Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “GRAIN ORIENTATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Transformation-induced fracture toughening in CuAlBe shape memory alloys: A phase-field study

Stress-induced transformation ahead of a crack tip can relax the stress concentration and produce fracture toughness in shape memory alloys (SMAs). In this manuscript, we utilize a nonisothermal phase-field model (PFM) to study the martensitic transformation induced crack tip toughening in CuAlBe SMA. The force-displacement curve, transformation zone and high stress zone in single crystalline samples show high dependency on the grain orientation with respect to the crack alignment. Comparison between isothermal and non-isothermal simulations reveals that the transformation-induced self-heating decreases the toughening capability by increasing the critical transformation stress. Investigating the high stress zones in CuAlBe and the nontransforming CuAl alloy shows that the toughening is obtained by redistributing the stress concentration far from the crack tip, as the high stress zone follows the tip of the transformation zone. Increasing the acuity of the crack tip is found to generate more symmetric martensite wings on both side of the crack axis and a more localized high stress zone. The polycrystal specimen displays higher toughening due to the internal constraints related to the presence of various grains with difference orientations. Depending on the orientation of the grain inclosing the crack tip, the toughening can be lower or higher. Finally, coincidence of the crack tip with a triple junction is found to improve the toughening behavior.

42 ENGINEERING↗

Dependence of the Bulk Electrical Properties of Multisilicon on the Grain Misorientation Parameters

The recombination activity of intragrain defects in multicrystalline silicon is investigated by the electron or laser beam induced current methods. The interrelation of the grain orientation with the character of the distribution of intragrain defects (dislocations and impurity inclusions) and their recombination activity is revealed. The defect grain structure is investigated using various etching procedures to reveal the defects. It is shown that the defect density and distribution in the grains depend on their orientation relative the growth axis. Therefore, it is intragrain defects and impurities that are to a large degree responsible for degradation of the nonequilibrium carrier lifetime when compared with grain boundaries.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Intragranular twinning, detwinning, and twinning-like lattice reorientation in magnesium alloys

We present that deformation twinning plays a critical role on improving metals or alloys ductility, especially for hexagonal close-packed materials with low symmetry crystal structure. A rolled Mg alloy was selected as a model system to investigate the extension twinning behaviors and characteristics of parent-twin interactions by nondestructive in situ 3D synchrotron X-ray microbeam diffraction. Besides twinning- detwinning process, the twinning-like lattice reorientation process was captured within an individual grain inside a bulk material during the strain reversal. The distributions of parent, twin, and reorientated grains and sub-micron level strain variation across the twin boundary are revealed. A theoretical calculation of the lattice strain confirms that the internal strain distribution in parent and twinned grains correlates with the experimental setup, grain orientation of parent, twin, and surrounding grains, as well as the strain path changes. In conclusion, the study suggests a novel deformation mechanism within the hexagonal close-packed structure that cannot be determined from surface-based characterization methods.

36 MATERIALS SCIENCE↗

A study on texture stability and the biaxial creep behavior of as-hydrided CWSR Zircaloy-4 cladding at the effective stresses from 55 MPa to 65 MPa and temperatures from 300°C to 400°C

The creep rupture of high burnup used nuclear fuel (> 45 GWD/MTU) cladding is regarded as one of the failure mechanisms during long-term dry storage. A high amount of zirconium hydride in the cladding matrix would degrade the mechanical properties of the cladding especially leading to delayed hydride cracking. To better understand the influence of zirconium hydride on the biaxial thermal creep performance and the crystalline texture stability of Zircaloy-4 cladding, the pressurized tube technique is applied to test the durability of the as-hydrided material. Tests were performed on as-received Zircaloy-4 tubular specimens as well as-hydrided ones with targeted 300 wt parts per million (wppm) or 750 wppm hydrogen. The biaxial creep experiments were conducted at temperatures from 300 degrees C to 400 degrees C and at equivalent stresses at mid-wall from 55 MPa to 65 MPa. The hydridation process prior to creep tests induces the formation of FCC delta-hydride platelets along the circumferential direction of the tube. This alignment and phase structure of hydride show no significant change after biaxial creep tests. The creep strain-rate negatively depends on the hydrogen content. The synchrotron wide-angle X-ray diffraction (WAXD) technique and electron backscatter diffraction (EBSD) analysis were applied for the study of the crystallographic orientation relationship. zirconium-to-hydride grain orientation follows Shoji-Nishiyama crystallographic relationship. This relationship is stable before and after creep deformation. These results of creep performance and texture stability of Zircaloy-4 claddings can help support the design basis of interim and long-term dry storage facilities.

