A Dendrite-Resistant Sodium/Porous-Carbon Anode for Solid-State Batteries – Strategies and Challenges for Low-Pressure Operation

Sodium solid-state batteries (Na-SSB) have gained interest recently due to the abundance of Na over Li, but they still tend to fail due to dendrites under practical current densities and cycling capacities. To overcome this, Na-SSBs are frequently tested with impractically high applied pressure. In this work, a porous carbon interfacial layer is utilized in conjunction with Na-ß”-Al2O3 solid electrolytes to enable Na-cycling at milder cell pressures. This sodium/porous carbon layer enables improved solid-state Na cycling in symmetric cells, up to a current density of 10 mA cm-2 at 25 °C. Cycling up to 1 mAh cm-2 is challenging with low pressure, but 1 mAh cm-2 capacity can be reliably cycled at 1 mA cm-2 at an elevated temperature of 60 °C in symmetric cells. Finally, the evolution of the interface and sodium/carbon anode is evaluated with cryogenic ion-milling and cross-sectional imaging revealing that, depending on testing temperature, pressure, current density, and capacity, void formation, Na-extraction from porous carbon, delamination of the porous carbon matrix, or a combination of these occurs at the interface between Na-metal and BASE. Despite this, excellent dendrite resistance is achieved, and a full-cell design utilizing a Na-transition metal oxide cathode is still able to achieve an areal capacity of ~ 2.7 mAh cm-2 at 0.125 mA cm-2. This work demonstrates an alternative pathway toward a Na-metal anode for Na-SSBs without the requirement of excessive stack pressure.

low-cost↗

Uncovering the Relationship between Diameter and Height of Electrodeposited Lithium Protrusions in a Rigid Electrolyte

A promising approach for enabling rechargeable batteries with significantly higher energy densities than current lithium-ion batteries is by deploying lithium-metal anodes. However, the growth of lithium protrusions during charging presents significant challenges. Since these protrusions are often branched and filamentous in conventional liquid electrolytes, this problem is referred to in the literature as the “dendrite problem”. While solid electrolytes have the potential to solve this problem, protrusions grow in all electrolytes when the current density exceeds a critical value. Fundamentally understanding the formation is necessary to develop a rational approach for increasing the critical current density, but it is challenging due to the complex interplay between electrochemical and material properties. The diameters and heights of protrusions on lithium-metal anodes stabilized by a rigid block copolymer electrolyte were measured in situ by synchrotron hard X-ray microtomography. The diameter of the shorting protrusions increased linearly with increasing electrolyte thickness. Further, a universal linear relationship between protrusion height and diameter of both shorting and non-shorting protrusions was observed. A model based on the concentrated solution theory was used to establish the electrochemical and mechanical sources for our observations. Here, the computational analysis indicates that elastic and plastic deformation of both the lithium metal and the polymer are important to describe protrusion growth. Both stress-induced current density effects due to the deformation of the electrolyte near the protrusion and plastic deformation of lithium metal combine to give the counterintuitive result: the fastest-growing protrusions have the largest diameter.

25 ENERGY STORAGE↗

Dendritic deformation modes in additive manufacturing revealed by operando x-ray diffraction

Abstract Dynamic solidification behavior during metal additive manufacturing directly influences the as-built microstructure, defects, and mechanical properties of printed parts. How the formation of these features is driven by temperature variation (e.g., thermal gradient magnitude and solidification front velocity) has been studied extensively in metal additive manufacturing, with synchrotron x-ray imaging becoming a critical tool to monitor these processes. Here, we extend these efforts to monitoring full thermomechanical deformation during solidification through the use of operando x-ray diffraction during laser melting. With operando diffraction, we analyze thermomechanical deformation modes such as torsion, bending, fragmentation, assimilation, oscillation, and interdendritic growth. Understanding such phenomena can aid the optimization of printing strategies to obtain specific microstructural features, including localized misorientations, dislocation substructure, and grain boundary character. The interpretation of operando diffraction results is supported by post-mortem electron backscatter diffraction analyses.

