Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ROLL”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Hot Rolling of ZK60 Magnesium Alloy with Isotropic Tensile Properties from Tubing Made by Shear Assisted Processing and Extrusion (ShAPE)

In the present work, we utilized Shear Assisted Processing and Extrusion (ShAPE), a solid-phase processing technique, to extrude hollow tubes of ZK60 Mg alloy. Hot rolling was performed on these as-extruded tubes (after slitting them longitudinally) to thickness reductions of 37%, 68%, and 93% to investigate their viability as rolling feedstock material. EBSD analysis showed the formation of twinned grains in the ShAPE processed material and a gradual re-orientation of the basal texture parallel to the extrusion direction with each rolling step. Moreover, an equiaxed grain size of 5.15 ± 3.39 μm was obtained in the ShAPE extruded material, and the microstructure was retained even after 93% rolling reduction. The rolled sheets also showed excellent tensile strengths and no mechanical anisotropy, a critical characteristic for formability. The unique microstructures developed and their excellent mechanical properties, combined with the ease of scalability of the process, make ShAPE a promising alternative to existing methods for producing rolling feedstock material.

36 MATERIALS SCIENCE↗

Effect of rolling motion on critical heat flux for subcooled flow boiling in vertical tube

This paper presents defining characteristics of the critical heat flux (CHF) for the boiling of R-134a in vertical tube operation under rolling motion in marine reactor. It is important to predict CHF of marine reactor having the rolling motion in order to increase the safety of the reactor. Marine Reactor Moving Simulator (MARMS) tests are conducted to measure the critical heat flux using R-134a flowing upward in a uniformly heated vertical tube under rolling motion. MARMS was rotated by motor and mechanical power transmission gear. The CHF tests were performed in a 9.5 mm I.D. test section with heated length of 1 m. Mass fluxes range from 285 to 1300 kg m{sup -2}s{sup -1}, inlet subcooling from 3 to 38 deg. C and outlet pressures from 13 to 24 bar. Amplitudes of rolling range from 15 to 40 degrees and periods from 6 to 12 sec. To convert the test conditions of CHF test using R-134a in water, Katto's fluid-to-fluid modeling was used in present investigation. A CHF correlation is presented which accounts for the effects of pressure, mass flux, inlet subcooling and rolling angle over all conditions tested. Unlike existing transient CHF experiments, CHF ratio of certain mass flux and pressure are different in rolling motion. For the mass fluxes below 500 kg m{sup -2}s{sup -1} at 13, 16 (region of relative low mass flux), CHF ratio was decreased but was increased above that mass flux (region of relative high mass flux). Moreover, CHF tend to enhance in entire mass flux at 24 bar. (authors)

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

An investigation of the microstructure and ductility of annealed cold-rolled tungsten

Tungsten is notoriously brittle metal at room temperature. Furthermore, contrary to most metals, plastic deformation increases ductility and recrystallization decreases ductility of tungsten. The fundamentals that govern this behavior have challenged academia and industry for decades. This paper focuses on understanding the controlling factors of ductility through a systematic investigation of the changes in microstructure and mechanical properties of cold-rolled tungsten that occur during annealing. Cold-rolled tungsten samples were annealed at temperatures up to 1400 °C, and mechanical testing and microstructural analysis was performed before and after annealing. Furthermore, a dislocation mobility model based on the Orowan equation was applied. The mechanisms of deformation are discussed within the context of deformed and annealed microstructures. The high fraction of low angle grain boundaries and high density of edge dislocations were found to be the most important factors for ductility. Although there were gradual changes in microstructure and mechanical properties, the ductility of cold-rolled tungsten was maintained up to 1300 °C. The material recrystallized when annealed above this temperature, had no ductility, and suffered brittle fracture. Microstructural characterizations of the as-rolled material revealed a typical BCC texture, with grains elongated in rolling direction and a large amount of edge dislocations and low angle grain boundaries. The level of texturing and the fraction of low angle grain boundaries diminished after recrystallization. It was found that, compared to the recrystallized material, as-rolled tungsten can accommodate over 7 orders of magnitude higher deformation velocity due to the high density of edge dislocations.

