Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “PRESSES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Phase transformations of NbCr{sub 2} intermetallics produced by mechanical alloying followed by hot-pressing consolidation

Mechanical alloying followed by hot-pressing consolidation has been used to produce NbCr{sub 2} intermetallics under different conditions. High-purity Nb and Cr crystalline powders, in the relative (molar) ratio of 13:1, were milled for periods up to 100 h. This powder was vacuum-sintered at temperatures ranging from 1423 to 1573 K for 0.5 h under a pressure of 45 MPa. The phase transformations of the NbCr{sub 2} were investigated by X-ray diffraction and scanning electron microscopy; several different phase transformations were observed. Increasing the milling time up to 100 h transforms into a mixture of C14, Nb, Cr and C15. The experimental results show that new evidence based on X-ray diffraction measurements further establishes the existence of a high-temperature C14 Laves polytype; an intermediate C36 structure for NbCr{sub 2}, reported in the literature, was not detected in this study. The relationship between the various phase transformations, based on the atomic radii and different preparation techniques, is discussed.

36 MATERIALS SCIENCE↗

Effect of rapid solidification on the microstructure and mechanical properties of hot-pressed Al-20Si-5Fe alloys

The aim of this work is to study the effect of cooling rate and subsequent hot consolidation on the microstructural features and mechanical strength of Al-20Si-5Fe-2X (X = Cu, Ni and Cr) alloys. Powder and ribbons were produced by gas atomization and melt spinning processes at two different cooling rates of 1 x 10{sup 5} K/s and 5 x 10{sup 7} K/s. The microstructure of the products was examined using optical microscopy, scanning electron microscopy, transmission electron microscopy, and X-ray diffraction. The particles were consolidated by hot pressing at 400 deg. C/250 MPa/1 h under a high purity argon atmosphere and the microstructure, hardness and compressive strength of the compacts were evaluated. Results showed a profound effect of the cooling rate, consolidation stage, and transition metals on the microstructure and mechanical strength of Al-20Si-5Fe alloys. While microstructural refining was obtained at both cooling rates, the microstructure of the atomized powder exhibited the formation of fine primary silicon ({approx} 1 {mu}m), eutectic Al-Si phase with eutectic spacing of {approx} 300 nm, and {delta}-iron intermetallic. Supersaturated Al matrix containing 5-7 at.% silicon and nanometric Si precipitates (20-40 nm) were determined in the microstructure of the melt-spun ribbons. The hot consolidation resulted in coarsening of Si particles in the atomized particles, and precipitation of Si and Fe-containing intermetallics from the supersaturated Al matrix in the ribbons. The consolidated ribbons exhibited higher mechanical strength compared to the atomized powders, particularly at elevated temperatures. The positive influence of the transition metals on the thermal stability of the Al-20Si-5Fe alloy was noticed, particularly in the Ni-containing alloy.

36 MATERIALS SCIENCE↗

The role of grain orientation in microstructure evolution of pure aluminum processed by equal channel angular pressing

A new approach describing the role of crystallographic orientation in the microstructural refinement of commercially pure aluminum during the successive passes of equal channel angular pressing (ECAP) is introduced. The study is based on analysis of X-ray diffraction texture data that is used to calculate the geometrical position of crystallographic slip planes with respect to the shearing plane of the ECAP die. The angular deviations of {l_brace}111{r_brace} slip planes from the macroscopic deformation plane for different processing routes were calculated and compared. The microstructure evolution was investigated using electron back-scattered diffraction (EBSD). The grain size and grain boundary character distribution obtained for each processing route are related to the angles between {l_brace}111{r_brace} planes and the shearing plane. It was shown that the more effective routes in grain refinement have higher angles between {l_brace}111{r_brace} slip planes and the shearing plane. - Research Highlights: {yields} The grain refinement of commercially pure aluminum during ECAP highly depends on the processing routes. {yields} The differences between the processing routes could be explained by the crystallographic orientations of the grains which become parallel to the shearing plane and direction. {yields} Texture results could be used to calculate the angle between the slip planes of the grains and the shearing plane of the ECAP die. {yields} The routes making higher angles between {l_brace}111{r_brace} planes and the shearing plane result in better grain refinement during the process.