Dass, Adrita (ORCID:000000019100635X)↗

Solidification and grain formation in alloys: a 2D application of the grand-potential-based phase-field approach

Solidification is a significant step in the forming of crystalline structures during various manufacturing and material processing techniques. Solidification characteristics and the microstructures formed during the process dictate the properties and performance of the materials. Hence, understanding how the process conditions relate to various microstructure formations is paramount. In this work, a grand-potential-based multi-phase, multi-component, multi-order-parameter phase-field model is used to demonstrate the solidification of alloys in 2D. This model has several key advantages over other multi-phase models such as it decouples the bulk energy from the interfacial energy, removes the constraints for the phase concentration variable, and prevents spurious third-phase formation at the two phase interfaces. Here, the model is implemented in a finite-element-based phase-field modeling code. The role of various modeling parameters in governing the solidification rate and the shape of the solidified structure is evaluated. It is demonstrated that the process conditions such as temperature gradient, thermal diffusion, cooling rate, etc, influence the solidification characteristics by altering the level of undercooling. Furthermore, the capability of the model to capture directional solidification and polycrystalline structure formation exhibiting various grain shapes is illustrated. In both these cases, the process conditions have been related to the growth rate and associated shape of the dendritic structure. As a result, this work serves as a stepping stone towards resolving the larger problem of understanding the process–structure–property–performance correlation in solidified materials.

36 MATERIALS SCIENCE↗

Observation of nanoparticle coalescence during core-shell metallic nanowire growth in colloids via nanoscale imaging

The surface morphology and shape of crystalline nanowires significantly influence their functional properties, including phonon transport, electrocatalytic performance, to name but a few. However, the kinetic pathways driving these morphological changes remain underexplored due to challenges in real-space and real-time imaging at single-particle and atomic resolutions. This study investigates the dynamics of shell (Au, Pd, Pt, Fe, Cu, Ni) deposition on AuAg alloy seed nanowires during core-shell formation. By using chiral/non-chiral seed nanowires, advanced imaging techniques, including liquid-phase transmission electron microscopy (LPTEM), cryogenic TEM, and three-dimensional electron tomography, a three-step deposition process is revealed: heterogeneous nucleation, nanoparticle attachment, and coalescence. It is found that colloidal Ostwald ripening, metal reactivity, and deposition amount modulate nanoparticle size and surface roughness, shaping final morphologies. Noble metal nanoparticles (Au, Ag, Pd, Pt) coalesce with seed nanowire along the 〈111〉 direction, distinct from that of other metals. These findings are consistent across different metals, including Ru, Cu, Fe, and Ni, highlighting the hypothesis of these processes in nanowire formation. These findings enhance traditional crystallographic theories and provide a framework for designing nanowire morphology. Additionally, our imaging techniques may be applied to investigate phenomena like electrodeposition, dendrite growth in batteries, and membrane deformation.

Yang, Dahai↗

The effects of field history on magnetic skyrmion formation in [Pt/Co/Ir] 3 multilayers

Here, we report on the formation of Néel-type magnetic bubble skyrmions at room temperature in [Pt/Co/Ir] 3 multilayered thin films after an in-plane magnetic field treatment. Polar magneto-optical Kerr Effect (p-MOKE) microscopy images show that the dendritic magnetic configurations observed after AC demagnetization evolve into magnetic bubble skyrmions after the application and subsequent removal of an in-plane magnetic field. Micromagnetic simulations were used to systematically investigate the role of the in-plane magnetic field magnitude, misalignment of the sample, and the Dzyaloshinskii-Moriya interactions (DMI) in generating bubble skyrmions during the field treatment. The simulations show that in-plane fields slightly below the saturation field are the most effective at producing skyrmions, and, furthermore, a small field angle away from the sample plane not only leads to improved skyrmion formation but also provides a means to select the skyrmion polarity where the direction of the out-of-plane component of the field is opposite to the direction of the skyrmion cores. This field treatment scheme leads to a simple and reliable way to create magnetic bubble skyrmions in multilayered thin films with DMI.

