A Transmission Electron Microscopy Study of a Refractory Metal Grain from a Calcium-Aluminum-Rich Inclusion in the Leoville CV3 Chondrite

Introduction: Calcium-aluminum-rich inclusions (CAIs) are an important component of chondritic meteorites. They can contain materials that are thermodynamically predicted and isotopically age dated to be among the first-formed solids in our solar system [1-5]. Observed in some CAIs are micron to sub-micron sized inclusions rich in Fe, Ni, and high-Z elements such as Pt, Os, Ir and W, in the form of refractory metal nuggets (RMNs), fremdlinges, and ‘nugget like objects’ (NLOs) [1,6]. Refractory siderophile elements such as Os, Ir and Ru are thermodynamically predicted to condense at temperatures well in excess of the major CAI phases such as melilite, perovskite, spinel and hibonite [2,7-9]. These refractory metal inclusions in CAIs can therefore serve as probes into the thermodynamic landscape of the early solar protoplanetary disk. Here we report on a refractory grain identified in a CAI of the Leoville CV3 chondrite. This work is part of an ongoing effort to gain insight into the thermochemistry of the early solar system through systematic analyses of the structure and chemistry of various components in CAIs [10-13]. Sample and Analytical Techniques: A fluffy type A CAI (Fig. 1A) was identified in a section of the Leoville, CV3 chondrite (Center for Meteorite Studies, Arizona State University collection, #821_C_3) using a JOEL-JXA 8530F electron microprobe at Arizona State University. Backscattered electron (BSE) imaging and energy-dispersive X-ray spectroscopy (EDS) were used to identify refractory metal grains in the CAI using a Thermo Fisher (formerly FEI) Helios NanoLab 660 G3 focused-ion-beam scanning-electron microscope (FIBSEM) located at the Kuiper Materials Imaging and Characterization Facility (KMICF) at the Lunar and Planetary Laboratory, University of Arizona. The FIB is equipped with an EDAX EDS system. We selected one of the larger (micron-sized) refractory metal grains, designated as ‘Spud’ (Fig. 1B) for further analysis. ‘Spud’ was extracted and thinned to electron transparency (<100 nm) using the FIB-SEM located in KMICF, following methods described by [14- 15]. The FIB section was analyzed using a 200 keV Hitachi HF5000 scanning transmission electron microscope (S/TEM) located at KMICF. The HF5000 is equipped with cold-field emission gun, 3rd-order spherical aberration corrector for STEM imaging, and an Oxford Instruments X-Max N 100 TLE energydispersive spectroscopy (EDS) system with dual 100 mm2 windowless silicon-drift detectors (Ω = 2.0 sr). Selected-area electron-diffraction (SAED) patterns were acquired to aid in determination of crystallinity and phase. Results: The mineralogy, texture, and morphology of the CAI are consistent with that of a fluffy type A (FTA) CAI [16]. BSE imaging at high magnifications revealed grains with high contrast, indicative of compositions rich in elements of higher atomic number relative to surrounding material. These high-Z grains have sizes that range from ∼250 nm to 4 µm. EDS analyses confirm that the bright grains are metal-rich inclusions. A minor fraction of the grains are composed of only Fe and Ni, but the majority (∼60%) of the identified inclusions also contained various refractory siderophiles including Os, Ru, Zr, Ir and Mo. EDS analysis on the FIB-SEM of Spud shows that it contains Fe, Ni, Mo and Ru. High-angle annular dark-field (HAAFD) imaging and EDS mapping in the TEM (Fig. 2) show that Spud occurs in melilite (Ca1.9Al1.99Si1.06O7). Spud contains a subhedral to anhedral morphology and is compositionally heterogenous (polyphasic, Fig. 2). Local spatial correlation occurs among Fe, Ni, and Pt, and also among Os, Ru, and Mo. SAED patterns show that the Fe-Ni-Pt, Fe-Os-Mo-Ru and Fe-Pt regions are crystalline. Discussion: CAIs can contain various types of inclusions rich in Fe, Ni and refractory siderophiles such as Os, Ru, W and Pt [1]. RMNs are micron-sized, single phase alloy grains and can contain Os, Ir, Ru and Rh [1,7,17]. NLOs are also micron-sized inclusions, but contain two phases, a refractory metal, and an oxide [6]. Fremdlinge are the largest of such inclusions (tens of microns in size) and are complex aggregates of Fe-Ni alloy, silicates, oxides, and sulfides [1,17]. While the size of Spud matches previous descriptions of RMNs and NLOs, Spud is neither a single-phase alloy like RMNs, nor does it contain one metal phase and one oxide like NLOs. Spud does not match the above described categories of refractory metal inclusions. The presence of refractory siderophiles such as Mo, Os, Ru, and Pt suggests a high-temperature origin. Thermodynamic modelling by [7] indicates condensation temperatures of 1917 K, 1693 K, 1613 K and 1415 K for Os, Mo, Ru and Pt respectively. These models also show that following the initial condensation of a refractory metal, alloying of solutes such as Fe, Ni and W, occurs in levels proportional to their partial pressures in the surrounding gas. Such alloying occurs at temperatures above the condensation temperatures of common CAI phases such as melilite (1529 K), perovskite (1441 K), spinel (197 K) and forsterite (1354 K) [2]. The polyphasic nature of Spud could be the result of such high-temperature alloying, possibly shortly after the condensation of Mo and Ru at 1693 K and 1613 K respectively. That Spud occurs as an inclusion is consistent with it having formed prior to and at temperature above that of its host melilite in this FTA CAI, which is qualitatively consistent with such prior thermodynamic modeling. Further, the polyphasic nature of Spud is similar to refractory grains from a FTA CAI in the Northwest Africa (NWA) 8323, CV3 chondrite [11-13]. These data suggest that such refractory metal grains could have been widespread in the inner and early solar protoplanetary disk and represent some of the earliest formed solids to have condensed. Acknowledgments: Research and instrumentation supported by NASA grants #NNX12AL47G, #NNX15AJ22G and #80NSSC19K0509, and NSF grants #1531243 and #0619599. Fig 2. STEM data on ‘Spud’. HAADF Image (Top) False-color EDS Maps (Bottom) References: [1] MacPherson G. J. (2014) T. of Geochem. Vol I: Met. And Cosmochem. Processes, 139-179. [2] Lodders K. (2003) ApJ, 591, 1220-1247. [3] Ebel D. S. (2006) Met. & the Early S. Sys. II., 253- 277. [4] Amelin Y. (2002) Science, 297, 1678-1683. [5] Connelly J.N. et.al. (2012) Science, 338, 651-655. [6] Schwander D. et al. (2015) GCA, 18, 70-87. [7] Palme H. and Wlotzka F. (1976) EPSL, 33, 45-60. [8] Berg T. et al. (2009) ApJ, 702, 172-176. [9] Liffman K. et al. (2021) Icarus, 221, 89-105. [10] Zega T.J. et al. (2021) PSJ, 2, 115. [11] Ramprasad T. et al. (2020) LPSC LI, Abstract #2472. [12] Ramprasad T. et al. (2021) Microscopy & Microanalysis, S1, 2792-2794. [13] Ramprasad T. et al. (2021) 84th MetSoc, Abstract #6123. [14] Zega T.J. et al. (2007) MAPS, 42, 1373-1386. [15] Ramprasad T. et al. (2022) MAPS, in revision. [16] Grossman L. (1975), GCA, 39, 433-454. [17] El Goresy A. et al. (1978) LPSC IX, Abstract#1100

