Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ATOMIC DISPLACEMENTS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 199 records · Page 11

Mechanical behavior of additively manufactured and wrought 316L stainless steels before and after neutron irradiation

Fabrication of nuclear reactor components using additive manufacturing (AM) methods is now a practical option since the AM technologies have advanced to allow for building of complex parts with high quality materials. To assess the mechanical performance of printed components in reactor-relevant conditions and to build a property database for the AM 316L stainless steel (SS), mechanical testing and characterization were performed before and after neutron irradiation. In this work, miniature tensile specimens were irradiated at the High Flux Isotope Reactor (HFIR) to 0.2 and 2 displacements per atom (dpa) at 300 and 600°C. The AM 316L SS was tested in the as-built, stress-relieved, and solution-annealed conditions, and the wrought (WT) 316L SS in solution-annealed condition as a reference alloy. The baseline test result showed that the AM 316L SS, regardless of the post-build heat treatment, had higher strength than the WT 316L SS, but similar ductility. Post-irradiation tensile testing was conducted at RT, 300°C, and 500°C for selected irradiation conditions. Neutron irradiation induced significant changes in the mechanical behavior of the AM stainless steels, including both hardening and softening. Although the as-built 316L steel after 300°C irradiation showed necking just after yielding, the overall property changes of the as-printed alloy became less significant after 600°C irradiation. Irradiation-induced ductilization was also observed after the higher temperature irradiation. In general, the strength change was smaller in the relatively stronger as-built and stress-relieved AM SSs than in the solution-annealed AM and WT SSs. These relatively lower strength 316L SSs overall retained higher ductility in the irradiation conditions tested, but the stronger 316L SSs demonstrated a similar level of ductility after the higher temperature (600°C) irradiation. It is a positive assessment for the AM 316L materials that no embrittlement was observed within the test and irradiation conditions of the experiment.

36 MATERIALS SCIENCE↗

Investigation of hardening mechanisms and size effects in proton-irradiated HT-9 steels

Ferritic/martensitic steels, such as HT-9, are known for their complex microstructural features and mechanical properties. Here in this paper, in-situ micro-tensile tests and traditional fractography methods were utilized to study the fracture behavior of proton-irradiated HT-9 steels. First, to evaluate the viability of micro-tensile tests for nuclear material qualification process, meso-tensile tests on as-received HT-9 steels were performed. Fracture mechanisms of unirradiated HT-9 steels at both length scales were compared and underlying mechanisms discussed. The direct comparison of micro- and meso-scale data shows a distinctive size effect demonstrated by the increase in yield stress (YS). Upon completion of initial assessment, specimens were irradiated with 4 MeV + protons to three fluences, all of which were lower than 0.01 displacements per atom (dpa). As expected, the YS increases with irradiation. However, at 7 × 10 -3 dpa, the reversal of the trend was observed, and the YS exhibited sharp decline. We demonstrate that at lower length scales, grain structure has a more profound impact on the mechanical properties of irradiated materials, which provides information needed to fill in the gap in current understanding of the HT-9 fracture at different length scales.

36 MATERIALS SCIENCE↗

Molecular dynamics simulations of radiation cascade evolution near cellular dislocation structures in additively manufactured stainless steels

The dislocation dense cellular structures observed in additively manufactured (AM) stainless steels can allow these materials to have enhanced strength and ductility compared to conventionally manufactured materials. Effective design of radiation resistant materials often necessitates creating microstructures containing of a high density of dislocations that act as sinks for radiation induced defects. This work uses molecular dynamics simulations to study the impact of pre-existing defects on radiation damage in stainless steel 316L fabricated by the laser powder bed fusion process. The evolution of synthetically generated dislocations in a crystal system in response to multiple radiation collision cascades suggest that dislocation dense regions reduce the probability of surviving point defects forming clusters. This finding seems to result from the dislocation cores’ ability to absorb point defects, thereby limiting the formation of clusters during the recombination phase. However, after successive cascades, the ability of the dislocation entanglement to prevent defect formation is diminished and defect cluster formation trends to an equilibrium. Accordingly, it is hypothesized that in an experimental setting the dislocation cells will initially act as neutral sinks for point defects, potentially delaying the onset of radiation damage effects; but, these structures will be degraded due to radiation-enhanced diffusion and lose their effectiveness at doses above 1.5–2 displacements per atom. Nevertheless, the ability to produce complex and feature-specific microstructures suggests promise for the design of radiation tolerant materials using AM methods.

