Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MAGNETRONS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

High power pulsed magnetron sputtering: A method to increase deposition rate

High power pulsed magnetron sputtering (HPPMS) is a state-of-the-art physical vapor deposition technique with several industrial applications. One of the main disadvantages of this process is its low deposition rate. In this work, the authors report a new magnetic field configuration, which produces deposition rates twice that of conventional magnetron's dipole magnetic field configuration. Three different magnet pack configurations are discussed in this paper, and an optimized magnet pack configuration for HPPMS that leads to a higher deposition rate and nearly full-face target erosion is presented. The discussed magnetic field produced by a specially designed magnet assembly is of the same size as the conventional magnet assembly and requires no external fields. Comparison of deposition rates with different power supplies and the electron trapping efficiency in complex magnetic field arrangements are discussed.

42 ENGINEERING↗

Determination of the number density of excited and ground Zn atoms during rf magnetron sputtering of ZnO target

A combination of optical absorption spectroscopy (OAS) and optical emission spectroscopy measurements was used to monitor the number density of Zn atoms in excited 4s4p ({sup 3}P{sub 2} and {sup 3}P{sub 0}) metastable states as well as in ground 4s{sup 2} ({sup 1}S{sub 0}) state in a 5 mTorr Ar radio-frequency (RF) magnetron sputtering plasma used for the deposition of ZnO-based thin films. OAS measurements revealed an increase by about one order of magnitude of Zn {sup 3}P{sub 2} and {sup 3}P{sub 0} metastable atoms by varying the self-bias voltage on the ZnO target from −115 to −300 V. Over the whole range of experimental conditions investigated, the triplet-to-singlet metastable density ratio was 5 ± 1, which matches the statistical weight ratio of these states in Boltzmann equilibrium. Construction of a Boltzmann plot using all Zn I emission lines in the 200–500 nm revealed a constant excitation temperature of 0.33 ± 0.04 eV. In combination with measured populations of Zn {sup 3}P{sub 2} and {sup 3}P{sub 0} metastable atoms, this temperature was used to extrapolate the absolute number density of ground state Zn atoms. The results were found to be in excellent agreement with those obtained previously by actinometry on Zn atoms using Ar as the actinometer gas [L. Maaloul and L. Stafford, J. Vac. Sci. Technol., A 31, 061306 (2013)]. This set of data was then correlated to spectroscopic ellipsometry measurements of the deposition rate of Zn atoms on a Si substrate positioned at 12 cm away from the ZnO target. The deposition rate scaled linearly with the number density of Zn atoms. In sharp contrast with previous studies on RF magnetron sputtering of Cu targets, these findings indicate that metastable atoms play a negligible role on the plasma deposition dynamics of Zn-based coatings.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Silicon oxynitride films deposited by reactive high power impulse magnetron sputtering using nitrous oxide as a single-source precursor

Silicon oxynitride thin films were synthesized by reactive high power impulse magnetron sputtering of silicon in argon/nitrous oxide plasmas. Nitrous oxide was employed as a single-source precursor supplying oxygen and nitrogen for the film growth. The films were characterized by elastic recoil detection analysis, x-ray photoelectron spectroscopy, x-ray diffraction, x-ray reflectivity, scanning electron microscopy, and spectroscopic ellipsometry. Results show that the films are silicon rich, amorphous, and exhibit a random chemical bonding structure. The optical properties with the refractive index and the extinction coefficient correlate with the film elemental composition, showing decreasing values with increasing film oxygen and nitrogen content. The total percentage of oxygen and nitrogen in the films is controlled by adjusting the gas flow ratio in the deposition processes. Furthermore, it is shown that the film oxygen-to-nitrogen ratio can be tailored by the high power impulse magnetron sputtering-specific parameters pulse frequency and energy per pulse.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Boron carbide films with reduced nodular defect density deposited by full-face erosion radio-frequency magnetron sputtering

Boron carbide coatings deposited by sputtering with conventional planar magnetrons exhibit nodular growth defects. Here, we demonstrate that the density of nodular defects in B 4 C films can be greatly reduced by using a full-face-erosion magnetron source that achieves a more uniform target erosion by sweeping the confining magnetic field over the target surface. Here, we systematically study properties of B 4 C films deposited on substrates with different tilt angles and demonstrate deposition of ultrathick films with compressive residual stress below 200MPa.