36 MATERIALS SCIENCE↗

Precipitation in cold-rolled Al–Sc–Zr and Al–Mn–Sc–Zr alloys prepared by powder metallurgy

The effects of cold-rolling on thermal, mechanical and electrical properties, microstructure and recrystallization behaviour of the AlScZr and AlMnScZr alloys prepared by powder metallurgy were studied. The powder was produced by atomising in argon with 1% oxygen and then consolidated by hot extrusion at 350 °C. The electrical resistometry and microhardness together with differential scanning calorimetry measurements were compared with microstructure development observed by transmission and scanning electron microscopy, X-ray diffraction and electron backscatter diffraction. Fine (sub)grain structure developed and fine coherent Al{sub 3}Sc and/or Al{sub 3}(Sc,Zr) particles precipitated during extrusion at 350 °C in the alloys studied. Additional precipitation of the Al{sub 3}Sc and/or Al{sub 3}(Sc,Zr) particles and/or their coarsening was slightly facilitated by the previous cold rolling. The presence of Sc,Zr-containing particles has a significant antirecrystallization effect that prevents recrystallization at temperatures minimally up to 420 °C. The precipitation of the Al{sub 6}Mn- and/or Al{sub 6}(Mn,Fe) particles of a size ∼ 1.0 μm at subgrain boundaries has also an essential antirecrystallization effect and totally suppresses recrystallization during 32 h long annealing at 550 °C. The texture development of the alloys seems to be affected by high solid solution strengthening by Mn. The precipitation of the Mn-containing alloy is highly enhanced by a cold rolling. The apparent activation energy of the Al{sub 3}Sc particles formation and/or coarsening and that of the Al{sub 6}Mn and/or Al{sub 6}(Mn,Fe) particle precipitation in the powder and in the compacted alloys were determined. The cold deformation has no effect on the apparent activation energy values of the Al{sub 3}Sc-phase and the Al{sub 6}Mn-phase precipitation. - Highlights: • The Mn, Sc and Zr additions to Al totally suppresses recrystallization at 550 °C. • The Sc,Zr-containing particle precipitation is slightly facilitated by cold rolling. • The Mn-containing particle precipitation is highly enhanced by cold rolling. • Cold rolling has no effect on activation energy of the Al{sub 3}Sc and Al{sub 6}Mn precipitation. • The texture development is affected by high solid solution strengthening by Mn.

36 MATERIALS SCIENCE↗

Calcium and zirconium as texture modifiers during rolling and annealing of magnesium–zinc alloys

Rolling experiments were carried out on a ternary Mg–Zn–Ca alloy and its modification with zirconium. Short time annealing of as-rolled sheets is used to reveal the microstructure and texture development. The texture of the as-rolled sheets can be characterised by basal pole figures with split peak towards the rolling direction (RD) and a broad transverse angular spread of basal planes towards the transverse direction (TD). During annealing the RD split peaks as well as orientations in the sheet plane vanish whereas the distribution of orientations tilted towards the TD remains. It is shown in EBSD measurements that during rolling bands of twin containing structures form. During subsequent annealing basal orientations close to the sheet plane vanish based on a grain nucleation and growth mechanism of recrystallisation. Orientations with tilt towards the TD remain in grains that do not undergo such a mechanism. The addition of Zr delays texture weakening. - Highlights: • Ca in Mg–Zn-alloys contributes to a significant texture weakening during rolling and annealing. • Grain nucleation and growth in structures consisting of twins explain a texture randomisation during annealing. • Grains with transverse tilt of basal planes preferentially do not undergo a grain nucleation and growth mechanism. • Zr delays the microstructure and texture development.

36 MATERIALS SCIENCE↗

Slow-roll approximation in loop quantum cosmology

The slow-roll approximation is an analytical approach to study dynamical properties of the inflationary universe. In this article, systematic construction of the slow-roll expansion for effective loop quantum cosmology is presented. The analysis is performed up to the fourth order in both slow-roll parameters and the parameter controlling the strength of deviation from the classical case. The expansion is performed for three types of the slow-roll parameters: Hubble slow-roll parameters, Hubble flow parameters and potential slow-roll parameters. An accuracy of the approximation is verified by comparison with the numerical phase space trajectories for the case with a massive potential term. The results obtained in this article may be helpful in the search for the subtle quantum gravitational effects with use of the cosmological data.

