Impact damage tolerance of thin wall composite struts

An experimental investigation was made to study the impact damage tolerance of thin wall composite struts made of both brittle epoxy and toughened epoxy based composite materials. Damage parameters such as barely visible surface damage and internal damage represented by the ultrasonic C-scan, and residual compressive strengths were evaluated against impact energy for two impactor sizes. From both a damage resistance (internal damage vs. impact energy) and a damage tolerance (residual compressive strength vs. internal damage) point of view, the toughened IM7/977-2 struts exhibited better performance than the brittle epoxy based T50/934 struts. This is attributed to the toughening mechanism in 977-2 which impedes delamination initiation from impact, and delamination growth and subsequent buckling under a compression loading. At barely visible damage thresholds, regardless of the impactor sizes, a maximum strength reduction of 45-55 percent was observed for the T50/934 struts, and approximately 10 percent for IM7/977-2 struts. This is of great interest for developing a damage tolerance design approach and risk assessment methodology in which the design allowable would be defined by the residual strength at the threshold of barely visible damage.

Chen, G.-S.↗

Carbon fiber design improvements based on economic models

Circular fiber geometries are predominant in commercial carbon fiber material systems, but the use of this fiber shape has numerous limitations. Circular geometries have continuous symmetry, which is helpful for various processing considerations, but also have the largest possible maximum diffusion thickness for a given fiber area. This characteristic means that circular carbon fibers always have the highest material processing cost and lowest production throughput compared to any other fiber shape with the same area and tow count. To quantify material cost and other benefits for non-circular carbon fiber geometries, process models for polyacrylonitrile based carbon fiber production are developed in relationship to the carbon fiber shape, size, and tow count. For a given fiber shape, precursor production costs are shown to favor maximizing fiber size while conversion costs are minimized by the smallest fiber size. These competing cost trends result in a numerically optimal fiber size for a given shape and tow count, while both cost components are decreased by increasing tow count. Cost–performance tradeoffs for three lobe fiber geometries are studied by supplementing the cost trends with a numerical failure model to predict compressive strength for discrete shape variants. The shape selection is shown to be more sensitive to variations in cost than compressive strength while suboptimal shape designs can improve manufacturing robustness and achievable fiber volume fractions. Finally, an optimal three lobe carbon fiber is identified that balances the set of considerations while reducing costs and embodied energy and increasing production throughput compared to a commercial carbon fiber.

Carbon fiber↗

Determining and analyzing the strength and impact resistance of high modulus glass

A number of new glass compositions have been prepared with increased emphasis on compositions without beryllia. Glass preparations have been much more broadly based and have included the eutectic glass fields, and the mullite-rare earth glass systems. Of the new glasses, the best non-toxic composition is UARL 472 with a bulk modulus of only 18.20 million psi. A second experimental glass, UARL 417, was chosen for research in making large quantities of fiber in monofilament form. Tests of these UARL 417 epoxy resin samples in comparison to similar composites made with the DuPont organic fiber, PRD-49-1, show that the UARL composites have a compressive strength 41/2 times higher and a specific compressive strength at least 21/2 times greater. Much of the research effort attempted to answer the question of why a given glass should have an impact strength superior to other glasses. No definitive answer to the question was found.

Bacon, J. F.↗

Mechanical strength and thermophysical properties of PM212: A high temperature self-lubricating powder metallurgy composite

A powder metallurgy composite, PM212, composed of metal bonded chromium carbide and solid lubricants is shown to be self-lubricating to a maximum application temperature of 900 C. The high temperature compressive strength, tensile strength, thermal expansion and thermal conductivity data needed to design PM212 sliding contact bearings and seals are reported for sintered and isostatically pressed (HIPed) versions of PM212. Other properties presented are room temperature density, hardness, and elastic modulus. In general, both versions appear to have adequate strength to be considered as sliding contact bearing materials, but the HIPed version, which is fully dense, is much stronger than the sintered version which contains about 20 percent pore volume. The sintered material is less costly to make, but the HIPed version is better where high compressive strength is important.

