Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CORROSION PRODUCTS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Use of Monte Carlo simulation to quantify CIPS risk

Crud Induced Power Shift (CIPS), caused by the accumulation of boron compounds in corrosion product deposits on high power fuel assemblies, is an important operational issue for Pressurized Water Reactors (PWRs). The Boron-induced Offset Analysis (BOA) computer code has been developed by EPRI in collaboration with Westinghouse to help utility engineers avoid onset of CIPS. The code, used with an established procedure, predicts the maximum boron mass that will be accumulated in the upcoming cycle for a given core design and plant chemistry and operating program. The calculated boron mass above a given threshold predicts the risk of CIPS to the upcoming cycle. BOA has been successful in correctly predicting the risk for onset or lack of CIPS in many cycles. However, like most codes modeling complex physical phenomena, it is subject to uncertainties in several of the inputs used to describe these phenomena. The current BOA procedure results in a single 'best estimate' prediction, which has been judged to provide engineers with a practical way to assess CIPS risk. As such, however, there is a probability that the actual plant CIPS performance may be underestimated. This paper describes a method to assess the probability (with an associated confidence level) of no CIPS, mild to moderate CIPS, or severe CIPS using BOA for a given core design. This is accomplished through the use of a Monte Carlo simulation. The simulation is applied to several plant examples, and the results are evaluated in terms of the likelihood of mild or severe CIPS. A suggested set of criteria for decision making regarding CIPS risk is presented in the conclusion. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

In-Situ Characterization of Underwater Radioactive Sludge

A fundamental requirement underpinning safe clean-up technologies for legacy spent nuclear fuel (SNF) ponds, pools and wet silos is the ability to characterize the radioactive waste form prior to retrieval. The corrosion products resulting from the long term underwater storage of spent nuclear fuel, reactor components and reprocessing debris present a major hazard to facility decontamination and decommissioning in terms of their radioactive content and physical / chemical reactivity. The ability to perform in-situ underwater non-destructive characterization of sludge and debris in a safe and cost-effective manner offers significant benefits over traditional destructive sampling methods. Several techniques are available for underwater measurements including (i) Gross gamma counting, (ii) Low-, Medium- and High- Resolution Gamma Spectroscopy, (iii) Passive neutron counting and (iv) Active Neutron Interrogation. The optimum technique depends on (i) the radioactive inventory (ii) mechanical access restrictions for deployment of the detection equipment, interrogation sources etc. (iii) the integrity of plant records and (iv) the extent to which Acceptable Knowledge which may be used for 'fingerprinting' the radioactive contents to a marker nuclide. Prior deployments of underwater SNF characterization equipment around the world have been reviewed with respect to recent developments in gamma and neutron detection technologies, digital electronics advancements, data transfer techniques, remote operation capabilities and improved field ruggedization. Modeling and experimental work has been performed to determine the capabilities, performance envelope and operational limitations of the future generation of non-destructive underwater sludge characterization techniques. Recommendations are given on the optimal design of systems and procedures to provide an acceptable level of confidence in the characterization of residual sludge content of legacy wet storage facilities such that retrieval and repackaging of SNF sludges may proceed safely and efficiently with support of the regulators and the public. (author)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

ITER's Tokamak Cooling Water System and the the Use of ASME Codes to Comply with French Regulations of Nuclear Pressure Equipment

