Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CMC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Nozzle assembly and method for forming nozzle assembly

A nozzle assembly is disclosed, including a CMC nozzle shell, a nozzle spar, and an endwall. The CMC nozzle shell includes a CMC composition and an interior cavity. The nozzle spar is partially disposed within the interior cavity and includes a metallic composition, a cross-sectional conformation, a plurality of spacers protruding from the cross-sectional conformation, the plurality of spacers contacting the CMC nozzle shell, and a spar cap. The endwall includes at least one surface in lateral contact with the spar cap and maintains a lateral orientation of the CMC nozzle shell and the nozzle spar relative to the endwall. The lateral orientation maintains a predetermined throat area of the nozzle assembly. A method for forming the nozzle assembly includes inserting the nozzle spar into the interior cavity, rotating the CMC nozzle shell and the nozzle spar laterally relative to the endwall, and maintaining the lateral orientation.

Hafner, Matthew Troy↗

Constant mean curvature slicings of Kantowski-Sachs spacetimes

We investigate existence, uniqueness, and the asymptotic properties of constant mean curvature (CMC) slicings in vacuum Kantowski-Sachs spacetimes with positive cosmological constant. Since these spacetimes violate the strong energy condition, most of the general theorems on CMC slicings do not apply. Although there are in fact Kantowski-Sachs spacetimes with a unique CMC foliation or CMC time function, we prove that there also exist Kantowski-Sachs spacetimes with an arbitrary number of (families of) CMC slicings. The properties of these slicings are analyzed in some detail.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Self-degradable Slag/Class F Fly Ash-Blend Cements

Self-degradable slag/Class F fly ash blend pozzolana cements were formulated, assuming that they might serve well as alternative temporary fracture sealers in Enhanced Geothermal System (EGS) wells operating at temperatures of {ge} 200 C. Two candidate formulas were screened based upon material criteria including an initial setting time {ge} 60 min at 85 C, compressive strength {ge} 2000 psi for a 200 C autoclaved specimen, and the extent of self-degradation of cement heated at {ge} 200 C for it was contacted with water. The first screened dry mix formula consisted of 76.5 wt% slag-19.0 wt% Class F fly ash-3.8 wt% sodium silicate as alkali activator, and 0.7 wt% carboxymethyl cellulose (CMC) as the self-degradation promoting additive, and second formula comprised of 57.3 wt% slag, 38.2 wt% Class F fly ash, 3.8 wt% sodium silicate, and 0.7 wt% CMC. After mixing with water and autoclaving it at 200 C, the aluminum-substituted 1.1 nm tobermorite crystal phase was identified as hydrothermal reaction product responsible for the development of a compressive strength of 5983 psi. The 200 C-autoclaved cement made with the latter formula had the combined phases of tobermorite as its major reaction product and amorphous geopolymer as its minor one providing a compressive strength of 5271 psi. Sodium hydroxide derived from the hydrolysis of sodium silicate activator not only initiated the pozzolanic reaction of slag and fly ash, but also played an important role in generating in-situ exothermic heat that significantly contributed to promoting self-degradation of cementitious sealers. The source of this exothermic heat was the interactions between sodium hydroxide, and gaseous CO{sub 2} and CH{sub 3}COOH by-products generated from thermal decomposition of CMC at {ge} 200 C in an aqueous medium. Thus, the magnitude of this self-degradation depended on the exothermic temperature evolved in the sealer; a higher temperature led to a sever disintegration of sealer. The exothermic temperature was controlled by the extent of thermal decomposition of CMC, demonstrating that CMC decomposed at higher temperature emitted more gaseous reactants. Hence, such large emission enhanced the evolution of in-situ exothermic heat. In contrast, the excessive formation of geopolymer phase due to more incorporation of Class F fly ash into this cementitious system affected its ability to self-degrade, reflecting that there was no self-degradation. The geopolymer was formed by hydrothermal reactions between sodium hydroxide from sodium silicate and mullite in Class F fly ash. Thus, the major reason why geopolymer-based cementitiuos sealers did not degrade after heated sealers came in contact with water was their lack of free sodium hydroxide.