Edwards, Phillip M.↗

The effect of resin on the impact damage tolerance of graphite-epoxy laminates

The effect of the matrix resin on the impact damage tolerance of graphite-epoxy composite laminates was investigated. The materials were evaluated on the basis of the damage incurred due to local impact and on their ability to retain compression strength in the presence of impact damage. Twenty-four different resin systems were evaluated. Five of the systems demonstrated substantial improvements compared to the baseline system including retention of compression strength in the presence of impact damage. Examination of the neat resin mechanical properties indicates the resin tensile properties influence significantly the laminate damage tolerance and that improvements in laminate damage tolerance are not necessarily made at the expense of room temperature mechanical properties. Preliminary results indicate a resin volume fraction on the order of 40 percent or greater may be required to permit the plastic flow between fibers necessary for improved damage tolerance.

Williams, J. G.↗

On Characterizing Particle Shape

It is well known that particle shape affects flow characteristics of granular materials, as well as a variety of other solids processing issues such as compaction, rheology, filtration and other two-phase flow problems. The impact of shape crosses many diverse and commercially important applications, including pharmaceuticals, civil engineering, metallurgy, health, and food processing. Two applications studied here include the dry solids flow of lunar simulants (e.g. JSC-1, NU-LHT-2M, OB-1), and the flow properties of wet concrete, including final compressive strength. A multi-dimensional generalized, engineering method to quantitatively characterize particle shapes has been developed, applicable to both single particle orientation and multi-particle assemblies. The two-dimension, three dimension inversion problem is also treated, and the application of these methods to DEM model particles will be discussed. In the case of lunar simulants, flow properties of six lunar simulants have been measured, and the impact of particle shape on flowability - as characterized by the shape method developed here -- is discussed, especially in the context of three simulants of similar size range. In the context of concrete processing, concrete construction is a major contributor to greenhouse gas production, of which the major contributor is cement binding loading. Any optimization in concrete rheology and packing that can reduce cement loading and improve strength loading can also reduce currently required construction safety factors. The characterization approach here is also demonstrated for the impact of rock aggregate shape on concrete slump rheology and dry compressive strength.

Ennis, Bryan J.↗

Repair of Sandwich Structure in Support of the Payload Adapter Fitting (PAF) Part II: Severe Damage Repair

As part of a program examining a Payload Adaptor Fitting (PAF) for NASA’s Space Launch System (SLS), a repair study of impact damage and misdrilled holes in composite sandwich structure was undertaken.1 In that study, it was shown that small holes and barely visible impact damage (BVID) could be repaired and all the measured undamaged in-plane compression strength recovered without removing the damaged material using a simple patch repair. It was noted that for more severe damage, either larger patches or removal of damage (or both) may be necessary to regain all of the measured undamaged compression strength. This Technical Memorandum (TM) presents the results of an experimental investigation into repair of more severely damaged sandwich structure than what was studied in reference 1.

Nettles, A. T.↗

Lunar cement and lunar concrete

Results of a study to investigate methods of producing cements from lunar materials are presented. A chemical process and a differential volatilization process to enrich lime content in selected lunar materials were identified. One new cement made from lime and anorthite developed compressive strengths of 39 Mpa (5500 psi) for 1 inch paste cubes. The second, a hypothetical composition based on differential volatilization of basalt, formed a mineral glass which was activated with an alkaline additive. The 1 inch paste cubes, cured at 100C and 100 percent humidity, developed compressive strengths in excess of 49 Mpa (7100 psi). Also discussed are tests made with Apollo 16 lunar soil and an ongoing investigation of a proposed dry mix/steam injection procedure for casting concrete on the Moon.

Lin, T. D.↗

Computational Micromechanics Model for the Analysis of Fiber Kinking in Unidirectional FRP

A computational micromechanics (CMM) model is developed to analyze fiber kinking, which is a failure mechanism that takes place in fiber-reinforced composites when they are loaded under longitudinal compression. The CMM model consists of a single AS4 carbon fiber with an initial misalignment embedded in an 8552 polymer matrix. The deformation of the model is governed by periodic boundary conditions (PBC). The relatively simple CMM model enables the evaluation of the role played by initial misalignment of the fiber, shear yielding of the matrix and fiber-matrix debonding. A novel microscale experimental technique devoted to the characterization of the longitudinal compressive strength of the fibers, X(sup f)(sub c) , was developed. By exercising the model and comparing it with several existing models in the literature, the nonlinear shear response of the composite lamina was shown to play a fundamental role not only in the prediction of the compressive strength X(sub c), but also during the post-peak regime in terms of residual stress σ(sub r) and fiber rotation φ. Finally, the influence of the fiber-matrix interface damage (not considered in most other fiber kinking models) on the fiber kinking phenomenon was assessed through a parametric study.

