Dose dependence of helium bubble formation in nano-engineered SiC at 700 °C

Knowledge of radiation-induced helium bubble nucleation and growth in SiC is essential for applications in fusion and fission environments. Here we report the evolution of microstructure in nano-engineered (NE) 3C SiC, pre-implanted with helium, under heavy ion irradiation at 700 °C up to doses of 30 displacements per atom (dpa). Elastic recoil detection analysis confirms that the as-implanted helium depth profile does not change under irradiation to 30 dpa at 700 °C. While the helium bubble size distribution becomes narrower with increasing dose, the average size of bubbles remains unchanged and the density of bubbles increases somewhat with dose. These results are consistent with a long helium bubble incubation process under continued irradiation at 700 °C up to 30 dpa, similar to that reported under dual and triple beam irradiation at much higher temperatures. The formation of bubbles at this low temperature is enhanced by the nano-layered stacking fault structure in the NE SiC, which enhances point defect mobility parallel to the stacking faults. Here, this stacking fault structure is stable at 700 °C up to 30 dpa and suppresses the formation of dislocation loops normally observed under these irradiation conditions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Correlation between switching to n-type conductivity and structural defects in highly Mg-doped InN

The effect of Mg doping on the microstructure of InN epitaxial films in relation to their free-charge carrier properties has been investigated by transmission electron microscopy (TEM) and aberration corrected scanning TEM. We observe a direct correlation between Mg concentration and the formation of stacking faults. The threading dislocation density is found to be independent of Mg concentration. The critical Mg concentration for the on-set of stacking faults formation is determined and found to correlate with the switch from p- to n-type conductivity in InN. Potential mechanisms involving stacking faults and point defect complexes are invoked in order to explain the observed conductivity reversal. Finally, the stacking faults are structurally determined and their role in the reduction of the free electron mobility in highly doped InN:Mg is discussed.

36 MATERIALS SCIENCE↗

Dislocation decorrelation and relationship to deformation microtwins during creep of a y' precipitate strengthened Ni-based superalloy

The evolution of microtwins during high temperature creep deformation in a strengthened Ni-base superalloy has been investigated through a combination of creep testing, TEM characterization, theoretical modeling and computer simulation. Experimentally, microtwin nucleation sources were identified and their evolution was tracked by characterizing the deformation substructure at different stages of the creep deformation. Initially, deformation is highly localized around stress concentrators such as carbides, borides and serrated grain boundaries, which act as sources of a/2<110> matrix type dislocations. Due to microstructural effects such as fine channels between particles and low matrix stacking fault energies, the a/2<110> matrix dislocations dissociate into a/6<112> Shockley partials, which were commonly observed to be decorrelated from one another, creating extended intrinsic stacking faults in the matrix. As deformation progress further, microtwins form via partial dislocations cooperatively shearing both and phases on adjacent {111} glide planes. The TEM observations lead directly to an analysis of dislocation-precipitate interactions. Through phase field simulations and theoretical analysis based on Orowan looping, the important processes of dislocation dissociation and decorrelation are modeled in detail, providing comprehensive insight into the microstructural features and applied stress conditions that favor the microtwinning deformation mode in strengthened Ni-based superalloys.

36 MATERIALS SCIENCE↗

Deformation mechanisms in an additively manufactured dual-phase eutectic high-entropy alloy