15 GEOTHERMAL ENERGY↗

Cellulose Nanofibers as Rheological Modifiers to Improve Biomass Slurry Processing and Fermentation

This study investigates the enhancement of biomass slurry processability through the addition of rheological modifiers, focusing on carboxymethyl cellulose (CMC) and TEMPO-mediated oxidized cellulose nanofibrils (TCNF). Three sets of experiments were conducted to assess the effects of these additives on slurry processing and fermentation. Initial experiments evaluated the slurry extrudability, concluding that TCNF aids extrusion similarly to CMC. Subsequent experiments explored slurry viscosity reduction mechanisms, revealing that while CMC significantly reduced the viscosity, TCNF’s impact is negligible. Additionally, TCNF performed comparably to CMC in water retention tests across different conditions, which suggests that TCNF have potential as an effective additive for maintaining slurry fluidity at high solid concentrations through enhanced water retention. Lastly, both additives were investigated to ensure that they did not impact hydrolyzed biomass fermentation. The findings suggest that TCNF’s mechanisms differ from those of traditional water-soluble polymers like CMC, offering insights into novel approaches to improve the biomass processing efficiency and subsequent fermentation.

Jamieson, Zachary↗

Postural responses of head and foot cutaneous microvascular flow and their sensitivity to bed rest

To explore the mechanism for facial puffiness, headache, and nasal congestion associated with microgravity and cephalad fluid shifts, the postural responses of the cutaneous microcirculation (CMC) in the forehead and dorsum of the foot of eight healthy men were studied by changing body position on a tilt table and measuring blood flows with a laser Doppler flowmeter. Increasing arterial pressure in the feet by moving from a -6-deg head-down tilt to a 60-deg head-up posture decreased foot CMC by 46.5 + or - 12.0 percent. Raising arterial pressure in the head increased forehead CMC by 25.5 + or - 0.7 percent (p less than 0.05). To investigate the possibility that these opposite responses could be modified by simulated microgravity, tilt test were repeated after 7 d of -6-deg head-down-tilt bed rest. The responses were not significantly different from those recorded before bed rest. Therefore, CMC in the feet is well regulated to prevent edema when shifting to an upright position, whereas there is less regulation in the head CMC.

Aratow, Michael↗

Advanced satellite communication system

The objective of this research program was to develop an innovative advanced satellite receiver/demodulator utilizing surface acoustic wave (SAW) chirp transform processor and coherent BPSK demodulation. The algorithm of this SAW chirp Fourier transformer is of the Convolve - Multiply - Convolve (CMC) type, utilizing off-the-shelf reflective array compressor (RAC) chirp filters. This satellite receiver, if fully developed, was intended to be used as an on-board multichannel communications repeater. The Advanced Communications Receiver consists of four units: (1) CMC processor, (2) single sideband modulator, (3) demodulator, and (4) chirp waveform generator and individual channel processors. The input signal is composed of multiple user transmission frequencies operating independently from remotely located ground terminals. This signal is Fourier transformed by the CMC Processor into a unique time slot for each user frequency. The CMC processor is driven by a waveform generator through a single sideband (SSB) modulator. The output of the coherent demodulator is composed of positive and negative pulses, which are the envelopes of the chirp transform processor output. These pulses correspond to the data symbols. Following the demodulator, a logic circuit reconstructs the pulses into data, which are subsequently differentially decoded to form the transmitted data. The coherent demodulation and detection of BPSK signals derived from a CMC chirp transform processor were experimentally demonstrated and bit error rate (BER) testing was performed. To assess the feasibility of such advanced receiver, the results were compared with the theoretical analysis and plotted for an average BER as a function of signal-to-noise ratio. Another goal of this SBIR program was the development of a commercial product. The commercial product developed was an arbitrary waveform generator. The successful sales have begun with the delivery of the first arbitrary waveform generator.

Staples, Edward J.↗

Concept for Determining the Life of Ceramic Matrix Composites Using Nondestructive Characterization Techniques

Damping measurements have been taken on ceramic matrix composite (CMC) turbopump blisks in the as fabricated, post proof testing, and post turbopump testing conditions. These results indicate that damping is able to quantify fatigue of the CMC blisk. This gives hope for the potential of determining the actual and residual life of CMC materials using a combination of nondestructive techniques. If successful, then this new paradigm for life prediction of CMCs could revolutionize the approach for designing and servicing CMC components, thereby significantly reducing costs for design, development, health monitoring, and maintenance of CMC components and systems. The Nondestructive Characterization (NDC) life prediction approach would complement life prediction using micromechanics and continuum finite element models. This paper reports on the initial concept of NDC life prediction and how changes in damping and ultrasonic elastic modulus data have established the concept as a possibility.

