Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “WEAR”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

GTRF Cladding Wear Modeling and Experimental Validation

Coolant flow-induced relative motions between certain structural components in the cores of lightwater nuclear reactor cores, a phenomenon called Grid-To-Rod Fretting (GTRF), can result in progressive wear damage. Wear-through of the cladding on fuel rods can introduce radioactive species into the coolant loop. Such an event is termed a “leaker” and may cause premature and expensive reactor shut-down. GTRF results in wear scars of various sizes, shapes, and depths on the sides of the fuel rod cladding. Fretting damage may also occur on the springs and dimples that hold the fuel rods in place, resulting in the formation of gaps. Due to variability in the operating conditions of the reactor (burn-up rates and operating campaigns) and the associated variable cladding surface oxide film growth and removal rates, the wear coefficient is unlikely to remain constant over time. Therefore, constant wear rate models do not accurately account for transients in the operating conditions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Friction and wear of nuclear graphite exposed to molten FLiNaK salt environment

This report formally documents the completion of the Advanced Reactor Technologies Level 3 Milestone (M3TG-25OR0501104), “Initiate graphite wear studies of graphite samples exposed to molten salt environment,” due August 1, 2025. The report summarizes the ongoing activities aimed at characterizing the friction and wear behavior of graphite in molten LiF–NaF–KF (FLiNaK) salt environment. The wear and friction behavior of self-mated ET-10 nuclear graphite were tested at varying temperatures (550°C and 650°C), contact loads (40 and 80 N) and sliding speeds (1 and 10 mm/s) in a controlled argon environment. The results were compared to the wear and friction behavior of the same graphite material in a dry argon environment. This report presents initial studies on the friction and wear behavior of graphite in sliding contact mode, with future work focused on investigating the graphite matrix materials, as well as rolling and impact contact modes. The outcomes of this report could provide insights into assessing the integrity of the graphitic components of pebble-bed fluoride salt–cooled high-temperature reactors (PB-FHRs) to enhance their safe operation.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

A fundamental review of the friction and wear behavior of ceramics

The basic concepts associated with the friction and wear of materials are discussed as they relate to ceramics. Properties of ceramics such as crystal structure, crystallographic orientation, mechanical deformation, and surface chemistry are reviewed as they influence friction and wear. Both adhesive and abrasive wear of ceramics are discussed. The friction and wear of ceramics are examined in contact with themselves and when in contact with metals. The influences of environmental constituents such as water and hydrocarbons on friction and wear are reviewed. Materials discussed, by way of example, include aluminum oxide, rutile, calcium fluoride, and lithium fluoride.

Buckley, D. H.↗

A fundamental review of the friction and wear behavior of ceramics.

The basic concepts associated with the friction and wear of materials are discussed as they relate to ceramics. Properties of ceramics such as crystal structure, crystallographic orientation, mechanical deformation and surface chemistry are reviewed as they influence friction and wear. Both adhesive and abrasive wear of ceramics are discussed. The friction and wear of ceramics are examined in contact with themselves and when in contact with metals. The influences of environmental constituents such as water and hydrocarbons on friction and wear are reviewed. Materials discussed, by way of example, include aluminum oxide, rutile, calcium fluoride, and lithium fluoride.

Buckley, D. H.↗

Wear and related characteristics of an aircraft tire during braking

Wear and related characteristics of friction and temperature developed during braking of size 22 x 5.5, type aircraft tires are studied. The testing technique involved gearing the tire to a driving wheel of a ground vehicle to provide operations at constant slip ratios on asphalt, concrete, and slurry-seal surfaces. Data were obtained over the range of slip ratios generally attributed to an aircraft braking system during dry runway operations. The results show that the cumulative tire wear varies linearly with distance traveled and the wear rate increases with increasing slip ratio and is influenced by the runway-surface character. Differences in the wear rates associated with the various surfaces suggest that runways can be rated on the basis of tire wear. The results also show that the friction coefficients developed during fixed-slip-ratio operations are in good agreement with those obtained by other investigators during cyclic braking, in that the dry friction is insensitive to the tire tread temperature is shown to increase with increasing slip ratio and, at the higher ratios, to be greater during braking on asphalt and slurry seal than on concrete.

Mccarty, J. L.↗

Dynamic-scanning-electron-microscope study of friction and wear

A friction and wear apparatus was built into a real time scanning electron microscope (SEM). The apparatus and SEM comprise a system which provides the capability of performing dynamic friction and wear experiments in situ. When the system is used in conjunction with dispersive X-ray analysis, a wide range of information on the wearing process can be obtained. The type of wear and variation with speed, load, and time can be investigated. The source, size, and distribution of wear particles can be determined and metallic transferal observed. Some typical results obtained with aluminum, copper, and iron specimens are given.

