At least 199 records · Page 11

Delineating the Impact of Transition‐Metal Crossover on Solid‐Electrolyte Interphase Formation with Ion Mass Spectrometry

Abstract Lithium‐metal batteries (LMB) employing cobalt‐free layered‐oxide cathodes are a sustainable path forward to achieving high energy densities, but these cathodes exhibit substantial transition‐metal dissolution during high‐voltage cycling. While transition‐metal crossover is recognized to disrupt solid‐electrolyte interphase (SEI) formation on graphite anodes, experimental evidence is necessary to demonstrate this for lithium‐metal anodes. In this work, advanced high‐resolution 3D chemical analysis is conducted with time‐of‐flight secondary‐ion mass spectrometry (TOF‐SIMS) to establish spatial correlations between the transition metals and electrolyte decomposition products found on cycled lithium‐metal anodes. Insights into the localization of various chemistries linked to crucial processes that define LMB performance, such as lithium deposition, SEI growth, and transition‐metal deposition are deduced from a precise elemental and spatial analysis of the SEI. Heterogenous transition‐metal deposition is found to perpetuate both heterogeneous SEI growth and lithium deposition on lithium‐metal anodes. These correlations are confirmed across various lithium‐metal anodes that are cycled with different cobalt‐free cathodes and electrolytes. An advanced electrolyte that is stable to higher voltages is shown to minimize transition‐metal crossover and its effects on lithium‐metal anodes. Overall, these results highlight the importance of maintaining uniform SEI coverage on lithium‐metal anodes, which is disrupted by transition‐metal crossover during operation at high voltages.

Chemistry↗

Control of Two Solid Electrolyte Interphases at the Negative Electrode of an Anode‐Free All Solid‐State Battery based on Argyrodite Electrolyte

Abstract Anode‐free all solid‐state batteries (AF‐ASSBs) employ “empty” current collector with three active interfaces that determine electrochemical stability; lithium metal – Solid electrolyte (SE) interphase (SEI‐1), lithium – current collector interface, and collector – SE interphase (SEI‐2). Argyrodite Li 6 PS 5 Cl (LPSCl) solid electrolyte (SE) displays SEI‐2 containing copper sulfides, formed even at open circuit. Bilayer of 140 nm magnesium/30 nm tungsten (Mg/W‐Cu) controls the three interfaces and allows for state‐of‐the‐art electrochemical performance in half‐cells and fullcells. AF‐ASSB with NMC811 cathode achieves 150 cycles with Coulombic efficiency (CE) above 99.8%. With high mass‐loading cathode (8.6 mAh cm −2 ), AF‐ASSB retains 86.5% capacity after 45 cycles at 0.2C. During electrodeposition of Li, gradient Li‐Mg solid solution is formed, which reverses upon electrodissolution. This promotes conformal wetting/dewetting by Li and stabilizes SEI‐1 by lowering thermodynamic driving force for SE reduction. Inert refractory W underlayer is required to prevent ongoing formation of SEI‐2 that also drives electrochemical degradation. Inert Mo and Nb layers likewise protect Cu from corroding, while Li‐alloying layers (Mg, Sn) are less effective due to ongoing volume changes and associated pulverization. Mechanistic explanation for observed Li segregation within alloying Li x Mg layer is provided through mesoscale modelling, considering opposing roles of diffusivity differences and interfacial stresses.

Wang, Yixian [Materials Science and Engineering Pr↗

Solvation Rule for Solid‐Electrolyte Interphase Enabler in Lithium‐Metal Batteries

Abstract Despite the exceptionally high energy density of lithium metal anodes, the practical application of lithium‐metal batteries (LMBs) is still impeded by the instability of the interphase between the lithium metal and the electrolyte. To formulate a functional electrolyte system that can stabilize the lithium‐metal anode, the solvation behavior of the solvent molecules must be understood because the electrochemical properties of a solvent can be heavily influenced by its solvation status. We unambiguously demonstrated the solvation rule for the solid‐electrolyte interphase (SEI) enabler in an electrolyte system. In this study, fluoroethylene carbonate was used as the SEI enabler due to its ability to form a robust SEI on the lithium metal surface, allowing relatively stable LMB cycling. The results revealed that the solvation number of fluoroethylene carbonate must be ≥1 to ensure the formation of a stable SEI in which the sacrificial reduction of the SEI enabler subsequently leads to the stable cycling of LMBs.

