Magnetic properties of the ammonolysis product of α-Fe powder containing a small amount of aluminum

Magnetite was prepared containing a small amount of aluminum and its nitride was generated through low temperature ammonolysis following reduction under hydrogen. The nitrided product was determined by XRD to be a mixture of “α″-Fe{sub 16}N{sub 2}” having a slightly deformed crystal structure from α″-Fe{sub 16}N{sub 2} and the residual α-Fe. Magnetic coercivity of the mixture was decreased from the value of 150 mT obtained for the nitride product made without aluminum, due to the precipitation of nonmagnetic amorphous alumina in the low temperature nitrided bcc (Fe{sub 1−x}Al{sub x}) with x≤0.03. The aluminum-doped nitride product in which the “α″-Fe{sub 16}N{sub 2}” fraction was 30 at% exhibited magnetization at 1.5 T of approximately 200 Am{sup 2}kg{sup −1} at room temperature and its magnetic coercivity was 20 mT. - Graphical abstract: Magnetic iron nitride particles were separated by nonmagnetic amorphous γ-alumina. Magnetic coercivity was decreased by reducing the magnetic interaction between the particles. - Highlights: • Magnetic coercivity decreased in α”-Fe{sub 16}N{sub 2} like compound as a soft magnet. • Small amount of Al addition was effective in its preparation. • Magnetic interaction decreased between the “α”-Fe{sub 16}N{sub 2}” particles.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Influence of Al substitution on magnetism and adsorption properties of hematite

A series of Al-substituted hematite was prepared. The structures and properties of as-prepared samples were characterized by various techniques. The magnetic property of the samples was determined and the adsorption of three dyes Acid Blue 74, Methylene Blue and Phenol Red onto the samples was investigated. The results showed that Al incorporation into the crystal structure of hematite occurs via isomorphous ionic substitution of Al for Fe. With increasing Al content, the particle size of samples decreases, the magnetization increases and the remanent magnetization remains unchanged. The coercivity of the samples increases with Al substitution up to n{sub Al}/n{sub Fe} 0.03, and then decreases as Al content further increases. Compared with Al-free hematite, Al-substituted samples exhibit better adsorption ability to all of the three dyes. The adsorption rates of the three dyes on the surface of Al substituted samples depend on the structure of dye, pH and Al content in hematite. - Graphical abstract: Effect of Al on the structure, magnetic properties and adsorption performance of hematite was investigated. - Highlights: • A series of Al-substituted α-Fe{sub 2}O{sub 3} was prepared. • Effect of Al content on the crystal structure and magnetic property of hematite was investigated. • Al-substituted hematite exhibits better adsorption ability than hematite.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Giant magnetic coercivity in orthorhombic YNi{sub 4}Si-type SmNi{sub 4}Si compound

Magnetic properties, magnetocaloric effect and heat capacity of the YNi{sub 4}Si-type SmNi{sub 4}Si compound have been investigated. SmNi{sub 4}Si exhibits ferromagnetic transition at 17 K. Below ~9 K, the magnetic isotherms of SmNi{sub 4}Si show metamagnetic-like behavior with critical field of 20 kOe at 5 K. Heat capacity measurements of SmNi{sub 4}Si show the electronic heat capacity coefficient γ=94 mJ/(mol K{sup 2}), phonon coefficient β=0.35 mJ/(mol K{sup 4}) and Debye temperature T{sub D}=310 K. The magnetocaloric effect of SmNi{sub 4}Si is calculated in terms of isothermal magnetic entropy change which is obtained by the isothermal magnetization (ΔS{sub m}{sup magn}) and heat capacity measurements (ΔS{sub m}{sup heat}). Both ΔS{sub m}{sup magn} and ΔS{sub m}{sup heat} reach a maximum of –1.0 J/kg K at 17 K for a field change of 50 kOe and they show positive values for a field change of 20 kOe at ~9 K. Below 15 K, SmNi{sub 4}Si shows large magnetic hysteresis with considerable remanence. At 5 K it exhibits giant coercive field of 58 kOe in an applied field of 90 kOe. - Highlights: • YNi{sub 4}Si-type SmNi{sub 4}Si has Curie point at 17 K. • ΔS{sub m}{sup magn} of SmNi{sub 4}Si reaches value of –1.0 J/kg K in 0–50 kOe near Curie point. • ΔS{sub m}{sup magn} of SmNi{sub 4}Si shows value of –0.4 and +0.8 J/kg K at 17 and 9 K in 0–20 kOe. • SmNi{sub 4}Si shows electronic heat capacity the 94 mJ/(mol K{sup 2}) and Debye T{sub D}=310 K. • SmNi{sub 4}Si shows huge magnetic hysteresis with coercive field of 58 kOe at 5 K.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synthesis, microstructure and magnetic properties of Fe{sub 3}Si{sub 0.7}Al{sub 0.3}@SiO{sub 2} core–shell particles and Fe{sub 3}Si/Al{sub 2}O{sub 3} soft magnetic composite core