creep↗

High stereographic resolution texture and residual stress evaluation using time-of-flight neutron diffraction

Neutron diffraction texture measurements provide bulk averaged textures with excellent grain orientation statistics, even for large-grained materials, owing to the probed volume being of the order of 1 cm 3 . Furthermore, crystallographic parameters and other valuable microstructure information such as phase fraction, coherent crystallite size, root-mean-square microstrain, macroscopic or intergranular strain and stress, etc. can be derived from neutron diffractograms. A procedure for combined high stereographic resolution texture and residual stress evaluation was established on the pulsed-neutron-source-based engineering materials diffractometer TAKUMI at the Materials and Life Science Experimental Facility of the Japan Proton Accelerator Research Center, through division of the neutron detector panel regions. Pole figure evaluation of a limestone standard sample with a well known texture suggested that the precision obtained for texture measurement is comparable to that of the established neutron beamlines utilized for texture measurement, such as the HIPPO diffractometer at the Los Alamos Neutron Science Center (New Mexico, USA) and the D20 angle-dispersive neutron diffractometer at the Institut Laue–Langevin (Grenoble, France). A high-strength martensite–austenite multilayered steel was employed for further verification of the reliability of simultaneous Rietveld analysis of multiphase textures and macro stress tensors. By using a texture-weighted geometric mean micromechanical (BulkPathGEO) model, a macro stress tensor analysis with a plane stress assumption showed a rolling direction–transverse direction (RD–TD) in-plane compressive stress (about –330 MPa) in the martensite layers and an RD–TD in-plane tensile stress (about 320 MPa) in the austenite layers. The phase stress partitioning was ascribed mainly to the additive effect of the volume expansion during martensite transformation and the linear contraction misfit between austenite layers and newly transformed martensite layers during the water quenching process.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-temperature electrical transport behaviors in textured Ca{sub 3}Co{sub 4}O{sub 9}-based polycrystalline ceramics

Highly (00l) oriented Ca{sub 3}Co{sub 4}O{sub 9}-based ceramics were fabricated by spark plasma sintering combined with a dynamic forging process. The grain orientation is effective in lowering the electrical resistivity and enhancing the thermoelectric power factor but with little influence on the Seebeck coefficient. A metallic-to-semiconducting transition temperature can be observed and the activation energy is almost independent of the La-doping. All of the Ca{sub 3}Co{sub 4}O{sub 9}-based ceramic samples exhibit large thermoelectric power, and the figure of merit for La-doped Ca{sub 3}Co{sub 4}O{sub 9} sample can reach 0.26 at 975 K, which can be a promising candidate of p-type material for high-temperature thermoelectric application.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of strain on evolution of dynamic recrystallization in Nb-1 wt%Zr-0.1 wt%C alloy at 1500 and 1600 °C

Uniaxial compression tests were carried out on Nb-1 wt%Zr-0.1 wt%C alloy at temperature of 1500 and 1600 °C and strain rate of 0.1 s{sup −1} to study the evolution of dynamic recrystallization with strain. Electron back scatter diffraction was used to quantify the microstructural evolution. Nb-1Zr-0.1C alloy showed a necklace structure at a strain of 0.9 when deformed at 1500 °C and at strain of 0.6 when deformed at 1600 °C, both at strain rate of 0.1 s{sup −1}. This suggested the occurrence of dynamic recrystallization. At 1500 °C and strain of 0.9 the local average misorientation and the grain orientation spread was low confirming the presence of dynamic recrystallization at this deformation condition. At both 1500 and 1600 °C and all measured strains the recrystallized grains had a strong fiber component of <001>. - Highlights: • Necklace formation of dynamically recrystallized grains occurred at strain of 0.6 and 0.9 for 1500 and 1600 °C, respectively. • Equiaxed microstructures were seen with increase in strain for both 1500 and 1600 °C. • At large strains the predominant recrystallized texture evolved to <001> pole.

36 MATERIALS SCIENCE↗

Pre-compression effect on microstructure evolution of extruded pure polycrystalline magnesium during reversed tension load