36 MATERIALS SCIENCE↗

Neutron irradiation induced defects and clustering in NF616 and T91

NF616 is a third-generation ferritic martensitic steel, developed to have better creep resistance than the prior generation T91. Unlike relatively numerous studies of T91, there is a lack of understanding of the irradiation effect on the microstructural evolution and mechanical response of NF616. This work evaluated the microstructures and radiation hardening of NF616 irradiated up to 8.2 displacement per atom (dpa) at 292 °C – 431 °C, compared with T91 from two heats. Dislocation loops were observed in all investigated samples. NF616 exhibited comparable loop size but slightly lower loop density than those in the general T91 heat at 430 °C. Cavities were only observed in NF616 at 431 °C but absent at lower irradiation temperatures (292 °C and 359 °C). Ni-rich clusters were also observed in NF616 at 431 °C, while only weak Ni-clustering were observed at lower irradiation temperatures. Compared to the general T91 heat, NF616 demonstrated better swelling resistance (e.g., one third of swelling in the general T91 heat at 430 °C), a slightly higher number density of Ni-rich clusters, and slightly lower radiation hardening. The low-carbon T91 showed the greatest hardening with the largest swelling and loop sizes, despite its lowest irradiation temperature and intermediate dose. The calculated hardening from loops, cavities and Ni-rich clusters using the classic dispersed barrier-hardening model had reasonable agreement with the experiment-derived results, with the primary hardening contribution attributed to dislocation loops.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of high thermal conductivity fuel surrogates before and after ion irradiation

High thermal conductivity nuclear fuels offer important potential advantages over traditional oxide-based fuels such as higher burnup, reduction in fission gas release, and better overall safety of the system. One proposed approach to high thermal conductivity fuels utilizes high thermal conductivity nonfissile additives with UO 2 fuel to lower the fuel operating temperature and thereby take advantage of the highly favorable radiation resistance of UO 2 at lower operating temperatures. However, differential swelling in the matrix and high conductivity additive phases during high dose irradiation could lead to internal cracking and poor performance. In the current study, ceria (CeO 2 ) and zirconia (ZrO 2 ) surrogate matrices were used to model UO2 behavior. Additives of 10 vol. % Al 2 O 3 or SiC in the form of short fibers or platelets were used for the high conductivity second phase. The nuclear fuel surrogates were sintered to achieve densities greater than 93% of the ideal values. Scanning electron microscopy (SEM) imaging and X-ray diffraction confirmed the uniform distribution of the second phase and that no intermetallic second phase was formed during sintering. The thermal conductivity of the sintered samples was measured from 50 °C to 900 °C and confirmed the desirable increase compared to pure CeO 2 /ZrO 2 pellets. Samples were irradiated with 20 MeV Ni 6+ ions at midrange doses ranging from 1 to 15 displacements per atom (dpa) and temperatures from 300 °C to 700 °C. Post irradiation characterization revealed a good stability of the samples at low to medium doses with matrix lattice parameter swelling of < 0.14 % but showed a significant microstructural deterioration and decrease of the mechanical properties at 15 dpa.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Helium causing disappearance of a/2<111> dislocation loops in binary Fe-Cr ferritic alloys