Fe{sub 3}Si{sub 0.7}Al{sub 0.3}@SiO{sub 2} core–shell particles and Fe{sub 3}Si/Al{sub 2}O{sub 3} soft magnetic composite core have been synthesized via a modified stöber method combined with following high temperature sintering process. Most of conductive Fe{sub 3}Si{sub 0.7}Al{sub 0.3} particles could be uniformly coated by insulating SiO{sub 2} using the modified stöber method. The Fe{sub 3}Si{sub 0.7}Al{sub 0.3}@SiO{sub 2} core–shell particles exhibited good soft magnetic properties with low coercivity and high saturation magnetization. The reaction 4Al+3SiO{sub 2}=2α-Al{sub 2}O{sub 3}+3Si took place during the sintering process. As a result the new Fe{sub 3}Si/Al{sub 2}O{sub 3} composite was formed. The Fe{sub 3}Si/Al{sub 2}O{sub 3} composite core displayed more excellent soft magnetic properties, better frequency stability at high frequencies, much higher electrical resistivity and lower core loss than the pure Fe{sub 3}Si{sub 0.7}Al{sub 0.3} core. The method of introducing insulating layers surrounding magnetic particles provides a promising route to develop new and high compact soft magnetic materials with good magnetic and electric properties. - Graphical abstract: In Fe{sub 3}Si/Al{sub 2}O{sub 3} composite, Fe{sub 3}Si phases are separated by Al{sub 2}O{sub 3} layers and the eddy currents are confined in Fe{sub 3}Si phases, thus increasing resistivity and reducing core loss. - Highlights: • Fe{sub 3}Si{sub 0.7}Al{sub 0.3}@SiO{sub 2} core–shell particles and Fe{sub 3}Si/Al{sub 2}O{sub 3} cores were prepared. • Fe{sub 3}Si{sub 0.7}Al{sub 0.3} particles could be uniformly coated by nano-sized SiO{sub 2} clusters. • Fe{sub 3}Si{sub 0.7}Al{sub 0.3}@SiO{sub 2} particles and Fe{sub 3}Si/Al{sub 2}O{sub 3} cores showed good soft magnetic properties. • Fe{sub 3}Si/Al{sub 2}O{sub 3} had lower core loss and better frequency stability than Fe{sub 3}Si{sub 0.7}Al{sub 0.3} cores.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Giant magnetic coercivity in CaCu{sub 5}-type SmNi{sub 3}TSi (T=Mn–Cu) solid solutions

