Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MORTARS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Characterization of composite materials based on cement-ceramic powder blended binder

Characterization of newly developed composite mortars with incorporated ceramic powder coming from precise brick cutting as partial Portland cement replacement up to 40 mass% is presented in the paper. Fine ceramic powder belongs to the pozzolanic materials. Utilization of pozzolanic materials is accompanied by lower request on energy needed for Portland clinker production which generally results in lower production costs of blended binder and lower CO{sub 2} emission. In this paper, the ceramic powder is used in cement based mortar composition in amount of 8, 16, 24, 32, and 40 mass% of cement. Chemical composition of ceramic powder is analyzed by X-Ray Fluorescence and X-Ray Diffraction. The particle size distribution of ceramics is accessed on laser diffraction principle. For 28 days cured mortar samples, basic physical and mechanical properties are experimentally determined. The obtained results demonstrate that ceramic powder has potential to replace a part of Portland cement in composition of cement based composites and to reduce negative environmental impact of their production.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Flight Test of a 40-Foot Nominal-Diameter Disk-Gap-Band Parachute Deployed at a Mach Number of 1.91 and a Dynamic Pressure of 11.6 Pounds per Square Foot

A 40-foot (12.2 meter) nominal-diameter disk-gap-band parachute was flight tested as part of the NASA Supersonic Planetary Entry Decelerator Program (SPED-I). The test parachute was ejected by a deployment mortar from an instrumented payload at an altitude of 140,000 feet (42.5 kilometers). The payload was at a Mach number of 1.91 and the dynamic pressure was 11.6 pounds per square foot (555 newtons per square meter) at the time the parachute deployment mortar was fired. The parachute reached suspension line stretch in 0.43 second with a resultant snatch force loading of 1990 pounds (8850 newtons). The maximum parachute opening load of 6500 pounds (28,910 newtons) came 0.61 second later at a total elapsed time from mortar firing of 1.04 seconds. The first full inflation occurred at 1.12 seconds and stable inflation was achieved at approximately 1.60 seconds. The parachute had an average axial-force coefficient of 0.53 during the deceleration period. During the steady-state descent portion of the flight test, the average effective drag coefficient was also 0.53 and pitch-yaw oscillations of the canopy averaged less than 10 degrees in the altitude region above 100,000 feet (30.5 meters).

EXPERIMENTS↗

Flight Test of a 30-Foot Nominal-Diameter Disk-Gap-Band Parachute Deployed at Mach 1.56 and Dynamic Pressure of 11.4 Pounds per Square Foot

A 30-foot (9.1 meter) nominal-diameter disk-gap-band parachute (reference area 707 sq ft (65.7 m(exp 2)) was flight tested with a 200-pound (90.7 kg) instrumented payload as part of the NASA Planetary Entry Parachute Program. A deployment mortar ejected the test parachute when the payload was at a Mach number of 1.56 and a dynamic pressure of 11.4 lb/sq ft (546 newtons per m 2 ) at an altitude of 127,500 feet (38.86 km). The parachute reached suspension line stretch in 0.37 second resulting in a snatch force loading of 1270 pounds (5650 N). Canopy inflation began 0.10 second after line stretch. A delay in the opening process occurred and was apparently due to a momentary interference of the glass-fiber shroud used in packing the parachute bag in the mortar. Continuous canopy inflation began 0.73 second after initiation of deployment and 0.21 second later full inflation was attained for a total elapsed time from mortar fire of 0.94 second. The maximum opening load of 3915 pounds (17,400 newtons) occurred at the time the canopy was first fully opened. The parachute exhibited an average drag coefficient of 0.52 during the deceleration period and pitch-yaw oscillations of the canopy were less than 5 degrees. During the steady-state descent portion of the test period, the average effective drag coefficient was about 0.47 (based on vertical descent velocity and total system weight).