Su, Chi‐Cheung↗

An Inorganic‐Rich Solid Electrolyte Interphase for Advanced Lithium‐Metal Batteries in Carbonate Electrolytes

Abstract In carbonate electrolytes, the organic–inorganic solid electrolyte interphase (SEI) formed on the Li‐metal anode surface is strongly bonded to Li and experiences the same volume change as Li, thus it undergoes continuous cracking/reformation during plating/stripping cycles. Here, an inorganic‐rich SEI is designed on a Li‐metal surface to reduce its bonding energy with Li metal by dissolving 4 m concentrated LiNO 3 in dimethyl sulfoxide (DMSO) as an additive for a fluoroethylene‐carbonate (FEC)‐based electrolyte. Due to the aggregate structure of NO 3 − ions and their participation in the primary Li + solvation sheath, abundant Li 2 O, Li 3 N, and LiN x O y grains are formed in the resulting SEI, in addition to the uniform LiF distribution from the reduction of PF 6 − ions. The weak bonding of the SEI (high interface energy) to Li can effectively promote Li diffusion along the SEI/Li interface and prevent Li dendrite penetration into the SEI. As a result, our designed carbonate electrolyte enables a Li anode to achieve a high Li plating/stripping Coulombic efficiency of 99.55 % (1 mA cm −2 , 1.0 mAh cm −2 ) and the electrolyte also enables a Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) full cell (2.5 mAh cm −2 ) to retain 75 % of its initial capacity after 200 cycles with an outstanding CE of 99.83 %.

Liu, Sufu↗

Solvation Rule for Solid-Electrolyte Interphase Enabler in Lithium-Metal Batteries

Despite the exceptionally high energy density of lithium metal anodes, the practical application of lithium-metal batteries (LMBs) is still impeded by the instability of the interphase between the lithium metal and the electrolyte. To formulate a functional electrolyte system that can stabilize the lithium-metal anode, the solvation behavior of the solvent molecules must be understood because the electrochemical properties of a solvent can be heavily influenced by its solvation status. Here, we unambiguously demonstrated the solvation rule for the solid-electrolyte interphase (SEI) enabler in an electrolyte system. In this study, fluoroethylene carbonate was used as the SEI enabler due to its ability to form a robust SEI on the lithium metal surface, allowing relatively stable LMB cycling. The results revealed that the solvation number of fluoroethylene carbonate must be ≥ 1 to ensure the formation of a stable SEI in which the sacrificial reduction of the SEI enabler subsequently leads to the stable cycling of LMBs.

25 ENERGY STORAGE↗

An Inorganic-Rich Solid Electrolyte Interphase for Advanced Lithium-Metal Batteries in Carbonate Electrolytes

In carbonate electrolytes, the organic-inorganic solid electrolyte interphase (SEI) formed on the lithium (Li) metal anode surface is strongly bonded to Li and experiences the same volume change as Li, thus it undergoes continuous cracking/reformation during plating/stripping cycles. Here we report, an inorganic-rich SEI is designed on a Li metal surface to reduce its bonding energy with Li metal by dissolving 4 M concentrated LiNO 3 in dimethyl sulfoxide (DMSO) as an additive for a fluoroethylene carbonate (FEC) based electrolyte. Due to the aggregate structure of NO 3 - ions and its participation in the primary Li + solvation sheath, abundant Li 2 O, Li 3 N, and LiN x O y grains are formed in the resulting SEI, in addition to the uniform LiF distribution from the reduction of PF 6 - ions. The inorganic-rich SEI’s weak bonding (high interface energy) to Li can effectively promote Li diffusion along the SEI/Li interface and prevent Li dendrite penetration into the SEI. As a result, our designed carbonate electrolyte enables a Li anode to achieve a high Li plating/stripping CE of 99.55% (1 mA cm -2 , 1.0 mAh cm -2 ) and the electrolyte also enables a Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) full cell (2.5 mAh cm -2 ) to retain 75%of its initial capacity after 200 cycles with an outstanding CE of 99.83%.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Resolving Graphite‐Electrolyte Interphase of Lithium‐Ion Batteries using Air‐Tight Ambient Mass Spectrometry

