Tuning exciton energy and fine-structure splitting in single InAs quantum dots by applying uniaxial stress

Exciton and biexciton emission energies as well as excitonic fine-structure splitting (FSS) in single InAs/GaAs quantum dots (QDs) have been continuously tuned in situ in an optical cryostat using a developed uniaxial stress device. With increasing tensile stress, the red shift of excitonic emission is up to 5 nm; FSS decreases firstly and then increases monotonically, reaching a minimum value of approximately 10 μeV; biexciton binding energy decreases from 460 to 106 μeV. This technique provides a simple and convenient means to tune QD structural symmetry, exciton energy and biexciton binding energy and can be used for generating entangled and indistinguishable photons.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Size-Scaling of Tensile Failure Stress in a Hot-Pressed Silicon Carbide

Quasi-static Weibull strength-size scaling of hot-pressed silicon carbide is described. Two surface conditions (uniaxial ground and uniaxial ground followed by grit blasting) were explored. Strength test coupons sampled effective areas from the very small (4 x 10{sup -3} mm{sup 2}) to the very large (4 x 10{sup 4} mm{sup 2}). Equibiaxial flexure and Hertzian ring crack initiation were used for the strength tests, and characteristic strengths for several different specimen geometries were analyzed as a function of effective area. Characteristic strength was found to substantially increase with decreased effective area for both surface conditions. Weibull moduli of 9.4- and 11.7 well-represented strength-size scaling for the two ground conditions between an effective area range of 10{sup -1} and 4 x 10{sup 4} mm{sup 2}. Machining damage was observed to be the dominant flaw type over this range. However, for effective areas <10{sup -1} mm{sup 2}, the characteristic strength increased rapidly for both ground surface conditions as the effective area decreased, and one or more of the inherent assumptions behind the classical Weibull strength-size scaling were in violation in this range. The selections of a ceramic strength to account for ballistically induced tile deflection and expanding cavity modeling are considered in context with the measured strength-size scaling. The observed size-scaling is briefly discussed with reference to dynamic strength.

36 MATERIALS SCIENCE↗

Stress evolution and defect diffusion in Cu during low energy ion irradiation: Experiments and modeling

Measurements of stress generation in Cu during low energy ion irradiation show that the induced stress depends on temperature and ion flux. A steady-state compressive stress is observed during irradiation, which turns into tensile stress after the irradiation is stopped. The results cannot be explained by the incorporation of gas ions alone, and point defects generated by the ions must be considered. In this work, the authors develop a continuum model that includes ion implantation, sputtering, and defect diffusion to explain the experimental data. The authors show that the experimental results can be reproduced primarily by considering a difference in diffusivity between interstitials and vacancies.

36 MATERIALS SCIENCE↗

Size-scaling of tensile failure stress in boron carbide

Weibull strength-size-scaling in a rotary-ground, hot-pressed boron carbide is described when strength test coupons sampled effective areas from the very small (~ 0.001 square millimeters) to the very large (~ 40,000 square millimeters). Equibiaxial flexure and Hertzian testing were used for the strength testing. Characteristic strengths for several different specimen geometries are analyzed as a function of effective area. Characteristic strength was found to substantially increase with decreased effective area, and exhibited a bilinear relationship. Machining damage limited strength as measured with equibiaxial flexure testing for effective areas greater than ~ 1 mm2 and microstructural-scale flaws limited strength for effective areas less than 0.1 mm2 for the Hertzian testing. The selections of a ceramic strength to account for ballistically-induced tile deflection and to account for expanding cavity modeling are considered in context with the measured strength-size-scaling.

36 MATERIALS SCIENCE↗

CRADA Final Report for CRADA Number NFE-08-01671 Materials for Advanced Turbocharger Designs

Results were obtained on residual stresses in the weld of the steel shaft to the Ni-based superalloy turbine wheel for turbochargers. Neutron diffraction studies at the HFIR Residual Stress Facility showed asymmetric tensile stresses after electron-beam welding of the wheel and shaft. A post-weld heat-treatment was found to relieve and reduce the residual stresses. Results were also obtained on cast CF8C-Plus steel as an upgrade alternative to cast irons (SiMo, Ni-resist) for higher temperature capability and performance for the turbocharger housing. CF8C-Plus steel has demonstrated creep-rupture resistance at 600-950oC, and is more creep-resistant than HK30Nb, but lacks oxidation-resistance at 800oC and above in 10% water vapor. New modified CF8C-Plus Cu/W steels with Cr and Ni additions show better oxidation resistance at 800oC in 10% water vapor, and have capability to higher temperatures. For automotive gasoline engine turbocharger applications, higher temperatures are required, so at the end of this project, testing began at 1000oC and above.

diesel engine applications↗

Tensile stress-strain behavior of hybrid composite laminates

A study was made of the stress-strain response of several hybrid laminates, and the damage was correlated with nonlinear stress-strain response and ultimate strength. The fibers used in the laminates were graphite, S-glass, and Kevlar. Some laminates with graphite fibers had perforated Mylar film between plies, which lowered the interlaminar bond strength. The laminate configurations were chosen to be like those of buffer strips in large panels and fracture coupons. Longitudinal and transverse specimens were loaded in tension to failure. Some specimens were radiographed to reveal damage due to edge effects. Stress-strain response is discussed in terms of damage shown by the radiographs. Ultimate strengths are compared with simple failure criteria, one of which account for damage.