EXPERIMENTS↗

Design and Analysis of Outer Mold Line Close-outs for the Max Launch Abort System (MLAS) Flight Experiment

In 2007, the NASA Exploration Systems Mission Directorate (ESMD) chartered the NASA Engineering Safety Center (NESC) to demonstrate an alternate launch abort concept as risk mitigation for the Orion project's baseline "tower" design. On July 8, 2009, a full scale, passive aerodynamically stabilized Max Launch Abort System (MLAS) pad abort demonstrator was successfully launched from NASA Goddard Space Flight Center's Wallops Flight Facility. Aerodynamic close-outs were required to cover openings on the MLAS fairing to prevent aerodynamic flow-through and to maintain the MLAS OML surface shape. Two-ply duct tape covers were designed to meet these needs. The duct tape used was a high strength fiber reinforced duct tape with a rubberized adhesive that demonstrated 4.6 lb/in adhesion strength to the unpainted fiberglass fairing. Adhesion strength was observed to increase as a function of time. The covers were analyzed and experimentally tested to demonstrate their ability to maintain integrity under anticipated vehicle ascent pressure loads and to not impede firing of the drogue chute mortars. Testing included vacuum testing and a mortar fire test. Tape covers were layed-up on thin Teflon sheets to facilitate installation on the vehicle. Custom cut foam insulation board was used to fill mortar hole and separation joint cavities and provide support to the applied tape covers. Flight test results showed that the tape covers remained adhered during flight.

Woods-Vedeler, Jessica A.↗

Reconstruction of the Mars Science Laboratory Parachute Performance and Comparison to the Descent Simulation

The Mars Science Laboratory used a single mortar-deployed disk-gap-band parachute of 21.35 m nominal diameter to assist in the landing of the Curiosity rover on the surface of Mars. The parachute system s performance on Mars has been reconstructed using data from the on-board inertial measurement unit, atmospheric models, and terrestrial measurements of the parachute system. In addition, the parachute performance results were compared against the end-to-end entry, descent, and landing (EDL) simulation created to design, develop, and operate the EDL system. Mortar performance was nominal. The time from mortar fire to suspension lines stretch (deployment) was 1.135 s, and the time from suspension lines stretch to first peak force (inflation) was 0.635 s. These times were slightly shorter than those used in the simulation. The reconstructed aerodynamic portion of the first peak force was 153.8 kN; the median value for this parameter from an 8,000-trial Monte Carlo simulation yielded a value of 175.4 kN - 14% higher than the reconstructed value. Aeroshell dynamics during the parachute phase of EDL were evaluated by examining the aeroshell rotation rate and rotational acceleration. The peak values of these parameters were 69.4 deg/s and 625 deg/sq s, respectively, which were well within the acceptable range. The EDL simulation was successful in predicting the aeroshell dynamics within reasonable bounds. The average total parachute force coefficient for Mach numbers below 0.6 was 0.624, which is close to the pre-flight model nominal drag coefficient of 0.615.

Cruz, Juan R.↗

Reconstructed Performance of the Mars InSight Lander’s Supersonic Parachute & Comparison with the Phoenix Lander

On November 26th, 2018 the Mars InSight landersuccessfully touched down at Elysium Planitia. InSight’s Entry,Descent, and Landing sequence included an 11.8-m supersonicallydeployed Disk-Gap-Band parachute that was a largelybuild-to-print version of the parachute used to successfully landthe Phoenix lander a decade earlier. This paper describes thereconstructed performance of InSight’s supersonic parachuteat Mars, highlighting the differences and similarities with theperformance of Phoenix’s parachute. Measurements from theonboard inertial measurement unit along with pre-launch measurementsof the parachute system and spacecraft, assumptionsabout the vehicle’s aerodynamics, and models for the Martianatmosphere were used to reconstruct the spacecraft’s trajectoryand the parachute system’s performance. The reconstruction resultswere compared against pre-flight predictions. Reconstructionof the InSight trajectory leading up to parachute deploymentshowed that the vehicle trimmed in a lift-down orientationduring entry and thus experienced greater deceleration thanexpected by most pre-flight simulations. This led to parachutedeployment conditions that diverged from the nominal preflightpredictions. The parachute was mortar-deployed at aMach number of approximately 1.5, below the nominal preflightexpectation of 1.66. The approximate dynamic pressureat mortar fire was between 518 Pa and 546 Pa, which agreedwell with pre-flight expectations. The mortar system performednominally, and the system’s deployment (0.755 s) and inflation(1.1 s) times were in line with pre-flight modeling. The peakinflation load was 45 kN, well below the parachute’s 67 kNdesign limit load. Following deployment of the parachute,the vehicle’s rotational rates and the dynamics of the systemwere in excellent agreement with pre-flight expectations. Theperformance of the InSight parachute system was also foundto agree well with that of the Phoenix parachute system, asexpected given the similarities between the two systems.