The effects of transition metal substitution for Ni on the magnetic properties of the CaCu{sub 5}-type SmNi{sub 3}TSi (T=Mn, Fe, Co, Cu) solid solutions have been investigated. SmNi{sub 3}MnSi, SmNi{sub 3}FeSi, SmNi{sub 3}CoSi and SmNi{sub 3}CuSi show ferromagnetic ordering at 125 K, 190 K, 46 K and 12 K and field induced transitions at 65 K, 110 K, 30 K and 6 K, respectively. The magnetocaloric effects of SmNi{sub 3}TSi (T=Mn, Fe, Co, Cu) were calculated in terms of isothermal magnetic entropy change (ΔS{sub m}). The magnetic entropy ΔS{sub m} reaches value of −1.1 J/kg K at 130 K for SmNi{sub 3}MnSi, −0.4 J/kg K at 180 K for SmNi{sub 3}FeSi, −0.37 J/kg K at 45 K for SmNi{sub 3}CoSi and −0.5 J/kg K at 12 K for SmNi{sub 3}CuSi in field change of 0–50 kOe around the ferromagnetic ordering temperature. They show positive ΔS{sub m} of +2.4 J/kg K at 30 K for SmNi{sub 3}MnSi, −2.6 J/kg K at 65 K for SmNi{sub 3}FeSi, +0.73 J/kg K at 15 K for SmNi{sub 3}CoSi and −0.5 J/kg K at 6 K for SmNi{sub 3}CuSi in field change of 0–50 kOe around the metamagnetic-like transition temperature. Below the field induced transition temperature, SmNi{sub 3}TSi (T=Mn, Fe, Co, Cu) exhibits giant magnetic coercivity of 80 kOe at 20 K for SmNi{sub 3}MnSi, 87 kOe at 40 K for SmNi{sub 3}FeSi, 27 kOe at 20 K for SmNi{sub 3}CoSi and 54 kOe at 5 K for SmNi{sub 3}CuSi. - Graphical abstract: CaCu{sub 5}-type SmNi{sub 3}MnSi, SmNi{sub 3}FeSi, SmNi{sub 3}CoSi and SmNi{sub 3}CuSi show ferromagnetic ordering at 125 K, 190 K, 46 K and 12 K and field induced transitions at 65 K, 110 K, 30 K and 6 K, respectively. The magnetic entropy ΔS{sub m} reaches value of −1.1 J/kg K at 130 K for SmNi{sub 3}MnSi, −0.4 J/kg K at 180 K for SmNi{sub 3}FeSi, −0.37 J/kg K at 45 K for SmNi{sub 3}CoSi and −0.5 J/kg K at 12 K for SmNi{sub 3}CuSi in field change of 0–50 kOe around the ferromagnetic ordering temperature. They show positive ΔS{sub m} of +2.4 J/kg K at 30 K for SmNi{sub 3}MnSi, −2.6 J/kg K at 65 K for SmNi{sub 3}FeSi, +0.73 J/kg K at 15 K for SmNi{sub 3}CoSi and −0.5 J/kg K at 6 K for SmNi{sub 3}CuSi in field change of 0–50 kOe around the metamagnetic-like transition temperature. Below the field induced transition temperature, SmNi{sub 3}TSi (T=Mn, Fe, Co, Cu) exhibits giant magnetic coercivity of 80 kOe at 20 K for SmNi{sub 3}MnSi, 87 kOe at 40 K for SmNi{sub 3}FeSi, 27 kOe at 20 K for SmNi{sub 3}CoSi and 54 kOe at 5 K for SmNi{sub 3}CuSi. - Highlights: • CaCu{sub 5}-type SmNi{sub 3}{Mn, Fe, Co, Cu}Si exhibit the Curie points at 12–190 K. • SmNi{sub 3}{Mn, Fe, Co, Cu}Si show field induced transition at 6–110 K. • SmNi{sub 3}MnSi shows huge magnetic hysteresis with coercive field of 80 kOe at 20 K. • SmNi{sub 3}FeSi shows huge magnetic hysteresis with coercive field of 87 kOe at 40 K. • SmNi{sub 3}CuSi shows giant coercive field of 54 kOe at 5 K.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Directly obtained τ-phase MnAl, a high performance magnetic material for permanent magnets

The metastable tetragonal τ-phase has been directly obtained from casting Mn{sub 0.54}Al{sub 0.46} and (Mn{sub 0.55}Al{sub 0.45}){sub 100}C{sub 2} using the drop synthesis method. The as-casted samples were ball milled to decrease the particle size and relaxed at 500 °C for 1 h. The phase composition, crystallographic parameters, magnetic properties and microstructure were systematically studied. The results reveal that the τ-phase could be directly obtained from drop synthesis. The highest M{sub s} of 117 emu/g was achieved in the (Mn{sub 0.55}Al{sub 0.45}){sub 100}C{sub 2} where the τ-phase was stabilized by doping with carbon. Carbon doping increased the c/a ratio of the τ-phase as it occupies specific interstitial positions (½, ½, 0) in the structure. Furthermore, ball milling increases the coercivity (H{sub c}) at the expense of a decrease in magnetic saturation (M{sub s}). The increase in coercivity is explained by a decrease of grain size in conjunction with domain wall pinning due to defects introduced during the ball milling process. - Graphical abstract: The tetragonal τ-phase has been directly obtained from casting Mn{sub 0.54}Al{sub 0.46} and (Mn{sub 0.55}Al{sub 0.45}){sub 100}C{sub 2} using the drop synthesis method. The phase composition, crystallographic parameters, magnetic properties and microstructure were systematically studied. The highest M{sub s} of 117 emu/g was achieved for (Mn{sub 0.55}Al{sub 0.45}){sub 100}C{sub 2} ball milling increases the coercivity (H{sub c}) at the expense of a decrease in magnetic saturation (M{sub s}). - Highlights: • The ferromagnetic τ-phase has been directly obtained from casting. • The highest M{sub s} of 117 emu/g was achieved for (Mn{sub 0.55}Al{sub 0.45}){sub 100}C{sub 2}. • Ball milling increases the coercivity but decreases the magnetic saturation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