During inductive plasma operation of ITER, fusion power will reach 500 MW with an energy multiplication factor of 10. The heat will be transferred by the Tokamak Cooling Water System (TCWS) to the environment using the secondary cooling system. Plasma operations are inherently safe even under the most severe postulated accident condition a large, in-vessel break that results in a loss-of-coolant accident. A functioning cooling water system is not required to ensure safe shutdown. Even though ITER is inherently safe, TCWS equipment (e.g., heat exchangers, piping, pressurizers) are classified as safety important components. This is because the water is predicted to contain low-levels of radionuclides (e.g., activated corrosion products, tritium) with activity levels high enough to require the design of components to be in accordance with French regulations for nuclear pressure equipment, i.e., the French Order dated 12 December 2005 (ESPN). ESPN has extended the practical application of the methodology established by the Pressure Equipment Directive (97/23/EC) to nuclear pressure equipment, under French Decree 99-1046 dated 13 December 1999, and Order dated 21 December 1999 (ESP). ASME codes and supplementary analyses (e.g., Failure Modes and Effects Analysis) will be used to demonstrate that the TCWS equipment meets these essential safety requirements. TCWS is being designed to provide not only cooling, with a capacity of approximately 1 GW energy removal, but also elevated temperature baking of first-wall/blanket, vacuum vessel, and divertor. Additional TCWS functions include chemical control of water, draining and drying for maintenance, and facilitation of leak detection/localization. The TCWS interfaces with the majority of ITER systems, including the secondary cooling system. U.S. ITER is responsible for design, engineering, and procurement of the TCWS with industry support from an Engineering Services Organization (ESO) (AREVA Federal Services, with support from Northrop Grumman, and OneCIS). ITER International Organization (ITER-IO) is responsible for design oversight and equipment installation in Cadarache, France. TCWS equipment will be fabricated using ASME design codes with quality assurance and oversight by an Agreed Notified Body (approved by the French regulator) that will ensure regulatory compliance. This paper describes the TCWS design and how U.S. ITER and fabricators will use ASME codes to comply with EU Directives and French Orders and Decrees.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Safety Issues and Approach to Meet the Safety Requirements in Tokamak Cooling Water System of ITER

The ITER (Latin for 'the way') tokamak cooling water system (TCWS) consists of several separate systems to cool the major ITER components - the divertor/limiter, the first wall blanket, the neutral beam injector and the vacuum vessel. The ex-vessel part of the TCWS systems provides a confinement function for tritium and activated corrosion products in the cooling water. The Vacuum Vessel System also has a functional safety requirement regarding the residual heat removal from in-vessel components. A preliminary hazards assessment (PHA) was performed for a better understanding of the hazards, initiating events, and defense in depth mechanisms associated with the TCWS. The PHA was completed using the following steps. (1) Hazard Identification. Hazards associated with the TCWS were identified including radiological/chemical/electromagnetic hazards and physical hazards (e.g., high voltage, high pressure, high temperature, falling objects). (2) Hazard Categorization. Hazards identified in step (1) were categorized as to their potential for harm to the workers, the public, and/or the environment. (3) Hazard Evaluation. The design was examined to determine initiating events that might occur and that could expose the public, environment, or workers to the hazard. In addition the system was examined to identify barriers that prevent exposure. Finally, consequences to the public or workers were qualitatively assessed, should the initiating event occur and one or more of the barriers fail. Frequency of occurrence of the initiating event and subsequent barrier failure was qualitatively estimated. (4) Accident Analysis. A preliminary hazards analysis was performed on the conceptual design of the TCWS. As the design progresses, a detailed accident analysis will be performed in the form of a failure modes and effects analysis. The results of the PHA indicated that the principal hazards associated with the TCWS were those associated with radiation. These were low compared to hazards associated with nuclear fission reactors and were limited to potential exposure to the on-site workers if appropriate protective actions were not used. However, the risk to the general public off-site was found to be negligible even under worst case accident conditions.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

A Preliminary Analysis of Dose Rates Associated with ITER CVCS Equipment/Area Location

