Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Age”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Simultaneous improvement in strength and ductility in 7xxx Al through a combination of natural aging and deformation

Room temperature processing methods of reaching near-T6 yield and ultimate tensile strength in Al–Zn–Mg–Cu alloys provide a potentially lower cost alternative to high temperature forming and post-forming artificial aging methods. Here, this study demonstrates a method, where a combination of pre-deformation and natural aging matched T6 strength along with ductility and strain hardening greater than the T6 values. Tensile deformation of 5% and 10% was applied to naturally aged samples at 144 h (6 days) and the samples were further naturally aged up to 220 days. The pre-deformed samples showed strong type A Portevin-Le Chatelier (PLC) banding with limited ductility and strain hardenability. Further natural aging increased both strength and ductility simultaneously and converted PLC to type B. This resulted in the same yield strength as T6 temper in the 10% deformed sample but with almost 77% greater total ductility (including the 10% pre-deformation). The simultaneous increase in strength and ductility was attributed to the small, shearable clusters/precipitates and solutes present in the microstructure as suggested by the changes in the PLC behavior.

36 MATERIALS SCIENCE↗

Simulated Aging of Metal Tritides by Ball Milling Induced Gas Incorporation

The study of tritium aging effects on materials requires a significant time commitment as a consequence of its 12.3-year half-life, making developmental studies prohibitively difficult and expensive. However, detailed knowledge of long-term aging effects is critical to the development of structural and storage materials for future fusion reactor technologies. As a result, multiple approaches to simulated aging effects have been investigated. Here, we report a method of simulated tritium aging achieved though the incorporation of trapped gases via high-energy ball milling of LaNi 4.25 Al 0.75 alloy storage material. Experimental results verify the presence of trapped gases by a combination of temperature programmed desorption and LECO chemical analysis. Following gas incorporation, we find that many of the degraded hydrogen sorption properties found in aged storage materials are reproduced by the ball milled powders.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Sequential versus Simultaneous Aging of EPDM Nuclear Cable Insulation Subjected to Elevated Temperature and Gamma Radiation

Electrical cables are integral to power, control, and instrumentation systems within nuclear power plants (NPPs). Exposure of cable systems within nuclear containment to elevated temperatures and gamma radiation during decades-long operation of NPPs can lead to degradation of cable polymeric insulation. Prediction of nuclear cable insulation degradation is complicated as thermal and radiation stress are not additive. In this work, we explore the relative effects of simultaneous and sequential thermal and gamma irradiation on the aging of ethylene-propylene-diene (EPDM) elastomer insulation to better understand realistic scenarios of cable insulation degradation. Cable insulation samples of EPDM were subjected to up to 320 kGy of gamma radiation at a dose rate of 300 Gy/hr in two heating scenarios: (1) simultaneously aged samples were heated at 150°C during irradiation and (2) sequentially aged samples were heated at 150°C for designated durations followed by corresponding periods of irradiation at ambient temperature. The mass, tensile elongation at break, and carbonyl index were assessed to quantify aging of the polymers. The simultaneous aging scenario was found to the more severe of the two for EPDM insulation degradation.

ethylene-propylene-diene elastomer, EPDM, nuclear ↗

Investigating the Crosslinking, Degradation, and Adhesion Behavior of Photovoltaic Encapsulants Under Thermal Accelerated Aging

Degradation of photovoltaic (PV) module encapsulant characteristics that lead to mechanical embrittlement and delamination remains a cause of failure in solar installations. A multiscale reliability model connecting the encapsulant mechanical and fracture properties to the degraded molecular structure and interfacial bonding to adjacent solar cell and glass substrates was previously published. The model, developed primarily for poly(ethylene-co-vinyl acetate) acetate (EVA) encapsulants, remains to be experimentally validated. Determining the degradation and crosslinking kinetics of alternative encapsulants, such as polyolefin elastomer (POE) and EVA/POE/EVA composites (EPE), can generalize the model. In this work, we subject fully cured EVA, POE, and EPE encapsulants to accelerated thermal aging to determine how high temperatures impact reaction kinetics. An increase in gel content (crosslinking) and decrease in crystallinity of the encapsulants under hot-aerobic (90 degrees C, 22% RH) and hot-anaerobic (90 degrees C, sealed in N 2 air) aging were observed, even in the absence of UV and crosslinking initiators. Fourier transform infrared spectroscopy (FTIR)-attenuated total reflectance analysis showed insignificant encapsulant degradation, demonstrating the critical role of UV and moisture in accelerating degradation. Adhesion testing performed on coupon-level specimens (cell/encapsulant/glass laminates) showed decreases in adhesion energy, Gc , from 5000 h of hot-dry (90 degrees C, ~1% RH) and hot-humid (90 degrees C, 60% RH) aging. POE coupons demonstrated the best stability, followed by EPE then EVA. For EVA and POE, hot-humid aged coupons experienced a larger decrease in Gc due to enhanced hydrolytic degradation. Hot-dry aging condition demonstrated that thermal degradation of the interface could be significant even if the encapsulant experiences negligible degradation in the absence of UV and elevated humidity.