Nanostructured metals and alloys often exhibit high strengths but at the expense of reduced ductility. Through harnessing the far-from-equilibrium processing conditions of laser powder-bed fusion (L-PBF) additive manufacturing, we develop a dual-phase nanolamellar structure comprised of FCC/L1 2 and BCC/B2 phases in a Ni 40 Co 20 Fe 10 Cr 10 Al 18 W 2 eutectic high-entropy alloy (EHEA), which exhibits a combination of ultrahigh yield strength (>1.4 GPa) and large tensile ductility (~17%). The deformation mechanisms of the additively manufactured EHEA are studied via in-situ synchrotron X-ray diffraction and high-resolution transmission electron microscopy. The high yield strength mainly results from effective blockage of dislocation motion by the high density of lamellar interfaces. The refined nanolamellar structures and low stacking fault energy (SFE) promote stacking fault (SF)-mediated deformation in FCC/L1 2 nanolamellae. The accumulation of abundant dislocations and SFs at lamellar interfaces can effectively elevate local stresses to promote dislocation multiplication and martensitic transformation in BCC/B2 nanolamellae. The cooperative deformation of the dual phases, assisted by the semi-coherent lamellar interfaces, gives rise to the large ductility of the as-printed EHEA. In addition, here we also demonstrate that post-printing heat treatment allows us to tune the non-equilibrium microstructures and deformation mechanisms. After annealing, the significantly reduced SFE and thicknesses of the FCC nanolamellae facilitate the formation of massive SFs. The dissolution of nano-precipitates in the BCC/B2 nanolamellae reduces spatial confinement and further promotes martensitic transformation to enhance work hardening. Our work provides fundamental insights into the rich variety of deformation mechanisms underlying the exceptional mechanical properties of the additively manufactured dual-phase nanolamellar EHEAs.

36 MATERIALS SCIENCE↗

Effects of neutron irradiation of Ti 3 SiC 2 and Ti 3 AlC 2 in the 121–1085 °C temperature range

Herein we report on the formation of defects in response to neutron irradiation of polycrystalline Ti 3 SiC 2 and Ti 3 AlC 2 samples exposed to doses of 0.14±0.01, 1.6±0.1, and 3.4±0.1 displacements per atom (dpa) at irradiation temperatures of 121±12, 735±6 and 1085±68 °C. After irradiation to 0.14 dpa at 121 °C and 735 °C, black spots are observed in both Ti 3 SiC 2 and Ti 3 AlC 2 . After irradiation to 1.6 and 3.4 dpa at 735 °C, basal dislocation loops, with a Burgers vector of b = ½ [0001] are observed in Ti 3 SiC 2 , with loop diameters of 21±6 and 30±8 nm for 1.6 dpa and 3.4 dpa, respectively. In Ti3AlC2, larger dislocation loops, 75±34 nm in diameter are observed after 3.4 dpa at 735 °C, in addition to stacking faults. Impurity particles of TiC, as well as stacking fault TiC platelets in the MAX phases, are seen to form extensive dislocation loops under all conditions. Voids are observed at grain boundaries and within stacking faults after 3.4 dpa irradiation, with extensive void formation in the TiC regions at 1085 °C. Remarkably, denuded zones on the order of 1 µm are observed in Ti 3 SiC 2 after irradiation to 3.4 dpa at 735 °C. Small grains, 3-5 µm in diameter, are damage free after irradiation at 1085 °C at this dose. The presence of the A-layer in the MAX phases is seen to provide enhanced irradiation tolerance. Based on these results, and up to 3.41 dpa, Ti 3 SiC 2 remains a promising candidate for high temperature nuclear applications.

36 MATERIALS SCIENCE↗

Interaction of extended dislocations with nanovoid clusters

Voids of nanoscale dimensions in irradiated metals can act as obstacles to dislocation motion and cause strengthening. In this work, nanovoid strengthening and the influences of void size, void spacing and material properties, such as stacking fault energies, on dislocation bypass mechanisms are investigated using Phase Field Dislocation Dynamics, a three-dimensional mesoscale model that predicts the minimum energy pathway taken by discrete dislocations. A broad range of face centered cubic metals (copper, nickel, silver, rhodium, and platinum) and nanovoid sizes and spacings are treated, altogether spanning void size–to–dislocation stacking fault width ratios from less than unity to ten. Material γ-surfaces, calculated from ab initio methods, are input directly into the formulation. The analysis reveals that the critical bypass stress scales linearly with the linear void fraction, effective isotropic shear modulus, and ratio of the intrinsic to unstable stacking fault energies. With only a few exceptions, the critical stress is controlled by the stress required for the leading partial to impinge the voids (to move within range of the attractive image stress field of the void). When the void diameter is nearly an order of magnitude greater than the stacking fault width, the mechanism determining critical strength shifts to the stress for the dislocation to breakaway after partially cutting the void. Furthermore, this situation corresponds to that treated by line tension models and is realized here for Pt, with a sub-nanometer stacking fault width.