A preliminary analysis of the ITER Chemical and Volume Control System (CVCS) Area was performed to assess dose rates outside the walls and ceiling of the facility after 1.5 years of operation at shutdown, 2 days, and 10 days after shutdown. For this purpose a simplified Monte Carlo computer model was developed using the MCNP (MCNP5 Ver. 1.51) code. Two components are included: the smaller filter tank and the larger ion exchanger. These pieces of equipment are associated with the Integrated Blanket ELM Divertor Primary Heat Transfer System, which will have the largest dose rates associated with activated corrosion products during operation in comparison with other systems. The ion exchanger contained two source regions, a 1.2-m-thick resin bed above a 0.55 m-thick skirt, and a 0.8-m-thick water region. The filter constituted an additional source. Thus the model consisted of three sources (filter, resin, water), homogeneously distributed within the appropriate source regions. However, much of the results (that address individual isotopes) are presented with the two sources in the ion exchanger combined. In these cases the sources are referred to as the 'ion exchanger source' and the 'filter source.' Dimensions for the facility and components, as well as source isotopes and strengths, and material densities, were supplied by US ITER. Because of its simplification, the model does not contain pipes. Consequently, radiation streaming through pipe penetrations, radiation emanating from the pipes, and shielding from the pipes were not considered in this analysis. Dose rates on the outside of two walls and the ceiling were calculated. The two walls are labeled as the 'long' wall (aligned with the X-axis) and the 'short' wall (aligned with the Y-axis). These walls and ceiling were nominally set to 30-cm-thick concrete. In the original analysis, standard concrete (2.3 g/cc density) was used. In addition to the shielding walls/ceiling, a floor and an additional wall opposite the long wall were added for photon scattering contributions. These were both 10-cm-thick, standard concrete structures. Other components (tanks, pipes, etc.), that were not included in the model, would potentially add additional scattering and shielding. Possibly these additional effects will be addressed in a later, more detailed analysis. The room was 29.6 m in length (X-axis), but was limited to 15 m in the model. The inside width (Y axis) and height (Z axis) were 4 m and 3.4 m, respectively. The origin for the model was located inside the room at the corner opposite the long wall and adjacent to the short wall at the floor level. The room was filled with air at standard temperature and pressure. The stainless steel (SS304) wall thicknesses for the ion exchanger and filter were 2.2 cm and 0.8 cm, respectively. The axial center of the filter was located 140 cm from the short wall and 100 cm from the long wall (outer surface). The axial center of the ion exchanger was located 440 cm from the short wall and 250 cm from the long wall (inner surface). The resin was assumed to be a homogeneous mixture of equal atom density fractions of hydrogen and carbon* at a specified density of 1.136 g/cc. The filter material was assumed to be homogeneous carbon at a specified density of 1.8 g/cc. If the filter media were stainless steel and the accumulated activity were the same, the dose rate outside the filter would be lower, provided the density of the stainless steel sintered filter material is significantly higher than 1.8g/cc. The densities of the water and air were assumed to be 1.0 g/cc and 1.096E-3 g/cc, respectively. The model included 10 small volumes placed outside the model adjacent to the wall at locations where the dose rates were expected to be highest and which showed to a degree the fall-off of the dose rate with distance along a particular wall or ceiling. These 'tally cells' are shown in Fig. 2 and are described in Table 1. Each cell had dimensions of 50 cm x 50 cm x 1 cm and was oriented so that the 1-cm-thick dimension was perpendicular to the wall against which the cell was located. Also, smaller tally volumes were placed at 5 cm (updated model), 30 cm, 50 cm, and 100 cm from each source, both radially from the outside of each component at the height of each source mid-plane, and vertically, along the axial centerline, above the ion-exchanger and below the filter. (For the ion exchanger, the vertical distance was limited to 75 cm because of interference from the ceiling.) These tally regions can be seen in Fig. 3. Each cell had dimensions of 5 cm x 5 cm x 1 cm, oriented so that the 1-cm-thick dimension was perpendicular to the X, Y or Z axis.