Highlights: • Number of twin variants under compression along ED is dependent on grain orientation. • Tension after pre-compression results in low-SF twinning and secondary twinning. • Secondary twinning is facilitated by increasing pre-compression. • Sub-grains due to twinning enhance material strength. - Abstract: The microstructure evolution of extruded pure polycrystalline magnesium under compression followed by subsequent tension in ambient air was investigated. Solid round dog-bone shaped specimens were compressed along the extrusion direction (ED) to − 7.3% and − 12.8% true strains, respectively, and then tensioned along the ED to failure. Electron backscatter diffraction (EBSD) was used to examine the microstructure evolution using companion specimens unloaded at multiple points along the deformation curves. Pre-compression along the ED resulted in {10 1-bar 2} tension twinning which increased in volume with increasing strain until exhaustion at approximately − 10.5% true strain. Tensile reloading of the pre-compressed specimens led to a combination of low Schmid factor twinning, detwinning, and secondary {10 1-bar 2} tension twinning. Detwinning was more significant than secondary twinning in the − 7.3% pre-compressed specimens, where only one secondary twin variant was observed. {10 1-bar 2} secondary twinning was more significant in the − 12.8% pre-compressed specimens, where up to three secondary twin variants were observed. After complete detwinning of primary twins, the secondary twins were retained and appeared as sub-grains. The residual sub-grains resulted from secondary twinning may provide a strengthening mechanism for wrought Mg alloys.

36 MATERIALS SCIENCE↗

Magnetic-field-dependent morphology of self-organized Fe on stepped Si(111) surfaces

The present work reports on Fe thin films grown on vicinal Si(111) substrates via rf magnetron sputtering. The dependencies of the growth mode and magnetic properties of the obtained iron nanostructures on both crystallographic surface orientation and on the direction of the very weak stray magnetic field from the magnetron gun were studied. Scanning tunneling microscopy images showed strong dependence of the Fe grains' orientation on the stray field direction in relation to the substrate's steps demonstrating that, under appropriately directed magnetic field, Si surfaces can be used as templates for well-defined self-assembled iron nanostructures. Magneto-optical Kerr effect hysteresis loops showed an easy-axis coercivity almost one order of magnitude smaller for the film deposited with stray field applied along the steps, accompanied with a change in the magnetization reversal mode. Phenomenological models involving coherent rotation and/or domain-wall unpinning were used for the interpretation of these results.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Well-aligned polycrystalline lanthanum silicate oxyapatite grown by reactive diffusion between solid La{sub 2}SiO{sub 5} and gases [SiO+1/2O{sub 2}]

The c-axis-oriented polycrystalline lanthanum silicate oxyapatite, La{sub 9.48}(Si{sub 5.89}□{sub 0.11})O{sub 26} (□ denotes a vacancy in the Si site), was successfully prepared by the reactive diffusion between randomly grain-oriented La{sub 2}SiO{sub 5} polycrystal and [SiO+1/2O{sub 2}] gases at 1873 K in Ar atmosphere. The polycrystal was characterized using optical microscopy, scanning electron microscopy equipped with energy dispersive X-ray spectroscopy, micro-Raman spectroscopy, X-ray diffractometry, and impedance spectroscopy. The crystal structure (space group P6{sub 3}/m) showed the deficiency of Si site at ca. 1.9%. The bulk oxide-ion conductivity along the grain-alignment direction steadily increased from 9.2 × 10{sup −3} to 1.17 × 10{sup −2} S/cm with increasing temperature from 923 to 1073 K. The activation energy of conduction was 0.23(2) eV. - Graphical abstract: We have successfully prepared the highly c-axis-oriented polycrystalline La{sub 9.48}(Si{sub 5.89}□{sub 0.11})O{sub 26} by the reactive diffusion between randomly grain-oriented La{sub 2}SiO{sub 5} polycrystal and [SiO + 1/2O{sub 2}] gases at 1873 K in Ar atmosphere. The crystal structure (space group P6{sub 3}/m) showed the deficiency of Si site of ca. 1.9%. - Highlights: • The c-axis-oriented polycrystalline La{sub 9.48}(Si{sub 5.89}□{sub 0.11})O{sub 26} is successfully prepared. • Crystal structure of La{sub 9.48}(Si{sub 5.89}□{sub 0.11})O{sub 26} is determined by single-crystal XRD. • The polycrystal shows relatively high oxide ion conductivity along the common c-axis. • Reactive diffusion is successfully used for the preparation of grain-aligned ceramics.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Methodology for analyzing stress states during in-situ thermomechanical cycling in individual lead free solder joints using synchrotron radiation

To examine how a lead-free solder joint deforms in a thermal cycling environment, both the elastic and plastic stress and strain behavior must be understood. Methods to identify evolution of the internal strain (stress) state during thermal cycling are described. A slice of a package containing a single row of solder joints was thermally cycled from 0 C to 100 C with a period of about 1 h with concurrent acquisition of transmission Laue patterns using synchrotron radiation. These results indicated that most joints are single crystals, with some being multicrystals with no more than a few Sn grain orientations. Laue patterns were analyzed to estimate local strains in different crystal directions at different temperatures during a thermal cycle. While the strains perpendicular to various crystal planes all vary in a similar way, the magnitude of strain varies. The specimens were subsequently given several hundred additional thermal cycles and measured again to assess changes in the crystal orientations. These results show that modest changes in crystal orientations occur during thermal cycling.