Karlgaard, Chris↗

M3 milestone: Advanced contact 2021

This report describes advanced contact approaches and implementations in FY21 for use in emerging reactors with geometries that differ from LWR/EBR-II cylindrical fuel. Contact remains a challenging and crucially important component of our modeling toolkit. While significant improvements have been made through mortar and automatic differentiation, we explored advanced approaches (i.e., dual mortar) that yields better conditioned systems and will improve the robustness and performance of BISON contact problems. This effort is relevant to emerging reactor types, such as micro reactors and the corresponding complex and numerous contact surfaces. In this report, improvements of the mortar-based contact formulation are described. Benchmark problems and BISON assessment cases are included to demonstrate the improvements and advantages that are brought by the recent capability. Remaining issues are discussed and corresponding development plans are outlined.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Developing an Innovative Field Expedient Fracture Toughness Testing Protocol for Concrete Materials

The Spiral Notch Torsion Fracture Toughness Test (SNTT) was developed recently to determine the intrinsic fracture toughness (KIC) of structural materials. The SNTT system operates by applying pure torsion to uniform cylindrical specimens with a notch line that spirals around the specimen at a 45 pitch. KIC values are obtained with the aid of a three-dimensional finite-element computer code, TOR3D-KIC. The SNTT method is uniquely suitable for testing a wide variety of materials used extensively in pressure vessel and piping structural components and weldments. Application of the method to metallic, ceramic, and graphite materials has been demonstrated. One important characteristic of SNTT is that neither a fatigue precrack or a deep notch are required for the evaluation of brittle materials, which significantly reduces the sample size requirement. In this paper we report results for a Portland cement-based mortar to demonstrate applicability of the SNTT method to cementitious materials. The estimated KIC of the tested mortar samples with compressive strength of 34.45 MPa was found to be 0.19 MPa m.

36 MATERIALS SCIENCE↗

Effects of the secondary minerals of the natural pozzolans on their pozzolanic activity

Natural pozzolans have been widely used as substitutes for Portland cement, because of their binding properties. Some of them are natural volcanic rocks which contain secondary minerals such as clays and zeolites corresponding to products of the alteration of the rock. The objective of this study was to document the potential effect of the secondary minerals on the strength development of pozzolanic mortars. We chose to investigate this effect by thermally destabilising these minerals in three different pozzolanic deposits (poz-1, poz-2 and poz-3). We first did a detailed mineralogical study, to identify the occurrence and the nature of the different secondary minerals. Kaolinite is abundant in poz-1 and different types of zeolite were identified in poz-2 and poz-3. Thermal treatments were monitored by X-ray Diffraction (XRD) analysis, in order to document mineralogical transformations. The effect on the pozzolanic activity has been tested by strength measurements on normalised mortars at 1, 7 and 28 days. Strength of all blended cements is enhanced while destabilising secondary alteration minerals. For kaolinite, we showed that a strength improvement occurs as soon as it is destructured, even if it is not transformed in metakaolin. For zeolites, destabilisation takes place at low temperature (350 deg. C), but as recrystallisation products are easily formed, activation temperature window is narrow. Endly, we have evidence that the presence of calcite in pozzolans has an effect on early strength. Therefore this study is giving new perspectives for a better use of natural pozzolanic materials in the cement industry.

36 MATERIALS SCIENCE↗

The role of calcium hydroxide in the formation of thaumasite

It has recently been derived by thermodynamic calculation that the presence or absence of calcium hydroxide plays a vital role in the resistance of cement paste or concrete against the formation of thaumasite. To obtain experimental data on this matter, special binders have been mixed and used for the preparation of mortar bars. These specimens were exposed to moderate sulphate attack for a period of 18 months at a temperature of 8 deg. C. Mortar bars containing calcium hydroxide showed visual signs of attack a few months after exposure, leading to expansion, mass loss and complete failure. In contrast to this, no signs of attack were observed when no calcium hydroxide was present in the microstructure. These results confirm the conclusions of earlier thermodynamic calculations that the presence of calcium hydroxide has an important impact on the formation of thaumasite. Calcium-rich C-S-H formed in the presence of calcium hydroxide is vulnerable against sulphate attack and the formation of thaumasite. In the absence of calcium hydroxide, C-S-H has a much lower calcium/silicon ratio and a higher resistance against the formation of thaumasite.