T. Ramprasad↗

Characterization of Inclusion Populations in Mn-Si Deoxidized Steel

Four plant heats of Mn-Si deoxidized steel were conducted to follow the evolution of the inclusion population through ladle furnace (LF) treatment and subsequent vacuum treatment (VT). The liquid steel was sampled, and the chemical composition and size distribution of the inclusion populations were characterized. The Gumbel generalized extreme-value (GEV) and generalized Pareto (GP) distributions were used for the statistical analysis of the inclusion size distributions. The inclusions found at the beginning of the LF treatment were mostly fully liquid SiO{sub 2}-Al{sub 2}O{sub 3}-MnO inclusions, which then evolved into fully liquid SiO{sub 2}-Al{sub 2}O{sub 3}-CaO-MgO and partly liquid SiO{sub 2}-CaO-MgO-(Al{sub 2}O{sub 3}-MgO) inclusions detected at the end of the VT. The final fully liquid inclusions had a desirable chemical composition for plastic behavior in subsequent metallurgical operations. The GP distribution was found to be undesirable for statistical analysis. The GEV distribution approach led to shape parameter values different from the zero value hypothesized from the Gumbel distribution. According to the GEV approach, some of the final inclusion size distributions had statistically significant differences, whereas the Gumbel approach predicted no statistically significant differences. The heats were organized according to indicators of inclusion cleanliness and a statistical comparison of the size distributions.