79 ASTRONOMY AND ASTROPHYSICS↗

Stochastic disks that roll

We study a model of rolling particles subject to stochastic fluctuations, which may be relevant in systems of nano- or microscale particles where rolling is an approximation for strong static friction. We consider the simplest possible nontrivial system: a linear polymer of three disks constrained to remain in contact and immersed in an equilibrium heat bath so the internal angle of the polymer changes due to stochastic fluctuations. We compare two cases: one where the disks can slide relative to each other and the other where they are constrained to roll, like gears. Starting from the Langevin equations with arbitrary linear velocity constraints, we use formal homogenization theory to derive the overdamped equations that describe the process in configuration space only. The resulting dynamics have the formal structure of a Brownian motion on a Riemannian or sub-Riemannian manifold, depending on if the velocity constraints are holonomic or nonholonomic. We use this to compute the trimer's equilibrium distribution with and without the rolling constraints. Surprisingly, the two distributions are different. We suggest two possible interpretations of this result: either (i) dry friction (or other dissipative, nonequilibrium forces) changes basic thermodynamic quantities like the free energy of a system, a statement that could be tested experimentally, or (ii) as a lesson in modeling rolling or friction more generally as a velocity constraint when stochastic fluctuations are present. In the latter case, we speculate there could be a “roughness” entropy whose inclusion as an effective force could compensate the constraint and preserve classical Boltzmann statistics. Regardless of the interpretation, our calculation shows the word “rolling” must be used with care when stochastic fluctuations are present.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Effects of Rolling Reduction on Critical Current Density and Microstructure of Bi-2212 Wires

Bi-2212 Rutherford cables have been fabricated into flat racetrack coils and canted-cosine-theta dipole magnets. The performance gap between the magnets made with Rutherford cables and the “short-sample-limit” is about 30%. To better understand the influence of Rutherford cable processing on the strand performance, we studied three Bi-2212 wires with filament architectures of 37 × 18 and 55 × 18 and diameters of 0.8 and 1.0 mm. To simulate the deformation caused by cabling process, the three wires were rolled with thickness reductions ranging from 10% to 30%. The aspect ratios of rolled strands are between 1.29 and 2.05. The low aspect-ratio wire is also an interesting form for fabricating solenoid coils with higher packing density. The round and rolled strands were heat-treated under 50 bar and with maximum heat treatment temperatures of 885.5 °C and 890.5 °C. The rolling deformation reduced filament size uniformity, resulting in filament merging in fully heat-treated wires. It was found that rolling reduction reduced wire critical current density (JE) by 16 to 18%, but the JE decrease saturated at 15 to 20% of the thickness reduction. It is believed that the reduced JE results from the filament merging caused by rolling and non-uniform shrinking during overpressure heat treatment.

Bi-2212 wire↗

SU-E-J-56: Dosimetric Impact of Patient Roll Variability in Peripheral-Lung SBRT

Purpose: Positional variation about the patient longitudinal axis may introduce deleterious effects to clinical treatment plans, the effects of which are exacerbated by hypo-fractionated treatment regimens. Our goal is to evaluate the dosimetric impact of rotational setup error in stereotactic body radiation therapy (SBRT) for peripherally-located lung lesions. Methods: Six patients who had been treated for peripheral lung lesions using varying SBRT techniques were analyzed. Each patient's planning CT was processed using custom in-house software to simulate 1, 3, and 5 degree roll in both directions about their longitudinal axis. The original plan was fused and re-calculated. Agreement between planned and error-simulated dose distributions was quantified using 3%, 3mm criteria for the 3-dimensional gamma metric, and changes in target coverage and adjacent normal anatomy were also quantified. Results: Increased rotational setup error resulted in reduced target coverage, with changes in equivalent uniform dose ranging from −1.24% to −6.11% for simulated roll greater than or equal to 3 degrees, increasing with magnitude of error and skewed for roll directed toward the involved side. Changes to normal tissue metrics are linearly related to simulated roll, with rib D(1cc) changes ranging from −4.23% to 3.27% relative to the original treatment plan. Error-simulated dose distributions demonstrate agreement by the gamma metric in the planned target of 72.56%, 81.02%, and 99.52% for 5, 3, and 1 degree simulated roll scenarios, respectively. Corresponding agreement for the regional dose in excess of 50% of the maximum were 65.71%,70.77%, and 97.88%. Conclusion: This study suggests that the ability to detect and compensate for rotational positioning variations beyond a threshold level may improve care for patients with peripherally-located lesions beyond that which may be accomplished using only translational axes. Positional error of one degree of roll had little influence, though three or more degrees of error introduced significant discrepancy.