accelerated aging↗

Aging phenomena in the two-dimensional complex Ginzburg-Landau equation

The complex Ginzburg-Landau equation with additive noise is a stochastic partial differential equation that describes a remarkably wide range of physical systems which include coupled non-linear oscillators subject to external noise near a Hopf bifurcation instability and spontaneous structure formation in non-equilibrium systems, e.g., in cyclically competing populations or oscillatory chemical reactions. Here, we employ a finite-difference method to numerically solve the noisy complex Ginzburg-Landau equation on a two-dimensional domain with the goal to investigate its non-equilibrium dynamics when the system is quenched into the “defocusing spiral quadrant”. We observe slow coarsening dynamics as oppositely charged topological defects annihilate each other, and characterize the ensuing aging scaling behavior. We conclude that the physical aging features in this system are governed by non-universal aging scaling exponents. We also investigate systems with control parameters residing in the “focusing quadrant”, and identify slow aging kinetics in that regime as well. Finally, we provide heuristic criteria for the existence of slow coarsening dynamics and physical aging behavior in the complex Ginzburg-Landau equation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Key Degradation Products in Nitroplasticizer Thermal Aging

Upon thermal aging, nitroplasticizer (NP) can thermally degrade and release numerous degradation products depending on aging conditions. In this report, we summarize our recent findings, a library of key degradation products in the NP thermal aging is provided. The library contains 25 identified species with their corresponding MS/MS spectrum and intensity profiles, which are derived from our 44-month thermal aging experiment of NP conducted in air, nitrogen, and water at room temperature (RT), 38, 45, 55, and 64°C. To provide a comprehensive yet simplified overview of NP degradation, we summarized the proposed mechanisms of HONO elimination and decomposition, acid generation, PBNA nitrosation and nitration, acid-catalyzed hydrolyses of NP and polynitrated PBNAs, as well as the formation of NP degradants. As the last part of a series of publications and reports on the investigation of NP degradation mechanisms, this work further unfolds complex chemistry that occurs in the entire aging process of NP.

36 MATERIALS SCIENCE↗

Real time lithium metal calendar aging in common battery electrolytes

Li metal anodes are highly sought after for high energy density applications in both primary commercial batteries and next-generation rechargeable batteries. In this research, Li metal electrodes are aged in coin cells for a year with electrolytes relevant to both types of batteries. The aging response is monitored via electrochemical impedance spectroscopy, and Li electrodes are characterized post-mortem. It was found that the carbonate-based electrolytes exhibit the most severe aging effects, despite the use of LiBF 4 -based carbonate electrolytes in Li/CF x Li primary batteries. Highly concentrated LiFSI electrolytes exhibit the most minimal aging effects, with only a small impedance increase with time. This is likely due to the concentrated nature of the electrolyte causing fewer solvent molecules available to react with the electrode surface. LiI-based electrolytes also show improved aging behavior both on their own and as an additive, with a similar impedance response with time as the concentrated LiFSI electrolytes. Since I − is in its most reduced state, it likely prevents further reaction and may help protect the Li electrode surface with a primarily organic solid electrolyte interphase.

25 ENERGY STORAGE↗

Advances in statistical methods for cancer surveillance research: an age-period-cohort perspective

Background: Analysis of Lexis diagrams (population-based cancer incidence and mortality rates indexed by age group and calendar period) requires specialized statistical methods. However, existing methods have limitations that can now be overcome using new approaches. Methods: We assembled a “toolbox” of novel methods to identify trends and patterns by age group, calendar period, and birth cohort. We evaluated operating characteristics across 152 cancer incidence Lexis diagrams compiled from United States (US) Surveillance, Epidemiology and End Results Program data for 21 leading cancers in men and women in four race and ethnicity groups (the “cancer incidence panel”). Results: Nonparametric singular values adaptive kernel filtration (SIFT) decreased the estimated root mean squared error by 90% across the cancer incidence panel. A novel method for semi-parametric age-period-cohort analysis (SAGE) provided optimally smoothed estimates of age-period-cohort (APC) estimable functions and stabilized estimates of lack-of-fit (LOF). SAGE identified statistically significant birth cohort effects across the entire cancer panel; LOF had little impact. As illustrated for colon cancer, newly developed methods for comparative age-period-cohort analysis can elucidate cancer heterogeneity that would otherwise be difficult or impossible to discern using standard methods. Conclusions: Cancer surveillance researchers can now identify fine-scale temporal signals with unprecedented accuracy and elucidate cancer heterogeneity with unprecedented specificity. Birth cohort effects are ubiquitous modulators of cancer incidence in the US. The novel methods described here can advance cancer surveillance research.