36 MATERIALS SCIENCE↗

Formation of Plastic Inclusions in U71Mnk High-Speed Heavy-Rail Steel Refined by CaO-SiO{sub 2}-Al{sub 2}O{sub 3}-MgO Slag

To precisely control the characteristics of nonmetallic inclusions with high plasticity in U71Mnk high-speed heavy-rail steel deoxidized by Si and Mn, the chemical composition of CaO-SiO{sub 2}-Al{sub 2}O{sub 3}-MgO slag in the ladle furnace (LF) refining process was optimized by thermodynamic calculations. Relationships among the refining slag, nonmetallic inclusions, and elemental concentrations in the steels were analyzed to obtain the conditions for determining the optimal composition of refining slag. The optimal compositions and the component activities of CaO-SiO{sub 2}-Al{sub 2}O{sub 3}-MgO refining slag were determined and discussed according to calculations using FactSage 7.0. Finally, ten industrial experiments were performed. Variations in the compositions of LF refining slag, inclusions, and steel, as well as the sizes of the inclusions, and metallographic classification assessment of the U71Mnk steel product, were investigated and discussed to verify the feasibility and effectiveness of the optimized LF refining slag. Kinetics of steel–slag and steel-inclusion reactions during LF refining was studied and compared. The results show that to obtain low [O], [Al], and [S] contents and inclusions with high plasticity in molten steel, the optimal composition of the LF refining slag should be CaO: 44.2 to 51.7 wt pct, SiO{sub 2}: 41.4 to 47.0 wt pct, Al{sub 2}O{sub 3}: 0 to 4.7 wt pct and MgO 5.0 to 7.0 wt pct, where the basicity R is above 1.00 and the C/A ratio is above 9.00. After the LF refining process, the contents of total oxygen (T.O.), [Al], and [S] gradually stabilized in the range of 0.0008 to 0.0012 wt pct, 0.002 to 0.0028 wt pct and 0.0026 to 0.0037 wt pct, respectively. The densities of the three kinds of typical inclusions (CaO-SiO{sub 2}-Al{sub 2}O{sub 3}-MgO, MnS, and CaO-SiO{sub 2}-Al{sub 2}O{sub 3}-MgO-MnS) also decreased and reached approximately 0.25/mm{sup 2}, and no inclusion larger than 6.0 μm was found. The composition of the inclusions gradually changed into the optimal range in the CaO-SiO{sub 2}-Al{sub 2}O{sub 3}-MgO slag system during the LF refining process.

36 MATERIALS SCIENCE↗

Deformability of Oxide Inclusions in Tire Cord Steels

The deformation of oxide inclusions in tire cord steels during hot rolling was analyzed, and the factors influencing their deformability at high and low temperatures were evaluated and discussed. The aspect ratio of oxide inclusions decreased with the increasing reduction ratio of the steel during hot rolling owing to the fracture of the inclusions. The aspect ratio obtained after the first hot-rolling process was used to characterize the high-temperature deformability of the inclusions. The deformation first increased and then decreased with the increasing (MgO + Al{sub 2}O{sub 3})/(SiO{sub 2} + MnO) ratio of the inclusions. It also increased with the decreasing melting temperatures of the inclusions. Young’s modulus was used to evaluate the low-temperature deformability of the inclusions. An empirical formula was fitted to calculate the Young’s moduli of the oxides using the mean atomic volume. The moduli values of the inclusions causing wire fracture were significantly greater than the average. To reduce fracture in tire cord steel wires during cold drawing, it is proposed that inclusions be controlled to those with high SiO{sub 2} content and extremely low Al{sub 2}O{sub 3} content. This proposal is based on the hypothesis that the deformabilities of oxides during cold drawing are inversely proportional to their Young’s moduli. The future study thus proposed includes an experimental confirmation for the abovementioned predictions.