60 APPLIED LIFE SCIENCES↗

Carbide Particle Redistribution in U10Mo Alloy during Hot Rolling Process

The influence of initial carbide particle distribution features on the evolution of particle and stringer distribution within U10Mo alloy during hot rolling was investigated in this study. This work will provide guidance to casting optimization work and identify actionable process changes to eliminate the surface features directly attributed to carbides. Various synthetic microstructure-based finite-element (FE) models were generated with consideration of different parameters (i.e., particle shape, particle volume fraction and particle distribution). Plane-strain compression loading was employed in the FE models to simulate hot rolling to 40% and 80% reductions. Stringer statistics analyses and two-point correlation functions were then performed with the simulated hot-rolling results. The results from stringer analyses show that stringer volume fraction substantially increases with increased rolling reduction for microstructure with particles distributed along grain boundaries, and that microstructures with elliptical particles may have slightly higher stringer volume fractions than those with circular particles. The results also show that the maximum stringer length can increase substantially with increased rolling reduction for microstructures with elliptical particles along grain boundaries, and that the microstructures with higher-aspect-ratio elliptical particles may have higher stringer volume fraction and higher maximum stringer length. Near-surface numbers of particles and particle volume fractions also increase with increased rolling reduction. The results from application of the two-point correlation function show that the particle shape (i.e., circular or elliptical) may not have significant influence on the overall shapes of the correlation curves, and that the correlation curves tend to show higher peaks at short distance and then gradually decrease for microstructures with higher particle volume fractions and particles distributed along grain boundaries.

36 MATERIALS SCIENCE↗

Rolled-up transformer structure for a radiofrequency integrated circuit (RFIC)

A rolled-up transformer structure comprises a multilayer sheet having a rolled configuration comprising multiple turns about a longitudinal axis. The multilayer sheet comprises more than one conductive pattern layer on a strain-relieved layer, including a first conductive film and a second conductive film separated from the first conductive film in a thickness direction. The first conductive film comprises an even number of primary conductive strips, where each primary conductive strip has a length extending in the rolling direction, and the second conductive film comprises an even number of secondary conductive strips, where each secondary conductive strip has a length extending in the rolling direction. In the rolled configuration, turns of the primary conductive strips and turns of the secondary conductive strips wrap around the longitudinal axis. The primary conductive strips serve as a primary winding and the secondary conductive strips serve as a secondary winding of the rolled-up transformer structure.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Hot rolling of thick uranium molybdenum alloys

Disclosed herein are processes for hot rolling billets of uranium that have been alloyed with about ten weight percent molybdenum to produce cold-rollable sheets that are about one hundred mils thick. In certain embodiments, the billets have a thickness of about 7/8 inch or greater. Disclosed processes typically involve a rolling schedule that includes a light rolling pass and at least one medium rolling pass. Processes may also include reheating the rolling stock and using one or more heavy rolling passes, and may include an annealing step.