08 HYDROGEN↗

Corrosion Behavior of Steels in Supercritical CO 2 for Power Cycle Applications

In order to understand issues with corrosion of heat exchanger materials in direct supercritical carbon dioxide (sCO 2 ) power cycles, a series of autoclave exposure experiments and electrochemical experiments have been conducted. Corrosion behaviors of 347H stainless steel and P91 martensitic-ferrtic steel in sCO 2 environment have been compared. In autoclave exposure tests performed at 50°C- 245°C and 80 bar. Mass change measurements, surface characterization, and corrosion product analysis have been conducted to understand the corrosion behavior of steels in sCO 2 containing H 2 O and O 2 . Electrochemical tests performed at room temperature and 50°C, a simulation environment of water condensation phase with dissolved CO 2 was prepared to evaluate the corrosion resistance of materials. From both types of experiments, generally 347H showed higher corrosion resistance than P91.

01 COAL, LIGNITE, AND PEAT↗

Development of an Accelerated Test Method for the Determination of Susceptibility to Atmospheric Corrosion

The theoretical rationale is presented for use of a repetitive cyclic current reversal voltammetric technique for characterization of localized corrosion processes, including atmospheric corrosion. Applicability of this proposed experimental protocol is applied to characterization of susceptibility to crevice and pitting corrosion, atmospheric corrosion and stress corrosion cracking. Criteria upon which relative susceptibility is based were determined and tested using two iron based alloys commonly in use at NASA-Kennedy; A36 (a low carbon steel) and 4130 (a low alloy steel). Practicality of the procedure was demonstrated by measuring changes in anodic polarization behavior during high frequency current reversal cycles of 25 cycles per second with 1 mA/sq cm current density amplitude in solutions containing Cl anions. The results demonstrated that, due to excessive polarization which affects conductivity of barrier corrosion product layers, A36 was less resistant to atmospheric corrosion than its 4130 counterpart; behavior which was also demonstrated during exposure tests.

Ambrose, John R.↗

Field Testing of High Current Electrokinetic Nanoparticle Treatment for Corrosion Mitigation in Reinforced Concrete

Electrokinetic Nanoparticle (EN) treatment was used as a rapid repair measure to mitigate chloride induced corrosion of reinforced concrete in the field. EN treatment uses an electric field to transport positively charged nanoparticles to the reinforcement through the concrete capillary pores. Cylindrical reinforced concrete specimens were batched with 4.5 wt % salt content (based on cement mass). Three distinct electrokinetic treatments were conducted using high current density (up to 5 A/m2) to form a chloride penetration barrier that was established in 5 days, as opposed to the traditional 6-8 weeks, generally required for electrochemical chloride extraction (ECE). These treatments included basic EN treatment, EN with additional calcium treatment, and basic ECE treatment. Field exposures were conducted at the NASA Beachside Corrosion Test Site, Kennedy Space Center, Florida, USA. The specimens were subjected to sea water immersion at the test site as a posttreatment exposure. Following a 30-day post-treatment exposure period, the specimens were subjected to indirect tensile testing to evaluate treatment impact. The EN treated specimens exhibited 60% and 30% increases in tensile strength as compared to the untreated controls and ECE treated specimens respectively. The surfaces of the reinforcement bars of the control specimens were 67% covered by corrosion products. In contrast, the EN treated specimens exhibited corrosion coverage of only 4%. Scanning electron microscopy (SEM) revealed a dense concrete microstructure adjacent to the bars of the treated specimens as compared to the control and ECE specimens. Energy dispersive spectroscopic (EDS) analysis of the polished EN treated specimens showed a reduction in chloride content by a factor of 20 adjacent to the bars. This study demonstrated that EN treatment was successful in forming a chloride penetration barrier rapidly. This work also showed that the chloride barrier was effective when samples were exposed to field conditions at one of the most severely corrosive environments in North America.