Kennedy, J. M.↗

The effect of ion plated silver and sliding friction on tensile stress-induced cracking in aluminum oxide

A Hertzian analysis of the effect of sliding friction on contact stresses in alumina is used to predict the critical load for crack generation. The results for uncoated alumina and alumina coated with ion plated silver are compared. Friction coefficient inputs to the analysis are determined experimentally with a scratch test instrument employing an 0.2 mm radius diamond stylus. A series of scratches were made at constant load increments on coated and uncoated flat alumina surfaces. Critical loads for cracking are detected by microscopic examination of cross sections of scratches made at various loads and friction coefficients. Acoustic emission (AE) and friction trends were also evaluated as experimental techniques for determining critical loads for cracking. Analytical predictions correlate well with micrographic evidence and with the lowest load at which AE is detected in multiple scratch tests. Friction/load trends are not good indicators of early crack formation. Lubrication with silver films reduced friction and thereby increased the critical load for crack initiation in agreement with analytical predictions.

Sliney, Harold E.↗

The effect of ion-plated silver and sliding friction on tensile stress-induced cracking in aluminum oxide

A Hertzian analysis of the effect of sliding friction on contact stresses in alumina is used to predict the critical load for crack generation. The results for uncoated alumina and alumina coated with ion plated silver are compared. Friction coefficient inputs to the analysis are determined experimentally with a scratch test instrument employing an 0.2 mm radius diamond stylus. A series of scratches were made at constant load increments on coated and uncoated flat alumina surfaces. Critical loads for cracking are detected by microscopic examination of cross sections of scratches made at various loads and friction coefficients. Acoustic emission (AE) and friction trends were also evaluated as experimental techniques for determining critical loads for cracking. Analytical predictions correlate well with micrographic evidence and with the lowest load at which AE is detected in multiple scratch tests. Friction/load trends are not good indicators of early crack formation. Lubrication with silver films reduced friction and thereby increased the critical load for crack initiation in agreement with analytical predictions.

Sliney, Harold E.↗

Some Observations of Solder Joint Failure Under Tensile-Compressive Stress

It has long been known that solder joints under mechanical stress are subject to failure. In early electronic systems, such failures were avoided primarily by avoiding the use of solder as a mechanical structural component. The rule was to first make sound wire connections that did not depend mechanically on solder, and only then to solder them. Careful design and miniaturization in modern electronic systems limits the mechanical stresses exerted on solder joints to values less than their yield points, and these joints have become integral parts of the mechanical structures. Unfortunately, while these joints are strong enough when new, they have proven vulnerable to fatigue failures as they age.Details of the fatigue process are poorly understood, making predictions of expected lifetimes difficult.

solder joints fatigue failure thermal cycling test↗

Piezoelectric Bolt Breakers and Bolt Fatigue Testers

A proposed family of devices for inducing fatigue in bolts in order to break the bolts would incorporate piezoelectric actuators into resonant fixtures as in ultrasonic/ sonic drills/corers and similar devices described in numerous prior NASA Tech Briefs articles. These devices were originally intended primarily for use as safer, more-reliable, more-versatile alternatives to explosive bolts heretofore used to fasten spacecraft structures that must subsequently be separated from each other quickly on command during flight. On Earth, these devices could be used for accelerated fatigue testing of bolts. Fatigue theory suggests that a bolt subjected to both a constant-amplitude dynamic (that is, oscillatory) stress and a static tensile stress below the ultimate strength of the bolt material will fail faster than will a bolt subjected to only the dynamic stress. This suggestion would be applied in a device of the proposed type. The device would be designed so that the device and the bolt to be fatigue-tested or broken would be integral parts of an assembly (see figure). The static tension in the tightened bolt would apply not only the clamping force to hold the joined structures (if any) together but also the compression necessary for proper operation of the piezoelectric actuators as parts of a resonant structural assembly. The constant-amplitude dynamic stress would be applied to the bolt by driving the piezoelectric actuators with a sinusoidal voltage at the resonance frequency of longitudinal vibration of the assembly. The amplitude of the excitation would be made large enough so that the vibration would induce fatigue in the bolt within an acceptably short time. In the spacecraft applications or in similar terrestrial structural-separation applications, devices of the proposed type would offer several advantages over explosive bolts: Unlike explosive bolts, the proposed devices would be reusable, could be tested before final use, and would not be subject to catastrophic misfire. In fatigue-testing applications, devices of the proposed type would offer advantages of compactness and low cost, relative to conventional fatigue- testing apparatuses. In both structural- separation and fatigue-testing applications, bolts to be broken or tested could be instrumented with additional ultrasonic transducers for monitoring of pertinent physical properties and of fatigue failure processes.