36 MATERIALS SCIENCE↗

Optoelectronic and structural characterization of trapezoidal defects in 4H-SiC epilayers and the effect on MOSFET reliability

To this day, trapezoidal defects are found in clusters and high counts in wafers representing the industry standard in terms of material quality being produced. This study sheds light on the nature, origin, behavior, and impact of this defect on device yield and reliability. Trapezoidal defects in 4H-SiC epitaxial layers were investigated by photoluminescence (PL) imaging, scanning electron microscopy (SEM), cathodoluminescence spectrum imaging (CLSI), SEM electron beam induced current (EBIC) imaging, and by transmission electron microscopy (TEM) observation. The bar-shaped stacking faults were identified by the PL and CL measurements with a peak emission wavelength of 420 and 450 nm. An optoelectronic behavioral study based on the recombination enhanced dislocation glide mechanism revealed how expanding dislocations and stacking faults interact with each other. Combining the luminescence and microscopy results, the nature of the stacking faults was identified as being a combination of Shockley-type and Frank-type stacking faults. The TEM analysis showed that these defects originate from the substrate and the stacking sequences of some of the faults were determined as (…2, 4, 2…) and (…2, 3, 2…) in the Zhdanov's notation by high-resolution TEM. The origin of this defect is speculated based on our results and previous reports. The EBIC imaging showed that the high density of SFs in these towers is a strong site of carrier recombination, which presumably has an impact on the transfer characteristics of SiC devices. Furthermore, these defects have shown to impact metal oxide semiconductor field effect transistors electrical performance via an increase in the on-state resistance depending on the coverage percentage of the tower of defects in the active area of the device.

4H-SiC↗

Surface dislocation nucleation controlled deformation of Au nanowires

We investigate deformation in high quality Au nanowires under both tension and bending using in-situ transmission electron microscopy. Defect evolution is investigated during: (1) tensile deformation of 〈110〉 oriented, initially defect-free, single crystal nanowires with cross-sectional widths between 30 and 300 nm, (2) bending deformation of the same wires, and (3) tensile deformation of wires containing coherent twin boundaries along their lengths. We observe the formation of twins and stacking faults in the single crystal wires under tension, and storage of full dislocations after bending of single crystal wires and after tension of twinned wires. The stress state dependence of the deformation morphology and the formation of stacking faults and twins are not features of bulk Au, where deformation is controlled by dislocation interactions. Instead, we attribute the deformation morphologies to the surface nucleation of either leading or trailing partial dislocations, depending on the Schmid factors, which move through and exit the wires producing stacking faults or full dislocation slip. The presence of obstacles such as neutral planes or twin boundaries hinder the egress of the freshly nucleated dislocations and allow trailing and leading partial dislocations to combine and to be stored as full dislocations in the wires. We infer that the twins and stacking faults often observed in nanoscale Au specimens are not a direct size effect but the result of a size and obstacle dependent transition from dislocation interaction controlled to dislocation nucleation controlled deformation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Dislocation baskets in thick In x Ga 1–x N epilayers

Dislocation clusters have been observed in thick In x Ga 1–x N films with 0.07 ≤ x ≤ 0.12. The clusters resemble baskets with a higher indium content at their interior. Threading dislocations at the basket boundaries are of the misfit edge type, and their separation is consistent with misfit strain relaxation due to the difference in indium content between the baskets and the surrounding matrix. The interior of the base of the baskets reflects no observable dislocations connecting the threading dislocations, and often no net displacements like those due to stacking faults. We believe that the origin of these threading dislocation arrays is associated with misfit dislocations at the basal plane that dissociate, forming stacking faults. And when the stacking faults form simultaneously satisfying the crystal symmetry, the sum of their translation vectors add up to a lattice vector, or equivalently to no change in the stacking sequence, which is consistent with our observations.