36 MATERIALS SCIENCE↗

Rolled-up transformer structure for a radiofrequency integrated circuit (RFIC)

A rolled-up transformer structure comprises a multilayer sheet having a rolled configuration comprising multiple turns about a longitudinal axis. The multilayer sheet comprises more than one conductive pattern layer on a strain-relieved layer, including a first conductive film and a second conductive film separated from the first conductive film in a thickness direction. The first conductive film comprises an even number of primary conductive strips, where each primary conductive strip has a length extending in the rolling direction, and the second conductive film comprises an even number of secondary conductive strips, where each secondary conductive strip has a length extending in the rolling direction. In the rolled configuration, turns of the primary conductive strips and turns of the secondary conductive strips wrap around the longitudinal axis. The primary conductive strips serve as a primary winding and the secondary conductive strips serve as a secondary winding of the rolled-up transformer structure.

36 MATERIALS SCIENCE↗

Minimizing thickness variation in monolithic U-10Mo fuel foil and Zr interlayer during hot rolling: A microstructure-based finite element method analysis

Low-enriched uranium alloyed with 10 wt. % molybdenum (U-10Mo) has been identified as a promising alternative to highly enriched uranium fuel for the United States’ high performance research reactors. The monolithic U-10Mo fuel plate consists of a metallic U-10Mo fuel foil with a 25 µm Zr interlayer and a relatively thick cladding of aluminum alloy 6061. The Zr interlayer is typically applied during the hot co-rolling process, and this process dictates the uniformity of the Zr interlayer. Thickness variation observed in the U-10Mo and Zr interlayer has been attributed to several sources: the initial grain size of the U-10Mo castings, can materials, rolling temperature, inhomogeneous molybdenum content, and porosity in the cast U-10Mo. This thickness variation limits the ability to meet the dimensional specification; thus, a better understanding of the factors causing the nonuniform thickness is needed. In this work, we used a novel, microstructure-based finite element method to model the hot rolling process to address these concerns. Grain microstructures in U-10Mo were tessellated and explicitly considered in the finite element model. Each grain was assigned a random material property to mimic the grain strength variations induced by different grain orientations. Simulations were performed using six steel can thicknesses, four grain sizes, and with or without a Zr interlayer to investigate the influences of those variables on the thickness nonuniformity. The simulation results showed that a thinner steel can and finer U-10Mo grain size reduce thickness variations in both the U-10Mo fuel foil and Zr interlayer. The direct findings from the simulations and analysis can be used to optimize the hot rolling schedule, reduce fabrication defects, and meet the dimensional specifications. The proposed microstructure-based finite element model can be also coupled with experimental microstructure characterization data, images, and models to simulate multi-pass hot rolling.

36 MATERIALS SCIENCE↗

Evolution of Residual Stress and Distortion of Cold-Rolled Bearing Ring from Annealing to Quenched-Tempered Heat Treatment

This study investigates the correlation between the residual stress and distortion behavior of a cold-rolled ring from the annealing to quenching-tempering (QT) process. Due to the cold-rolled process, the external periphery of the bearing ring experiences a compressive residual stress. To relieve the residual stress, cold-rolled rings are annealed at 700 °C which is higher than the starting temperature of recrystallization. When cold-rolled rings are annealed at 700 °C for 15 min, the compressive residual stress is reduced to zero and the outer diameter of the annealed ring becomes larger than that of a non-annealed sample, which is unrelated to annealing time. Simultaneously, the roundness and taper deviation do not obviously change compared with those of non-annealed sample. The stress relaxation during the annealing process was attributed to the recovery and recrystallization of ferrite. Annealing has a genetic influence on the following QT heat treatment, wherein the lowest residual stress is in the non-annealed cold-rolled ring. From the annealing to QT process, the deviation of the outer diameter, roundness, and taper increased with annealing time, a large extend than that of non-annealed samples.

36 MATERIALS SCIENCE↗

Properties of Rolled AZ31 Magnesium Alloy Sheet Fabricated by Continuous Variable Cross-Section Direct Extrusion

Rolling is currently a widely used method for manufacturing and processing high-performance magnesium alloy sheets and has received widespread attention in recent years. Here, we combined continuous variable cross-section direct extrusion (CVCDE) and rolling processes. The microstructure and mechanical properties of the resulting sheets rolled at different temperatures from CVCDE extrudate were investigated by optical microscopy, scanning electron microscope, transmission electron microscopy and electron backscatter diffraction. The results showed that a fine-grained microstructure was present with an average grain size of 3.62 μm in sheets rolled from CVCDE extrudate at 623 K. Dynamic recrystallization and a large strain were induced by the multi-pass rolling, which resulted in grain refinement. In the 573-673 K range, the yield strength, tensile strength and elongation initially increased and then declined as the CVCDE temperature increased. The above results provide an important scientific basis of processing, manufacturing and the active control on microstructure and property for high-performance magnesium alloy sheet.