One-step solution combustion synthesis of pure Ni nanopowders with enhanced coercivity: The fuel effect

In this paper, we report a new modified one-step combustion synthesis technique for production of Ni metal nanoparticles. The main unique feature of our approach is the use of microwave assisted foam preparation. Also, the effect of different types of fuels (urea, citric acid, glycine and hexamethylenetetramine) on the combustion process and characteristics of resultant solid products were investigated. It is observed that the combination of microwave assisted foam preparation and using of hexamethylenetetramine as a fuel allows producing pure ferromagnetic Ni metal nanoparticles with enhanced coercivity (78 Oe) and high value of saturation magnetization (52 emu/g) by one-step solution combustion synthesis under normal air atmosphere without any post-reduction processing. - Highlights: • The new approach in one-step SCS rote for Ni nanoparticles preparation is proposed. • Ni particles were synthesized with microwave-assistance and under air atmosphere. • The effect of different type of fuels on the combustion process was investigated. • Using of hexamethylenetetramine allows obtaining pure Ni nanoparticles. • Ni nanoparticles have enhanced coercivity and high saturation magnetization.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Coercivity and superparamagnetic evolution of high energy ball milled (HEBM) bulk CoFe{sub 2}O{sub 4} material

Ball milling (BM) of bulk CoFe{sub 2}O{sub 4} powder material carried out in order to study its structural stability and attendant property changes with respect to coercivity enhancements and superparamagnetic behaviors, showed that drastic crystallite size reduction occurred within the first 1 h of ball milling. Crystallite size dropped from 74 nm for the as-received material to a value of 11.6 nm for 600 min of ball milling. Combined X-ray diffraction (XRD) and scanning electron microscopy (SEM) analyses confirmed crystallite size reduction with corresponding increase in interparticle agglomeration/pores with increasing milling time. The maximum coercivity of 0.46 T and the crystallite size of 15.6 nm were recorded with 20 min, while peak residual strain of 0.0066 mm/mm was for 180 min of BM. Material with peak coercivity value did not have peak residual strain, or minimum crystallite size, thereby suggesting that other structural defects contributed to coercivity enhancement. The saturation magnetization (M{sub s}) value decreased continuously with increasing milling time, while remanence magnetization (M{sub r}) and coercivity decreased with increasing BM time, after an initial increase. Moessbauer spectroscopy (MS) measurements confirmed both particle size distribution and decomposition/disordering of the material together with superparamagnetism as BM time increased. The degree of inversion ranged from 41% to 71.7% at different milled states from Moessbauer spectroscopy. The internal magnetic fields of the Fe sites associated with the tetrahedral and octahedral sites were 507.4 kOe and 492 kOe respectively in the unmilled state, while 484 kOe and 468.5 kOe in the 600 min milled state correspondingly.

36 MATERIALS SCIENCE↗

Structural, magnetic, and magnetothermal properties of R{sub 2}Co{sub 2}Al (R = Tb, and Dy) compounds

The Tb{sub 2}Co{sub 2}Al and Dy{sub 2}Co{sub 2}Al alloys prepared in this study consist of 2:2:1 and 1:1:1 phases, which were identified by using the powder x-ray diffraction and scanning electron microscopy techniques. Considerable thermomagnetic irreversibility between the zero field cooled and field cooling magnetization were observed in the two alloys because of the energy barriers needed to overcome the alignment of domains. Remarkable intrinsic coercivity and remanence at temperatures close to absolute zero were also observed. The maximum magnetic entropy changes of the Tb{sub 2}Co{sub 2}Al and Dy{sub 2}Co{sub 2}Al alloys are 6.4 J/kg K and 10.6 J/kg K, respectively, with a field change from 0 to 50 kOe. The low magnetic entropy changes result from the low magnetization of the alloys even with a 50 kOe of applied field. - Research Highlights: {yields} Two-phase structure was observed in the heat treated R{sub 2}Co{sub 2}Al (R = Tb, and Dy) alloys. {yields} Considerable irreversibility was observed between the ZFC and FC magnetization. {yields} Intrinsic, remarkable coercivity and remanence were also observed. {yields} Relatively low magnetic entropy changes were obtained and reasons are given.