43 PARTICLE ACCELERATORS↗

Fabrication of L1{sub 1}-type (Co-Ni)-Pt ordered alloy films by sputter deposition

L1{sub 1}-type (Co-Ni)-Pt ordered alloy perpendicular films were successfully fabricated on MgO(111) single crystal substrates using ultrahigh vacuum sputter film deposition; the addition of Ni to Co-Pt was effective to reduce saturation magnetization, M{sub s}, maintaining a large K{sub u} of the order of 10{sup 7} erg/cm{sup 3}. L1{sub 1}-type ordered structures, with the <111> direction (easy axis of magnetization) perpendicular to the films, were successfully fabricated at a substrate temperature of 360 deg. C in a wide composition range with Co content less than 60 at. %. The order parameter, S, was almost a constant of about 0.5 in the stoichiometric composition of (Co{sub 1-X}Ni{sub X}){sub 50}Pt{sub 50}, independent of Ni content, X. L1{sub 1}-type Co-Ni-Pt perpendicular films having a large K{sub u} of (1-2.5)x10{sup 7} erg/cm{sup 3} and a relatively low M{sub s} of 400-700 emu/cm{sup 3} were successfully fabricated in the composition range of 10-35 at. % Co, 20-55 at. % Ni, and bal. Pt. K{sub u} should increase further with enhanced ordering. Experimental results demonstrated the potential of these Co-Ni-Pt ordered films for use in data storage applications due to very high K{sub u} potential comparable to L1{sub 0}-type Fe{sub 50}Pt{sub 50} films, relatively low M{sub s}, the relatively low fabrication temperature, and good controllability of the grain orientation.

36 MATERIALS SCIENCE↗

Deposition of ultrathin AlN films for high frequency electroacoustic devices

The authors investigate the microstructure, crystal orientation, and residual stress of reactively sputtered aluminum nitride (AlN) films having thicknesses as low as 200 down to 25 nm. A two-step deposition process by the dual cathode ac (40 kHz) powered S-gun magnetron enabling better conditions for AlN nucleation on the surface of the molybdenum (Mo) bottom electrode was developed to enhance crystallinity of ultrathin AlN films. Using the two-step process, the residual in-plane stress as well as the stress gradient through the film thickness can be effectively controlled. X-ray rocking curve measurements have shown that ultrathin films grown on Mo using this technology are highly c-axis oriented with full widths at half maximum of 1.8 deg. and 3.1 deg. for 200- and 25-nm-thick films, respectively, which are equal to or even better than the results previously reported for relatively thick AlN films. High-resolution transmission electron microscopy and fast Fourier transform analyses have confirmed strong grain orientation in 25-100-nm-thick films. A fine columnar texture and a continuous lattice microstructure within a single grain from the interface with the Mo substrate through to the AlN surface have been elicited even in the 25-nm-thick film.

36 MATERIALS SCIENCE↗

Automated Crystal Orientation Mapping in py4DSTEM using Sparse Correlation Matching

Crystalline materials used in technological applications are often complex assemblies composed of multiple phases and differently oriented grains. Robust identification of the phases and orientation relationships from these samples is crucial, but the information extracted from the diffraction condition probed by an electron beam is often incomplete. We have developed an automated crystal orientation mapping (ACOM) procedure which uses a converged electron probe to collect diffraction patterns from multiple locations across a complex sample. We provide an algorithm to determine the orientation of each diffraction pattern based on a fast sparse correlation method. We demonstrate the speed and accuracy of our method by indexing diffraction patterns generated using both kinematical and dynamical simulations. We have also measured orientation maps from an experimental dataset consisting of a complex polycrystalline twisted helical AuAgPd nanowire. From these maps we identify twin planes between adjacent grains, which may be responsible for the twisted helical structure. All of our methods are made freely available as open source code, including tutorials which can be easily adapted to perform ACOM measurements on diffraction pattern datasets.