Cardenas, Henry↗

Corrosion Testing of Brazed Space Station IATCS Materials

Increased nickel concentrations in the IATCS coolant prompted a study of the corrosion rates of nickel-brazed heat exchangers in the system. The testing has shown that corrosion is occurring in a silicon-rich intermetallic phase in the braze filler of coldplates and heat exchangers as the result of a decrease in the coolant pH brought about by cabin carbon dioxide permeation through polymeric flexhoses. Similar corrosion is occurring in the EMU de-ionized water loop. Certain heat exchangers and coldplates have more silicon-rich phase because of their manufacturing method, and those units produce more nickel corrosion product. Silver biocide additions did not induce pitting corrosion at silver precipitate sites.

Pohlman, Matthew J.↗

Modeling of fission and activation products in molten salt reactors and their potential impact on the radionuclide monitoring stations of the International Monitoring System

Molten Salt Reactors (MSRs) are one of six Generation IV reactor designs currently under development around the world. Because of the unique operating conditions of MSRs, which include molten fuel and the continuous removal of gaseous fission products during operation, work was performed to analyze the potential impact of emissions on the International Monitoring System (IMS) of the Comprehensive Nuclear-Test-Ban Treaty (CTBT). Simulations were performed to predict the production of IMS-relevant radionuclides in four MSR designs operating under two scenarios: (1) a sealed reactor with releases only during operational shutdown, and (2) continuous reprocessing or sparging of the fuel salt. From these production estimates the radioxenon and radioiodine signatures were extracted and compared to three current reactor designs (Pressurized Water Reactor (PWR), BWR, RBMK). In cases where continuous reprocessing of the fuel salt occurred, both the radioxenon and radioiodine signatures were nearly indistinguishable from a nuclear explosion. Estimates were also made of the potential emission rate of radioxenon for three reactor designs and it was found that MSRs have the potential to emit radioxenon isotopes at a rate of 10^15-8×10^16 Bq/d for 133Xe if no abatement is used. An assessment was made of activation products using a candidate fuel salt (FLiBe) mixed with corrosion products for the Thorium Molten Salt Reactor (TMSR-LF1).

Johnson, Christine M.↗

First steps toward predicting corrosion behavior of structural materials in molten salts

To address the need for physics-based models to predict corrosion behavior of materials in molten salts, here we propose potential methods to aid in selection of optimum materials for structural components in molten salt powered technologies. In the present work, the role of alloy thermodynamics and kinetics on governing corrosion rates of Ni-based alloys will be discussed combining experimental and computational methods. A few strategies are presented to quantify corrosion rates of Ni-based materials isothermally exposed in purified KCl-MgCl 2 salts at 600° C-800° C. The influence of capsule material, potential corrosion products and role of alloy composition on the observed corrosion rates was discussed with coupled thermodynamic-kinetic models. Larger depths of corrosion attack were observed in alloy 230 specimens compared to other alloys under similar conditions was attributed to the much higher chemical activity of Cr in the alloy that results in a larger Cr chemical potential gradient.

36 MATERIALS SCIENCE↗

Modeling of fission and activation products in molten salt reactors and their potential impact on the radionuclide monitoring stations of the International Monitoring System

Molten Salt Reactors (MSRs) are one of six Generation IV reactor designs currently under development around the world. Because of the unique operating conditions of MSRs, which include molten fuel and the continuous removal of gaseous fission products during operation, work was performed to analyze the potential impact of emissions on the International Monitoring System (IMS) of the Comprehensive Nuclear-Test-Ban Treaty (CTBT). Simulations were performed to predict the production of IMS-relevant radionuclides in four MSR designs operating under two scenarios – (1) a sealed reactor with releases only during operational shutdown and (2) continuous reprocessing or sparging of the fuel salt. From these production estimates the radioxenon and radioiodine signatures were extracted and compared to three current reactor designs (PWR, BWR, RBMK). In the cases where continuous reprocessing of the fuel salt occurred both the radioxenon and radioiodine signatures are nearly indistinguishable from a nuclear explosion. Estimates were also made of the potential emission rate of radioxenon for three reactor designs and it was found that MSRs have the potential to emit radioxenon isotopes at a rate of 1015 – 8×1016 Bq/d for 133Xe if no abatement is used. An assessment was also made of activation products using a candidate fuel salt (FLiBe) mixed with corrosion products for the Thorium Molten Salt Reactor (TMSR-LF1)