36 MATERIALS SCIENCE↗

Model of Inclusion Evolution During Calcium Treatment in the Ladle Furnace

Calcium treatment of steel is typically employed to modify alumina inclusions to liquid calcium aluminates. However, injected calcium also reacts with the dissolved sulfur to form calcium sulfide. The current work aims to develop a kinetic model for the evolution of oxide and sulfide inclusions in Al-killed alloyed steel during Ca treatment in the ladle refining process. The model considers dissolution of the calcium from the calcium bubbles into the steel and reduction of calcium oxide in the slag to dissolved calcium. A steel–inclusion kinetic model is used for mass transfer to the inclusion interface and diffusion within the calcium aluminate phases formed on the inclusion. The inclusion–steel kinetic model is then coupled with a previously developed steel–slag kinetic model. The coupled inclusion–steel–slag kinetic model is applied to the chemical composition changes in molten steel, slag, and evolution of inclusions in the ladle. The result of calculations is found to agree well with an industrial heat for species in the steel as well as inclusions during Ca treatment.

36 MATERIALS SCIENCE↗

Inclusion Characterization and Formation Mechanisms in Spring Steel Deoxidized by Silicon

To elucidate the mechanism of formation of inclusions in microalloyed spring steel deoxidized by Si, their number, morphology, and chemical compositions were analyzed by electron probe X-ray microanalysis. Wavelength-dispersive spectrometry and Monte Carlo simulation were used to confirm the existence of inherent FeO in the inclusions. Additions of Nb and V did not have an observable influence on the formation of inclusions. Based on the major chemical compositions, the inclusions in spring steel were classified into four types: CaO-SiO{sub 2}, Al{sub 2}O{sub 3}-SiO{sub 2}, Al{sub 2}O{sub 3}-SiO{sub 2}-CaO, and MnS. Most CaO-SiO{sub 2} inclusions were around 10 μm in diameter, with their composition close to that of the refining slag and liquidus temperatures all below 1400 °C. The Al{sub 2}O{sub 3}-SiO{sub 2} inclusions were mainly attributed to deoxidization products. They were usually multiphased with liquidus temperatures higher than 1500 °C and smaller than 10 μm in diameter. Most Al{sub 2}O{sub 3}-SiO{sub 2}-CaO inclusions with high Al{sub 2}O{sub 3} and SiO{sub 2} contents originated from the coalescence of CaO-SiO{sub 2} and Al{sub 2}O{sub 3}-SiO{sub 2} inclusions; those with high CaO and SiO{sub 2} contents were considered to form via reduction of CaO-SiO{sub 2} inclusions by Al dissolved in the steel.

36 MATERIALS SCIENCE↗

Evolution Mechanism of Inclusions in Medium-Manganese Steel by Mg Treatment with Different Aluminum Contents

To investigate the effect of magnesium addition on the evolution of inclusions in medium-manganese steel with different aluminum contents, both thermodynamic calculation and high-temperature simulation experiments were carried out in the present work. The in situ observation experiments were used to clarify the related evolution process of inclusions. The samples taken from the melts were analyzed by scanning electron microscopy and energy dispersive spectroscopy. The compositions of steel were determined by inductively coupled plasma-optical emission spectrometer. The results show that the aluminum content in steel has a certain influence on the magnesium content, under the same conditions, magnesium content increases with increasing aluminum content. The inclusions transformed from MnO·Al{sub 2}O{sub 3} to Al{sub 2}O{sub 3} when the aluminum content was higher than 0.0076 mass pct. After magnesium treatment, the inclusions gradually transformed into MgO·Al{sub 2}O{sub 3}, and the MgO/Al{sub 2}O{sub 3} mole ratio in inclusions decreased with the increase of aluminum content. The diameter of the inclusions decreased, and number density of inclusions increased in steel after magnesium addition. The phenomenon that large-sized cluster-like Al{sub 2}O{sub 3} inclusions transform into finely dispersed Mg-containing inclusions was firstly observed in situ by confocal laser scanning microscope.

36 MATERIALS SCIENCE↗

Characteristics of Nozzle Clogging and Evolution of Oxide Inclusion for Al-Killed Ti-Stabilized 18Cr Stainless Steel