36 MATERIALS SCIENCE↗

Orientation Relationships of Pure Tin on Single Crystal Germanium Substrates

The limited number of independent β-Sn grain orientations resulting from the difficulty in nucleating β-Sn during solidification of Sn-based solders has a large effect on the resulting β-Sn grain size and, hence, on overall solder joint performance and reliability. This study analyzes the efficacy of Ge as a heterogeneous nucleation agent for β-Sn by observing the morphologies and orientation relationships of as-deposited, solid-state annealed, and liquid-state annealed pure Sn films on single crystal Ge (100), (110), and (111) substrates. Here, the results from scanning electron microscopy and electron backscatter diffraction showed that the as-deposited Sn films all deposited with a Sn (001)|| z-axis texture, regardless of the underlying Ge substrate orientation. Solid-state annealing at 150 °C for 5 min did not result in significant dewetting of the Sn films, and the films maintained their as-deposited texture of Sn (001)|| z-axis, regardless of the underlying Ge substrate orientation. Liquid-state annealing at 235 °C for 1 min resulted is large-scale dewetting of the Sn films and re-orientation of the Sn films on the various Ge substrates. After solidification, the Ge (100) and (110) single crystal substrates produced patches of dewetted grains of the same orientation but there were no consistent Sn grain textures after liquid-state annealing, suggesting no single orientation relationship. In contrast, solidification on Ge (111) single crystal substrates resulted in isolated grains with a single Sn film texture and an orientation relationship of (100) Sn ∥(111) Ge and [100] Sn ∥[110] Ge . Density Functional Theory simulations of the experimentally observed Ge (111) sample orientation relationship and the Ge/Sn cube-on-cube orientation relationship suggest favorable relative interfacial binding energies for both interface orientations.

36 MATERIALS SCIENCE↗

Correlating whisker growth and grain structure on Sn-Cu samples by real-time scanning electron microscopy and backscattering diffraction characterization

Whiskers/hillocks grow out of Pb-free Sn coatings used in electronics manufacturing. To determine which grains form whiskers/hillocks, we use scanning electron microscopy and backscattering diffraction to simultaneously monitor the surface morphology and grain structure. To reduce surface roughness, we developed a ''peel-off'' method to prepare ultra-flat samples that were measured repeatedly while whiskers/hillocks formed. We find grains that form into whiskers/hillocks are present in the as-deposited film (i.e., not re-nucleated) and many have horizontal grain boundaries beneath them. Grain rotation during whisker/hillock formation means that measurements performed after the features grow do not indicate their initial grain orientations.

36 MATERIALS SCIENCE↗

Ambient aging of rhenium filaments used in thermal ionization mass spectrometry: Growth of oxo-rhenium crystallites and anti-aging strategies

Degassing is a common preparation technique for rhenium filaments used for thermal ionization mass spectrometric analysis of actinides, including plutonium. Although optimization studies regarding degassing conditions have been reported, little work has been done to characterize filament aging after degassing. In this study, the effects of filament aging after degassing were explored to determine a “shelf-life” for degassed rhenium filaments, and methods to limit filament aging were investigated. Zone-refined rhenium filaments were degassed by resistance heating under high vacuum before exposure to ambient atmosphere for up to 2 months. After degassing the nucleation and preferential growth of oxo-rhenium crystallites on the surface of polycrystalline rhenium filaments was observed by atomic force microscopy and scanning electron microscopy (SEM). Compositional analysis of the crystallites was conducted using SEM-Raman spectroscopy and SEM energy dispersive X-ray spectroscopy, and grain orientation at the metal surface was investigated by electron back-scatter diffraction mapping. Spectra collected by SEM-Raman suggest crystallites are composed primarily of perrhenic acid. The relative extent of growth and crystallite morphology were found to be grain dependent and affected by the dissolution of carbon into filaments during annealing (often referred to as carbonization or carburization). Crystallites were observed to nucleate in region specific modes and grow over time through transfer of material from the surface. Factors most likely to affect the rates of crystallite growth include rhenium substrate properties such as grain size, orientation, levels of dissolved carbon, and relative abundance of defect sites; as well as environmental factors such as length of exposure to oxygen and relative humidity. Thin (~180 nm) hydrophobic films of poly(vinylbenzyl chloride) were found to slow the growth of oxo-rhenium crystallites on the filament surfaces and may serve as an alternative carbon source for filament carburization.

36 MATERIALS SCIENCE↗

Structure of Ultrathin Polycrystalline Iron Films Grown on SiO{sub 2}/Si(001)

The structure of polycrystalline Fe films grown on an oxidized Si(001) surface at room temperature has been studied by the technique of high-energy electron diffraction. It has been found that the grain orientation in the films depends of the amount of deposited iron. In Fe films less than 5 nm thick, grains have been found to be randomly oriented. Fe films more than 5 nm in thickness exhibit the (111) texture with an axis coinciding with the surface normal. The angular dispersion of the [111] direction in the Fe lattice from the surface normal is ±25°. It has been found that as the Fe films become thicker, the (111) texture changes to the (110) texture.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