36 MATERIALS SCIENCE↗

Magnetic property enhancement and characterization of nano-structured barium ferrite by mechano-thermal treatment

In this research a mixture of barium ferrite and graphite powders was milled in a planetary ball mill and then heat treated in vacuum to produce BaFe{sub 12}O{sub 19}/Fe{sub 3}O{sub 4} and Fe/Fe{sub 3}O{sub 4} magnetic nano-composites. The effects of milling time and heat treatment temperature on the characteristics of powder mixture were investigated by X-ray diffraction analysis, vibrating sample magnetometer, transmission electron microscopy and Moessbauer spectroscopy. Phase analysis results showed that Fe{sub 2}O{sub 3} in barium ferrite partially reduced to Fe{sub 3}O{sub 4} during milling; hence, the reduced phase and remaining barium ferrite formed a nano-composite of BaFe{sub 12}O{sub 19}/Fe{sub 3}O{sub 4} after 20 h of milling. Heat treatment of the 40 h milled samples at 750-900 Degree-Sign C resulted in formation of Fe containing nano-composite. Magnetic measurements indicated that the coercivity of 267.92 Oe for 40 h milled sample decreased to 22.57 Oe by heat treatment at 900 Degree-Sign C, while its saturation magnetization increased from 31.56 to 169.43 emu/g due to the formation of Fe nano-crystallites. - Highlights: Black-Right-Pointing-Pointer Barium hexaferrite and graphite were treated mechano-thermally. Black-Right-Pointing-Pointer After 20 h milling, a nano-composite of BaFe{sub 12}O{sub 19}/Fe{sub 3}O{sub 4} formed. Black-Right-Pointing-Pointer Heat treatment of milled sample resulted in formation of Fe/Fe{sub 3}O{sub 4} composite. Black-Right-Pointing-Pointer Increasing heat treatment temperature results in higher saturation magnetization. Black-Right-Pointing-Pointer The milled and heat treated samples were nano-crystalline.

36 MATERIALS SCIENCE↗

Microstructural and compositional characterization of terbium-doped Nd-Fe-B sintered magnets

Anisotropic sintered magnets based on the Nd{sub 2}Fe{sub 14}B phase doped with Tb were prepared using a grain-boundary diffusion process (GBDP) in order to enhance their coercivity. A FEGSEM microstructural analysis revealed that these GBDP magnets had a core-shell structure, where thin, Tb-rich, (NdTb){sub 2}Fe{sub 14}B shells are formed on the original matrix Nd{sub 2}Fe{sub 14}B grains after diffusion of the Tb. This shell thickness varies from a few tens of nanometres in the middle of the magnet up to a few micrometers near the edge. The exact chemical composition of these shells was determined using EDS and WDS electron-probe microanalyses, which were modified and optimized for submicrometer scale analyses. When analyzing the common Nd-L{alpha}, Tb-L{alpha} and Fe-K{alpha} lines a mutual multiple overlap in the EDS spectra is present and, as a result, an accurate quantitative analysis was only feasible when using WDS. Using this technique we were able to achieve a lateral analytical resolution of 0.4 {mu}m. A further improvement in resolution, down to 0.15 {mu}m, was realized with a dedicated set-up using low-voltage EDS, analyzing the 'atypical' low-energy Nd-M{alpha}, Tb-M{alpha} and Fe-L{alpha} lines. Quantitative analyses confirmed that the reaction phase (Nd{sub x}Tb{sub 1} {sub -x}){sub 2}Fe{sub 14}B is formed after the diffusion of Tb with the equilibrium concentration of Tb being equal to x Almost-Equal-To 0.5, i.e., with the atomic ratio of Nd/Tb equal to 1/1. We also found that a relatively sharp Tb concentration gradient from the shell to the core occurs within a length of Almost-Equal-To 0.5 {mu}m, while the Fe concentration remains unchanged. In terms of magnetic properties, the Tb-doping significantly increased coercivity by Almost-Equal-To 30% while the remanence remained at the same value as in the undoped Nd-Fe-B. - Highlights: Black-Right-Pointing-Pointer Nd-Fe-B sintered magnets were doped with Tb using grain-boundary diffusion process. Black-Right-Pointing-Pointer A tiny core-shell reaction phase was formed around the Nd{sub 2}Fe{sub 14}B matrix grains. Black-Right-Pointing-Pointer EDS and WDS analyses confirmed (Nd{sub 0.5}Tb{sub 0.5}){sub 2}Fe{sub 14}B equilibrium shell composition. Black-Right-Pointing-Pointer Coercivity of Tb-doped Nd-Fe-B increases by 30% without a drop in remanence.