Characteristics of nozzle clogging and evolution of oxide inclusion were studied by sampling the deposits of submerged entry nozzle (SEN) and the molten steel in tundish during Al-killed Ti-stabilized 18Cr stainless steelmaking process. The deposits found in the clogging of SEN were mainly composed of frozen steel and inclusions. The inclusions in the deposits and tundish were both mainly (MgO-Al{sub 2}O{sub 3}){sub rich}-CaO-TiO{sub x}. The compositions of most inclusions were Liquid+Spinel or Liquid+TiSp phase. The (MgO-Al{sub 2}O{sub 3}){sub rich}-CaO inclusions that were not effectively modified by calcium treatment could be a source of clogging. By combining both the experimental results and thermodynamic calculation, (MgO-Al{sub 2}O{sub 3}){sub rich}-TiO{sub x} inclusions (TiSp inclusions) would be formed with the decreasing temperature in steel during continuous casting, which could be transported and accumulated on the inner wall of the SEN. Increasing the calcium content in the molten steel could decrease the formation of TiSp inclusions. During continuous casting, these inclusions accumulated on the inner wall of the SEN and gradually formed porous network of clog. Molten steel would gradually solidify in the porous space of the clog due to the increased residence time of the molten steel when flowing through it. The clogging gradually increased and caused the shutdown of continuous casting.

36 MATERIALS SCIENCE↗

Effects of excess Te on flux inclusion formation in the growth of cadmium zinc telluride when forced melt convection is applied

The presence of second phase defects, particularly flux inclusions of tellurium rich composition, are of great concern for charge collection efficiency in cadmium zinc telluride (CZT) and cadmium telluride (CT) material intended for applications such as radiation detection. These inclusions can distort applied electric field lines within the detector as well as act as trapping centers for charge carriers. Reduction and/or elimination of these inclusions is required to achieve appropriate charge collection efficiencies, especially in detectors of thicknesses greater than 5 mm. These so-called flux inclusions are understood to form as a consequence of constitutional undercooling at the crystal growth interface. In this study, a forced melt convection technique was applied in Vertical Bridgman (VB) melt growth of CZT without reducing imposed growth rates of ~2 mm/hr. Several rotation profiles were tested while adjusting the melt composition from 51.62 to 61.75 atomic percent (at%) Te where the Te concentration was initially increased to improve overall material purity. With forced melt convection, the best inclusion distributions were achieved with highly Te rich melt compositions, far beyond the stoichiometric composition range for the CZT system. Average inclusion diameters were reduced to 2 µm while inclusions greater than 5 µm were essentially eliminated. Composition analyses of these ingots revealed near equilibrium concentrations of Te, even with ingots grown from Te concentrations as high as 61.75 at% Te. In this paper, a recipe for the reduction of inclusions in CZT melt growth is put forward and the implications of this method on our understanding of inclusion formation are discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The effects of carbonaceous inclusions and their distributions on dynamic failure processes in boron carbide ceramics

Commercially available boron carbide ceramics typically have heterogeneous microstructures that contain distributions of processing-induced inclusions. The inclusions that are rich in carbon (i.e., carbonaceous) govern the underlying mechanisms of brittle fracture through wing crack formation, and thus dictate the mechanical response of the ceramic. In this study, we investigate the dynamic failure of five boron carbide ceramic materials with different inclusion populations. All of the materials were prepared by hot-pressing; four of these boron carbides contained different sizes and concentrations of carbonaceous inclusions, while one contained no carbonaceous inclusions. The heterogeneity distributions were characterized in some detail for statistical analysis using scanning electron microscopy and quantitative image analysis. A modified compression Kolsky bar setup with in situ ultra-high-speed microscopic imaging (10 million frames per second) was then used to study the influence of the inclusion distributions on the dynamic failure processes in these materials, at nominal high strain rates of 10 2 -10 3 s -1 . The in situ ultra-high-speed microscopy highlighted the link between micro and macroscale failure processes and demonstrated that the carbonaceous inclusions are indeed the preferential sites for nucleation of wing cracks, as previously hypothesized based on post-mortem observations. The relative orientation of an inclusion with respect to the compression axis was shown to affect the likelihood that it would participate in crack nucleation. In conclusion, all of the ceramics were also found to have orientation-dependent peak compressive stress, regardless of the presence of carbonaceous inclusions, suggesting that grain orientation distributions are also important.