36 MATERIALS SCIENCE↗

Study of the plasma parameters in a high-current pulsed magnetron sputtering system

Results are presented from experimental studies of the current-voltage characteristics and spatial and temporal parameters of the plasma in a high-current pulsed magnetron sputtering system with a 10-cm-diameter plane disk cathode. It is shown that the plasma density in such a system is three orders of magnitude higher than that in conventional dc magnetron discharges and reaches 10{sup 13} cm{sup -3} at a distance of 250 mm from the cathode at a peak discharge current of 500 A. The plasma propagates from the cathode region at a velocity of 1 cm/{mu}s in the axial direction and 0.25 cm/{mu}s in the radial direction. Optical emission spectroscopy shows that the degree of plasma ionization increases severalfold with increasing discharge current, mainly at the expense of the sputtered material.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Effect of electric field in the course of obtaining a-SiO{sub x}:H(Er, O) films by dc magnetron sputtering on their composition and photoluminescence intensity of erbium ions

The effect of electric field on the elemental composition and photoluminescence of films of amorphous hydrogenated silicon doped with erbium and oxygen (a-SiO{sub x}:H(Er, O)) in the course of obtaining these films by dc magnetron sputtering is studied. Two series of films were studied in relation to the electric-field strength in the magnetron, the area of the metallic erbium target, and oxygen content in the working chamber. The first series of films was obtained using an electrically insulated substrate holder, and the second series was obtained with a positive potential at the substrate holder with respect to the cathode. It is shown that, although the character of variation in the elemental composition and photoluminescence intensity for erbium Er{sup 3+} ions differ appreciably in the films of the two series, both of these factors are determined, as a result, by the processes of sputtering oxidation of the Si and Er targets that represent the cathode.

36 MATERIALS SCIENCE↗

Magnetron-assisted deposition of thin (SiC){sub 1-x}(AlN){sub x} alloy films

The results of theoretical estimations of important parameters of the process of magnetron-assisted sputtering are reported. The parameters are the extent of the zone of thermalization of atoms and the distance from the target to the conditional anode. The method of magnetron-assisted sputtering of polycrys-talline SiC-AlN targets is applied to produce thin (SiC){sub 1-x}(AlN){sub x} alloy films on SiC and Al{sub 2}O{sub 3} substrates. The structure and composition of the films are studied by X-ray diffraction measurements and electron microscopy. The factors that control the composition and structure of the films and the conditions of formation of the single-crystal (SiC){sub 1-x}(AlN){sub x} films on the SiC substrates are established.

36 MATERIALS SCIENCE↗

On the formation of silicon nanoclusters ncl-Si in a hydrogenated amorphous silicon suboxide matrix a-SiO{sub x}:H (0 < x < 2) with time-modulated dc magnetron plasma

Activation of the process of amorphous-silicon-nanocluster formation in a hydrogenated amorphous- silicon suboxide matrix with time-modulated dc discharge plasma is investigated. The plasma is modulated by repeatedly switching on and off a dc magnetron magnetic coil. It is demonstrated that the resulting self-induction effect leads eventually to an increase in the probability of collisions between discharge electrons and gaseous components. The infrared (IR) spectra of the films showed that plasma modulation enhances predominantly the content of bridging oxygen in the a-SiO{sub x}:H matrix by strengthening the oxygenionization process. It is assumed that this also increases the concentration of silicon nanoclusters ncl-Si with an oxidized outer surface in the plasma and, thus, enhances the ncl-Si flux toward the electrodes of the dc magnetron. The photoluminescence spectra include two broad overlapping bands characteristic of amorphous ncl-Si with maxima in the range of 600–1000 nm.