Sherrit, Stewart↗

Study of Mechanical Properties, Microstructure, and Residual Stresses of AISI 304/304L Stainless Steel Submerged Arc Weld for Spent Fuel Dry Storage Systems

The confinement boundaries of spent nuclear fuel (SNF) canisters are typically fusion welded. Welded microstructures, strain hardening, and residual stresses combined with a chemically aggressive, chloride-rich environment led to concerns that the welded canister may be susceptible to chloride-induced stress corrosion cracking (CISCC). A comprehensive understanding of the modification of stainless steel (SS) metallurgical and mechanical properties by fusion welding could accelerate the predictive analysis of CISCC susceptibility. This paper describes a submerged arc welding (SAW) procedure that was developed and qualified on 12.7 mm (0.5 in.) thick AISI 304/304L SS to produce joints in a way similar to actual SNF canister manufacturing. This procedure has the potential to reduce the production cost and weld CISCC susceptibility by using fewer welding passes and lower heat input than current industrial applications. Global and local mechanical behaviors and properties, as well as residual stress distributions on the welded joint, were studied. The results indicate that hardness values in the fusion zone (FZ) and heat-affected zone (HAZ) are slightly higher than that of the base metal. Strain localization was presented in the HAZ before the tensile stress reached its maximum value, and then it shifted to the FZ. The specimen finally broke in the FZ. High tensile residual stresses exhibited in the FZ and the nearby HAZ suggest the highest CISCC-susceptible spots. The maximum tensile residual stresses were along the welding direction, indicating that if cracks occur, they would be perpendicular to the welding direction. This study involved developing and qualifying a SAW procedure for SNF canister production. The new procedure yielded cost savings (SAW working efficiency increased by about 80%), improved mechanical properties, and presented moderate residual stresses. Analysis revealed that the welded joint’s low-stress and high-stress damage assessments may be affected by shifts in the strain localization spot under loading.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Tensile testing and fracture mechanism analysis of polyvinyl alcohol nanofibrous webs

Abstract A tensile properties testing study was conducted to understand the influence of thickness, cross‐head speed (speed of testing), gauge length (GL; specimen test length), and sample shape on important tensile properties of polyvinyl alcohol (PVA) nanofiber webs. The effects of each testing parameter on load at break, extension at break, Young's modulus, and tensile stress–strain curve of PVA nanofiber webs are analyzed. The Welch two sample t ‐tests show the significant difference among tested data. Using interaction plots, two‐way analysis of variance, and margin mean plots, the interaction effects among testing parameters have been analyzed. Of all the factors, cross‐head speed, the interaction among GL, and sample thickness (GL: Thickness) and the interaction among GL, testing speed and sample thickness (GL: Speed: Thickness) have significant influence on the tensile properties of PVA nanofiber webs. Moreover, the hypothesized model of mechanism of tensile strain–stress curve of PVA nanofiber webs has been proposed. Based on the model, the tensile strain–stress curve can be split into three stages: linear elastic, partial break up, and complete breakage. This study will provide a better understanding of tensile testing parameters' effects and their interaction effects on the tensile properties of nanowebs.

Lou, Lihua↗

Microstructure, Hardness, and Residual Stress of the Dissimilar Metal Weldments of SA508-309L/308L-304L

A dissimilar metal weldment consisting of SA508-309L-308L-304L is widely used in light-water nuclear reactors. These weldments demonstrate dissimilar susceptibility to stress corrosion cracking that are related to the microstructure, properties, and residual stress. In this work, microstructures, hardness, and the residual stress distribution of the dissimilar metal weldments were investigated, with the correlation of increased hardness in the heat-affected zone (HAZ) to the microstructure. 304L HAZ demonstrated similar grain morphology as the base material, and the increase in hardness was primarily attributed to the increased dislocation density. SA508 HAZ demonstrated a change of grain morphology resulting from the different peak temperatures and cooling rates. The increased hardness in the SA508 HAZ was attributed to the refined grain morphology, higher dislocation density, and higher number density of precipitates. A ~ 20–30-μm-wide martensitic zone formed at the fusion boundary of SA508-309L, where Cr-rich carbide precipitates were observed, with the average size and the number density of 44.1 ± 16.9 nm and 1.5 × 10 21 m ₋3 , respectively. In conclusion, residual stress results demonstrated the largest tensile stress at 309L butter, indicating its high cracking susceptibility.

36 MATERIALS SCIENCE↗