Polymer-matrix composites (PMC)↗

Three-Dimensional Polybenzobisoxazoles and Polybenzobisthiazoles

Due to the poor compressive strength properties of high performance liquid crystalline polymers such as polybenzobisoxazoles (PBOs) and polybenzobisthiazoles (PBTs), we have prepared homopolymers and copolymers with PBO and PBT pendant groups on a central star-like unit, 2.7-diamino-9,9'-bis(4-aminophenyl)fluorene, in order to improve upon their compressive strength properties. The fluorene moiety was prepared by the reaction of 2,7-dinitro-9-fluorene with aniline and aniline hydrochloride, followed by reduction with palladium on carbon. The central star-like unit was characterized by FTIR, FTNMR, and elemental analysis. The PBO and PBT pendant groups were synthesized by the polycondensation of 4,6-diaminoresorcinol dihydrochloride with terephthaloyl chloride and 2,5-diamino-1,4-benzendithiol dihydrochloride with terephthaloyl chloride in poly(phosphoric acid), respectively. The resulting linear polymers containing the dicarboxylic end groups were attached to the central star-like unit by refluxing with 2,7-diamino-9,9'-bis(4-aminophenyl) fluorene to give the star-like polymers. The star-like PBO and PBT were soluble in methanesulfonic acid. Further characterization of the polymers is ongoing.

Bray, M.↗

Modeling Fiber Kinking at the Microscale and Mesoscale

A computational micromechanics (CMM) model is employed to interrogate the assumptions of a recently developed mesoscale continuum damage mechanics (CDM) model for fiber kinking. The CMM model considers an individually discretized three dimensional fiber and surrounding matrix accounting for nonlinearity in the fiber, matrix plasticity, fiber/matrix interface debonding, and geometric nonlinearity. Key parameters of the CMM model were measured through experiments. In particular, a novel experimental technique to characterize the in situ longitudinal compressive strength of carbon fibers through indentation of micropillars is presented. The CDM model is formulated on the basis of Budiansky's fiber kinking theory (FKT) with a constitutive deformation-decomposition approach to alleviate mesh size sensitivity. In contrast to conventional mesoscale CDM models that prescribe a constitutive response directly, the response of the proposed model is an outcome of material nonlinearity and large rotations of the fiber direction following FKT. Comparison of the predictions from the CMM and CDM models shows remarkable correlation in strength, post-peak residual stress, and fiber rotation, with less than 10% difference between the two models in most cases. Additional comparisons are made with several fiber kinking models proposed in the literature to highlight the efficacy of the two models. Finally, the CMM model is exercised in parametric studies to explore opportunities to improve the longitudinal compression strength of a ply through the use of nonconventional microstructures.

Herraez, Miguel↗

ASSESSMENT OF HIGH-VOLUME HARVESTED FLY ASH BLENDS FOR USE IN PRECAST CONSTRUCTION

Declining supplies of fresh fly ashes in some regions have further driven the importance of using harvested fly ash as a supplementary cementitious material and thus replacement for more energy-intensive ordinary Portland cement (OPC). Higher replacement rates of OPC with fly ash in general has traditionally been limited in precast operations due to stringent early-age strength requirements necessitated by initial prestress and lifting/handling of hardened components – often well within 24 hours after fresh concrete placement. Therefore, a series of mix designs were developed, as part of a larger framework for reassessing high-volume fly ash (HVFA) use in the context of precast construction, to demonstrate the feasibility of using larger fractions of harvested fly ash in concrete formulations suitable for precast fabrication demands. More specifically, a target minimum 24-hour compressive strength of 24.1 MPa (3500 psi) was set, in accordance with conventional precast structural design checks, while increasing the fly ash content to 40% replacement of OPC – at least a 15% increase above the traditional limit of 25%. The effect of using more sustainable Type IL cement in contrast to conventional Type III Portland cement (the traditional standard for precast use) – both in conjunction with HVFA use – was also examined. Early-age mechanical properties including compressive strength, modulus of rupture, and modulus of elasticity were evaluated within the aforementioned early-age window. Lastly, corresponding design equations were then reassessed for their applicability with respect to the high-early strength HVFA mixes examined herein.