36 MATERIALS SCIENCE↗

Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} nanoparticles dispersed in a SiO{sub 2} matrix synthesized by sol-gel processing

(Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4})x/(SiO{sub 2})(100 - x) (x = 5, 20 and 50 wt.%) nanocomposites are synthesized by a sol-gel method using tetraethylorthosilicate (TEOS) and metallic nitrates as precursors, and by further annealing the powders for 1 h at 1273 K. X-ray diffraction (XRD), transmission electron microscopy (TEM), room temperature vibrating sample magnetometry (VSM) and SQUID measurements are employed for structural, morphological and magnetic sample characterization. For all the concentrations analyzed, the powder nanocomposites actually consist of spinel NiZn ferrite nanoparticles, dispersed in an amorphous silica matrix. TEM studies reveal different particle size distributions and particle morphologies for the three ferrite contents. The 20 wt.%-NiZn ferrite samples consist of nearly spherical nanoparticles, of about 8 nm, mainly superparamagnetic, well-dispersed in the amorphous silica matrix, while the 5 wt.%-NiZn ferrite samples exhibit a bimodal particle size distribution (5 and 30 nm) of single-domain nanoparticles embedded in the silica. In the 50 wt.%-NiZn ferrite samples, two particle families are observed: small round superparamagnetic nanoparticles of about 8 nm embedded in the amorphous silica matrix and large, non-spherical, ferrimagnetic ones, forming agglomerates outside the matrix. In all the synthesized samples, thickness fringes are observed inside some of the ferrite nanoparticles in dark field images. This contrast is explained using the theory of electron diffraction in a weak beam dark field (WBDF) condition and considering spherical ferrite nanoparticles. A large range of tailored magnetic properties varying the fraction, dispersion and mean size of the ferrimagnetic NiZn ferrite particles is obtained. Room temperature saturation magnetization values are found in the range 3.0-30.4 Am{sup 2}/kg for the different concentration samples. Coercivity values, between 1.9 and 7.6 mT, are more than 50% higher than those measured in powders of pure stoichiometric NiZn ferrite nanoparticles and somewhat higher than those reported for similar NiZn ferrite/SiO{sub 2} nanocomposites also synthesized by sol-gel processes. A correlation between the nanocomposite microstructure and the observed magnetic properties is established. - Highlights: Black-Right-Pointing-Pointer NiZn ferrite/SiO{sub 2} nanocomposites are successfully synthesized by a sol-gel route. Black-Right-Pointing-Pointer Depending on the NiZn ferrite content single or bimodal size distributions result. Black-Right-Pointing-Pointer Coercivity (1.9-7.6 mT) is 50% higher than in stoichiometric NiZn ferrite powders. Black-Right-Pointing-Pointer Microstructure and magnetic properties are correlated.

36 MATERIALS SCIENCE↗

Synthesis and characterization of barium ferrite–silica nanocomposites

In this work, we prepared barium ferrite-silica (BaM-SiO{sub 2}) nanocomposites of different molar ratios by high-energy ball milling, followed by heat-treatment at different temperatures. The microstructure, morphology and magnetic properties were characterized for different synthesis conditions by using X-ray diffraction (XRD), scanning electron microscopy (SEM) and vibrating sample magnetometry (VSM). The results indicate that 15 h of milling was enough to avoid the generation of hematite phase and to get a good dispersion of barium ferrite particles in the ceramic matrix. For milling periods beyond 15 h and heat treatment above 900 °C, the XRD patterns showed the presence of hematite phase caused by the decomposition of BaM. The agglomerate size observed through SEM analysis was around 150 nm with a good BaM dispersion into the SiO{sub 2} matrix. The highest saturation magnetization (Ms) value obtained was 43 emu/g and the corresponding coercivity (Hc) value of 3.4 kOe for the composition 60BaM-40SiO{sub 2} milled for 15 h and heat treated at 900 °C. This coercivity value is acceptable for the application in magnetic recording media. Highlights: • Barium ferrite–silica nanocomposites were prepared by high energy ball milling. • Optimal processing time is 15 h milling and heat treatment at 900 °C. • This is enough to avoid the generation of hematite phase. • Obtain good dispersion of barium ferrite particles in the ceramic matrix • Above this processing time shows the presence of increased amount of hematite.