Effinger, Michael↗

An Assessment of Variability in the Average Tensile Properties of a Melt-Infiltrated SiC/SiC Composite

Woven SiC/SiC Ceramic Matrix Composites (CMCs), manufactured by the slurry-cast, melt-infiltration process are under consideration as combustor liner materials in aircraft gas turbine engines. Tensile properties (elastic modulus, proportional limit strength, in-plane tensile strength and strain to failure) of the CMC, manufactured during two separate time periods (9/99 and 1/01) were determined at 816 and 1024 C by conducting tensile tests on specimens machined from the CMC plates. A total of 24 tensile tests were conducted for each temperature and CMC variant combination. In this study average tensile properties of the two cMC variants were statistically compared to evaluate significant differences, if any, within the CMC's properties.

Kalluri, Sreeramesh↗

Lightweight, Actively Cooled Ceramic Matrix Composite Thrustcells Successfully Tested in Rocket Combustion Lab

In a joint effort between the NASA Glenn Research Center and the NASA Marshall Space Flight Center, regeneratively cooled ceramic matrix composite (CMC) thrustcells were developed and successfully tested in Glenn's Rocket Combustion Lab. Cooled CMC's offer the potential for substantial weight savings over more traditional metallic parts. Two CMC concepts were investigated. In the first of these concepts, an innovative processing approach utilized by Hyper-Therm, Inc., allowed woven CMC coolant containment tubes to be incorporated into the complex thruster design. In this unique design, the coolant passages had varying cross-sectional shapes but maintained a constant cross-sectional area along the length of the thruster. These thrusters were silicon carbide matrix composites reinforced with silicon carbide fibers. The second concept, which was supplied by Ceramic Composites, Inc., utilized copper cooling coils surrounding a carbon-fiber-reinforced carbon matrix composite. In this design, a protective gradient coating was applied to the inner thruster wall. Ceramic Composites, Inc.'s, method of incorporating the coating into the fiber and matrix eliminated the spallation problem often observed with thermal barrier coatings during hotfire testing. The focus of the testing effort was on screening the CMC material's capabilities as well as evaluating the performance of the thermal barrier or fiber-matrix interfacial coatings. Both concepts were hot-fire tested in gaseous O2/H2 environments. The test matrix included oxygen-to-fuel ratios ranging from 1.5 to 7 with chamber pressures to 400 psi. Steady-state internal wall temperatures in excess of 4300 F were measured in situ for successful 30-sec test runs. Photograph of actively cooled composite thrustcell fabricated by Hyper-Therm is shown. The thrustcell is a silicon-carbide-fiber-reinforced silicon carbide matrix composite with woven cooling channels. The matrix is formed via chemical vapor infiltration. Photograph of hot-fire test of an actively cooled carbon-fiber-reinforced carbon matrix composite thrustcell is also shown. This composite thrustcell, which was fabricated by CCI, Inc., was wound with copper cooling coils to contain the water coolant. The tests were run with oxygen fuel ratios up to seven with chamber pressures of 200 psia.

Jaskowiak, Martha H.↗

Advanced Constituents and Processes for Ceramic Composite Engine Components

The successful replacement of metal alloys by ceramic matrix composites (CMC) in hot-section engine components will depend strongly on optimizing the processes and properties of the CMC microstructural constituents so that they can synergistically provide the total CMC system with improved temperature capability and with the key properties required by the components for long-term structural service. This presentation provides the results of recent activities at NASA aimed at developing advanced silicon carbide (Sic) fiber-reinforced hybrid Sic matrix composite systems that can operate under mechanical loading and oxidizing conditions for hundreds of hours at 2400 and 2600 F, temperatures well above current metal capability. These SiC/SiC composite systems are lightweight (-30% metal density) and, in comparison to monolithic ceramics and carbon fiber-reinforced ceramic composites, are able to reliably retain their structural properties for long times under aggressive engine environments. It is shown that the improved temperature capability of the SiC/SiC systems is related first to the NASA development of the Sylramic-iBN Sic fiber, which displays high thermal stability, creep resistance, rupture resistance, and thermal conductivity, and possesses an in-situ grown BN surface layer for added environmental durability. This fiber is simply derived from Sylramic Sic fiber type that is currently produced at ATK COI Ceramics. Further capability is then derived by using chemical vapor infiltration (CVI) to form the initial portion of the hybrid Sic matrix. Because of its high creep resistance and thermal conductivity, the CVI Sic matrix is a required base constituent for all the high temperature SiC/SiC systems. By subsequently thermo- mechanical-treating the CMC preform, which consists of the S ylramic-iBN fibers and CVI Sic matrix, process-related defects in the matrix are removed, further improving matrix and CMC creep resistance and conductivity.

