexural strength, lower critical stress, and tensile strength of P91 steel welds were also determined with respect to different electrode conditions. To investigate the effect of diffusible hydrogen on multipass welding, top and root side flexural tests were performed. The residual stresses (axial stress and transverse stress) were also measured using the blind hole drilling method for different conditions of welding consumable. The peak value of residual stresses was measured at the center of the weld fusion zone. The maximum value of transverse stress was measured to be 355 MPa for case II (6.21 mL/100 g of diffusible hydrogen), while the maximum axial stress was about 218 MPa for case IV (12.43 mL/100 g of diffusible hydrogen). A three-dimensional finite element simulation was also performed to predict the residual stress distribution and thermal profile along the welded joint. The experimentally determined residual stresses correlated well with the numerically estimated residual stresses. The diffusible hydrogen content was not observed to have any significant effect on the residual stresses. The corrected residual stress values were also predicted by considering the plasticity-induced error. However, the flexural performance of the welded joint was affected by the diffusible hydrogen content. The top and root flexural strength was measured to be optimum for the low level of diffusible hydrogen content, and the values decreased with an increase in diffusible hydrogen content.

36 MATERIALS SCIENCE↗

Modeling of Keyhole-Induced Pore Formation in Laser-Arc Hybrid Welding of Aluminum Alloy with a Horizontal Fillet Joint

A three-dimensional transient model is proposed to investigate the weld pool dynamic behavior in laser + metal inert gas (MIG) hybrid fillet welding of aluminum alloy in the horizontal position, which allows for the joint configuration and coupling of the keyhole, droplet and weld pool as well as the heat and mass exchange between gas and liquid phases and is able to simulate the temperature distribution, fluid flow and formation process of a keyhole-induced pore in hybrid welding with a horizontal fillet joint. The weld porosity is also measured using x-ray nondestructive testing technology. Keyhole behavior and the formation mechanism of keyhole-induced porosity were analyzed. The calculated results are in generally good agreement with the experimental ones. A clockwise vortex always exists at the middle part of the weld pool. The formation and growth of the molten metal bulge on the keyhole wall are responsible for the occurrence of a gas bubble, which has a variation in size and shape and can be split during welding. The keyhole collapses easily at its middle or upper part in horizontal fillet welding, and the capture of the bubble by the upper molten pool boundary enhances the possibility of porosity formation to some degree. The keyhole-induced pore is mainly formed at the regions near the keyhole bottom and the upper fusion line of the weld pool.

36 MATERIALS SCIENCE↗

Stability of zirconium hydride

This reports complete Milestone M2.2.1 Stability of zirconium hydride: Experimental investigation of the hydrogen concentration of encapsulated zirconium hydride before and after joining. In this milestone, we first report the successful fabrication of crack-free bulk zirconium hydride by using the ORNL static hydriding system. The fabricated hydride was characterized by using X-ray diffraction (XRD) and X-ray computed tomography (XCT). XRD results showed that the δ-phase zirconium hydride, α-zirconium, and ε-phase hydride were present. XCT confirmed the absence of the internal cracking. The hydrogen concentration was determined by the weight change before and after hydrogen loading, given the fact that the oxide phase was not found during XRD analysis. Two metallic cladding materials, i.e., molybdenum and FeCrAl, were selected to encapsulate the fabricated zirconium hydride pellets. Demonstration capsules were designed and machined. Mo crucible was successfully sealed by using a combination of electron beam welding and gas tungsten arc welding. Due to the undesired neutronics property of Mo, further investigation of this cladding material was not pursued. Electron beam welding and laser beam welding were employed to seal the FeCrAl capsules. XRD were performed on the zirconium hydride before and after the sealing. The results showed that the welding process has negligible impact on the hydrogen content in the FeCrAl-canned zirconium hydride. The presented work fulfilled the proposed work under this milestone and paves a pathway to fabricate single-phase zirconium hydride and to develop robust cladding materials to can bulk zirconium hydride.

36 MATERIALS SCIENCE↗

Rolling Behavior of Surface Tagged Aluminum 6061 using Photoluminescent Oxides

Physical tagging of nuclear fuel is potentially one way of tracking throughout the fuel lifecycle. The process of tagging can take many forms, but one promising method is to embed a small amount of photoluminescent particles in the surface of a material which are not detectable under normal illumination but are readily visible under excitation by ultraviolet light. The goal of this project was to explore the potential to tag simulated nuclear fuel cladding with small ceramic particles, via laser beam welding or gas tungsten arc welding, and measure the photoluminescent response. Surface tagging using this method has demonstrated viability and detectability throughout this project; work in FY24 focused on the survivability of these tags through subsequent deformation processing similar to what taggants in a fuel manufacturing environment would be subjected to. This work demonstrated that particles are readily visible in the as-welded state (i.e., before subsequent rolling treatment to represent mechanical processing of a fuel material), but visibility is reduced as the deformation is induced. Despite the reduction in photoluminescence, the taggants are still visible after rolling processes are performed, making this surface tagging technique a promising candidate for nuclear fuel cladding tagging. This work demonstrated, though, that targeted optimization work would be necessary to develop a robust taggant depending on the fidelity and luminescent properties required.

36 MATERIALS SCIENCE↗

Gas Metal Arc /GMA/ weld torch proximity control

Adjustable transducer probe, which is attached to a welding torch and maintains a preset touch-to-work distance, accurately follows irregular surfaces, is less sensitive to heat and static interference, and has more positive response because of electro-mechanical control.

Hawkes, E. D.↗