Abstract The formation of a stable solid electrolyte interphase (SEI) at graphite electrode is necessary for lithium‐ion batteries (LIB) to prevent excessive degradation of electrolytes. Until now, the exact organic composition of SEI has not been decisively determined with lithium ethylene mono‐carbonate (LEMC) being one of the debated components. An air‐tight ambient mass spectrometry (MS) platform is developed to directly characterize the air‐sensitive organic components present in SEI. Ionization occurs via a solvent‐free field‐induced process at atmospheric pressure. Our experimental data, based on tandem MS analysis, revealed LEMC to be the major organic component in SEI. This result resolves a long‐standing mystery surrounding the composition of native SEI in LIB, where no trace of the other debated compound, lithium ethylene dicarbonate, was detected. The energetics of fragmentation of LEMC and the corresponding stabilities of various ionic species detected during the air‐tight ambient MS analysis were calculated using density functional theory (DFT). Our findings confirmed favorable protonation energies and suggested the molecular structures for many of the detected species. Solvent (i. e., ethylene carbonate)‐induced stabilization effects observed during the ionization process were also confirmed by DFT. The reported study encourages the routine use of ambient mass spectrometry to characterize both anodic and cathodic electrodes of all battery types as well as to study other air‐sensitive materials in their native state.

25 ENERGY STORAGE↗

Automatic Generation of Chemical Mechanisms for Electrochemical Systems: Solid Electrolyte Interphase Formation in Lithium Batteries

Electrolytes in many lithium ion batteries decompose at the low potentials near the anode. The decomposition products form a layer termed the solid electrolyte interphase (SEI). The composition and growth of the SEI layer significantly affect both the capacity fade and safety of lithium ion batteries. However, SEI formation and growth kinetics are not well understood. In this work, we present an extension of the Reaction Mechanism Generator (RMG) software to automatically generate mechanisms for SEI formation. We extend RMG’s solvation correction framework to account for kinetic solvent effects and demonstrate the accuracy of our technique. We calculate thermochemical parameters for 252 species and rate coefficients for 69 reactions, most with associated solvation corrections. This and additional quantum chemistry data are used to extend RMG’s thermodynamic group additivity and solute parameter estimation schemes to handle lithiated species and add 14 new reaction families to RMG. RMG is additionally extended to simulate electrocatalytic systems. Lastly, we demonstrate RMG on the decomposition of acetonitrile and ethylene carbonate near a battery anode. Furthermore, while this framework does not yet resolve individual ions, as appropriate thermochemistry estimators are not available, and thus, cannot yet resolve more complex electrochemical pathways, RMG is able to generate reasonable pathways for SEI formation that match literature pathways and products. In particular, RMG identifies a new important reaction pathway that is not present in literature.

Chemical reactions↗

Resolving Current-Dependent Regimes of Electroplating Mechanisms for Fast Charging Lithium Metal Anodes

Poor fast-charge capabilities limit the usage of rechargeable Li metal anodes. Understanding the connection between charging rate, electroplating mechanism, and Li morphology could enable fast-charging solutions. In this report we develop a combined electroanalytical and nanoscale characterization approach to resolve the current-dependent regimes of Li plating mechanisms and morphology. Measurement of Li + transport through the solid electrolyte interphase (SEI) shows that low currents induce plating at buried Li||SEI interfaces, but high currents initiate SEI-breakdown and plating at fresh Li||electrolyte interfaces. The latter pathway can induce uniform growth of {110}-faceted Li at extremely high currents, suggesting ion-transport limitations alone are insufficient to predict Li morphology. At battery relevant fast-charging rates, SEI-breakdown above a critical current density produces detrimental morphology and poor cyclability. Thus, prevention of both SEI-breakdown and slow ion-transport in the electrolyte is essential. This mechanistic insight can inform further electrolyte engineering and customization of fast-charging protocols for Li metal batteries.