36 MATERIALS SCIENCE↗

Resistance spot welding of ultra-fine grained steel sheets produced by constrained groove pressing: Optimization and characterization

Constrained groove pressing as a severe plastic deformation method is utilized to produce ultra-fine grained low carbon steel sheets. The ultra-fine grained sheets are joined via resistance spot welding process and the characteristics of spot welds are investigated. Resistance spot welding process is optimized for welding of the sheets with different severe deformations and their results are compared with those of as-received samples. The effects of failure mode and expulsion on the performance of ultra-fine grained sheet spot welds have been investigated in the present paper and the welding current and time of resistance spot welding process according to these subjects are optimized. Failure mode and failure load obtained in tensile-shear test, microhardness, X-ray diffraction, transmission electron microscope and scanning electron microscope images have been used to describe the performance of spot welds. The region between interfacial to pullout mode transition and expulsion limit is defined as the optimum welding condition. The results show that optimum welding parameters (welding current and welding time) for ultra-fine grained sheets are shifted to lower values with respect to those for as-received specimens. In ultra-fine grained sheets, one new region is formed named recrystallized zone in addition to fusion zone, heat affected zone and base metal. It is shown that microstructures of different zones in ultra-fine grained sheets are finer than those of as-received sheets. - Highlights: Black-Right-Pointing-Pointer Resistance spot welding process is optimized for joining of UFG steel sheets. Black-Right-Pointing-Pointer Optimum welding current and time are decreased with increasing the CGP pass number. Black-Right-Pointing-Pointer Microhardness at BM, HAZ, FZ and recrystallized zone is enhanced due to CGP.

36 MATERIALS SCIENCE↗

Microstructure stability of ultra-fine grained magnesium alloy AZ31 processed by extrusion and equal-channel angular pressing (EX–ECAP)

Thermal stability of the ultra-fine grained (UFG) microstructure of magnesium AZ31 alloy was investigated. UFG microstructure was achieved by a combined two-step severe plastic deformation process: the extrusion (EX) and subsequent equal-channel angular pressing (ECAP). This combined process leads to refined microstructure and enhanced microhardness. Specimens with UFG microstructure were annealed isochronally at temperatures 150–500 °C for 1 h. The evolution of microstructure, mechanical properties and dislocation density was studied by electron backscatter diffraction (EBSD), microhardness measurements and positron annihilation spectroscopy (PAS). The coarsening of the fine-grained structure at higher temperatures was accompanied by a gradual decrease of the microhardness and decrease of dislocation density. Mechanism of grain growth was studied by general equation for grain growth and Arrhenius equation. Activation energies for grain growth were calculated to be 115, 33 and 164 kJ/mol in temperature ranges of 170–210 °C, 210–400 °C and 400–500 °C (443–483 K, 483–673 K and 673–773 K), respectively. - Highlights: • Microhardness of UFG AZ31 alloy decreases with increasing annealing temperature. • This fact has two reasons: dislocation annihilations and/or grain growth. • The activation energies for grain growth were calculated for all temperature ranges.

36 MATERIALS SCIENCE↗

Characterization of hot-pressed short ZrO{sub 2} fiber toughened ZrB{sub 2}-based ultra-high temperature ceramics

Two different ZrB{sub 2}-based ultra-high temperature ceramics were produced by hot pressing: ZrB{sub 2} + 20 vol.% SiC particle + 15 vol.% ZrO{sub 2} fiber and ZrB{sub 2} + 20 vol.% SiC whisker + 15 vol.% ZrO{sub 2} fiber. The microstructures were analyzed by using transmission electron microscopy and high-resolution transmission electron microscopy. It was shown that a clean interface without any impurities was identified in ZrB{sub 2}-based hybrid ceramics with SiC whiskers and ZrO{sub 2} fibers, which would significantly improve the toughening mechanism. The results of high-resolution transmission electron microscopy showed that stacking faults in SiC whiskers resulted from an insertion of a (111) layer, which would be one of the main reasons for material anisotropy. However, the interface between the SiC particle and ZrO{sub 2} fiber was found to be ambiguous in ZrB{sub 2}-based hybrid ceramics with SiC particles and ZrO{sub 2} fibers due to the slight reaction. The orientation relationship between t-ZrO{sub 2} and m-ZrO{sub 2} phases obeyed the classical correspondence: (100){sub m}//(100){sub t} and [001]{sub m}//〈001〉{sub t}, which further verified the feasibility of phase transformation toughening mechanism. - Highlights: • ZrB{sub 2}-based ceramics toughened by short ZrO{sub 2} fiber are characterized by TEM and HRTEM. • The orientation relationship of t- and m-ZrO{sub 2} are (100){sub m}//(100){sub t}, [001]{sub m}//〈001〉{sub t} • The clean interface without any impurities leads to improve the toughening mechanism.