36 MATERIALS SCIENCE↗

Interface stability of LiCl-rich argyrodite Li 6 PS 5 Cl with propylene carbonate boosts high-performance lithium batteries

In solid-state lithium (Li)-metal batteries (SSLMBs), sulfide-based Li-ion conductors represent one of the most popular solid electrolytes (SEs). However, the development of sulfide-based SSLMBs is significantly hampered by interfacial issues including large solid-solid contact resistance and serious side reactions at the SE/electrode interface. To address these issues, here, we demonstrated a simple and efficient strategy by using LiCl-rich argyrodite Li 6 PS 5 Cl (Li 6 PS 5 Cl-LiCl) SE and trace amount of propylene carbonate (PC) at the SE/electrode interface to facilitate the formation of stable and robust solid electrolyte interphase (SEI). Additionally, the formed SEI not only serves as a buffer layer to passivate the interfacial reactions and suppress Li dendrite growth, but also acts as a bridge for Li-ion conduction to reduce the contact resistance. As a result, the Li||Li symmetric cell exhibited long-term electrochemical cycling stability over 1000 h at a current density of 0.2 mA cm -2 . Furthermore, the assembled Li||Li 4 Ti 5 O 12 (LTO) batteries delivered a specific capacity of 175 mAh g–1 at 0.2 C, and remained an excellent specific capacity of 116 mAh g –1 after 200 cycles at a high current rate of 1 C. These features indicate a feasible strategy to enhance the interfacial property of high-performance SSLMBs.

25 ENERGY STORAGE↗

Current Status and Future Directions of All-Solid-State Batteries with Lithium Metal Anodes, Sulfide Electrolytes, and Layered Ternary Oxide Cathodes

All-solid-state batteries (ASSBs) offer great promise as a next-generation energy storage technology with higher energy density, wider operating temperature range, and improved safety for electric vehicles. ASSBs employing lithium metal anodes (Li), sulfide-based solid-state electrolytes (SSE), and Ni-rich layered transition metal oxide cathodes (LiMO 2 , M = Ni, Mn, Co, Al) are particularly promising due to its superior electrochemical performance compared to other solid-electrolyte systems. However, the battery cycle life at high cathode mass loading and high current is still limited because the failure mechanism is not fully understood. Lithium dendrite growth at the anode or inside a solid electrolyte still represents as a serious risk of cell failure. Interfacial resistance increases attributed to electrolyte decomposition and interfacial void formation at both cathode–electrolyte and anode–electrolyte interfaces lead to gradual capacity fading. In this Review, we present the fundamental challenges and recent scientific understandings of each component in ASSBs. The novel diagnostic tools for these components, especially the interfaces buried under the surface that are often hard for characterization are mainly examined. Lastly, we offer a perspective for future research directions. We hope this Review will provide a timely snapshot of state-of-the-art research progress in ASSBs to accelerate the development of ASSBs.

25 ENERGY STORAGE↗

Epitaxial Electrodeposition of Fe with Controlled In-Plane Variants for a Reversible Metal Anode in an Aqueous Electrolyte

The development of reversible metal anodes is a key challenge for advancing aqueous battery technologies, particularly for scalable and safe stationary energy storage applications. Here, in this study, we demonstrate a strategy to realize epitaxial electrodeposition of iron (Fe) on single-crystal copper (Cu) substrates in aqueous electrolytes. We compare the electrodeposition behavior of Fe on polycrystalline and single-crystalline Cu substrates, revealing that the latter enables highly uniform, dense, and crystallographically aligned Fe growth. Comprehensive electron backscatter diffraction (EBSD) and X-ray diffraction (XRD) analysis confirms the formation of Fe with specific out-of-plane and in-plane orientations, including well-defined rotational variants. Our findings highlight that epitaxial electrodeposition of Fe can suppress dendritic growth and significantly enhance Coulombic efficiency during plating/stripping cycles. This approach bridges fundamental crystallography with practical electrochemical performance, providing a pathway toward high-efficiency aqueous batteries utilizing Earth-abundant materials.

aqueous battery↗

Dual Passivation of Cathode and Anode through Electrode–Electrolyte Interface Engineering Enables Long-Lifespan Li Metal–SPAN Batteries