25 ENERGY STORAGE↗

Surface SiO 2 Thickness Controls Uniform-to-Localized Transition in Lithiation of Silicon Anodes for Lithium-Ion Batteries

Silicon is a promising anode material for lithium-ion batteries because of its high capacity, but its widespread adoption has been hampered by a low cycle life arising from mechanical failure and the absence of a stable solid–electrolyte interphase (SEI). Understanding SEI formation and its impact on cycle life is made more complex by the oxidation of silicon materials in air or during synthesis, which leads to SiO x coatings of varying thicknesses that form the true surface of the electrode. Here, the lithiation of SiO 2 -coated Si is studied in a controlled manner using SiO 2 coatings of different thicknesses grown on Si wafers via thermal oxidation. SiO 2 thickness has a profound effect on lithiation: below 2 nm, SEI formation followed by uniform lithiation occurs at positive voltages versus Li/Li + . Si lithiation is reversible, and SiO 2 lithiation is largely irreversible. Above 2 nm SiO 2 , voltammetric currents decrease exponentially with SiO 2 thickness. For 2–3 nm SiO 2 , SEI formation above 0.1 V is suppressed, but a hold at low or negative voltages can initiate charge transfer whereupon SEI formation and uniform lithiation occur. Cycling of Si anodes with an SiO 2 coating thinner than 3 nm occurs at high Coulombic efficiency (CE). If an SiO 2 coating is thicker than 3–4 nm, the behavior is totally different: lithiation at positive voltages is strongly inhibited, and lithiation occurs at poor CE and is highly localized at pinholes which grow over time. As they grow, lithiation becomes more facile and the CE increases. Pinhole growth is proposed to occur via rapid transport of Li along the SiO 2 /Si interface radially outward from an existing pinhole, followed by the lithiation of SiO 2 from the interface outward.

25 ENERGY STORAGE↗

Impact of dual-layer solid-electrolyte interphase inhomogeneities on early-stage defect formation in Si electrodes

While intensive efforts have been devoted to studying the nature of the solid-electrolyte interphase (SEI), little attention has been paid to understanding its role in the mechanical failures of electrodes. Here we unveil the impact of SEI inhomogeneities on early-stage defect formation in Si electrodes. Buried under the SEI, these early-stage defects are inaccessible by most surface-probing techniques. With operando full field diffraction X-ray microscopy, we observe the formation of these defects in real time and connect their origin to a heterogeneous degree of lithiation. This heterogeneous lithiation is further correlated to inhomogeneities in topography and lithium-ion mobility in both the inner- and outer-SEI, thanks to a combination of operando atomic force microscopy, electrochemical strain microscopy and sputter-etched X-ray photoelectron spectroscopy. Our multi-modal study bridges observations across the multi-level interfaces (Si/LixSi/inner-SEI/outer-SEI), thus offering novel insights into the impact of SEI homogeneities on the structural stability of Si-based lithium-ion batteries. Severe structural deformation during (de)lithiation is the main factor limiting the stability of Si anodes in Li-ion batteries. Here, a multi-modal approach is used to visualize these deformations in their early-stage and link them to inhomogeneities in the dual-layer solid-electrolyte interphase.

25 ENERGY STORAGE↗

Real-time mass spectrometric characterization of the solid–electrolyte interphase of a lithium-ion battery

Solid-electrolyte interphase (SEI) is a key component that dictates the performance of most electrochemical devices, but the understanding of its chemistry and structure has been limited by the lack of in-situ tools. In this work, we report SEI live-formation in Li-ion battery under operando condition with liquid secondary ion mass spectrometry (SIMS), which, in combination with molecular dynamics (MD) simulation, presents the first dynamic picture with molecular-accuracy about this key component. Before any interphasial chemistry occurs during the initial charging, an electric double layer forms at the electrode-electrolyte interface via the self-assembly of solvent molecules directed by both Li+ and potential of the electrified surface. Such double layer structure predicts the eventual interphasial chemistries formed from the electrolytes, where the negatively-charged electrode surface repels salt anions from the inner-Helmholtz layer and results in an inner SEI that is thin, dense and inorganic in nature but LiF-depleted. It was this dense layer that exercises the major functions of an interphase, i.e., conducting Li+ but insulating electrons. An outer layer that is electrolyte-permeable and organic-rich appears after formation of the inner SEI. In highly-concentrated electrolyte, the presence of LiF in the inner-SEI is raised due to the high population of salt anions in the double layer. These real-time observations at nano-scale reveal in general sense how an interphase inherits chemistry from inner-Helmholtz layer structure, and establish guidelines in engineering desirable interphases for the future battery chemistries.