Brainard, W. A.↗

Friction and wear of carbon-graphite materials for high energy brakes

Caliper-type brakes simulation experiments were conducted on seven different carbon-graphite material formulations against a steel disk material and against a carbon-graphite disk material. The effects of binder level, boron carbide (B4C) additions, graphite fiber additions, and graphite cloth reinforcement on friction and wear behavior were investigated. Reductions in binder level and additions of B4C each resulted in increased wear. The wear rate was not affected by the addition of graphite fibers. Transition to severe wear and high friction was observed in the case of graphite-cloth-reinforced carbon sliding against a disk of similar composition. This transition was related to the disruption of a continuous graphite shear film that must form on the sliding surfaces if low wear is to occur. The exposure of the fiber structure of the cloth constituent is believed to play a role in the shear film disruption.

Bill, R. C.↗

Effect of design factors on surface temperature and wear in disk brakes

The temperatures, friction, wear and contact conditions that occur in high energy disk brakes are studied. Surface and near surface temperatures were monitored at various locations in a caliper disk brake during drag type testing, with friction coefficient and wear rates also being determined. The recorded transient temperature distributions in the friction pads and infrared photographs of the rotor disk surface both showed that contact at the friction surface was not uniform, with contact areas constantly shifting due to nonuniform thermal expansion and wear. The effect of external cooling and of design modifications on friction, wear and temperatures was also investigated. It was found that significant decreases in surface temperature and in wear rate can be achieved without a reduction in friction either by slotting the contacting face of the brake pad or by modifying the design of the pad support to improve pad compliance. Both design changes result in more uniform contact conditions on the friction surface.

Santini, J. J.↗

Friction and wear properties of three hard refractory coatings applied by radiofrequency sputtering

The adherence, friction, and wear properties of thin hard refractory compound coatings applied to 440C bearing steel by radiofrequency sputtering were investigated. Friction and wear tests were done with nonconforming pin on disk specimens. The compounds examined were chromium carbide, molybdenum silicide, and titanium carbide. The adherence, friction, and wear were markedly improved by the application of a bias voltage to the bearing steel substrate during coating deposition. Analysis by X-ray photoelectron spectroscopy indicated that the improvement may be due to a reduction in impurities in bias deposited coatings. A fivefold reduction in oxygen concentration in MoSi2 coating by biasing was noted. Chromium carbide was not effective as an antiwear coating. Molybdenum silicide provided some reduction in both friction and wear. Titanium carbide exhibited excellent friction and antiwear properties at light loads. Plastic flow and transfer of the coating material onto the pin specimen appears to be important in achieving low friction and wear.

Brainard, W. A.↗

Effect of carbon content on friction and wear of cast irons

Friction and wear experiments were conducted with cast irons and wrought steels containing various amounts of carbon in the alloy structure in contact with 52100 steel. Gray cast irons were found to exhibit lower friction and wear characteristics than white cast irons. Further, gray cast iron wear was more sensitive to carbon content than was white. Wear with gray cast iron was linearly related to load, and friction was found to be sensitive to relative humidity and carbon content. The form, in which the carbon is present in the alloy, is more important, as the carbon content and no strong relationship seems to exist between hardness of these ferrous alloys and wear.

Buckley, D. H.↗

Recrystallization as a controlling process in the wear of some f.c.c. metals

Detailed examination of copper specimens after sliding against 440 C steel in liquid methane at speeds up to 25 m/s and loads of up to 2 kg showed the metal comprising the wear surface to possess a fine cell recrystallized structure. Wear proceeded by the plastic shearing of metal in this near surface region without the occurrence of visible metal transfer. A dynamic balance between the intense shear process at the surface and the nucleation of recrystallized grains was proposed to account for the behavior of the metal at the wear surface. Sliding wear experiments were also conducted on Ag, Cu-10% Al, Cu-10% Sn, Ni and Al. It was found that low wear and the absence of heavy metal transfer were associated with those metals observed to undergo recrystallization nucleation without prior recovery.

Bill, R. C.↗

Friction and wear of radiofrequency-sputtered borides, silicides, and carbides

The friction and wear properties of several refractory compound coatings were examined. These compounds were applied to 440 C bearing steel surfaces by radiofrequency (RF) sputtering. The refractory compounds were the titanium and molybdenum borides, the titanium and molybdenum silicides, and the titanium, molybdenum, and boron carbides. Friction testing was done with a pin-on-disk wear apparatus at loads from 0.1 to 5.0 newtons. Generally, the best wear properties were obtained when the coatings were bias sputtered onto 440 C disks that had been preoxidized. Adherence was improved because of the better bonding of the coatings to the iron oxide formed during preoxidation. As a class the carbides provided wear protection to the highest loads. Titanium boride coatings provided low friction and good wear properties to moderate loads.