The reliability and durability of lithium metal (Li 0 )–sulfur batteries are largely limited by the undesired Li 0 plating-stripping irreversibility and the detrimental polysulfide dissolution, yet approaches that can simultaneously address the above anodic and cathodic problems are scarce. In this study, we report the stable operation of a Li 0 -SPAN (sulfurized polyacrylonitrile) battery via an anode–cathode dual-passivation approach. By combination of a fluorinated localized high concentration electrolyte (LHCE) and a Li 3 N-forming additive (TMS-N 3 ), robust and highly conductive electrode passivation layers are formed in situ on the surface of both the Li 0 anode and the SPAN cathode. The resulting highly reversible, dendrite-free, and high-density Li 0 plating morphology enables a high Coulombic efficiency of 99.4%. Advanced tender energy X-ray spectroscopy also reveals the eliminated Li 2 S formation and minimized polysulfide dissolution in SPAN cathodes, leading to a high capacity of 580 mAh/g SPAN and stable cycling with negligible capacity decay (0.7%) for 800 cycles. This electrode–electrolyte interphase engineering strategy has tackled the major limitations of Li–S batteries in both ether- and carbonate-based electrolyte systems and under a wide temperature range from –10 to +50 °C, thus providing insightful guidelines for the rational design of highly durable and high-energy-density Li 0 -S batteries.

25 ENERGY STORAGE↗

Development of HPC based phase field simulations tool for modification of alloy morphology to enhance material properties during additive manufacturing (AM) process

Currently, additive manufacturing (AM) technology is extensively used to manufacture aerospace components because of the unique advantages of the technique in producing custom designs, complex geometries in a near-net fashion that significantly reduces the manufacturing cost, and improved energy efficiency. However, the thermodynamic properties of existing aerospace alloys and the thermal conditions that prevail in most of the powder-bed based additive manufacturing processes lead to undesirable columnar / columnar-dendritic microstructures that promote solidification cracking during the process, and the development of anisotropy in the mechanical properties of the as-built components. Time consuming, energy-intensive post AM treatments are required to recover the mechanical properties of the wrought components for which the existing alloy compositions were designed for. However, novel alloy compositions, that exploit the AM thermal conditions to produce fine, equiaxed grain structures in the as-built condition, with mechanical properties equal to or exceeding those of the wrought work-horse alloy, Ti-6Al-4V has recently been demonstrated in Ti-Cu alloys. Significant energy savings up to 66% can be obtained for a typical aerospace component through digitally designing the AM process, process parameters, and alloy composition. The current project focused on developing a fundamental understanding of the evolution of the columnar to equiaxed transition (CET) occurring during solidification under AM thermal conditions in Ti-Cu and Ti-Cu-X alloys using high-fidelity phase field (PF) simulations using the leadership class computing facilities that exist in the national laboratories. The simulations were able to capture the effect of alloy and process conditions on CET, and clearly showed the beneficial effect of a ternary solute addition to Ti-Cu binary alloys on CET. The simulations indicated that bulk nucleation in the liquid ahead of the solidifying epitaxial front was promoted by a large, transient, thermal undercooling promoted by the mismatch between the growth rate of the dendrite tips in the epitaxial front and the imposed solidification rate. AM experiments performed at Raytheon Technologies Research Center using the same thermal conditions used in the PF simulations indicated the formation of equiaxed grains, although the grain size was bigger than the ones reported in the literature. On the other hand, the equiaxed grain size predicted by PF simulations were smaller than the grain size of Ti-Cu alloys reported in the literature. The industry will follow up the existing work in a future program that would involve further optimization of the process for the Ti-Cu-X alloys to demonstrate the application of the process and the alloy to a specific aerospace component.

36 MATERIALS SCIENCE↗

Interface velocity dependent solute trapping and phase selection during rapid solidification of laser melted hypo-eutectic Al-11at.%Cu alloy

Microstructure formation of a hypo-eutectic Al-11Cu (atom percent) alloy during solidification after laser melting has been studied by transmission electron microscopy (TEM). The evolution of the solid-liquid-interface velocity, V SL , during the solidification process has been determined from direct observation by in-situ TEM. This enabled correlating V SL with development of four distinct microstructure zones. Crystal growth mode transitions from planar to cellular, cellular to dendritic, dendritic to cellular, and cellular to planar, have been observed for the accelerating solid-liquid-interface. The transition from coupled two-phase growth to the single-phase growth occurred for V SL = V a = (0.80±0.05) m/s, where V a is the velocity of absolute stability, at the onset of banded morphology grain formation. The in-situ and post-mortem TEM uniquely permitted determination of the non-equilibrium solidus for the rapidly solidifying Al-11Cu alloy. Experimental evidence for solute clustering and chemical ordering tendencies at length scales on the order of ≤ 5nm has been detected in the single-phase regions of the banded grains. The structural features of the single-phase bands have been interpreted as signatures of ‘frozen in’ configurations present in the liquid boundary layer adjacent to the growing crystal, which has a width of about 3nm. Finally, the nano-scale spatiotemporal resolution experimental TEM studies performed here provided quantitative metrics, e.g. the solidification interface velocity dependent solute concentration of the α-Al phase and the near-atomic scale structure in the single-phase bands, that are uniquely suitable for comparison with theory and model predictions for solidification microstructure development in multicomponent alloys after laser melting.