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

SRB seawater corrosion project

The corrosion behavior of 2219 aluminum when exposed to seawater was characterized. Controlled corrosion experiments at three different temperatures (30, 60 and 100 C) and two different environments (seawater and 3.5 percent salt solution) were designed to elucidate the initial stages in the corrosion process. It was found that 2219 aluminum is an active catalytic surface for growth of Al2O3, NaCl, and MgO. Formation of Al2O3 is favored at lower temperatures, while MgO is favored at higher temperatures. Visible corrosion products are formed within 30 minutes after seawater exposure. Corrosion characteristics in 3.5 percent salt solution are different than corrosion in seawater. Techniques utilized were: (1) scanning electron microscopy, (2) energy dispersive x-ray spectroscopy, and (3) Auger electron spectroscopy.

Bozack, M. J.↗

Enhanced crevice corrosion of stainless steel 316 by degradation of Cr-containing hollandite crevice former

This study explores the corrosion interactions between stainless steel 316 (SS316), a candidate nuclear waste canister material, and Cr-containing hollandite (Ba 1.15 Cr 2.3 Ti 5.7 O 16 ), a model ceramic nuclear waste form. The two materials were corroded in close proximity in 0.6 M NaCl solution at 90 °C for 28 days. Severe crevice corrosion was observed on the stainless steel surface after the corrosion experiment, which is likely associated with the rapid accumulation of Cr 3+ cations originating from both SS316 and the Cr-containing hollandite. Furthermore, the enhanced corrosion of SS316 by the corrosion products of hollandite is quantitatively explained using a classical crevice corrosion model.

36 MATERIALS SCIENCE↗

Influence of solid corrosion by-products on the consumption of dissolved oxygen in copper pipes

Research on corrosion of copper pipes has given little consideration to the influence of solid corrosion by-products on the processes occurring at the metal-liquid interface. Consequently, the effect of such solid phases on the rate of dissolved oxygen (DO) consumption remains poorly understood. In-situ experiments were performed in copper pipes under different carbonate concentrations and ageing times. Our results show that the amount of solid corrosion by-products and concentration of hydrogen ions affect the rate of DO consumption during stagnation. Furthermore, our findings support the existing hypothesis that the available concentration of hydrogen ions, rather than DO, is the limiting factor for copper release into drinking water.

74 ATOMIC AND MOLECULAR PHYSICS↗

Introduction to Pits and Weapons Systems (U) [Slides]

A Nuclear Explosive Package includes the Primary, Secondary, Radiation Case and related components. This is the part of the weapon that produces nuclear yield and it converts mechanical energy into nuclear energy. The pit is composed of materials that allow mechanical energy to be converted to electromagnetic energy. Fabrication processes used are typical of any metal fabrication facility: casting, forming, machining and welding. Some of the materials used in pits include: Plutonium, Uranium, Stainless Steel, Beryllium, Titanium, and Aluminum. Gloveboxes are used for three reasons: (1) Protect workers and public from easily transported, finely divided plutonium oxides - (a) Plutonium is very reactive and produces very fine particulate oxides, (b) While not the 'Most dangerous material in the world' of Manhattan Project lore, plutonium is hazardous to health of workers if not properly controlled; (2) Protect plutonium from reactive materials - (a) Plutonium is extremely reactive at ambient conditions with several components found in air: oxygen, water, hydrogen, (b) As with most reactive metals, reactions with these materials may be violent and difficult to control, (c) As with most fabricated metal products, corrosion may significantly affect the mechanical, chemical, and physical properties of the product; and (3) Provide shielding from radioactive decay products: α, γ, and η are commonly associated with plutonium decay, as well as highly radioactive materials such as 241 Am and 238 Pu.