36 MATERIALS SCIENCE↗

Phase Formation and Electronic Structure Peculiarities in the Al{sub 1–} {sub x}Si{sub x} Film Composites under the Conditions of Magnetron and Ion-Beam Sputtering

The peculiarities of the phase composition and electronic structure of aluminum–silicon composite films near the Al{sub 0.75}Si{sub 0.25} composition obtained by the magnetron and ion-beam sputtering methods on a Si(100) silicon substrate are studied using the X-ray diffraction techniques and ultrasoft X-ray emission spectroscopy. In addition to silicon nanocrystals of about 25 nm in size, an ordered solid solution corresponding to the previously unknown Al{sub 3}Si phase is formed in magnetron sputtering on a polycrystalline Al matrix. Films obtained by ion-beam sputtering of the composite target are found to be monophasic and contained only one phase of an ordered solid solution of aluminum silicide Al{sub 3}Si of the Pm3m cubic system with the primitive cell parameter a = 4.085 Å. However, subsequent pulsed photon annealing of the composite with different radiation doses from 145 to 216 J/cm{sup 2} gives rise to the partial decomposition of the Al{sub 3}Si phase with the formation of free metallic aluminum and silicon nanocrystals with sizes in the range from 50 to 100 nm, depending on the pulsed photon radiation dose.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Plasma potential mapping of high power impulse magnetron sputtering discharges

Pulsed emissive probe techniques have been used to determine the plasma potential distribution of high power impulse magnetron sputtering (HiPIMS) discharges. An unbalanced magnetron with a niobium target in argon was investigated for pulse length of 100 μs at a pulse repetition rate of 100 Hz, giving a peak current of 170 A. The probe data were taken with a time resolution of 20 ns and a spatial resolution of 1 mm. It is shown that the local plasma potential varies greatly in space and time. The lowest potential was found over the target’s racetrack, gradually reaching anode potential (ground) several centimeters away from the target. The magnetic pre-sheath exhibits a funnel-shaped plasma potential resulting in an electric field which accelerates ions toward the racetrack. In certain regions and times, the potential exhibits weak local maxima which allow for ion acceleration to the substrate. Knowledge of the local E and static B fields lets us derive the electrons’ E×B drift velocity, which is about 105 m/s and shows structures in space and time.

36 MATERIALS SCIENCE↗

3D Magnetron simulation with CST STUDIO SUITE

The modeling of magnetrons compared to other tubes is more difficult since it requires 3D modeling rather than a 2D investigation. This is not only due to the geometry which can include complicated details to be modeled in 3D but also due to the interaction process itself. The electric field, magnetic field and particle movement span a 3D space. In this paper 3D simulations of a strapped magnetron with CSTSTUDIO SUITE{sup TM} are presented. (author)

43 PARTICLE ACCELERATORS↗

Magnetron sputtered nanostructured cadmium oxide films for ammonia sensing

Nanostructured cadmium oxide (CdO) films were deposited on to glass substrates by reactive dc magnetron sputtering technique. The depositions were carried out for different deposition times in order to obtain films with varying thicknesses. The CdO films were polycrystalline in nature with cubic structure showing preferred orientation in (1 1 1) direction as observed by X-ray diffraction (XRD). Field-emission scanning electron microscope (FE-SEM) micrographs showed uniform distribution of grains of 30–35 nm size and change in morphology from spherical to elliptical structures upon increasing the film thickness. The optical band gap value of the CdO films decreased from 2.67 to 2.36 eV with increase in the thickness. CdO films were deposited on to interdigitated electrodes to be employed as ammonia (NH{sub 3}) gas sensor. The fabricated CdO sensor with thickness of 294 nm has a capacity to detect NH{sub 3} as low as 50 ppm at a relatively low operating temperature of 150 °C with quick response and recovery time. - Highlights: • Nanostructured CdO films were deposited on to glass substrates using magnetron sputtering. • Deposition time was varied in order to obtain films with different thicknesses. • The CdO films were polycrystalline in nature with preferred orientation along (1 1 1) direction. • The optical bandgap values of the films decreased on increasing the thickness of the films. • CdO films with different thickness such as 122, 204, 294 nm was capable to detect NH{sub 3} down to 50 ppm at operating temperature of 150 °C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Investigation of microstructure, micro-mechanical and optical properties of HfTiO{sub 4} thin films prepared by magnetron co-sputtering