In this work, single and dual-beam self-ion irradiations were performed at 500°C on ultra-high purity Fe14%Cr alloy to ~0.33 displacements-per-atom (dpa), and 0 or 3030 atomic-parts-per-million (appm) helium/dpa, respectively. Using transmission electron microscopy, we reveal that helium can drastically modify the dislocation loop Burgers vector in Fe-Cr alloys. Helium co-implantation caused complete disappearance of a/2<111> type dislocation loops, and the microstructure consisted of only a<100> loops. Conversely, a/2<111> type loops were predominant without He co-implantation. The total loop density remained largely unaffected. The results strikingly contrast literature asserting that helium stabilizes a/2<111> type loops in bcc Fe alloys, based on low temperature irradiations. Collectively analyzing the results with literature suggest that the small positive interaction between helium and self-interstitial atoms (SIA) in Fe predicted by atomistic simulations maybe insufficient to holistically explain the dislocation loop microstructure development in presence of helium. Helium-SIA positive binding inadvertently implies elevated a/2<111> loop fraction and higher loop densities that the present results contradict. Helium induced high cavity density causing a preferential loss of highly glissile <111> clusters, leaving the matrix saturated with <100> type clusters is proposed as a potential mechanism. Further, the in-situ irradiations combined with Burgers vector analysis strengthened the evidence of Cr-induced dislocation loop mobility reduction that appears to stabilize the a/2<111> type loops and causes higher loop densities in Fe-Cr alloys.

36 MATERIALS SCIENCE↗

Optical transmission and dimensional stability of single-crystal sapphire after high-dose neutron irradiation at various temperatures up to 688 °C

The use of single-crystal sapphire optical fibers has been considered to extend fiber-optic sensing to the extreme temperature (>1000 °C) environments encountered in nuclear applications. However, before these sapphire fiber–based sensors can be deployed, their optical transmission and dimensional stability (which impacts drift of some sensors) must be characterized under representative testing conditions. Data regarding the optical transmission of sapphire following high-dose neutron irradiation at temperatures >100 °C is extremely limited. This work provides measurements of optical density (i.e., attenuation) and directional dimensional changes in bulk single-crystal sapphire materials irradiated to a fast neutron fluence of 2.4 × 10 21 n/cm 2 (3.5 displacements per atom) at temperatures ranging from 95 to 688 °C. Optical density measured after irradiation at 95 and 298 °C showed ultraviolet and visible absorption bands corresponding to known defect centers and temperature trends that were generally consistent with previous ex situ and in situ measurements made at much lower neutron fluence. However, optical density measured after irradiation at 688 °C was as much as two orders of magnitude higher, indicating that the fundamental mechanism for radiation-induced attenuation changes at this irradiation temperature. Additional analysis and comparison with previous works suggest that the attenuation may result from void formation, leading to increased Rayleigh scattering losses in the material and increased swelling that would also result in drift of Bragg grating-based sensors in sapphire fibers. These results pose serious questions regarding the feasibility of sapphire fiber–based sensors for high-temperature nuclear applications.

36 MATERIALS SCIENCE↗

Void swelling of conventional and composition engineered HT9 alloys after high-dose self-ion irradiation

Ferritic/martensitic (F/M) steels are being considered as potential structural materials for next generation nuclear reactors, and variants of the alloy HT9 are some of the most promising candidates. In this study, two conventional and two composition engineered HT9 alloys were irradiated using 3.5 MeV Fe 2+ up to 600 peak displacement-per-atom (dpa) at 450 °C. Void swelling and microstructure evolution were characterized for each alloy and compared. The two conventional HT9 alloys (INL and ACO3) showed similar void swelling behavior due to their similar elemental composition and processing conditions. The INL HT9 exhibited a maximum of 2.4% swelling and the ACO3 HT9 showed a maximum of 2.8% swelling at 342 and 393 average local dpa, respectively. On the other hand, the two-composition engineered HT9 alloys with varying N contents (10 ppm for low N and 440 ppm for high N) showed disparate swelling behavior. The low N HT9 exhibited a maximum of 4.6% swelling, while the high N HT9 showed a maximum of 0.7% swelling at 342 average local dpa. Changes in the N content also affected Ni/Si rich G-phase formation. The low N HT9 showed a larger size and lower density of G-phase precipitates compared with the high N HT9 after 600 peak dpa irradiation. This study compares the void swelling behavior of the ion irradiated four current HT9 alloys to extremely high doses, with the void swelling data from neutron irradiated HT9 alloys. Furthermore, the comparison lends critical insights into how well these current alloys can withstand high neutron fluxes in future reactors, especially since the low N and high N HT9 alloys have never been exposed to such high doses before.