60 APPLIED LIFE SCIENCES↗

The Gaia–Kepler Stellar Properties Catalog. II. Planet Radius Demographics as a Function of Stellar Mass and Age

Studies of exoplanet demographics require large samples and precise constraints on exoplanet host stars. Using the homogeneous Kepler stellar properties derived using the Gaia Data Release 2 by Berger et al., we recompute Kepler planet radii and incident fluxes and investigate their distributions with stellar mass and age. We measure the stellar mass dependence of the planet radius valley to be dlogR{sub p}/dlogM{sub ⋆} = 0.26{sub −0.16}{sup +0.21}, consistent with the slope predicted by a planet mass dependence on stellar mass (0.24–0.35) and core-powered mass loss (0.33). We also find the first evidence of a stellar age dependence of the planet populations straddling the radius valley. Specifically, we determine that the fraction of super-Earths (1–1.8 R{sub ⊕}) to sub-Neptunes (1.8–3.5 R{sub ⊕}) increases from 0.61 ± 0.09 at young ages (<1 Gyr) to 1.00 ± 0.10 at old ages (>1 Gyr), consistent with the prediction by core-powered mass loss that the mechanism shaping the radius valley operates over Gyr timescales. Additionally, we find a tentative decrease in the radii of relatively cool (F {sub p} < 150 F{sub ⊕}) sub-Neptunes over Gyr timescales, which suggests that these planets may possess H/He envelopes instead of higher mean molecular weight atmospheres. We confirm the existence of planets within the hot sub-Neptunian “desert” (2.2 R {sub ⊕} < R {sub p} < 3.8 R{sub ⊕}, F {sub p} > 650 F{sub ⊕}) and show that these planets are preferentially orbiting more evolved stars compared to other planets at similar incident fluxes. In addition, we identify candidates for cool (F {sub p} < 20 F{sub ⊕}) inflated Jupiters, present a revised list of habitable zone candidates, and find that the ages of single and multiple transiting planet systems are statistically indistinguishable.

79 ASTRONOMY AND ASTROPHYSICS↗

Three-dimensional Simulations of Massive Stars. II. Age Dependence

We present 3D full star simulations, reaching up to 90% of the total stellar radius, for three 7 M⊙ stars of different ages: zero-age main sequence (ZAMS), mid–main sequence (midMS), and terminal-age main sequence (TAMS). A comparison with several theoretical prescriptions shows that the generation spectra for all three ages are dominated by convective plumes. Two distinct overshooting layers are observed, with most plumes stopped within the layer situated directly above the convective boundary; overshooting to the second, deeper layer becomes progressively more infrequent with increasing stellar age. Internal gravity wave (IGW) propagation is significantly impacted in the midMS and TAMS models as a result of some IGWs getting trapped within their Brunt–Väisälä frequency spikes. A fundamental change in the wave structure across radius is also observed, driven by the effect of density stratification on IGW propagation causing waves to become evanescent within the radiative zone, with older stars being affected more strongly. We find that the steepness of the frequency spectrum at the surface increases from ZAMS to the older models, with older stars also showing more modes in their spectra.

79 ASTRONOMY AND ASTROPHYSICS↗

Accelerated Aging of Fast Pyrolysis Bio-Oils

Carbonyl content is a better metric for tracking aging than viscosity. Existing aging test (24 hours @ 80 °C) is too severe, and correlates to more room temperature aging than would realistically occur. New aging test proposed: 2 hours @ 80 °C correlates to 1-3 months of room temperature storage. Aging is slowed in cold storage, but still occurs.

aging↗

Impact of Synthesis and Aging on Titanium Carbide MXenes for Printed Microsystems

This work investigates the long-term electrical stability of Ti3C2Tx MXene Inks under accelerated aging conditions. Inks were synthesized from commercial MAX-Phase precursors, drop-cast onto custom PCB’s and monitored automated in-situ measurements. Samples aged at 85°C/85% RH, 85°C/0% RH and ambient conditions revealed distinct degradation trends. Wet aged inks showed rapid resistance increased while etched formulations exhibited long term stability. These findings highlight the influence of synthesis stage and environmental exposure on MXene Inks reliability, offering critical insights for printed MEMS and sensor applications. Ongoing measurements extend the aging timeline beyond prior studies, marking the longest evaluation under accelerated aging conditions to date.