36 MATERIALS SCIENCE↗

Development of mechanical properties in a CaO added AZ31 magnesium alloy processed by equal-channel angular pressing

Processing through the application of equal-channel angular pressing (ECAP) is recognized as one of the attractive severe plastic deformation techniques where the processed bulk metals generally achieve ultrafine-grained microstructure leading to improved physical characteristics and mechanical properties. Magnesium has received much attention to date for its lightweight, high strength and excellent elasticity. Mg alloys with addition of CaO is reported to provide the successful casting procedure without usage of greenhouse gas, SF{sub 6}, whereas it is generally used for preventing the oxidation of Mg during casting. In the present investigation, a CaO added AZ31 (AZ31-CaO) magnesium alloy was processed by ECAP at elevated temepratures with a few steps of reduction which result in significant grain refinement to ~ 1.5 μm after 6 passes. Compression testing at room temperature demonstrated the AZ31-CaO alloy after ECAP showed enhanced yield strength more than the as-processed commercial AZ31 alloy while both alloys maintained ductility in spite of significant reduction in grain size. The improved strength in the AZ31-CaO alloy was attributed to the formation of fine Al{sub 2}Ca precipitates which experience breaking-up through ECAP and accelerate the microstructural refinement. Moreover, the preservation of ductility was attributed to the enhancement of strain hardening capability in the AZ31 alloy at room temperature. This study discusses the feasibility of using ECAP to improve both strength and ductility on magnesium alloys by applying the diagram describing the paradox of strength and ductility. - Highlights: • AZ31 and AZ31-CaO magnesium alloys were processed by ECAP up to 6 passes. • AZ31-CaO alloy after ECAP showed improved yield strength without losing ductility. • CaO in AZ31 forms fine Al{sub 2}Ca accelerating microstructural refinement during ECAP. • Feasibility of using ECAP was shown to improve both strength and ductility in Mg.

36 MATERIALS SCIENCE↗

Thermal stability of Cu-Cr-Zr alloy processed by equal-channel angular pressing

Thermal stability of a Cu-Cr-Zr alloy processed by equal-channel angular pressing up to16 passes was investigated using isochronal annealing ranging from 250 to 850 °C for 1 h. The microstructure, crystallographic texture and micro hardness of samples were characterized through electron back scatter diffraction and Vickers micro hardness measurements. The recrystallized grain size was stable between 250 °C and 500 °C then increased quickly. The achieved mean grain size, after 1, 4 and 16 ECAP passes, was around 5.5 μm. A discontinuous mode of recrystallization was found to occur and a Particle Simulated Nucleation mechanism was evidenced. The evolution of the high angle grain boundary fraction increased notably after annealing above 550 °C. The crystallographic texture after isochronal annealing was similar to that of ECAP simple shear, no change of the texture during annealing was observed but only slight intensity variations. Micro hardness of all Cu–Cr–Zr samples showed a hardening with two peaks at 400 and 500 °C associated with precipitation of Cu cluster and Cu{sub 5}Zr phase respectively, followed by a subsequent softening upon increasing the annealing temperature due to recrystallization. - Highlight: •The Cu-1Cr-0.1Zr alloy shows a very good thermal stability up to 550 °C after ECAP. •A discontinuous recrystallization was found to occur and PSN mechanism was evidenced. •The annealing texture was found weak and some new components appear. •Hardening is attributed to the Cr clustering followed by the Cu{sub 51}Zr{sub 14} precipitation. •Softening is a result of recrystallization and grain growth progressing.