36 MATERIALS SCIENCE↗

Radiation induced amorphization of carbides in additively manufactured and conventional ferritic-martensitic steels: In-situ experiments on extraction replicas

In-situ irradiations using 1 MeV Kr 2+ ions in a transmission electron microscope were performed on extraction replica samples containing M 23 C 6 carbides and MX carbonitrides from two ferritic-martensitic (FM) steels: (i) 9%Cr-1%W-TaV based Eurofer97 and (ii) 9%Cr-1%Mo-VNb (all in wt.%) based additively manufactured (AM) Grade91 steel. The irradiations were performed between 100 and 773 K up to a maximum dose of ~2.4 displacements per atom (dpa). The M 23 C 6 carbides are highly susceptible to radiation induced amorphization (RIA), while the MX type nanoprecipitates are highly amorphization resistant across the entire irradiation temperature range. Between 100 and 423 K, RIA of M 23 C 6 carbides occurs very rapidly with critical amorphization doses ranging between ~0.35 and 0.9 dpa, increasing to higher doses at 573 K. Complete amorphization of the M 23 C 6 carbides up to doses of ~2.4 dpa is not possible at 773 K under the present irradiation conditions. The critical amorphization dose of M 23 C 6 carbides increases nearly exponentially with irradiation temperature. The critical temperature for the crystalline-to-amorphous phase transformation (T c→a ) of M 23 C 6 carbides irradiated as replica samples, i.e. without the surrounding metal matrix, was estimated to be ~812 K. Comparing the present results with neutron irradiation data on bulk samples reveals a decrease in the critical amorphization dose for M 23 C 6 and an increase of T c→a , highlighting the effect of dose rate on the amorphization behavior that is qualitatively consistent with literature on other non-metals. Changes in the minor chemistry of M 23 C 6 , such as presence or absence of W, V, Nb, Mo, seems to have little effect on the amorphization behavior. Here, in-situ irradiations on extraction replica samples provide a novel pathway to explore radiation tolerance of nanoprecipitates in nuclear structural materials

36 MATERIALS SCIENCE↗

The effect of helium on cavity swelling in dual-ion irradiated Fe and Fe-10Cr ferritic alloys

We report Ferritic-martensitic (FM) steels for in-vessel components in proposed fusion reactors are expected to suffer from high levels of displacement damage and helium (He) generation by neutron transmutation. However, a thorough understanding of the He synergistic effects on the cavity swelling in FM steels is still not well established. To gain fundamental insights into the He effect on cavity swelling, high purity Fe and Fe-10 wt.% Cr ferritic model alloys were irradiated with 8 MeV Ni ions and co-implanted He ions at 400 to 550 °C up to 30 displacements per atom (dpa) with He implantation rates of 0.1, 10 and 50 appm He/dpa. The current study focuses on the 50 appm He/dpa, 500 °C behavior vs. 0.1 and 10 appm He/dpa. Irradiation-induced defects, including cavities, dislocation loops, and dislocation networks were characterized using transmission electron microscopy (TEM). In the grain interior, a bimodal cavity size distribution was observed in the 10 and 50 appm He/dpa samples, but not for 0.1 appm He/dpa. Cavity swelling was maximized at intermediate He implantation rates of ~10 appm He/dpa for both ion-irradiated Fe and Fe-10Cr alloys. The cavity swelling behavior as a function of He implantation rate appears to be controlled by the He/dpa-dependent variation of cavity sink strengths. Treating small bubbles as biased sinks for interstitial absorption can significantly increase the ratio of biased to unbiased sink strengths (Q) and results in maximized cavity swelling for a Q ratio close to one.