36 MATERIALS SCIENCE↗

Li 2 S 6 ‐Integrated PEO‐Based Polymer Electrolytes for All‐Solid‐State Lithium‐Metal Batteries

Abstract The integration of Li 2 S 6 within a poly(ethylene oxide) (PEO)‐based polymer electrolyte is demonstrated to improve the polymer electrolyte's ionic conductivity because the strong interplay between O 2− (PEO) and Li + from Li 2 S 6 reduces the crystalline volume within the PEO. The Li/electrolyte interface is stabilized by the in situ formation of an ultra‐thin Li 2 S/Li 2 S 2 layer via the reaction between Li 2 S 6 and lithium metal, which increases the ionic transport at the interface and suppresses lithium dendrite growth. A symmetric Li/Li cell with the Li 2 S 6 ‐integrated composite electrolyte has excellent cyclability and a high critical current density of 0.9 mA cm −2 at 40 °C. Impressive electrochemical performance is demonstrated with all‐solid‐state Li/LiFePO 4 and high‐voltage Li/LiNi 0.8 Mn 0.1 Co 0.1 O 2 cells at 40 °C.

Fang, Ruyi↗

Li 2 S 6 ‐Integrated PEO‐Based Polymer Electrolytes for All‐Solid‐State Lithium‐Metal Batteries

Abstract The integration of Li 2 S 6 within a poly(ethylene oxide) (PEO)‐based polymer electrolyte is demonstrated to improve the polymer electrolyte's ionic conductivity because the strong interplay between O 2− (PEO) and Li + from Li 2 S 6 reduces the crystalline volume within the PEO. The Li/electrolyte interface is stabilized by the in situ formation of an ultra‐thin Li 2 S/Li 2 S 2 layer via the reaction between Li 2 S 6 and lithium metal, which increases the ionic transport at the interface and suppresses lithium dendrite growth. A symmetric Li/Li cell with the Li 2 S 6 ‐integrated composite electrolyte has excellent cyclability and a high critical current density of 0.9 mA cm −2 at 40 °C. Impressive electrochemical performance is demonstrated with all‐solid‐state Li/LiFePO 4 and high‐voltage Li/LiNi 0.8 Mn 0.1 Co 0.1 O 2 cells at 40 °C.

Fang, Ruyi↗

Microstructure prediction for Ti-22Al-25Nb in laser powder bed fusion

This work presents a physics-informed framework for predicting solidification morphology and defect susceptibility in additively manufactured Ti–22Al–25Nb across a broad processing space. The framework integrates solidification microstructure selection (SMS) analysis with a single-track defect-based printability map to establish a unified methodology linking processing parameters to both interfacial morphology and manufacturability. Thermal gradients G and solidification rates R are first computed using the Thermo-Calc Additive Manufacturing (TC-AM) module, a finite-interface-dissipation (FID) phase-field (PF) model coupled with CALPHAD method is then employed to systematically distinguish planar and dendritic regimes as functions of $G$ and $R$. By superimposing the printability map onto the morphology projections, a comprehensive process–structure framework is obtained. Across most processing conditions, the predicted microstructure is predominantly dendritic, while planar growth emerges only under selected laser power $P$ and scan speed $v$ combinations. In addition to morphology classification, the framework quantifies the dendritic area fraction and introduces a width-based morphology descriptor to characterize the spatial extent of planar/dendritic regions within the melt pool. It provides mechanistic insight into the interplay between solidification physics and defect formation, offering practical guidance for parameter selection and microstructural control in Ti–22Al–25Nb additive manufacturing (AM).