Highlights: • HfTiO{sub 4} thin films were deposited by magnetron co-sputtering. • As-prepared and annealed at 800 °C thin films were nanocrystalline. • Optical properties and hardness were investigated in relation to thin films structure. • Hardness was 3-times higher in the case of as-deposited thin films. • HfTiO{sub 4} thin films are suitable for use as optical coatings with protective properties. - Abstract: Titania (TiO{sub 2}) and hafnium oxide (HfO{sub 2}) thin films are in the focus of interest to the microelectronics community from a dozen years. Because of their outstanding properties like, among the others, high stability, high refractive index, high electric permittivity, they found applications in many optical and electronics domains. In this work discussion on the hardness, microstructure and optical properties of as-deposited and annealed HfTiO{sub 4} thin films has been presented. Deposited films were prepared using magnetron co-sputtering method. Performed investigations revealed that as-deposited coatings were nanocrystalline with HfTiO{sub 4} structure. Deposited films were built from crystallites of ca. 4–12 nm in size and after additional annealing an increase in crystallites size up to 16 nm was observed. Micro-mechanical properties, i.e., hardness and elastic modulus were determined using conventional load-controlled nanoindentation testing. the annealed films had 3-times lower hardness as-compared to as-deposited ones (∼9 GPa). Based on optical investigations real and imaginary components of refractive index were calculated, both for as-deposited and annealed thin films. The real refractive index component increased after annealing from 2.03 to 2.16, while extinction coefficient increased by an order from 10{sup −4} to 10{sup −3}. Structure modification was analyzed together with optical energy band-gap, Urbach energy and using Wemple–DiDomenico model.

36 MATERIALS SCIENCE↗

Ion-energy distributions at a substrate in reactive magnetron sputtering discharges in Ar/H{sub 2}S from copper, indium, and tungsten targets

Ion-energy distributions from copper, indium, and tungsten targets were measured during reactive sputtering in argon-hydrogen sulfide (H{sub 2}S) mixtures, since reactive magnetron sputtering of sulfides from metallic targets is of increasing interest, especially for photovoltaic applications (buffer and absorber layers, i.e., CuInS{sub 2}, In{sub 2}S{sub 3}, or WS{sub 2}). The mass spectra of the ions show a wide range of molecules H{sub x}S{sub n} derived from H{sub 2}S by plasma-assisted attachment both for positive (n{<=}9) and for negative (n{<=}6) ions. From the copper and the indium targets metallic ions (Cu{sup +}, In{sup +}) could be detected. While tungsten and indium sulfur compounds were found, copper does not form compounds with sulfur, caused by its lower chemical reactivity. Positive (Ar{sup +}, S{sup +}, W{sup +}, Cu{sup +}, In{sup +}, etc.) as well as negative ions (S{sup -}, InS{sup -}, WS{sub 3}{sup -}) were measured for dc and rf (27 MHz) plasma excitations. The positive ions originate mainly from the plasma in front of the substrate and exhibit energies of about 12 eV for the dc and 18 eV for the rf discharge for the substrate at floating potential. The energy difference is caused by the higher electron temperature in the rf compared to the dc discharge. The ion-energy distributions of negative ions exhibit two distinct peaks. The high-energetic peak can be attributed to ions accelerated in the cathode dark space to a high energy (up to more than 400 eV) corresponding to the cathode (target) voltage. The second peak has its maximum at zero energy decreasing steeply up to energies of about 100 eV. These ions are generated by charge-exchange collisions of energetic species from the target (reflected neutral argon, negative sulfur ions, etc.) on their passage from the target to the substrate caused by the high charge-exchange cross section. rf magnetron sputtering leads to significantly lower energies of negative ions from the target, caused by the lower discharge voltages, which could be advantageous for the deposition of active semiconducting sulfide films.

36 MATERIALS SCIENCE↗

Two-domain formation during the epitaxial growth of GaN (0001) on c-plane Al{sub 2}O{sub 3} (0001) by high power impulse magnetron sputtering

We study the effect of high power pulses in reactive magnetron sputter epitaxy on the structural properties of GaN (0001) thin films grown directly on Al{sub 2}O{sub 3} (0001) substrates. The epilayers are grown by sputtering from a liquid Ga target, using a high power impulse magnetron sputtering power supply in a mixed N{sub 2}/Ar discharge. X-ray diffraction, micro-Raman, micro-photoluminescence, and transmission electron microscopy investigations show the formation of two distinct types of domains. One almost fully relaxed domain exhibits superior structural and optical properties as evidenced by rocking curves with a full width at half maximum of 885 arc sec and a low temperature band edge luminescence at 3.47 eV with the full width at half maximum of 10 meV. The other domain exhibits a 14 times higher isotropic strain component, which is due to the higher densities of the point and extended defects, resulting from the ion bombardment during growth. Voids form at the domain boundaries. Mechanisms for the formation of differently strained domains, along with voids during the epitaxial growth of GaN are discussed.