Brainard, W. A.↗

Friction and wear of carbon-graphite materials for high-energy brakes

Caliper type brake simulation experiments were conducted on seven different carbon graphite materials formulations against a steel disk material and against a carbon graphite disk material. The effects of binder level, boron carbide (B4C) additions, SiC additions, graphite fiber additions, and graphite cloth reinforcement on friction and wear behavior were investigated. Reductions in binder level, additions of B4C, and additions of SiC each resulted in increased wear. The wear rate was not affected by the addition of graphite fibers. Transition to severe wear and high friction was observed in the case of graphite-cloth-reinforced carbon sliding against a disk of similar composition. The transition was related to the disruption of a continuous graphite shear film that must form on the sliding surfaces if low wear is to occur.

Bill, R. C.↗

X-ray photoelectron spectroscopic study of surface chemistry of dibenzyl disulfide on steel under mild and severe wear conditions

X-ray photoelectron spectroscopy was used to characterize the chemical composition of 304 stainless steel surfaces run in oil containing dibenzyl disulfide under both mild and severe wear conditions. In severe wear a sulfide was formed at the expense of the normal oxide. This was due to either chemical attack on the oxide or reaction with clean metal exposed by the wear process. In the mild wear scars there was no evidence of either sulfide or mercaptide. The oxide, however, was approximately twice as thick as the normal oxide on an unworn surface. The change in surface chemistry was primarily a function of wear rate rather than load.

Wheeler, D. R.↗

Evaluation of boundary lubricants using steady-state wear and friction

A friction and wear study was made at 20 C to establish operating limits and procedures for obtaining improved reproducibility and reliability in boundary lubrication testing. Ester base and C-other base fluids were used to lubricate a pure iron rider in sliding contact with a rotating M-50 steel disk in a pin-on-disk apparatus. Results of a parametric study with varying loads and speeds slowed that satisfactory test conditions for studying the direction and wear characteristics in the boundary lubrication regime with this test device were found to be 1 kilogram load; 7 to 9 meters-per-minute (50 rpm) surface speed; dry air test atmosphere (less than 100 ppm H2O); and use of a time stepwise procedure for measuring wear. Highly reproducible steady-state wear rates resulted from the two fluid studies which had a linearity of about 99 percent after initially higher wear rates and friction coefficients during run-in periods of 20 to 40 minutes.

Loomis, W. R.↗

Elucidation of wear mechanisms by ferrographic analysis

The use of ferrographic analysis in conjunction with light and scanning electron microscopy is described for the elucidation of wear mechanisms taking place in operating equipment. Example of adhesive wear, abrasive wear, corrosive wear, rolling element fatigue, lubricant breakdown, and other wear modes are illustrated. In addition, the use of magnetic solutions to precipitate nonmagnetic debris from aqueous and nonaqueous fluids is described.

Jones, W. R., Jr.↗

Friction and wear of ceramics

The adhesion, friction, wear and lubricated behaviors of both oxide and non-oxide ceramics are reviewed. Ceramics are examined in contact with themselves, other harder materials and metals. Elastic, plastic and fracture behavior of ceramics in solid state contact is discussed. The contact load necessary to initiate fracture in ceramics is shown to be appreciably reduced with tangential motion. Both friction and wear of ceramics are anisotropic and relate to crystal structure as with metals. Grit size effects in two- and three-body abrasive wear are observed for ceramics. Both free energy of oxide formation and the d valence bond character of metals are related to the friction and wear characteristics for metals in contact with ceramics. Surface contaminants affect friction and adhesive wear. For example, carbon on silicon carbide and chlorine on aluminum oxide reduce friction while oxygen on metal surfaces in contact with ceramics increases friction. Lubrication increases the critical load necessary to initiate fracture of ceramics both in indentation and with sliding or rubbing.

Buckley, D. H.↗

Friction and wear of ceramics

The adhesion, friction, wear, and lubricated behaviors of both oxide and non-oxide ceramics are reviewed. Ceramics are examined in contact with themselves, other harder materials, and metals. Elastic, plastic, and fracture behavior of ceramics in solid state contact is discussed. The contact load necessary to initiate fracture in ceramics is shown to be appreciably reduced with tangential motion. Both friction and wear of ceramics are anisotropic and relate to crystal structure as with metals. Grit size effects in two and three body abrasive wear are observed for ceramics. Both the free energy of oxide formation and the d valence bond character of metals are related to the friction and wear characteristics for metals in contact with ceramics. Surface contaminants affect friction and adhesive wear. For example, carbon on silicon carbide and chlorine on aluminum oxide reduce friction while oxygen on metal surfaces in contact with ceramics increases friction. Lubrication increases the critical load necessary to initiate fracture of ceramics both in indentation and with sliding or rubbing.

Buckley, Donald H.↗