36 MATERIALS SCIENCE↗

Development and Characterization of a Novel Ti-Modified High-Si Medium-Mn Steel Possessing Ultra-High Strength and Reasonable Ductility After Hot Rolling

The present work systematically correlates the strength–ductility relationship of a Ti-Si-modified Fe-Mn-Al-C steel with its microstructural characteristics such as grain size, type and morphology of precipitates, and the transformation-induced plasticity (TRIP) effect during hot deformation. The Ti-Si-modified multicomponent steel developed through melting and casting route is subjected to thermo-mechanical processing such as hot forging (at 1373 K) and subsequent hot rolling (at 1173 K). An excellent combination of ultra-high tensile strength (UTS ~ 1700 ± 20 MPa), reasonable ductility (elongation ~ 11%) and high work hardening behavior (n ~ 0.89) is achieved in the hot-rolled specimen as compared to the hot-forged one (UTS ~ 824 ± 9 MPa, n ~ 0.07) with negligible change in the elongation. The better tensile properties of the hot-rolled specimen in contrast to the hot-forged one are due to the combined effects of grain refinement during rolling, twin–twin interactions, precipitation strengthening by mixture of hexagonal structured Ti{sub 3}(Al,Si)C{sub 2} and Mn-Al-Si-rich carbide precipitates and most significantly the enhanced TRIP effect. The lower critical resolved shear stress value of martensitic transformation instigates the TRIP effect during tensile testing which resulted in the increased hardness and strength of the hot-rolled specimen. The above observation offers a strong support to the proposition that TRIP effect is the dominant plasticity-enhancing mechanism activated during the deformation of the low-stacking fault energy (~ 12.2 mJ/m{sup 2}) Si-Ti-modified, medium-Mn multicomponent steel employed in the present investigation.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment and Combination of Cold Rolling and Heat Treatment on Microstructure and Mechanical Properties of Titanium Alloy Ti6Al2V2Zr1.5Mo

The heat treatment and cold rolling combinations have been carried out on titanium alloy Ti6Al2V2Zr1.5Mo, and microstructure evolution and mechanical behavior have been studied. Solution treatment below the β-transus temperature, followed by air cooling, resulted in higher microhardness/strength as compared to the same with water quenching. A sudden drop in microhardness/strength is observed in sample solution heat-treated above β-transus temperature followed by air cooling. The former is attributed to the additional presence of fine secondary α-phase formed by dynamic aging during air cooling as compared to water-quenched samples which did not have fine secondary α-phase. Solution treatment above β-transus temperature resulted in Widmanstatten microstructure with no significant fine secondary α in air-cooled samples. Among the studied conditions of cold rolling (CR), gain in strength of the alloy from annealed condition is significant with first 15% reduction and thereafter it is marginal for 30% reduction. Initiation of cracks at the edges has been observed in 30% CR. The microstructure of cold-rolled samples confirms the fragmentation of α-plates with the presence of high dislocation density. Heat treatment of cold-rolled samples resulted in significant reduction in strength from the as-cold-rolled conditions. The marginally lower strength than the as-received (annealed) or heat-treated alloy samples is due to the recrystallization in CR samples and the formation of Widmanstatten microstructure in air-cooled samples. The alloy does not have fine secondary α or regions with large dislocation density in this condition. The microstructure in the samples heat-treated (with air cooling) below as well as above β-transus temperature (after CR) is similar to air-cooled samples (without prior CR) with heat treatment above β-transus temperature. This indicates the reduction in recrystallization temperature with cold working, which is substantiated with the reduction in strength as well.

36 MATERIALS SCIENCE↗