36 MATERIALS SCIENCE↗

A fusion relevant data-driven engineering void swelling model for 9Cr tempered martensitic steels

The UCSB database on cavity evolution in 9-12Cr tempered martensitic steels (TMS), includes the results for both dual heavy and helium ion (DII), and High Flux Isotope Reactor (HFIR) in situ helium injection (ISHI) neutron irradiations at 500°C. These results were combined with literature single ion and fission neutron irradiation data to derive a model for the void volume fraction, f v , as a function of displacements per atom (dpa) and transmutant helium concentrations in atomic parts per million (appm). The scientific foundation for the paper is described in a companion paper entitled “Cavity Evolution and Void Swelling in Dual Ion Irradiated Tempered Martensitic Steels”. Here, in this study, we show that f v (dpa, He/dpa) is described by the incubation dose, dpa i , for the onset of void growth, and the post-incubation growth rate, f v ’(%/dpa). Both dpa i and f v ’ decrease with increasing He/dpa at > ~ 5. The dpa i is also lower for the ISHI neutron irradiations at the same He/dpa. Single heavy ion and fission reactor neutron irradiations, with low He/dpa ratios, have a much larger dpa i . Based on a combined analysis of DII, single ion, ISHI and fission neutron data, we further show that the post-incubation f v data analyzed here have a common empirical curve shape, with f v ’ reaching up to ~ 0.2%/dpa at very high dpa. We also show that f v ’ can be predicted based on a physical model of defect partitioning between evolving sinks. At 500°C and fusion relevant He/dpa ≈ 10, the best-fit model predicts nominal swelling, S = f v /(1-f v ), of ~ 1.1, 4.9 and 16% at 50, 100 and 200 dpa, respectively. The physically motivated, data-driven model includes estimated uncertainties for both dpa i and f v ’.

36 MATERIALS SCIENCE↗

Heavy ion irradiation effects on CrFeMnNi and AlCrFeMnNi high entropy alloys

Co-free but Al-included medium/high entropy alloys (M/HEAs) have gained increasing interests due to their lower cost and the potential to tune the multi-phase microstructure. The irradiation response of two Co-free HEAs, face-centered cubic (FCC) CrFeMnNi with limited Cr enriched α' phase and body-centered cubic (BCC) AlCrFeMnNi with B2s phase and nanoprecipitates were explored. Ion irradiations using 5 MeV Fe 2+ ions were performed at 500°C to a peak fluence of 50 and/or 100 displacements per atom (dpa). In dual-phase AlCrFeMnNi, there was no significant radiation induced segregation or chemical intermixing at the coherent matrix (FeCrMn-rich)/second phase (AlNi-rich) boundaries. In CrFeMnNi, limited voids were only detected at the peak damage location of ~ 50 dpa. On the other hand, voids were widely distributed in AlCrFeMnNi: under 50 and 100 dpa irradiation conditions, voids were found with larger dimension and denser distribution in the FeCrMn-rich matrix, smaller and slightly lower density in an AlNi-rich second phase. In addition, the diameter of the FeCMn-rich nanoprecipitates didn't reveal any tendency of dissolution or growth. This is correlated with their superior structural stability against irradiation. Significant radiation-induced hardening (increases from 3.8 ± 0.2 GPa to 4.7 ± 0.6 GPa) was measured in CrFeMnNi, but only ~ 4% hardness increase (from 7.4 ± 0.8 GPa to 7.7 ± 0.4 GPa) was noted in AlCrFeMnNi. Finally, in addition to the radiation-induced defects, such as voids, dislocation loops and point defects, other factors, such as chemical short-range ordering may play an important role.

36 MATERIALS SCIENCE↗

Cavity evolution and void swelling in dual ion irradiated tempered martensitic steels

Microstructural evolutions in two variants of the F82H 8 wt%Cr tempered martensitic steel under dual (He + plus Fe 3+ ) ion irradiations at 500 °C have been characterized by transmission electron microscopy. Emphasis is on understanding the combined effects of displacements per atom (dpa) and the helium/dpa ratio (He/dpa) on cavity evolution and void swelling (f v ). The dual ion database includes 231 alloy-dpa-He/dpa conditions for irradiations up to ~ 82 dpa and 3700 appm helium. Here, we hypothesize that the large “scatter” observed in the f v data is primarily due to local microstructural variations, especially those that shield regions at shallower depths from the effects of injected interstitial atoms, which would otherwise reduce f v . More generally, our hypothesis is that the highest f v data, at a specified dpa and He/dpa, provides the most appropriate estimate of swelling for fusion neutron irradiation conditions. The dose dependence of f v can be described by an incubation dpa i , marking the onset of significant void growth, and a post-incubation swelling rate, f v ’ = Δf v /Δdpa. Both dpa i and f v ’ decrease with increasing He/dpa. The f v ’ data are quantitatively consistent with a simple model for defect partitioning between evolving bubble, void, and dislocation sinks strengths and biases. Most notably, the model correctly predicts both the incubation dpa i , and the subsequent f v ’, in spite of the fact that they reflect somewhat different physics. Our analysis also suggests that defect recombination is modest at 500 °C. Along with other considerations, this supports the hypothesis that, even at high dpa rates, dual ion irradiations can be used to reasonably emulate void nucleation and growth for a range of fusion-relevant neutron irradiation service conditions. A companion paper incorporates the results of this study in a reduced-order, data-driven void swelling model.