36 MATERIALS SCIENCE↗

Energy minimization mechanisms of semi-coherent interfaces

In this article, we discussed energy minimization mechanisms of semi-coherent interfaces based on atomistic simulations and dislocation theory. For example, of (111) interfaces between two face centered cubic (FCC) crystals, interface comprises of two stable structures (normal FCC stacking structure and intrinsic stacking fault structure), misfit dislocations, and misfit dislocation intersections or nodes (corresponding to the high energy stacking fault (HESF) structure). According to atomistic simulations of four interfaces, we found that (1) greater spacing between misfit dislocations and/or larger slopes of generalized stacking fault energy at the stable interface structures leads to a narrower dislocation core and a higher state of coherency in the stable interfaces; (2) the HESF region is relaxed by the relative rotation and dilation/compression of the two crystals at the node. The crystal rotation is responsible for the spiral feature at the vicinity of a node and the dilation/compression is responsible for the creation of the free volume at a node; (3) the spiral feature is gradually frail and the free volume decreases with decreasing misfit dislocation spacing, which corresponds to an increase in lattice mismatch and/or a decrease in lattice rotation. Finally, the analysis method and energy minimization mechanisms explored in FCC (111) semi-coherent interfaces are also applicable for other semi-coherent interfaces.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of dislocation pile-up on size-dependent yield strength in finite single-crystal micro-samples

Recent research has explained that the steeply increasing yield strength in metals depends on decreasing sample size. In this work, we derive a statistical physical model of the yield strength of finite single-crystal micro-pillars that depends on single-ended dislocation pile-up inside the micro-pillars. We show that this size effect can be explained almost completely by considering the stochastic lengths of the dislocation source and the dislocation pile-up length in the single-crystal micro-pillars. The Hall–Petch-type relation holds even in a microscale single-crystal, which is characterized by its dislocation source lengths. Our quantitative conclusions suggest that the number of dislocation sources and pile-ups are significant factors for the size effect. They also indicate that starvation of dislocation sources is another reason for the size effect. Moreover, we investigated the explicit relationship between the stacking fault energy and the dislocation “pile-up” effect inside the sample: materials with low stacking fault energy exhibit an obvious dislocation pile-up effect. Our proposed physical model predicts a sample strength that agrees well with experimental data, and our model can give a more precise prediction than the current single arm source model, especially for materials with low stacking fault energy.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

MAGNESIUM PRECIPITATION AND DIFUSSION IN Mg+ ION IMPLANTED SILICON CARBIDE

As a candidate material for fusion reactor applications, silicon carbide (SiC) undergoes transmutation reactions under high-energy neutron irradiation with magnesium as the major metallic transmutant; the others include aluminum, beryllium and phosphorus in addition to helium and hydrogen gaseous species. Calculations by Sawan et al. predict that at a dose of ~100 dpa (displacements per atom), there is ~0.5 at.% Mg generated in SiC. The impact of these transmutants on SiC structural stability is currently unknown. This study uses ion implantation to introduce Mg into SiC. Multiaxial ion-channeling analysis of the as-produced damage state indicates a lower dechanneling yield observed along the <100> axis. The microstructure of the annealed sample was examined using high-resolution scanning transmission electron microscopy. The results show a high concentration of likely non-faulted tetrahedral voids and possible stacking fault tetrahedra near the damage peak. In addition to lattice distortion, dislocations and intrinsic and extrinsic stacking faults are also observed. Magnesium in 3C–SiC prefers to substitute for Si and it forms precipitates of cubic Mg2Si and tetragonal MgC2. The diffusion coefficient of Mg in 3C–SiC single crystal at 1573 K has been determined to be 3.8 ± 0.4E-19 m2/s.