36 MATERIALS SCIENCE↗

Proximity-dependent proteomics of the Chlamydia trachomatis inclusion membrane reveals functional interactions with endoplasmic reticulum exit sites

Chlamydia trachomatis is the most common bacterial sexually transmitted infection, responsible for millions of infections each year. Despite this high prevalence, the elucidation of the molecular mechanisms of Chlamydia pathogenesis has been difficult due to limitations in genetic tools and its intracellular developmental cycle. Within a host epithelial cell, chlamydiae replicate within a vacuole called the inclusion. Many Chlamydia –host interactions are thought to be mediated by the Inc family of type III secreted proteins that are anchored in the inclusion membrane, but their array of host targets are largely unknown. To investigate how the inclusion membrane proteome changes over the course of an infected cell, we have adapted the APEX system of proximity-dependent biotinylation. APEX is capable of specifically labeling proteins within a 20 nm radius in living cells. We transformed C. trachomatis to express the enzyme APEX fused to known inclusion membrane proteins, allowing biotinylation and pull-down of inclusion-associated proteins. Using quantitative mass spectrometry against APEX labeled samples, we identified over 400 proteins associated with the inclusion membrane at early, middle, and late stages of epithelial cell infection. This system was sensitive enough to detect inclusion interacting proteins early in the developmental cycle, at 8 hours post infection, a previously intractable time point. Mass spectrometry analysis revealed a novel, early association between C. trachomatis inclusions and endoplasmic reticulum exit sites (ERES), functional regions of the ER where COPII-coated vesicles originate. Pharmacological and genetic disruption of ERES function severely restricted early chlamydial growth and the development of infectious progeny. APEX is therefore a powerful in situ approach for identifying critical protein interactions on the membranes of pathogen-containing vacuoles. Furthermore, the data derived from proteomic mapping of Chlamydia inclusions has illuminated an important functional role for ERES in promoting chlamydial developmental growth.

59 BASIC BIOLOGICAL SCIENCES↗

Physical Education Teachers’ Representations of Their Training to Promote the Inclusion of Students with Disabilities

School inclusion is based on the need to adopt and implement a holistic view of education, training, and human development embodied in the idea of everyone, for everyone. In the context of Physical Education (PE), there are still several constraints to the realization of this universal desideratum. Among these, teacher training and qualification for the inclusion of students with Specific Health Needs (SHNs) stands out. That is, students with physical and mental health problems whose impact is significantly manifested in the learning process. Thus, the objective of this study was to identify the representations of PE teachers about their training to develop inclusive processes with students with SES. Participants in this study were 151 PE teachers from different regions and districts of Portugal (Algarve, Aveiro, Castelo Branco, Lisbon, Porto, and Viseu) who had 23.6 ± 8.1 years of teaching service. Teachers answered an online questionnaire, on the Google Forms platform, with open and closed questions about their education and training to develop inclusive processes in PE. The results indicate two significant dimensions: (1) initial training for teaching inclusive PE and (2) continuous training for inclusion. Regarding initial training, a large majority of the teachers under study, at the end of their initial training, did not have the essential skills to teach PE to students with SES. It was also identified that a large majority reported not having had any contact with students with SES throughout their training process for teaching. It was also recognized that this training was not adjusted to the development of intervention skills with students with SHN. Regarding continuous training, it was identified that attendance at this training increased their skills to teach PE to students with SHN. Workshops/actions/training courses are the main training models adopted. However, it is recognized that the training provided does not respond concretely to their training needs to intervene with students with SHN, since teachers essentially seek to improve intervention in the context of inclusive physical education. We conclude that teacher training for inclusion is not yet fully adjusted to the reality of the inclusive school paradigm. In this sense, in practical terms, the following are suggested: (1) the need for reinforcement in study plans with specific and long-term curricular units; (2) the introduction of real practice components in context; and (3) supervised pedagogical practice in diverse contexts.

Celestino, Tadeu (ORCID:0000000163087981)↗

Shock Re-equilibration of Fluid Inclusions

Fluid inclusions (microscopic volumes of fluid trapped within minerals as they precipitate) are extremely common in terrestrial minerals formed under a wide range of geological conditions from surface evaporite deposits to kimberlite pipes. While fluid inclusions in terrestrial rocks are nearly ubiquitous, only a few fluid inclusion-bearing meteorites have been documented. The scarcity of fluid inclusions in meteoritic materials may be a result of (a) the absence of fluids when the mineral was formed on the meteorite parent body or (b) the destruction of fluid inclusions originally contained in meteoritic materials by subsequent shock metamorphism. However, the effects of impact events on pre-existing fluid inclusions trapped in target and projectile rocks has received little study. Fluid inclusions trapped prior to the shock event may be altered (re-equilibrated) or destroyed due to the high pressures, temperatures, and strain rates associated with impact events. By examining the effects of shock deformation on fluid inclusion properties and textures we may be able to better constrain the pressure-temperature path experienced by terrestrial and meteoritic shocked materials and also gain a clearer understanding of why fluid inclusions are rarely found in meteorite samples.