Aging↗

Ageing of PBF‐Grade Poly(Phenylene Sulfide) Powder and its Effect on Critical Printability Properties

Abstract Poly(phenylene sulfide) (PPS) is a high‐performance polymer suiting the needs of powder bed fusion (PBF) early‐adopter industries. Although there are many benefits to PBF's powder bed‐based, one drawback is thermal ageing of the powder not incorporated into printed parts. Ideally, unfused powder can be reused in future builds; however, it is unlikely that critical printability properties of the thermally aged powder will remain unchanged. Changes in properties lead to either limited reuse through a practice of mixing used and new powder, or elimination of all powder after each build. In this paper, the authors report effects of thermal ageing in simulated printing conditions on properties of PPS critical to PBF processing. PBF‐grade PPS powder is exposed to process‐mimicking conditions. Properties relevant to the three PBF manufacturing process sub‐functions are assessed for the aged powders. Single‐layer prints are made using aged powder to observe polymer‐PBF interactions ad machina. Significant and systematic deviations from the as‐received state of the powder are observed for thermal and coalescence related properties with increasing exposure time and temperature. These changes are interpreted both in terms of physical and chemical changes in PPS and in terms of how these changes may impact the PBF printing process.

Chatham, Camden A.↗

Solutionization via Severe Plastic Deformation: Effect on Natural Aging in an Al-Mg-Si-(Mn) Alloy

Shear Assisted Processing and Extrusion (ShAPE), a severe plastic deformation technique that is fast and scalable, was used to produce thin-wall tubing from alloy 6082 (Al-0.8Mg-0.9Si-0.7Mn) with in-situ solutionization during processing quickly followed by quenching. Quench medium and input material heat treatment were varied and natural aging behavior (T1 heat treatment) was evaluated using tensile testing. As-cast input material was found to have higher strength early in post-ShAPE natural aging and homogenized input material was found to have strengthening during natural aging. Compared to air quenching, water quenching gave greater strength both early in and after natural aging. These observations along with microscopy suggest that: 1. air quenching was too slow; 2. as-cast material was not fully solutionized but plastic deformation broke up the coarse intermetallic particles, which provided strengthening; and 3. homogenized material was solutionized well, which led to good natural aging behavior.

Milligan, Brian K.↗

Formation of the {gamma}ʹʹʹ-Ni2(Cr, Mo, W) phase during a two-step aging heat treatment in HAYNES® 244® Alloy

Precipitation hardening is the dominant method of achieving high strength in most Ni-based superalloys. The formation of nanoscale precipitates during thermal exposure is often studied to determine the optimal methods of attaining high strength. The commercial Ni-based superalloy, HAYNES® 244® alloy, is strengthened through a novel -Ni2(Cr, Mo, W) intermetallic phase that forms during a two-step aging cycle. The precipitation kinetics of this intermetallic phase are sluggish for single-step aging in comparison to the γʹ phase in precipitation-strengthened Ni-based alloys, but a two-step aging treatment has shown to reliably harden the alloy and improve high-temperature properties compared to a single-step aging heat treatment. To investigate the formation and coarsening of this phase, heat-treated samples of the 244 alloy were analyzed with high-energy in situ and ex situ X-ray techniques such as small angle X-ray scattering and wide angle X-ray scattering as well as Vickers micro-hardness, electron microscopy, and atom probe tomography. The relationship between hardness, aging parameters, and microstructure evolution is discussed. The enthalpy of formation and precipitate solvus temperature were determined with high-temperature differential scanning calorimetry and dilatometry analysis.