Gombeda, Matthew J.↗

Additive manufacturing of AISI M2 tool steel by binder jetting (BJ): Investigation of microstructural and mechanical properties

The presented research demonstrates for the first time the successful processing of AISI M2 tool steel by binder jetting, a promising additive manufacturing technique capable of producing complex shapes with minimal residual stresses and isotropic properties. The optimal printing parameters were explored by varying processing parameters such as the binder saturation (45 %–105 %), binder set time (0 to 10 s), targeted bed temperature (50–60 °C), oscillator (2600–2750 rpm), recoater (20–28 mm/s), and roller speeds (200–300 rpm). Microstructural characterization and evaluation of mechanical properties of binder jetted parts were performed using x-ray diffraction (XRD), scanning electron microscopy (SEM), and energy dispersive spectroscopy (EDS) to study their chemical composition, powder morphology, microstructure, carbide morphologies, relative density, hardness, compressive strength, and ductility. Two powder sizes (5 and 10 μm) were used, and sintering was performed at varying temperatures (1270, 1280, and 1300 °C) and durations (60 and 120 min), followed by a furnace, air, and water cooling. An optimum hardness of ~970 HV was obtained when parts were sintered at 1270 °C for 60 min, followed by water quenching. Impressive compressive strength of ~ 3580 MPa was observed in the sample sintered at 1280 °C for 60 min duration, followed by air cooling. Furnace-cooled parts showed the highest density of ~95 %, whereas the relative density of air- and water-cooled parts varied between ~91 to 93.50 %, respectively. The microstructure of sintered samples revealed the formation of M 6 C stable carbide, M 2 C metastable carbide, MC as a secondary carbide, and a-Fe matrix, which contributed to the observed increase in mechanical properties.

36 MATERIALS SCIENCE↗

Strength and compressibility of returned lunar soil.

Two oedometer and three direct shear tests have been performed in vacuum on a 200 g sample of lunar soil from Apollo 12 (12001, 119). The compressibility data have been used to calculate bulk density and shear wave velocity versus depth on the lunar surface. The shear wave velocity was found to increase approximately with the one-fourth power of the depth, and the results suggest that the Apollo 14 Active Seismic Experiment may not have detected the Fra Mauro formation at a depth of 8.5 m, but only naturally consolidated lunar soil. The shear data indicate that the strength of the lunar soil sample is about 65% that of a ground basalt simulant at the same void ratio.

Carrier, W. D., III↗

Geopolymer Lunar Concrete under Reduced-Pressure Curing and Vacuum Exposure

Geopolymer concrete has emerged as a promising material for constructing habitats, roads, landing pads, and other necessary infrastructure on the lunar surface. Proper in-situ resource utilization (ISRU) is an important aspect of any candidate lunar construction material. Geopolymer concrete is effective at ISRU, as the lunar regolith can be used in the “as found” condition and mixed with an alkaline solution, such as sodium silicate and sodium hydroxide, which could also be mostly produced in-situ. It is envisioned that any concrete material on the lunar surface would be deposited with additive manufacturing techniques and would require a temporary environmental enclosure to mitigate the harsh lunar environment during construction and curing, such as pressure and temperature. Data are needed to set a benchmark for the conditions to be achieved within the deployable environmental enclosure during printing, as well as the resultant material properties after the enclosure is removed. This novel study investigated the influence of reduced atmospheric pressures during the initial curing period on the compressive strength of geopolymer lunar concrete created with two types of lunar regolith simulant. The simulants used in the study represent the regolith for the lunar mare (OPRL2N) and lunar highlands (OPRH2N) regions. Results show a noticeable decline in strength with a reduction in pressure and visible degradation. After the deployable environmental enclosure is removed from the printed segment of infrastructure on the lunar surface, it would then be exposed to the harsh vacuum environment. To understand the importance of curing time required within the deployable enclosure before it is removed, samples were cast and cured for different lengths of time and then exposed to a vacuum chamber capable of achieving 100 mTorr. Control samples were also cast at the same time but left in a standard laboratory environment after curing. The weight change and compressive strength as a function of time in the vacuum chamber were monitored for up to 56 days. The results showed that exposure to the vacuum limits further reaction and strength gain in comparison to control samples left in the laboratory environment. This research is in strong alignment with the 2020 NASA Technology Taxonomy materials area (12.1) and the in-situ resource utilization area (7.1), as it provides necessary data on the geopolymer lunar concrete material to support safe and sustainable options for maintaining a human presence on the Moon.