36 MATERIALS SCIENCE↗

Influence of plasma-generated negative oxygen ion impingement on magnetron sputtered amorphous SiO{sub 2} thin films during growth at low temperatures

Growth of amorphous SiO{sub 2} thin films deposited by reactive magnetron sputtering at low temperatures has been studied under different oxygen partial pressure conditions. Film microstructures varied from coalescent vertical column-like to homogeneous compact microstructures, possessing all similar refractive indexes. A discussion on the process responsible for the different microstructures is carried out focusing on the influence of (i) the surface shadowing mechanism, (ii) the positive ion impingement on the film, and (iii) the negative ion impingement. We conclude that only the trend followed by the latter and, in particular, the impingement of O{sup -} ions with kinetic energies between 20 and 200 eV, agrees with the resulting microstructural changes. Overall, it is also demonstrated that there are two main microstructuring regimes in the growth of amorphous SiO{sub 2} thin films by magnetron sputtering at low temperatures, controlled by the amount of O{sub 2} in the deposition reactor, which stem from the competition between surface shadowing and ion-induced adatom surface mobility.

36 MATERIALS SCIENCE↗

Plasma potential mapping of high power impulse magnetron sputtering discharges

Pulsed emissive probe techniques have been used to determine the plasma potential distribution of high power impulse magnetron sputtering (HiPIMS) discharges. An unbalanced magnetron with a niobium target in argon was investigated for a pulse length of 100 {mu}s at a pulse repetition rate of 100 Hz, giving a peak current of 170 A. The probe data were recorded with a time resolution of 20 ns and a spatial resolution of 1 mm. It is shown that the local plasma potential varies greatly in space and time. The lowest potential was found over the target's racetrack, gradually reaching anode potential (ground) several centimeters away from the target. The magnetic presheath exhibits a funnel-shaped plasma potential resulting in an electric field which accelerates ions toward the racetrack. In certain regions and times, the potential exhibits weak local maxima which allow for ion acceleration to the substrate. Knowledge of the local E and static B fields lets us derive the electrons'ExB drift velocity, which is about 10{sup 5} m/s and shows structures in space and time.

36 MATERIALS SCIENCE↗

Pulsing frequency induced change in optical constants and dispersion energy parameters of WO{sub 3} films grown by pulsed direct current magnetron sputtering

In this work, we present the pulsing frequency induced change in the structural, optical, vibrational, and luminescence properties of tungsten oxide (WO{sub 3}) thin films deposited on microscopic glass and fluorine doped tin oxide (SnO{sub 2}:F) coated glass substrates by pulsed dc magnetron sputtering technique. The WO{sub 3} films deposited on SnO{sub 2}:F substrate belongs to monoclinic phase. The pulsing frequency has a significant influence on the preferred orientation and crystallinity of WO{sub 3} film. The maximum optical transmittance of 85% was observed for the film and the slight shift in transmission threshold towards higher wavelength region with increasing pulsing frequency revealed the systematic reduction in optical energy band gap (3.78 to 3.13 eV) of the films. The refractive index (n) of films are found to decrease (1.832 to 1.333 at 550 nm) with increasing pulsing frequency and the average value of extinction coefficient (k) is in the order of 10{sup −3}. It was observed that the dispersion data obeyed the single oscillator of the Wemple-Didomenico model, from which the dispersion energy (E{sub d}) parameters, dielectric constants, plasma frequency, oscillator strength, and oscillator energy (E{sub o}) of WO{sub 3} films were calculated and reported for the first time due to variation in pulsing frequency during deposition by pulsed dc magnetron sputtering. The E{sub o} is change between 6.30 and 3.88 eV, while the E{sub d} varies from 25.81 to 7.88 eV, with pulsing frequency. The Raman peak observed at 1095 cm{sup −1} attributes the presence of W-O symmetric stretching vibration. The slight shift in photoluminescence band is attributed to the difference in excitons transition. We have made an attempt to discuss and correlate these results with the light of possible mechanisms underlying the phenomena.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