36 MATERIALS SCIENCE↗

Microstructure evolution and mechanical properties of nano-SiCp/AZ91 composite processed by extrusion and equal channel angular pressing (ECAP)

Nano-SiCp/AZ91 magnesium matrix composite was fabricated by stir casting. The as-cast ingots were extruded at 350 °C, then processed by equal channel angular pressing (ECAP) at various temperatures (250 °C, 300 °C and 350 °C). Grains are significantly refined after the extrusion and the ECAP. A basal fibre texture was detected by neutron diffraction after the extrusion, which inclines about 45° to the extrusion direction (ED) after the ECAP. Nano-scaled SiC particles agglomerate in the as-cast composite. After the extrusion, the agglomeration tends to form continuous or discontinuous strips along the extrusion direction. By application of the ECAP, the agglomerated SiC particles are partly dispersed and the strips formed during the extrusion tend to be thinner and broken with the increasing pass number. The yield tensile strength (YTS) and the ultimate tensile strength (UTS) of the composite are dramatically increased after the extrusion. ECAP for one pass at various temperatures further increases the strength, however, the YTS decreases with the increasing ECAP temperature and the pass number. The Orowan equations predict the maximum YTS of the composite may be up to 400 MPa providing SiC particles are homogenously distributed in the matrix. - Highlights: •Nano-scaled SiC particles were successfully added into AZ91 by stirring casting. •Agglomeration of nano-particles were improved by extrusion and ECAP. •Yield strength of the composite is 328 MPa after one pass of ECAP. •Further ECAP process with optimized parameters may fully disperse nano-particles. •Yield strength is predicted to up to 400 MPa when particles are fully dispersed.

36 MATERIALS SCIENCE↗

Microstructure evolution and a new mechanism of B2 phase on room temperature mechanical properties of Ti-47Al-2Cr-2Nb alloy prepared by hot isostatic pressing

Highlights: • The microstructure evolution of Ti-47Al-2Cr-2Nb alolly was investigated in detail. • The foramtion of B{sub 2} phase can be adjusted in Ti-47Al-2Cr-2Nb alloy. • A new mechanism of B{sub 2} phase on room temperature mechanical properties of Ti-47Al-2Cr-2Nb alloy was proposed. - Abstract: The formation of B{sub 2} phase was adjusted via various hot isostatic pressing processes in Ti-47Al-2Cr-2Nb alloy. The microstructure evolution and a new mechanism of B{sub 2} phase on room temperature mechanical properties was investigated by BSE, EBSD and TEM in detail. The result shows that the formation of B{sub 2} phase leads to Cr element content decrease in γ matrix phase, which results in lattice parameter increase, namely the c/a ratio of γ matrix phase. Finally, at room temperature the mechanical properties of Ti-47Al-2Cr-2Nb alloy deteriorates.

36 MATERIALS SCIENCE↗

Effect of equal channel angular pressing on the mechanical and tribological behavior of Al-Zn-Mg-Cu alloy

Highlights: • The correlation of microstructure, mechanical and wear properties has been studied. • The correlation between tensile properties and shear properties has been also studied. • Mechanical and tribological properties have been improved through the ECAP process of the Al-7075 alloy. • The dominant wear mechanisms in the initial material were adhesive and oxidative wear as well as delamination. • Abrasive and oxidative wear were the dominant wear mechanisms in ECAP processed specimens. - Abstract: Microstructure, mechanical properties and wear behavior of severely deformed Al-7075 alloy by equal channel angular pressing (ECAP) were studied. Microhardness, tensile and shear strength tests were performed to evaluate the mechanical properties of the material. The relationship between tensile and shear strength was also extracted. In addition, with the aim of study the wear behavior, the wear tests were performed by using a pin-on-disk machine under different normal loads. The microscopic observations i.e. transmission electron microscopy (TEM) and scanning electron microscope (SEM), were used to analyze the microstructure of specimens as well as the surface, subsurface and debris of worn specimens. Mechanical properties results showed that the hardness and strength (tensile and shear) of the ECAP-processed alloy were higher than that of the annealed alloy and increased with the increment of pass number. The wear test data revealed that the wear rate and friction coefficient decreased with increasing ECAP passes. The SEM analysis of worn specimens demonstrated that the dominant wear mechanisms of the annealed alloy were adhesion wear and delamination and the dominant wear mechanisms of ECAP processed alloy were abrasive wear and plowing bands. Oxidative wear was also observed at both annealed and ECAPed alloy. Totally, these results demonstrated that ultrafine-grained structure fabricated by ECAP, improves the wear resistance of the Al-7075 alloy.