Moon to Mars Planetary Autonomous Construction Tec↗

Binder-jetted AISI M2 tool steel during hot isostatic pressing: Densification and carbide transformation

Binder jetting (BJ) enables fabrication of complex components from high-alloy steels such as AISI M2; however, residual porosity after sintering limits mechanical performance. This study investigates the coupled effects of binder chemistry, sintering conditions, cooling rate, and subsequent hot isostatic pressing (HIP) on densification, microstructure, and mechanical response in binder-jetted M2 tool steel. HIP increased relative density from ∼93 to 95% to >99% and improved compressive strength by ∼40-70%. Densification was governed by initial pore morphology, where closed porosity was effectively eliminated, while interconnected porosity limited full consolidation. Microstructural analysis (XRD, EBSD, SEM) shows that HIP promotes dissolution of metastable carbides and redistribution of alloying elements (W, Mo, V), transforming heterogeneous carbide networks into finer and more uniformly distributed M 2 C, MC, and M 6 C phases through diffusion-assisted homogenization. Among the investigated conditions, the FluidFuse binder combined with sintering at 1270 °C for 60 min and furnace cooling produced the most balanced response, achieving ∼99.7% density, ∼855 HV hardness, ∼4130 MPa compressive strength, and ∼24% strain. In contrast, higher sintering temperatures promoted carbide coarsening, reducing ductility despite high density. HIP reduces microstructural heterogeneity and drives the system toward a near-equilibrium state with reduced sensitivity to prior processing history. A comparative assessment with conventional and additive manufacturing routes (LPBF, DED, EBM, FFF) shows that the BJ-HIP approach achieves competitive densification and mechanical performance. These findings provide a mechanistic basis for controlling densification and microstructure in high-alloy steels processed via BJAM.

AISI M2 tool steel↗

A New Approach to Fibrous Composite Laminate Strength Prediction

A method of predicting the strength of cross-plied fibrous composite laminates is based on expressing the classical maximum-shear-stress failure criterion for ductile metals in terms of strains. Starting with such a formulation for classical isotropic materials, the derivation is extended to orthotropic materials having a longitudinal axis of symmetry, to represent the fibers in a unidirectional composite lamina. The only modification needed to represent those same fibers with properties normalized to the lamina rather than fiber is a change in axial modulus. A mirror image is added to the strain-based lamina failure criterion for fiber-dominated failures to reflect the cutoffs due to the presence of orthogonal fibers. It is found that the combined failure envelope is now identical with the well-known maximum-strain failure model in the tension-tension and compression-compression quadrants but is truncated in the shear quadrants. The successive application of this simple failure model for fibers in the 0/90 degree and +/- 45 degree orientations, in turn, is shown to be the necessary and sufficient characterization of the fiber-dominated failures of laminates made from fibers having the same tensile and compressive strengths. When one such strength is greater than the other, the failure envelope is appropriately truncated for the lesser direct strain. The shear-failure cutoffs are now based on the higher axial strain to failure since they occur at lower strains than and are usually not affected by such mechanisms as microbuckling. Premature matrix failures can also be covered by appropriately truncating the fiber failure envelope. Matrix failures are excluded from consideration for conventional fiber/polymer composites but the additional features needed for a more rigorous analysis of exotic materials are covered. The new failure envelope is compared with published biaxial test data. The theory is developed for unnotched laminates but is easily shrunk to incorporate reductions to allow for bolt holes, cutouts, reduced compressive strength after impact, and the like.

Hart-Smith, L. J.↗