36 MATERIALS SCIENCE↗

On equations for the total suction and its matric and osmotic components

A clear fundamental understanding of suctions is crucial for the study of the behaviour of plastic cement mortar and concrete, including plastic shrinkage cracking. In this paper, the expression relating the change in free energy of the pore water with an isothermal change in pressure is first derived. Based upon definitions of suctions, it is then shown that total, matric, and osmotic suctions can all be expressed in the same thermodynamic form. The widely accepted, but not yet satisfactorily validated, assumption that the total suction comprises matric and osmotic components is then confirmed theoretically. The well-known Kelvin equation for matric suction, and Morse and van't Hoff equations for osmotic suction are subsequently derived from the corresponding thermodynamic equations. The applicability of latter two equations in evaluating the osmotic suctions of cement mortar and concrete is highlighted.

36 MATERIALS SCIENCE↗

The origin of the pozzolanic activity of calcined clay minerals: A comparison between kaolinite, illite and montmorillonite

This paper investigates the decomposition of three clayey structures (kaolinite, illite and montmorillonite) when thermally treated at 600 {sup o}C and 800 {sup o}C and the effect of this treatment on their pozzolanic activity in cementitious materials. Raw and calcined clay minerals were characterized by the XRF, XRD, {sup 27}Al NMR, DTG and BET techniques. Cement pastes and mortars were produced with a 30% substitution by calcined clay minerals. The pozzolanic activity and the degree of hydration of the clinker component were monitored on pastes using DTG and BSE-IA, respectively. Compressive strength and sorptivity properties were assessed on standard mortars. It was shown that kaolinite, due to the amount and location of OH groups in its structure, has a different decomposition process than illite or montmorillonite, which results in an important loss of crystallinity. This explains its enhanced pozzolanic activity compared to other calcined clay-cement blends.

36 MATERIALS SCIENCE↗

Evaluation of pore structures and cracking in cement paste exposed to elevated temperatures by X-ray computed tomography

When cement-based materials are exposed to the high temperatures induced by fire, which can rapidly cause temperatures of over 1000 °C, the changes in pore structure and density prevail. In the present study, mortar specimens were subjected to a series of increasing temperatures to explore the temperature-dependent evolution of internal pore structure. High-performance X-ray computed tomography (CT) was used to observe the evolution of temperature-induced discontinuities at the sub-millimeter level. X-ray diffraction (XRD) and scanning electron microscopy (SEM) were employed to investigate the cause of physical changes in the heated mortar specimens. Results exhibit the changes in pore structure caused by elevated temperatures, and thermally induced fractures. We discuss the progressive formation of thermally induced fracture networks, which is a prerequisite for spalling failure of cement-based materials by fire, based on visual observations of the 3D internal structures revealed by X-ray CT.

36 MATERIALS SCIENCE↗

Hydration studies of calcium sulfoaluminate cements blended with fly ash

The main objective of this work is to study the hydration and properties of calcium sulfoaluminate cement pastes blended with fly ash (FA) and the corresponding mortars at different hydration ages. Laboratory X-ray powder diffraction, rheological studies, thermal analysis, porosimetry and compressive strength measurements were performed. The analysis of the diffraction data by Rietveld method allowed quantifying crystalline phases and overall amorphous contents. The studied parameters were: i) FA content, 0, 15 and 30 wt.%; and ii) water addition, water-to-CSA mass ratio (w/CSA = 0.50 and 0.65), and water-to-binder mass ratio (w/b = 0.50). Finally, compressive strengths after 6 months of 0 and 15 wt.% FA [w/CSA = 0.50] mortars were similar: 73 ± 2 and 72 ± 3 MPa, respectively. This is justified by the filler effect of the FA as no strong evidences of reactivity of FA with CSA were observed. These results support the partial substitution of CSA cements with FA with the economic and environmental benefits.