36 MATERIALS SCIENCE↗

Reactive Suspension Electrolytes for Lithium Metal Batteries

Lithium metal batteries (LMBs) suffer from dendrite growth and capacity loss, which compromise safety and cycle life. Here, we present a simple reactive suspension electrolyte (RSE) strategy. When metal oxide (MO x ) nanoparticles are dispersed in the liquid electrolyte, in situ formation of Li 2 O and Li–M phases occurs at the lithium metal anode. By studying two different types of RSEs, Type 1 RSEs (i.e., CuO RSE) without metal-Li alloying and Type 2 RSEs (i.e., ZnO RSE and In 2 O 3 RSE) with metal-Li alloying capability, we elucidate the roles of each reaction compound. Here, we find that Li 2 O can improve reversibility of Li metal anode by stabilizing the interphase while Li–M alloy phases guide uniform Li metal plating. Compared to the carbonate-type reference electrolyte, RSEs demonstrate reduced nucleation overpotential, lower interfacial impedance, and higher Coulombic efficiency, leading to an extended cycle life in Li|Li 1 Ni 0.8 Co 0.1 Mn 0.1 O 2 full cells.

Lee, Junyoung [Stanford Univ., CA (United States)]↗

Melt-Pool Dynamics and Microstructure of Mg Alloy WE43 under Laser Powder Bed Fusion Additive Manufacturing Conditions

Magnesium-based alloy WE43 is a state-of-the-art bioresorbable metallic implant material. There is a need for implants with both complex geometries to match the mechanical properties of bone and refined microstructure for controlled resorption. Additive manufacturing (AM) using laser powder bed fusion (LPBF) presents a viable fabrication method for implant applications, as it offers near-net-shape geometrical control, allows for geometry customization based on an individual patient, and fast cooling rates to achieve a refined microstructure. In this study, the laser–alloy interaction is investigated over a range of LPBF-relevant processing conditions to reveal melt-pool dynamics, pore formation, and the microstructure of laser-melted WE43. In situ X-ray imaging reveals distinct laser-induced vapor depression morphology regimes, with minimal pore formation at laser-scan speeds greater than 500 mm/s. Optical and electron microscopy of cross-sectioned laser tracks reveal three distinct microstructural regimes that can be controlled by adjusting laser-scan parameters: columnar, dendritic, and banded microstructures. These regimes are consistent with those predicted by the analytic solidification theory for conduction-mode welding, but not for keyhole-mode tracks. The results provide insight into the fundamental laser–material interactions of the WE43 alloy under AM-processing conditions and are critical for the successful implementation of LPBF-produced WE43 parts in biomedical applications.

36 MATERIALS SCIENCE↗

Stable Potassium Metal Anodes with an All-Aluminum Current Collector through Improved Electrolyte Wetting

This is the first report of successful potassium metal battery anode cycling with an aluminum-based rather than copper-based current collector. Dendrite-free plating/stripping is achieved through improved electrolyte wetting, employing an aluminum-powder-coated aluminum foil “Al@Al,” without any modification of the support surface chemistry or electrolyte additives. The reservoir-free Al@Al half-cell is stable at 1000 cycles (1950 h) at 0.5 mA cm -2 , with 98.9% cycling Coulombic efficiency and 0.085 V overpotential. The pre-potassiated cell is stable through a wide current range, including 130 cycles (2600 min) at 3.0 mA cm -2 , with 0.178 V overpotential. Al@Al is fully wetted by a 4 m potassium bis(fluorosulfonyl)imide-dimethoxyethane electrolyte (θCA = 0°), producing a uniform solid electrolyte interphase (SEI) during the initial galvanostatic formation cycles. On planar aluminum foil with a nearly identical surface oxide, the electrolyte wets poorly (θCA = 52°). This correlates with coarse irregular SEI clumps at formation, 3D potassium islands with further SEI coarsening during plating/stripping, possibly dead potassium metal on stripped surfaces, and rapid failure. The electrochemical stability of Al@Al versus planar Al is not related to differences in potassiophilicity (nearly identical) as obtained from thermal wetting experiments. Additionally, planar Cu foils are also poorly electrolyte-wetted and become dendritic. The key fundamental takeaway is that the incomplete electrolyte wetting of collectors results in early onset of SEI instability and dendrites.

25 ENERGY STORAGE↗