Madden, M. E. Elwood↗

Effectiveness of Shot Peening in Suppressing Fatigue Cracking at Non-Metallic Inclusions in Udimet(trademark) 720

The fatigue lives of modern powder metallurgy disk alloys can be reduced by over an order of magnitude by surface cracking at inherent non-metallic inclusions. The objective of this work was to study the effectiveness of shot peening in suppressing LCF crack initiation and growth at surface nonmetallic inclusions. Inclusions were carefully introduced at elevated levels during powder metallurgy processing of the nickel-base disk superalloy Udimet 720. Multiple strain-controlled fatigue tests were then performed on machined specimens at 427 and 650 C in peened and unpeened conditions. Analyses were performed to compare the low cycle fatigue lives and failure initiation sites as a function of inclusion content, shot peening, and fatigue conditions. A large majority of the failures in as-machined specimens with introduced inclusions occurred at cracks initiating from inclusions intersecting the specimen surface. The inclusions could reduce fatigue life by up to 100X. Large inclusions had the greatest effect on life in tests at low strain ranges and high strain ratios. Shot peening can be used to improve life in these conditions by reducing the most severe effects of inclusions.

Barrie, Robert L.↗

Diversity in C-Xanes Spectra Obtained from Carbonaceous Solid Inclusions from Monahans Halite

Monahans meteorite (H5) contains fluid inclusion- bearing halite (NaCl) crystals [1]. Microthermometry and Raman spectroscopy showed that the fluid in the inclusions is an aqueous brine and they were trapped near 25degC [1]. Their continued presence in the halite grains requires that their incorporation into the H chondrite asteroid was post metamorphism [2]. Abundant solid inclusions are also present in the halites. The solid inclusions include abundant and widely variable organics [2]. Analyses by Raman microprobe, SEM/EDX, synchrotron X-ray diffraction and TEM reveal that these grains include macromolecular carbon similar in structure to CV3 chondrite matrix carbon, aliphatic carbon compounds, olivine (Fo99−59), high- and low-Ca pyroxene, feldspars, magnetite, sulfides, lepidocrocite, carbonates, diamond, apatite and possibly the zeolite phillipsite [3]. Here we report organic analyses of these carbonaceous residues in Monahans halite using C-, N-, and O- X-ray absorption near edge structure (XANES). Samples and Methods: Approximately 100 nm-thick sections were extracted with a focused ion beam (FIB) at JSC from solid inclusions from Monahans halite. The sections were analyzed using the scanning transmission X-ray microscope (STXM) on beamline 5.3.2.2 at the Advanced Light Source, Lawrence Berkeley National Laboratory for XANES spectroscopy. Results and Discussion: C-XANES spectra of the solid inclusions show micrometer-scale heterogeneity, indicating that the macromolecular carbon in the inclusions have complex chemical variations. C-XANES features include 284.7 eV assigned to aromatic C=C, 288.4-288.8 eV assigned to carboxyl, and 290.6 eV assigned to carbonate. The carbonyl features obtained by CXANES might have been caused by the FIB used in sample preparation. No specific N-XANES features are observed. The CXANES spectra obtained from several areas in the FIB sections include type 1&2 chondritic IOM like, type 3 chondritic IOM like, and none of the above. The natures of the macromolecular carbon in the solid inclusions observed by C-XANES are consistent with the previous studies showing that the carbonaceous solid inclusions have not originated from Monahans parent body [1-3], and have various origins, including various chondritic meteorite parent bodies as well as other unknown source(s).