36 MATERIALS SCIENCE↗

Irradiation Effects on Stability of δ-UZr2 phase in U-50 wt% Zr Alloy

U-50wt%Zr is a candidate metallic nuclear fuel with potential application in light water reactors due to its excellent thermal properties and high radiation tolerance. The Zr-rich UZr fuels possess greater swelling resistance and fission gas release characteristics compared with U-rich UZr fuels. In this current study, the δ-phase U-50wt%Zr is proton irradiated at room temperature to 1 displacement per atom (dpa) to provide insights on phase stability under irradiation conditions. High resolution characterization of Transmission Electron Microscopy (TEM) and Atom Probe Tomography (APT) characterization techniques are used to elucidate microstructural changes due to irradiation. TEM and APT results show highly oriented bcc β-Zr-rich platelet precipitates nucleating adjacent to α-U phases inside the UZr 2 matrix. Formation of this platelet morphology is characteristic of Widmänstatten structure which can be attributed to a variety of factors such as differences in thermal expansion coefficient between the phases, grain size, alloy composition, and cooling rate. The phases present are distinctly different than those observed through in situ annealing, but irradiation accelerates diffusion and phase separation kinetics. These microstructural changes in U-50wt%Zr are different from those achieved by pure thermodynamic or high temperature heavy ion irradiation experiments. Finally, our work, together with previous ones, highlight the necessity to study the U-Zr phase diagram under non-equilibrium thermodynamics conditions to support this material's deployment as a viable nuclear fuel form.

36 MATERIALS SCIENCE↗

Irradiation-assisted cracking of SA508-304L weldments with 308L groove filler and 309L butter in hot water immersion constant rate extension tests

Low alloy SA508 bainitic steel is often welded to 300 series austenitic stainless steel in nuclear power plants. These dissimilar metal weldments use 309L butter applied to the low alloy steel and 308L groove filler material to join the 309L to austenite. High alloy steels (such as the 308L and 309L material used here) have been identified as having greater susceptibility to irradiation-assisted stress corrosion cracking (IASCC). Evidence is presented here of cracking under tensile loads in 309L weldment butter in LWR hydrothermal conditions that correlates irradiation induced changes at δ ferrite–γ austenite phase boundaries and γ–γ grain boundaries; specifically intergranular Cr 23 C 6 precipitates. Cracking is not observed in irradiated 308L groove filler under the same conditions. Both the 309L butter and 308L filler material have a duplex or mixed δ–γ phase microstructure due to solidification during the welding procedure. We have performed constant extension rate autoclave immersion tests in BWR normal water chemistry hot water (288 °C, 10 MPa, 2000 wt. ppb dissolved oxygen, <100 nS/cm conductivity, neutral pH) of proton irradiated (2 MeV, approximately 3 displacements per atom at a depth of 10 μm) tensile specimens. Proton irradiation to the dpa levels used here induced Cr 23 C 6 carbide precipitation at γ–γ grain boundaries and δ–γ phase boundaries in the 309L butter but not the 308L filler. Cracking was observed in the proton-irradiated volume of 309L at these interfaces in the vicinity of the Cr 23 C 6 precipitates. We hypothesis the SA508 is the source of carbon in the 309L butter. Cr depletion at γ–γ grain boundaries was also observed and may also be a root cause of cracking. Furthermore, the 309L butter is under significant tensile residual stress in the weldment that adds to applied tensile loads and this too may be a contributing factor.