Zhou, Yufan↗

Analysis of an all-solid state nanobattery using molecular dynamics simulations under an external electric field

Present Li-ion battery (LIB) technology requires strong improvements in performance, energy capacity, charging-time, and cost to expand their application to e-mobility and grid storage. Li-metal is one of the most promising materials to replace commercial anodes such as graphite because of its 10 times higher specific capacity. However, Li-metal has high reactivity with commercial liquid electrolytes; thus, new solid materials are proposed to replace liquid electrolytes when Li-metal anodes are used. We present a theoretical analysis of the charging process in a full nanobattery, containing a LiCoO 2 cathode, a Li 7 P2S 8 I solid-state electrolyte (SSE), a Li-metal anode as well as Al and Cu collectors for the cathode and anode, respectively. In addition, we added a Li 3 P/Li 2 S film as a solid electrolyte interphase (SEI) layer between the Li-anode and SSE. Thus, we focus this study on the SEI and SSE. We simulated the charging of the nanobattery with an external voltage by applying an electric field. We estimated temperature profiles within the nanobattery and analyzed Li-ion transport through the SSE and SEI. Here, we observed a slight temperature rise at the SEI due to reactions forming $PS_{3}^{–}$ and $P_{2}S_{7}^{4}$$^{–}$ fragments at the interfaces; however, this temperature profile changes due to the charging current under the presence of the external electric field ε = 0.75 V Å –1 . Without the external field, the calculated open-circuit voltage (OCV) was 3.86 V for the battery, which is within the range of values of commercial cobalt-based LIBs. This voltage implies a spontaneous fall of available Li-ions from the anode to the cathode (during discharge). The charge of this nanobattery requires overcoming the OCV plus an additional voltage that determines the charging current. Thus, we applied an external potential able to neutralize the OCV, plus an additional 1.6 V to induce the transport of Li + from the cathode up to the anode. Several interesting details about Li + transport paths through the SSE and SEI are discussed.

25 ENERGY STORAGE↗

Solvent oligomerization pathways facilitated by electrolyte additives during solid-electrolyte interphase formation

The solid–electrolyte interphase (SEI) layer formation is known to play an important role in determining the lifetime of lithium-ion batteries. A thin, stable SEI layer is linked to overall improved battery performance and longevity, however, the factors and mechanisms that lead to optimal SEI morphology and composition are not well understood. Inclusion of electrolyte additives (fluoroethylene carbonate, FEC; and vinylene carbonate, VC) is often necessary for improving SEI characteristics. To understand how these electrolyte additives impact SEI formation, we employed molecular dynamics (MD) and density functional theory (DFT) simulations to study the reaction networks and oligomerization pathways, respectively, for three systems containing ethylene carbonate (EC), a lithium ion, and FEC or VC. MD simulations suggest radical oligomerization pathways analogous to traditional oligomerization with nucleophilic alkoxide species via SN1 reaction mechanisms. Both S N 1 and S N 2 mechanisms were studied for all three systems using DFT. Oligomerization reactions were studied with both a standard alkoxide species and a ring-opened EC radical as the nucleophiles and EC, FEC, and VC as the electrophiles. For all cases, FEC and VC exhibited lower free energy barriers and more stable adducts when compared with EC. We conclude that one of the role of additives is to modify the oligomerization process of EC by introducing branching points (FEC) or termination points (VC).

25 ENERGY STORAGE↗

Interfacial solvation-structure regulation for stable Li metal anode by a desolvation coating technique