Yun, H. M.↗

Ceramic Composite Development for Gas Turbine Engine Hot Section Components

The development of ceramic materials for incorporation into the hot section of gas turbine engines has been ongoing for about fifty years. Researchers have designed, developed, and tested ceramic gas turbine components in rigs and engines for automotive, aero-propulsion, industrial, and utility power applications. Today, primarily because of materials limitations and/or economic factors, major challenges still remain for the implementation of ceramic components in gas turbines. For example, because of low fracture toughness, monolithic ceramics continue to suffer from the risk of failure due to unknown extrinsic damage events during engine service. On the other hand, ceramic matrix composites (CMC) with their ability to display much higher damage tolerance appear to be the materials of choice for current and future engine components. The objective of this paper is to briefly review the design and property status of CMC materials for implementation within the combustor and turbine sections for gas turbine engine applications. It is shown that although CMC systems have advanced significantly in thermo-structural performance within recent years, certain challenges still exist in terms of producibility, design, and affordability for commercial CMC turbine components. Nevertheless, there exist some recent successful efforts for prototype CMC components within different engine types.

DiCarlo, James A.↗

Effects of High-Temperature Annealing in Air on Hi-Nicalon Fiber-Reinforced Celsian Matrix Composites

BN/SiC-coated Hi-Nicalon fiber-reinforced celsian matrix composites (CMC) were annealed for 100 h in air at various temperatures to 1200 C, followed by flexural strength measurements at room temperature. Values of yield stress and strain, ultimate strength, and composite modulus remain almost unchanged for samples annealed up to 1100 C. A thin porous layer formed on the surface of the 1100 C annealed sample and its density decreased from 3.09 to 2.90 g/cu cm. The specimen annealed at 1200 C gained 0.43 wt%, was severely deformed, and was covered with a porous layer of thick shiny glaze which could be easily peeled off. Some gas bubbles were also present on the surface. This surface layer consisted of elongated crystals of monoclinic celsian and some amorphous phase(s). The fibers in this surface ply of the CMC had broken into small pieces. The fiber-matrix interface strength was characterized through fiber push-in technique. Values of debond stress, alpha(sub d), and frictional sliding stress, tau(sub f), for the as-fabricated CMC were 0.31+/-0.14 GPa and 10.4+/-3.1 MPa, respectively. These values compared with 0.53+/-0.47 GPa and 8.33+/-1.72 MPa for the fibers in the interior of the 1200 C annealed sample, indicating hardly any change in fiber-matrix interface strength. The effects of thermal aging on microstructure were investigated using scanning electron microscopy. Only the surface ply of the 1200 C annealed specimens had degraded from oxidation whereas the bulk interior part of the CMC was unaffected. A mechanism is proposed explaining the various steps involved during the degradation of the CMC on annealing in air at 1200 C.

Bansal, Narottam P.↗

Tensile Behavior of As-Fabricated and Burner-Rig Exposed SiC/SiC Composites with Hi-Nicalon Type-S Fibers

Tensile stress-strain curves were measured at room temperature and 1315 C for 2D-woven SiC/BN/SiC ceramic matrix composites (CMC) reinforced by two variations of Hi-Nicalon Type-S SiC fibers. These fibers, which contained a thin continuous carbon-rich layer on their as-produced surface, provided the as-fabricated CMC with good composite behavior and an ultimate strength and strain of -350 MPa and -0.5%, respectively. However, after un-stressed burner-rig exposure at 815 C for -100 hrs, CMC tensile specimens with cut edges and exposed interphases showed a significant decrease in ultimate properties with effectively no composite behavior. Microstructural observations show that the degradation was caused by internal fiber-fiber oxide bonding after removal of the carbon-rich fiber surface layer by the high-velocity combustion gases. On the other hand, SiC/BN/SiC CMC with Sylramic-iBN fibers without carbon-rich surfaces showed higher as-fabricated strength and no loss in strength after the same burner rig exposure. Based on the strong role of the carbon layer in these observations, a process method was developed and demonstrated for achieving better strength retention of Hi-Nicalon Type-S CMC during burner rig exposure. Other general approaches for minimizing this current deficiency with as-produced Type-S fibers are discussed.