36 MATERIALS SCIENCE↗

Three-dimensional microstructural analysis of fragmentation behavior of platelet Al3Ti particles in Al-Al3Ti composite deformed by equal-channel angular pressing

Highlights: • Particle distribution in ECAPed Al-Al{sub 3}Ti composite depends on material flow of matrix. • Fragmentation of Al{sub 3}Ti particles by ECAP occurs along twin boundary in the particles. • Al{sub 3}Ti particles in the composite fragment after twin deformation of the particles. - Abstract: The fragmentation of platelet Al{sub 3}Ti particles in an Al-Al{sub 3}Ti composite by equal-channel angular pressing (ECAP) is investigated using three-dimensional (3D) microstructural evaluation and crystallography. The Al-Al{sub 3}Ti composite comprises coarse platelet Al{sub 3}Ti particles in an α-Al matrix. The ECAP of this composite is performed for up to 4 passes under processing routes A, B{sub c}, and C. Route B{sub c} produces the smallest Al{sub 3}Ti particle fragments in comparison with the fragments produced under routes A and C. This is because that route B{sub c} produces the largest number of shearing directions and shearing planes. Platelet Al{sub 3}Ti particle fragments in the specimen deformed by ECAP under route A are homogeneously distributed along the deformation axis. In contrast, in the specimens deformed by four ECAP passes under routes B{sub c} and C, the Al{sub 3}Ti particle fragments are gathered into several groups. The fragment groups have a length similar to the initial length of the platelet Al{sub 3}Ti particles. These spatial distributions of particle fragments can be explained by material flow of α-Al matrix during ECAP. Moreover, from 3D microstructural evaluation and crystallographic analysis of the Al{sub 3}Ti particle fragments, it is found that the Al{sub 3}Ti particles are preferentially fragmented on the twin boundary plane of {112}{sub Al3Ti}. Therefore, it is concluded that fragmentation of a platelet Al{sub 3}Ti particle by ECAP occurs along the twin boundary plane after twin deformation.

36 MATERIALS SCIENCE↗

SA508 low alloy steel to 316L stainless steel dissimilar metal joint made by powder metallurgy hot isostatic pressing

Joining ferritic SA508 low alloy steel (LAS) and austenitic 316 L stainless steel (SS) via powder metallurgy hot isostatic pressing (PM-HIP) was evaluated as an alternative method to welding. This study investigated the mechanical and microstructural evolutions of the bimetallic interface under different joint designs and heat treatments. Here, the direct joining of dissimilar metal alloys by PM-HIP method resulted in two designs: 1) powder SA508 to solid bar 316 L (P508–B316L) and 2) powder 316 L solid bar SA508 (P316L-B508). In both cases, P508–B316L and P316L-demonstrated satisfactory tensile strength, however, high hardness and severe depreciation in toughness were located on the bimetallic interface. The mechanisms responsible for the detrimental mechanical properties were verified. Large oxides were observed in P508–B316L due to the prior powder boundary (PPB) oxides present in SA508 powder. The intense sensitization occurred from the formation of M 23 C 6 carbides, consequently from the slow cooling after PM-HIP in P316L-B508. Post-HIP heat treatments were explored to reduce the distance of carbide formation; however, the heat treatment could not eliminate the carbides. The experimental results were compared to the diffusion couple simulation as a function of carbide formation with distance. The analysis also showed the high hardness at the bimetallic interface was primarily contributed by solid solution strengthening. In conclusion, the direct joining of P316L-B508 and P508–B316L via PM-HIP was deemed to be unfeasible, and a transitional material is necessary to impede the diffusion of carbon.

316L stainless Steel↗

A visco-plastic constitutive model for accurate densification and shape predictions in powder metallurgy hot isostatic pressing

Powder metallurgy hot isostatic pressing (PM-HIP) is an advanced manufacturing process that produces near net shape parts with high material utilization and uniform microstructures. Despite being used frequently to produce small-scale components, the application of PM-HIP to large-scale components is limited due to inadequate understanding of its complex mechanisms that cause unpredictable post-HIP shape distortions. A computational model can provide necessary information about the intermediate and final stages of the HIP process that can help understand it better and make accurate predictions. Generally, two types of computational models are employed for PM-HIP of metal powders, namely, plastic and visco-plastic models. Between these, the plastic model is preferred due to its cheaper calibration approach requiring less experimental data. However, the plastic model sometimes produces incorrect predictions when slight variations of the HIP conditions are encountered in practical situations. Therefore, this work presents a visco-plastic model that addresses these limitations of the plastic model. A novel modified calibration approach is employed for the visco-plastic model that utilizes less experimental data than existing approaches. With the new approach, the data requirement is same for both plastic and visco-plastic models. This also enables a quantitative comparison of plastic and visco-plastic models, which have been only qualitatively compared in the past. When calibrated with the same experimental data, both the models are found to produce similar results. In conclusion, the calibrated visco-plastic model is applied to several complex geometries, and the predictions are found to be in good agreement with experimental observations.