diffusion↗

Phase-field-based calculations of the disregistry fields of static extended dislocations in FCC metals

In the continuum context, the displacements of atoms induced by a dislocation can be approximated by a continuum disregistry field. In this paper, two phase-field (PF)-based approaches and their variants are employed to calculate the disregistry fields of static, extended dislocations of pure edge and pure screw character in two face-centred cubic metals: Au and Al, which have distinct stable stacking fault energy and elastic anisotropy. A new truncated Fourier series form is developed to approximate the generalised stacking fault energy (GSFE) surface, which shows significant improvement over the previously employed Fourier series form. By measuring the intrinsic stacking fault (ISF) width and partial dislocation core size in different ways, the PF-based disregistry fields are quantitatively compared against those predicted by molecular statics. In particular, two new measures for the ISF widths are proposed and shown to overcome drawbacks of the more commonly used standards in the literature. Our calculations also show that continuum formulation of the elastic energy and the GSFE for a homogeneous surface can successfully characterise the core structure. Finally, our comparisons highlight the significance of including the gradient energy in the free energy formulation when an accurate description of the dislocation core structure is desired.

36 MATERIALS SCIENCE↗

Irradiation effects of medium-entropy alloy NiCoCr with and without pre-indentation

Medium entropy alloy NiCoCr draws great attention due to its excellent strength-ductility trade-off mechanical behavior. Its irradiation behavior at elevated temperatures has been investigated using ion beam irradiation in a temperature range of 420–580°C and transmission electron microscopy. Irradiation induced stacking fault tetrahedra were only observed at 420°C. With increasing irradiation temperature, all stacking fault tetrahedra vanished, while the size of voids and dislocation loops increased significantly. Nanoindentation-induced structural complexities, including dislocations, stacking faults and twins helped to reduce void swelling. However, at the elevated temperatures, NiCoCr is still much more susceptible to void swelling compared to high entropy alloys such as NiCoFeCrMn and NiCoFeCrPd.

36 MATERIALS SCIENCE↗

Interactions in misaligned layered materials

The deliberate introduction of stacking faults has been found to induce properties markedly distinct from those of perfectly stacked particles or sheets, with even minute deviations leading to significant alterations in material characteristics. In this review article, we discuss the effects of stacking faults – both linear and rotational – on surface structures influencing ion adsorption, particle–particle affinity governing crystal growth, friction, and electronic properties. In conclusion, our comprehensive overview sheds light on the multifaceted impact of stacking faults on these phenomena, offering insights that bridge multiple disciplines, and provides numerous interdisciplinary research questions, paving the way for future innovations.

36 MATERIALS SCIENCE↗

Pre- and post-annealing of mechanical damage in silicon wafers

Basic properties of mechanical damage in silicon consisting of cracks and abrasion were studied using transmission electron microscopy. The crystallographic structure of mechanical damage was determined before and after high temperature annealing. The main findings include that stresses in silicon around crack tips are not plastically relieved at room temperature and that abrasion at room temperature introduces shear loops into the silicon. It was also found that cracks of micron size can be annealed out, specifically, if cleavage occurs on 111 planes. The healing products of such cracks are 60 deg and 90 deg dislocations. Submicron cracks transform into stacking faults during annealing. Likewise high concentrations of shear loops due abrasion were found to anneal into stacking faults. A one to one correlation between surface areas containing small cracks and stacking faults was made. Measurements of damage removal on silicon surfaces through chemical-mechanical etching techniques are presented. It is shown that silicon dioxide repolishes damaged silicon surfaces most effectively.

Schwottke, G. H.↗