36 MATERIALS SCIENCE↗

Physical and electrochemical study of cobalt oxide nano- and microparticles

Cobalt oxide nanocrystals of size 17–21 nm were synthesized by a simple reaction between cobalt acetate (II) and dodecylamine. On the other hand, micrometric Co{sub 3}O{sub 4} was prepared using the ceramic method. The structural examination of these materials was performed using powder X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), and transmission electron microscopy (TEM and HRTEM). XRD studies showed that the oxides were pure, well-crystallized, spinel cubic phases with a-cell parameter of 0.8049 nm and 0.8069 nm for the nano and micro-oxide, respectively. The average particle size was 19 nm (nano-oxide) and 1250 μm (micro-oxide). Morphological studies carried out by SEM and TEM analyses have shown the presence of octahedral particles in both cases. Bulk and surface properties investigated by X-ray photoelectron spectroscopy (XPS), point zero charge (pzc), FTIR and cyclic voltammetry indicated that there were no significant differences in the composition on both materials. The magnetic behavior of the samples was determined using a vibrating sample magnetometer. The compounds showed paramagnetic character and no coercivity and remanence in all cases. Galvanostatic measurements of electrodes formed with nanocrystals showed better performance than those built with micrometric particles. - Highlights: • Spinel Co{sub 3}O{sub 4} nanoparticles and microparticles with same structure but with different cell parameters, particle size and surface area were synthesized. • Oxide nanoparticles showed better electrochemical behavior than micrometric ones due to area effect.

36 MATERIALS SCIENCE↗

Influence of ball milling on atomic structure and magnetic properties of Co{sub 40}Fe{sub 22}Ta{sub 8}B{sub 30} glassy alloy

The influence of ball milling on the atomic structure and magnetic properties of the Co{sub 40}Fe{sub 22}Ta{sub 8}B{sub 30} metallic glass with a high thermal stability and excellent soft magnetic properties has been investigated. After 14 h of milling, the obtained powders were found to consist mainly of an amorphous phase and a small fraction of the (Co,Fe){sub 21}Ta{sub 2}B{sub 6} nanocrystals. The changes in the reduced pair correlation functions suggest noticeable changes in the atomic structure of the amorphous upon ball milling. Furthermore, it has been shown that milling is accompanied by introduction of compressive and dilatational sites in the glassy phase and increasing the fluctuation of the atomic-level hydrostatic stress without affecting the coordination number of the nearest neighbors. Ball milling has decreased the thermal stability and significantly affected the magnetic properties through increasing the saturation magnetization, Curie temperature of the amorphous phase and coercivity. - Highlights: • Ball milling affected the atomic structure of Co{sub 40}Fe{sub 22}Ta{sub 8}B{sub 30} metallic glass. • Mechanically-induced crystallization started after 4 h milling. • Milling increased the fluctuation of the atomic-level hydrostatic stress in glass. • Ball milling influenced the thermal stability and magnetic properties.

36 MATERIALS SCIENCE↗

The stress, surface spin and dipolar interaction in the diluted NiFe{sub 2}O{sub 4} nanoparticles by the SiO{sub 2} matrix: Characterization and analyses

Well-dispersed uniform NiFe{sub 2}O{sub 4} nanoparticles (NPs) with an average particle size of 15.4 nm were synthesized by thermal decomposition of a metal–organic salt, and then were diluted in a SiO{sub 2} matrix via a sol–gel method with different concentration. The magnetization (M) dependence of NiFe{sub 2}O{sub 4}/SiO{sub 2} on the temperature (T) and on the applied magnetic field (H) was systematically characterized by the Quantum Design superconducting quantum interference device (SQUID) PPMS system. The results of M ~ H/T divide the magnetic properties between 10 K and 300 K into two regions: the low temperature blocked-particle regime below the blocking temperature T{sub B} and the interacting superparamagnetic (ISP) regime above T{sub B}. In the ISP regime, all samples deviate from the ideal Langevin superparamagnetic behavior due to the effective anisotropy induced by the stress, surface spins and interparticle dipolar interaction. The Raman spectra indicate that the stress in all samples exhibits the vibration behavior, which leads to the effective anisotropy and hence coercivity vibration. - Graphical abstract: Display Omitted - Highlights: • Increase of NiFe{sub 2}O{sub 4} NPs' concentration elevates T{sub B} and broadens ZFC peak. • NiFe{sub 2}O{sub 4}/SiO{sub 2} samples do not exhibit the ideal superparamagnetism above T{sub B}. • Stress leads to the effective anisotropy and hence H{sub c} vibration. • Stress vibration was characterized in detail by the Raman spectra.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Friction consolidation of gas-atomized Fe−Si powders for soft magnetic applications