36 MATERIALS SCIENCE↗

Speciation and distribution of vanadium in drinking water iron pipe corrosion by-products

Vanadium (V) when ingested from drinking water in high concentrations (> 15 {micro}g L{sup -1}) is a potential health risk and is on track to becoming a regulated contaminant. High concentrations of V have been documented in lead corrosion by-products as Pb{sub 5}(V{sup 5+}O{sub 4}){sub 3}Cl (vanadinite) which, in natural deposits is associated with iron oxides/oxyhydroxides, phases common in iron pipe corrosion by-products. The extent of potential reservoirs of V in iron corrosion by-products, its speciation, and mechanism of inclusion however are unknown. The aim of this study is to assess these parameters in iron corrosion by-products, implementing synchrotron-based {mu}-XRF mapping and {mu}-XANES along with traditional physiochemical characterization. The morphologies, mineralogies, and chemistry of the samples studied are superficially similar to typical iron corrosion by-products. However, we found V present as discrete grains of Pb{sub 5}(V{sup 5+}O{sub 4}){sub 3}Cl likely embedded in the surface regions of the iron corrosion by-products. Concentrations of V observed in bulk XRF analysis ranged from 35 to 899 mg kg{sup -1}. We calculate that even in pipes with iron corrosion by-products with low V concentration, 100 mg kg{sup -1}, as little as 0.0027% of a 0.1-cm thick X 100-cm long section of that corrosion by-product needs to be disturbed to increase V concentrations in the drinking water at the tap to levels well above the 15 {micro}g L{sup -1} notification level set by the State of California and could adversely impact human health. In addition, it is likely that large reservoirs of V are associated with iron corrosion by-products in unlined cast iron mains and service branches in numerous drinking water distribution systems.

36 MATERIALS SCIENCE↗

Lower-length-scale modeling of chemical additions, corrosion and fission products in select MSR base salts

Molten salts play a crucial role in advancing Generation IV nuclear energy technology, with chloride-based salts like NaCl-UCl 3 garnering significant attention due to their distinctive properties. However, the corrosive nature of molten salts causes the dissolution of chromium (Cr), leading to the formation of CrCl 2 and CrCl 3 species in molten chlorides. Moreover, the radioactive decay of nuclear fuel gives rise to fission products, including Cs, Sr, and I chlorides. The first part of this report presents a comprehensive study utilizing ab initio molecular dynamics (AIMD) simulations to investigate the properties of eutectic NaCl-UCl 3 molten salt in the presence of corrosion products (CrCl 2 and CrCl 3 ) and fission product (CsCl). The study focuses on essential structural and thermophysical properties such as density, mixing energy, coordination numbers (CN), and Radial Distribution Functions (RDF) of the salts with varying compositions of corrosion products and fission product, covering a range from 0% to 13.5%. The results offer valuable insights into the behavior of corrosion and fission products in uranium-based molten salts, providing essential data that can be used as input to the MTDB-TC and MSTDB-TP property databases being developed by the NEAMS program. Due to their favorable characteristics such as low melting points, high boiling points, and low costs, MgCl 2 +NaCl+KCl (MNK) eutectic salts have recently attracted attention as high-temperature heat transfer fluids. The incorporation of LiCl into MNK salts can further reduce their melting points and increase their specific heat capacities, which is de- sirable for high-temperature heat transfer applications. The second part of this report presents the development and validation of a new shell-model potential for the MgCl 2 +NaCl+KCl+LiCl system, which captures the polarization of Cl anions. The extensive comparison with experimental data and AIMD simulations demonstrates the accuracy and reliability of the potential. Furthermore, using this potential, we elucidate the intricate network structure in MNK eutectic salts that is formed through polyhedron sharing. This research contributes to a fundamental understanding of the atomic structures and thermophysical properties of multi-component molten salts, which is crucial for future development of heat transfer fluids for applications in molten salt reactors.

36 MATERIALS SCIENCE↗