Ni-based Superalloys↗

Effects of volitional emigration timing and smolt size on survival and age-at-return in a Pacific salmon hatchery population

Abstract Many Pacific salmon populations are returning from sea at younger ages and smaller sizes. Hatchery culture, management practices, and environmental factors influence juvenile release size and emigration timing, which in turn affect important demographic characteristics in returning adults. We analyzed data from approximately 345,000 tagged spring Chinook Salmon juveniles exiting Cle Elum Supplementation and Research Facility (Yakima River, Washington, USA) acclimation sites over thirteen brood years (2002–2014), evaluating smolt size, emigration timing, river flow, juvenile survival, and age-at-return. We observed a relationship between size and volitional exit timing of smolts from acclimation sites, with larger fish tending to emigrate earlier than smaller fish. Early emigration was also coincident with lower river flows near acclimation sites. Later emigration timing was correlated with an increase in apparent survival of juveniles to Bonneville Dam (500–530 km downstream of acclimation sites), but also with a lower rate of survival to return from sea. In general, for juveniles successfully emigrating downstream of Bonneville Dam, age-at-return increased with decreasing juvenile fish size and later emigration timing. Our results support a growing body of evidence that hatchery practices may result in larger smolts that tend to return at younger ages. Given the biological and economic consequences of younger age-at-maturation, methods to reverse this trend should be further explored and implemented.

Bosch, William J. (ORCID:0000000300447390)↗

Formation, cooling history and age of impact events on the IIE iron parent body: Evidence from the Miles meteorite

Most iron meteorites formed in planetary cores during differentiation, but the IIE iron meteorites have chemical and physical features that are inconsistent with this origin. By combining mineral chemistry, mineral modes and three-dimensional petrography, we reconstruct the bulk chemistry of the felsic silicate-bearing Miles IIE iron meteorite and demonstrate that the silicate inclusion compositions are similar to partial melts produced experimentally from an H chondrite composition. We use the reconstructed bulk composition, mineralogy and thermodynamic modelling to show that melting above ~ 1200°C under reducing conditions formed metal (Fe-Ni alloy) and felsic silicate partial melts. Upon cooling, the melts crystallized Mg-rich pyroxenes, Na- and K-rich feldspars, and tridymite. Importantly, this mechanism enriches cosmochemically volatile elements (i.e., those with a 50% condensation temperature of ~430–830°C, like Na and K) to the level found in the felsic silicate inclusions. The presence of crystallographically disordered srilankite (only stable above 1160°C) and an absence of Widmanstätten texture require both high peak temperatures and rapid cooling, which cannot be explained by core formation. Instead, they point to small melt volumes, a transient heat pulse, and small thermal mass, and imply efficient physical segregation of silicate and metallic melts through buoyancy separation followed by rapid cooling that arrested the separation of metal and silicate liquid phases. In situ 207 Pb/ 206 Pb age of 4542.3 ± 4.0 Ma in Zr-oxide and phosphate minerals dates the melting event that formed the silicate inclusions. This age aligns with the earliest ages found in other IIE iron meteorite silicates and requires a heating event ~25 million years after the solar system formed. We found 39 Ar/ 40 Ar ages of 3495 ± 52 Ma (low-T) and 4303 ± 7 Ma (high-T) in a K-feldspar grain, with the 3495 Ma age aligning with later thermal events recorded in other IIE iron meteorites. Dating reveals the complex petrogenetic and thermal history of Miles and the IIE iron meteorites. This is the first IIE iron meteorite found to record evidence of heating at 4.5 and 3.5 Ga likely from impact events. We propose that high-velocity impact(s) into an iron-rich, porous chondritic parent body at ~4.54 Ga produced immiscible metal and silicate melts that cooled rapidly and trapped low density silicate inclusions within high density metal. Other IIE irons that formed at lower peak temperatures (900–1000°C) contain chondritic silicate inclusions and relict chondrules, supporting this conceptual model. In conclusion, this petrogenesis is consistent with thermodynamic modelling, experimental data and the wide range of peak temperatures and cooling rates observed in the IIE iron meteorites.

58 GEOSCIENCES↗

Impact of zero valent iron aging on reductive removal of technetium-99

Zero valent iron (ZVI) is a promising material for reductive removal of technetium from industrial waste streams. An example application of this method could be to treatment of low activity aqueous waste that is currently stored in tanks at the Hanford site. However, there is still a lack of understanding of the useful lifetime of ZVI for treatment and the changes in reductive removal of Tc over time. In this research, we studied the reductive removal of Tc from aqueous solutions by ZVI aged with up to 30 days by contact with 0.08 M NaCl solutions. These results show that ZVI could be used to remove Tc(VII) from aqueous solutions by its reduction to the less soluble and relatively immobile Tc(IV) with greater than 99% removal in three hours. Still, greater than 90% of Tc is removed with ZVI aging up to one week. However, after 10 days of aging of zero valent iron, a significant decrease in removal of Tc occurs (55% removal at three hours) followed by negligible removal after aging for two weeks or more which is consistent with formation of iron oxides on the surface. Further, these results correlate with XRD and FTIR analysis showing an increase in magnetite followed by maghemite and goethite with aging time.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