Soft magnetic materials are often limited in scalability due to conventional processes that do not retain beneficial microstructures, and their associated physical properties, during densification. In this work, friction consolidation (FC) has been studied to fabricate Fe−Si soft magnetic materials from gas-atomized powder precursors. Fe−Si powder is consolidated using variable pressure and tool rotation speed in an effort to evaluate this unique densification approach for potential improvements in magnetic properties. FC, due to the high shear deformation involved, is shown to result in uniform gradual grain structure refinement across the consolidated workpiece from the center nearest the tool to the edge. Magnetic properties along different orientations indicate little, if any, textural orientation in the refined grain structure. The effect of annealing on the magnetic properties is evaluated and shown to decrease coercivity. FC processing was able to retain the magnetization of the original gas-atomized powders but further process optimization is needed to reach the optimal coercivity for the soft magnetic materials applications. - Highlights: •Friction stir processing was utilized to consolidate Fe−Si soft magnetic powders. •The resultant microstructure and magnetic properties were correlated to the processing conditions. •Friction consolidation refined the grain size of the materials by ~ 40%. •Annealing successfully reduced the coercivity induced by the stress during processing. •The results shine light on the possible scaling up of nanostructured materials.

36 MATERIALS SCIENCE↗

Thermodynamic, structural and magnetic studies of phase transformations in MnAl nanocomposite alloys

Highlights: • Small changes in MnAl stoichiometry (5 at.%) produce different phase structure. • In Mn{sub 60}Al{sub 40} as-cast alloy only hcp ε phase can be found • In Mn{sub 55}Al{sub 45} as-cast alloy, there is a mixture of γ{sub 2} (Al{sub 8}Mn{sub 5}) and ε as well as ferromagnetic MnAl τ-phase. • Energies of phase transformation of about 165 kJ/mol for Mn{sub 60}Al{sub 40} and 290 kJ/mol for Mn{sub 55}Al{sub 45} alloys are found. • hcp ε phase decomposes through the migration of interphase interfaces. - Abstract: We have undertaken a temperature-dependent, investigation of the thermodynamics, structure, morphology and magnetism of two MnAl nanocomposite alloys (Mn{sub 60}Al{sub 40} and Mn{sub 55}Al{sub 45}). Differential scanning calorimetry (DSC) studies allowed the determination of the exo-effects occurring in the structural phase transformation of MnAl, while by using temperature-dependent X-ray diffraction of synchrotron radiation we were able to monitor the phase transformation effects and the evolution with temperature of various structural phases occurring in the samples. We have shown that slight changes in stoichiometry (5 at.%) give rise to different phase structure in the as-cast state. While in Mn{sub 60}Al{sub 40} only hcp ε phase can be found, in Mn{sub 55}Al{sub 45} as-cast alloy, there is a quite complex phase structure with a mixture of γ{sub 2} (Al{sub 8}Mn{sub 5}) and ε as well as ferromagnetic MnAl τ-phase. Activation energies of about 165 kJ/mol and 290 kJ/mol have been calculated from the Ozawa-Flynn-Wall analysis of DSC experimental data. These findings are in good agreement with the results obtained from XRD. For the Mn{sub 55}Al{sub 45} as-cast alloy, we have confirmed by temperature-dependent synchrotron XRD that the hcp ε phase decomposes through the migration of interphase interfaces with the transformation rate controlled by boundary diffusion processes. High-resolution transmission electron microscopy have confirmed the phase structure obtained by XRD, while magnetic properties, obtained for the as-cast alloys are consistent with the multiphase character of the samples and in good agreement with previously reported results. The magnetization does not saturate for the maximum applied field of about 4 × 10{sup 6} A/m and a marked coercivity of about 160 kA/m is obtained for the Mn{sub 55}Al{sub 45} as-cast alloy.

77 NANOSCIENCE AND NANOTECHNOLOGY↗