Yun, H. M.↗

Ultra High Temperature (UHT) SiC Fiber (Phase 2)

Silicon-carbide fiber-reinforced silicon-carbide ceramic matrix composites (SiCSiC CMC) are emerginglightweight re-usable structural materials not only for hot section components in gas turbine engines, but also for controlsurfaces and leading edges of reusable hypersonic vehicles as well as for nuclear propulsion and reactor components. Ithas been shown that when these CMC are employed in engine hot-section components, the higher the upper usetemperature (UUT) of the SiC fiber, the more performance benefits are accrued, such as higher operating temperatures,reduced component cooling air, reduced fuel consumption, and reduced emissions. The first generation of SiCSiC CMC with a temperature capability of 2200-2400F are on the verge of being introduced into the hot-section components ofcommercial and military gas turbine engines.Today the SiC fiber type currently recognized as the worlds best in terms ofthermo-mechanical performance is the Sylramic-iBN fiber. This fiber was previously developed by the PI at NASA GRC using patented processes to improve the high-cost commercial Sylramic fiber, which in turn was derived from anotherlow-cost low-performance commercial fiber. Although the Sylramic-iBN fiber shows state-of-the art creep and rupture resistance for use temperatures above 2550oF, NASA has shown by fundamental creep studies and model developmentthat its microstructure and creep resistance could theoretically be significantly improved to produce an Ultra HighTemperature (UHT) SiC fiber.This Phase II Seedling Fund effort has been focused on the key objective of effectively repeating the similar processes used for producing the Sylramic-iBN fiber using a design of experiments approach to first understand the cause of the less than optimum Sylramic-iBN microstructure and then attempting to develop processconditions that eliminate or minimize these key microstructural issues. In so doing, it is predicted that that theseadvanced process could result in an UHT SiC fiber with 20 times more creep resistance than the Sylramic-iBN fiber,which in turn would allow SiCSiC CMC to operate up to 2700oF and above, thereby further enhancing the performancebenefits of SiCSiC components in aero-propulsion engines. It was also envisioned that the fiber processes developedduring Phase II efforts would not only reduce production costs for the UHT fiber by using low-cost precursor fibers andcombined processes, but also allow the UHT fibers to be directly produced in preforms of the precursor fibers, possibly atthe facilities of the CMC fabricator.

SiC Ceramic Fiber↗

Understanding the Durability of SiC Based Ceramic Matrix Composites (CMCs) for Gas Turbine Engine Hot Section Components

Silicon carbide fiber reinforced silicon carbide ceramic matrix composites (SiCf/SiC-CMCs) are being used in the fabrication of gas turbine engine hot section components due to their light weight and excellent thermal and chemical stabilities at high-temperature. These superior properties enable significant enhancements in engine efficiency and reduced fuel burn, emissions, and cooling requirements. In support of NASA’s Aeronautics Mission under various programs at Glenn Research Center, different types of composites have been developed and assessed for a high temperature (2700 °F) SiCf/SiC CMC system for turbine engine applications. These composites have creep-resistant SiC fibers, advanced 3D weaves, 2700 °F-capable hybrid SiC matrices, and durable environmental barrier coatings (EBCs). These efforts have resulted in improvements in the overall CMC thermomechanical and environmental durability. In order to study the role of different constituents and processing variables, a single fiber tow CVI (chemical vapor infiltration) SiC/SiC mini-composite can be considered the basic architectural feature of woven and laminate SiC/SiC CMCs. Moreover, the mini-composite mechanical and tensile creep damage behavior represents the creep behavior of 0° fiber tows in the axial loading direction of a macro-composite or component. In addition, a large number of mini-composite samples can be fabricated at relatively low cost within a short time, which makes them attractive for obtaining a robust set of experimental data and studying constituent behavior. In this presentation, the mini-composite approach to study damage mechanisms that limit CMC life in extreme environments including exposure to steam will be presented. The effects of constituent type and volume fraction on the CMC durability, which will help influence CMC design, will be discussed.