Kebukawa, Y.↗

First Ti-XANES analyses of refractory inclusions from Murchison

Ti valence in refractory phases is an important recorder of redox conditions in the early solar nebula. We report the valence of Ti in pyroxene, spinel and hibonite in spinel-hibonite and spinel-pyroxene inclusions and in a coarse hibonite grain. A system of solar composition is so reducing that Ti{sup 3+} and Ti{sup 4+} can coexist, making the valence of Ti a valuable indicator of f{sub O2} conditions during formation of nebular materials. The Ti{sup 3+}/Ti{sup 4+} ratios observed in the Ti-rich phases fassaite and rhoenite in coarse-grained refractory inclusions from CV3 chondrites have been shown to be quantitatively consistent with formation in a gas of solar composition (log f{sub O2} = IW-6.8), but these are the only objects in chondrites for which this is the case. Here, we report the valence of Ti in various phases in refractory inclusions from the Murchison CM2 chondrite. The second-highest temperature, major-element-bearing phase predicted to condense from a gas of solar composition, hibonite (ideally CaAl{sub 12}O{sub 19}), can contain significant amounts of Ti, but the hibonite structure can have oxygen vacancies, so calculation of Ti valence from stoichiometry of electron probe analyses is not recommended for hibonite. To date, the only reported measurement of Ti valence in meteoritic hibonite was done by electron spin resonance, on coarse crystals from a Murchison hibonite-perovskite-melilite inclusion. Spinel and most of the pyroxene in CM inclusions contain too little Ti for derivation of Ti{sup 3+}/Ti{sup 4+} ratios from electron probe analyses. X-ray absorption near edge spectroscopy (XANES), however, allows determination of Ti valence in relatively Ti-poor phases. In the present work, we apply synchrotron microXANES to a large hibonite grain from Murchison and to spinel-hibonite (sp-hib) and spinel-pyroxene (sp-pyx) inclusions from Murchison, refractory materials whose Ti{sup 3+}/Ti{sup 4+} ratios have not been previously measured. Analysis of these samples allows comparison of Ti valence of (1) pyroxene in sp-pyx inclusions with that of fassaite; (2) spinel in hibonite-bearing with that of hibonite-free inclusions; and (3) hibonite in sp-hib inclusions with that of large, single grains and the previously analyzed sample.

43 PARTICLE ACCELERATORS↗

Mathematical Model for Collision–Coalescence Among Inclusions in the Bloom Continuous Caster with M-EMS

Mathematical simulation is an effective tool to analyze the fluid flow and the inclusion behavior in the bloom continuous caster with mold electromagnetic stirring (M-EMS). The mathematical model is applied to the modeling of magnetic field, flow field, and inclusion field. Due to the introduction of Archimedes force, the collision mechanism and inclusion’s slipping velocity should be modified in the inclusion mass and population conservation model. Numerically predicted magnetic field, flow field, and the inclusion spatial distribution conform to the experimental results in the existing literature. Lorentz force plays an important role in the fluid flow, and Archimedes force plays an important role in the inclusion distribution in the continuous caster. Due to Brownian collision, Stokes collision, Archimedes collision, and turbulent collision, the coalescence among inclusions occurs in the bloom continuous caster with M-EMS. Among the four types of collisions, turbulent collision occurs most frequently, followed by Archimedes collision and Stokes collision. The frequency of Brownian collision is several orders of magnitudes smaller and is therefore negligible. The inclusion volume concentration, number density, and characteristic radius exhibit a U-shape in the continuous caster without M-EMS. However, with M-EMS, they exhibit an inverted U-shape.

36 MATERIALS SCIENCE↗

Rapid Identification of Calcium Aluminate Inclusions in Steels Using Cathodoluminescence Analysis

We propose a method to identify calcium aluminate inclusions in calcium-treated aluminum-killed steels (Ca{sub 12}Al{sub 14}O{sub 33}, CaAl{sub 4}O{sub 7}, CaAl{sub 12}O{sub 19}, and Al{sub 2}O{sub 3}) using cathodoluminescence (CL) analysis. Such inclusions result in nozzle clogging and melting of the stopper rod during continuous casting. We obtain CL images and CL spectra of calcium aluminate inclusions in model samples of calcium-treated aluminum-killed steel. The model samples are prepared by heating mixtures of Fe powder, Al powder, and Ca shot at 1550 °C in an argon atmosphere. On the basis of the CL colors and CL spectra of the calcium aluminate inclusions, we demonstrate that it is possible to distinguish Ca{sub 12}Al{sub 14}O{sub 33}, CaAl{sub 4}O{sub 7}, CaAl{sub 12}O{sub 19}, and Al{sub 2}O{sub 3} inclusions from CaAl{sub 2}O{sub 4} and Ca{sub 3}Al{sub 10}O{sub 18} inclusions, which do not cause nozzle clogging and melting of the stopper rod, by comparing CL images obtained using digital cameras with and without a built-in filter. The acquisition times for the CL images are less than 10 seconds. Thus, the method we present here can be applied for the rapid detection of harmful calcium aluminate inclusions during continuous casting. The CL spectra also provide basic information to specify compositions in agglomerated calcium aluminate inclusions.

36 MATERIALS SCIENCE↗