36 MATERIALS SCIENCE↗

Spatial distribution of crystalline corrosion products formed during corrosion of stainless steel in concrete

The mineralogy and spatial distribution of nano-crystalline corrosion products that form in the steel/concrete interface were characterized using synchrotron X-ray micro-diffraction (μ-XRD). Two types of low-nickel high-chromium reinforcing steels embedded into mortar and exposed to NaCl solution were investigated. Corrosion in the samples was confirmed by electrochemical impedance spectroscopy (EIS). μ-XRD revealed that goethite (α-FeOOH) and akaganeite (β-FeOOH) are the main iron oxide–hydroxides formed during the chloride-induced corrosion of stainless steel in concrete. Goethite is formed closer to the surface of the steel due to the presence of chromium in the steel, while akaganeite is formed further away from the surface due to the presence of chloride ions. Detailed microstructural analysis is shown and discussed on one sample of each type of steel. - Highlights: • Synchrotron micro-diffraction used to map the distribution of crystalline phases. • Goethite and akaganeite are the main corrosion products during chloride induced corrosion in mortar. • Layers of goethite and akaganeite are negatively correlated. • EDS showed Cr present in corrosion products identified by SEM.

36 MATERIALS SCIENCE↗

Effect of environmental exposure on autogenous self-healing of cracked cement-based materials

Despite abundant literature on self-healing of cement-based materials, there is dearth of information on how environmental exposure affects self-healing. In this study, self-healing of cracks in cement mortar under different environmental exposure was investigated. Pre-cracked mortar specimens were submerged in water, while identical specimens were exposed to cyclic temperature and relative humidity. Change in crack width was examined using optical microscopy. SEM coupled with energy dispersive X-ray analysis was used to identify healing compounds. Mercury Intrusion Porosimetry, water absorption and permeability were employed to assess porosity. X-ray computed tomography was deployed to explore healing of internal cracks. No significant self-healing occurred in specimens exposed to cyclic T and RH. Although crack self-healing was identified in submerged specimens, X-ray μCT demonstrated that it was limited to exposed surface of specimens. This warrants further research to bridge the gap between laboratory findings on self-healing and actual field performance of ageing civil infrastructure.

36 MATERIALS SCIENCE↗

Fracturing process of micro-concrete under uniaxial and triaxial compression: Insights from in-situ X-ray mechanical tests

This paper presents an experimental study of concrete at meso-scale (aggregates, macro-pores and mortar matrix) in order to get a better understanding of the local failure mechanisms known to drive the macroscopic mechanical behaviour of the material. The main originality comes from conducting in-situ X-ray mechanical tests on micro-concrete samples of realistic composition (including cement, sand, aggregates and water), under uniaxial compression and, for the first time, under triaxial compression at 5 MPa, 10 MPa and 15 MPa confining pressures. A timeseries analysis of the set of 3D images coming from each test allows for the measurement of the 3D kinematic fields (displacement and strain fields) throughout the experiments. The different failure patterns observed for each loading path are discussed, along with a quantification of the 3D fracturing processes at the scale of the largest heterogeneities (aggregates and macro-pores). With an increasing level of confinement, the transition from brittle to ductile response is observed, as well as an increase of the strength of the material. The pronounced impact of the meso-scale heterogeneities of concrete on their local failure mechanisms is highlighted. It is shown that strain localisation mainly originates between aggregates and mortar matrix, with the shape and location of the largest aggregates and macro-pores essentially driving the propagation of the cracking network.

36 MATERIALS SCIENCE↗

A simple route for making surfactant free lead sulfide (PbS) quantum dots

Highlights: • Surfactant free PbS NCs were successfully synthesised using CoSP technique. • The technique eliminates the requirements of washing to remove the ligands. • Grinding using mortar and pestle creates well separated PbS QDs. • Surfactant free PbS NCs are stable and do not show any degradation with time. - Abstract: An efficient, cost effective and less time consuming method suitable for mass production of surfactant free quantum dots (QDs) of lead sulfide (PbS) is reported. PbS nanocrystals (NCs) are first synthesised by continuous spray pyrolysis (CoSP) technique and de-agglomeration into PbS quantum dots (QDs) is achieved by vigorous mechanical grinding using mortar and pestle. Lead acetate and thiourea were used as the precursor materials for preparation of surfactant free PbS NCs. The broadening in XRD peaks of ground NCs as compared to as synthesized PbS NCs clearly indicated the reduction in particle size to be QDs of PbS. The TEM images also showed that ground PbS NCs were nearly spherical in shape having an average diameter in the range of 4–6 nm. The shift in optical gap from 0.41 eV to 1.47 eV supported the QD formation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