Ceramic Matrix Composites (CMCs)↗

Special Issue: Environmental Barrier Coatings

The global increase in air travel will require commercial vehicles to be more efficient than ever before. Advanced turbine hot section materials are a key technology required to keep fuel consumption and emission to a minimum. Ceramic matrix composites (CMCs) are the most promising material to revolutionize turbine hot section materials because of their excellent high‐temperature properties. Rapid surface recession due to volatilization by water vapor is the Achilles heel of CMCs. Environmental barrier coatings (EBCs), which protect CMCs from water vapor, is an enabling technology for CMCs. The first CMC component entered into service in 2016 in a commercial engine, and more CMC components are scheduled to follow within the next few years. One of the most difficult challenges to CMC components is EBC durability because failure of EBC leads to a rapid reduction in CMC component life. Novel EBC chemistries, creative EBC designs, and robust processes are required to meet EBC durability challenges. Engine-relevant testing, characterization, and lifing methods need to be developed to improve EBC reliability. The aim of this Special Issue is to present recent advances in EBC technology to address current EBC challenges.

EBC, CMC, Oxidation, Volatility, CMAS, Thermomecha↗

The Effect of Trailing Edge Grid Resolution in Large-Eddy Simulations

Ceramic Matrix Composite (CMC) with environmental barrier coating can tolerate significantly higher temperatures compared with the conventional metal alloy blades and thus can help achieve higher thermal efficiency in gas turbine engines. Due to the complex fabrication process of CMC blades, larger blade trailing edge thicknesses and larger leading-edge radii of curvature are expected. These features significantly alter aerodynamic performance especially near the trailing edge and thus the loss profile. In previous studies, the authors used the large eddy simulation (LES) as well as the Reynolds Averaged Navier-Stokes (RANS) coupled with an intermittency function-based transition model to simulate an aerodynamics performance of three different CMC blades and compared the predictions against the data acquired at NASA Glenn Transonic Turbine Blade Cascade Rig. Although we were able to successfully predict different characteristics of aerodynamic performance among three different blades (e.g., pressure loading and integrated losses), LES consistently predicted a small recirculation bubble at the end of the suction side. This was not inconsistent with the physics of the flow, but the pressure loading, locally, near the trailing edge, and as a result, the measured wake profiles did not match the experimental data. To delve further into these issues, a new LES grid with a much finer mesh near the trailing edge was generated where the spanwise extent of the grid was increased by 50%. An LES simulation for the CMC blade with the largest trailing edge thicknesses at the high-freestream turbulence (Tu=13%) condition showed that using such a mesh is necessary for LES to accurately capture the transition phenomena on the suction side. The resulting total pressure coefficient profile and the shift of the wake profile were greatly improved.

CMC↗

The Effect of Trailing Edge Grid Resolution in Large-Eddy Simulations

Ceramic Matrix Composite (CMC) with environmental barrier coating can tolerate significantly higher temperatures compared with the conventional metal alloy blades and thus can help achieve higher thermal efficiency in gas turbine engines. Due to the complex fabrication process of CMC blades, larger blade trailing edge thicknesses and larger leading-edge radii of curvature are expected. These features significantly alter aerodynamic performance especially near the trailing edge and thus the loss profile. In previous studies, the authors used the large eddy simulation (LES) as well as the Reynolds Averaged Navier-Stokes (RANS) coupled with an intermittency function-based transition model to simulate an aerodynamics performance of three different CMC blades and compared the predictions against the data acquired at NASA Glenn Transonic Turbine Blade Cascade Rig. Although we were able to successfully predict different characteristics of aerodynamic performance among three different blades (e.g., pressure loading and integrated losses), LES consistently predicted a small recirculation bubble at the end of the suction side. This was not inconsistent with the physics of the flow, but the pressure loading, locally, near the trailing edge, and as a result, the measured wake profiles did not match the experimental data. To delve further into these issues, a new LES grid with a much finer mesh near the trailing edge was generated where the spanwise extent of the grid was increased by 50%. An LES simulation for the CMC blade with the largest trailing edge thicknesses at the high-freestream turbulence (Tu=13%) condition showed that using such a mesh is necessary for LES to accurately capture the transition phenomena on the suction side. The resulting total pressure coefficient profile and the shift of the wake profile were greatly improved.

LES↗