Hot isostatic pressing↗

A fast and robust computational modeling approach for density and shape predictions in powder metallurgy hot isostatic pressing

Powder metallurgy hot isostatic pressing (PM-HIP) is an advanced manufacturing process that produces near-net-shape parts with high material utilization and uniform microstructures. PM-HIP is frequently used for producing small-scale parts with complicated geometries and is potentially economical for producing large-scale parts. However, excessive post-HIP shape distortions can reduce its effectiveness and economic advantage, especially for larger parts. A PM-HIP computational model can predict and help mitigate these distortions. However, due to complex deformation mechanisms and thermo-mechanical coupling present in PM-HIP processes, these non-linear computational models sometimes become numerically unstable. The numerical instabilities in these models can lead to very slow convergence or no convergence at all, which often translates to slow and unreliable models. These limitations are more pronounced in large models with complicated geometries. Hence, in this work, an alternative modeling approach is presented that improves numerical stability and computational performance. The presented approach achieves these improvements through approximating the fully coupled thermo-mechanical PM-HIP model as a decoupled model and adding inertial damping to the model’s mechanical part. In conclusion, a comparison with the fully coupled model indicated a slight dip in prediction accuracy (<5% error) but significant improvements in numerical stability (>20 times larger time step size) and computational performance (5-10 times speed-up with less computational resource usage) when using the presented approach.

Hot isostatic pressing↗

Influence of hot isostatic pressing on the performance of aluminum alloy fabricated by ultrasonic additive manufacturing

Ultrasonic additive manufacturing (UAM) is a solid-state manufacturing technique employing principles of ultrasonic welding coupled with mechanized tape layering to fabricate fully functional parts. However, UAM-fabricated parts often exhibit a reduction in strength when loaded normal to the welding interfaces (Z-direction). Here, the effect of hot isostatic pressing (HIP) on UAM builds of aluminum alloy was explored. Tensile testing and microstructure characterization were conducted; it was established that HIP eliminated the brittle Z-direction fracture and improved the strength and ductility of the Z-direction specimens. HIP eliminated voids and produced recrystallized structure; however, welding interfaces survived the HIP treatment.

36 MATERIALS SCIENCE↗

The study of dielectric, pyroelectric and piezoelectric properties on hot pressed PZT-PMN systems

Hot uniaxial pressing technique has been adopted for the densification of PZT-PMN system with an aim to yield dense ceramics and to lower the sintering temperature and time for achieving better and reproducible electronic properties. The ceramics having >97% theoretical density and micron size grains are investigated for their dielectric, pyroelectric and piezoelectric properties. The effect of Li and Mn addition has also been studied.

36 MATERIALS SCIENCE↗

Enhancement of the electrical characteristics of metal-free phthalocyanine films using cold isostatic pressing

Spatial gaps between grains and other grains, substrates, or electrodes in organic electronic devices are one of the causes of the reduction in the electrical characteristics. In this study, we demonstrate that cold isostatic pressing (CIP) is an effective method to crush the gaps and enhance the electrical characteristics. CIP of metal-free phthalocyanine (H{sub 2}PC) films induced a decrease in the film thickness by 34%–40% because of the gap crush. The connection of smaller grains into a larger grain and planarization of the film surface were also observed in the CIP film. The crystal axes of the H{sub 2}PC crystallites were rearranged from the a-axis to the c-axis of the α-phase crystal structure in a direction perpendicular to the substrate by CIP, indicating favorable hole injection and transport in this direction because of a better overlap of π orbitals. Thermally stimulated current measurements showed that deep hole traps disappeared and the total hole-trap density decreased after CIP. These CIP-induced changes of the film thicknesses, crystal axes and the hole traps lead to a marked increase in the hole mobility of the H{sub 2}PC films from 2.0 × 10{sup −7} to 4.0 × 10{sup −4} cm{sup 2}/V s by 2000 times in the perpendicular direction. We believe that these findings are important for unveiling the underlying carrier injection and transport mechanisms of organic films and for enhancing the performance of future organic electronic devices.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