Rechargeable lithium (Li) metal batteries face challenges in achieving stable cycling due to the instability of the solid electrolyte interphase (SEI). The Li-ion solvation structure and its desolvation process are crucial for the formation of a stable SEI on Li metal anodes and improving Li plating/stripping kinetics. This research introduces an interfacial desolvation coating technique to actively modulate the Li-ion solvation structure at the Li metal interface and regulate the participation of the electrolyte solvent in SEI formation. Through experimental investigations conducted using a carbonate electrolyte with limited compatibility to Li metal, the optimized desolvation coating layer, composed of 12-crown-4 ether-modified silica materials, selectively displaces strongly coordinating solvents while simultaneously enriching weakly coordinating fluorinated solvents at the Li metal/electrolyte interface. This selective desolvation and enrichment effect reduce solvent participation to SEI and thus facilitate the formation of a LiF-dominant SEI with greatly reduced organic species on the Li metal surface, as conclusively verified through various characterization techniques including XPS, quantitative NMR, operando NMR, cryo-TEM, EELS, and EDS. The interfacial desolvation coating technique enables excellent rate cycling stability (i.e., 1C) of the Li metal anode and prolonged cycling life of the Li||LiCoO 2 pouch cell in the conventional carbonate electrolyte (E/C 2.6 g/Ah), with 80% capacity retention after 333 cycles.

42 ENGINEERING↗

Atomistic modeling of LiF microstructure ionic conductivity and its influence on nucleation and plating

We report the formation and degradation of the solid electrolyte interphase (SEI) and its underlying transport properties play an essential role in the overall performance of lithium-ion batteries. This paper presents classical molecular dynamics studies on polycrystalline inorganic lithium fluoride (LiF) layers to model and predict the SEI transport properties. The ionic conductivity is obtained from the lithium-ion diffusivity in polycrystalline structures of LiF using the Nernst-Einstein relation. The predicted molecular dynamics data are used in a continuum scale phase-field model to evaluate the plating kinetics under fast charging conditions. The analysis emphasizes that the SEI ionic conductivity properties impact the plating dynamics, where SEI's low ion conductivity value is prone to large plating and subsequent capacity degradation. The combination of atomic and continuum scale studies shown herein lays a foundation to tune in SEI transport properties to decrease the amount of lithium plating and improve the performance of fast-charging batteries.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Engineering Solid Electrolyte Interphase Composition by Assessing Decomposition Pathways of Fluorinated Organic Solvents in Lithium Metal Batteries

Studies have shown fluorinated electrolyte solvents can form desirable solid electrolyte interphase (SEI) in lithium metal batteries. In this study, we develop a detailed mechanistic understanding of two high performing electrolytes, Fluoroethylene Carbonate (FEC) and Difluoroethylene Carbonate (DFEC) to demonstrate minimal structural variations can lead to different decomposition products, and thereby the nature of the SEI. Using density functional theory (DFT) calculations, we find different initial bond-breaking mechanisms between FEC and DFEC. We develop free energy diagrams for the decomposition pathways including both electrochemical and chemical steps. Using the computational Li electrode, we identify the largest limiting potential of 1.77 V for FEC decomposition, associated with the formation of lithium fluoride, lithium oxide and FEC oligomers, and 1.53 V for DFEC, which correspond to the formation of polymerized vinylene carbonate and lithium fluoride. We suggest the formation of oligomers in the case of FEC instead of long polymers may lead to better SEI compactness. We also demonstrate the SEI components of FEC and DFEC are not stable on typical cathode voltage (3.87 V). This study presents a unified electrocatalytic perspective on SEI formation and decomposition.

25 ENERGY STORAGE↗

The Solid Electrolyte Interphase Dispersion Can Predict Cycle and Calendar Lifetimes in Silicon Anodes for Lithium-Ion Batteries

The solid electrolyte interphase (SEI) plays a critical role in lithium-ion battery (LIB) anodes. It is responsible for passivating the reactive surface of lithiated anodes against degradation of the electrolyte which enables long cycle and calendar lifetimes for LIBs. This role is especially important in high energy density anodes like silicon, that undergo massive volumetric changes during electrochemical cycling. The mechanism by which the SEI performs this role, however, is not clear which makes designing an SEI to passivate silicon anodes impossible. Through decades of research, dozens of chemical species have been identified within the SEI ranging from inorganic solids to polymeric coatings all of which simultaneously exist in a 'mosaic' composition at the anode surface. This mosaic creates a highly dispersive environment in which electrostatic screening of the anode surface from the electrolyte is not always complete. Here, we present an electrochemical technique to directly test the dispersion at the anode surface. We use this technique to screen more than 20 different electrolytes against silicon anodes and find correlations between both the cycle life and calendar life. The insights from this study offer a new framework to think about the SEI and a rapid screening method to test novel electrode/electrolyte combinations.