309L weld butter↗

Hermeticity of SiC/SiC composite and monolithic SiC tubes irradiated under radial high-heat flux

Demonstration of hermetic SiC fiber–reinforced SiC matrix composite cladding under normal operating environments has been identified as one of the most critical feasibility issues for accident-tolerant fuel cladding in light-water reactors. This study provides critical experimental data needed for understanding the effects of irradiation on hermeticity. SiC composite and monolithic tubes were neutron-irradiated to 2 displacements per atom with and without a nominal radial heat flux of 0.6 MW/m2 to produce a simulated in-pile stress state for the normal operation of a light-water reactor. The through-thickness temperature gradient under irradiation results in a gradient in swelling, which causes a significant stress buildup. Such irradiation-induced stress was modeled using a commercial finite element analysis code. The radial heat flux–irradiation synergism was experimentally investigated by constructing a special irradiation capsule and evaluating the helium hermeticity of the specimens. The simulated stress state exhibited a near equi-biaxial tensile axial and hoop stress of ~150 MPa at the inner surface of the SiC composite tube. This stress level is potentially beyond the matrix cracking stress. Degradation of hermeticity of the SiC composite tubes was observed after irradiation, indicating irradiation-induced cracking, whereas the irradiated monolithic SiC tubes remained hermetic. In conclusion, the results indicate that loss of hermeticity caused by radiation-induced microcracking is a potential issue for SiC composite cladding, depending on the magnitude of the temperature gradients. Coating the outer surface of the cladding was identified as a mitigation strategy that might overcome the cracking issue.

36 MATERIALS SCIENCE↗

Microstructural evolution of compositionally complex solid-solution alloys under in-situ dual-beam irradiation

Here, this work attempts to link the microstructural evolution of single-phase compositionally complex alloy (CCA) compositions under dual-beam irradiation to their Mn-content via the stacking-fault energy (SFE) and vacancy migration energies. Two alloys, Cr 18 Fe 27 Mn 27 Ni 28 and Cr 15 Fe 35 Mn 15 Ni 35 , along with less compositionally complex pure Ni and Fe 56 Ni 44 binary were irradiated at 500 and 600 °C under dual-beam 1 MeV Kr 2+ and 16 keV He + heavy-ions up to 7 displacements per atom (dpa) with a He/dpa ratio of 0.75 %/dpa using in situ transmission electron microscopy (TEM). Due to the bubble-stabilizing effect of implanted He, bubbles were observed in all irradiations, and populations of faulted interstitial loops were characterized in Cr 18 Fe 27 Mn 27 Ni 28 and Cr 15 Fe 35 Mn 15 Ni 35 . A reduction in swelling was observed in the two CCAs compared to pure Ni and Fe 56 Ni 44 . Although swelling increased from 500 to 600 °C in Fe 56 Ni 44 , Cr 15 Fe 35 Mn 15 Ni 35 and Cr 18 Fe 27 Mn 27 Ni 28 both swelled slightly more at 500 °C. This was attributed to the difference in vacancy mobility, stronger pinning effect of vacancies on He, and the sink strength of faulted dislocation loops. Faulted interstitial loops nucleated with a higher number density and dislocation line density in Cr 15 Fe 35 Mn 15 Ni 35 at both temperatures, and at 600 °C in both materials. The differences in faulted loop population and temperature effect on swelling are correlated to the Mn-content and the measured SFE (20.2 ± 6.7 mJ/m 2 for Cr 18 Fe 27 Mn 27 Ni 28 and 9.2 ± 3.4 mJ/m 2 for Cr 15 Fe 35 Mn 15 Ni 35 ).

36 MATERIALS SCIENCE↗

Deformation localisation in ion-irradiated Fe and Fe10Cr

Determining the mechanisms for irradiation-induced ductility loss is crucial for the design of reactor structural components. Here, the deformation characteristics around nanoindents in Fe and Fe10Cr irradiated with Fe ions to ~1 displacement-per-atom at 313 K are non-destructively studied. Slip steps surrounding the nanoindents indicate that deformation is localised in the irradiated materials. Lattice rotation and strain fields near the indent site show over 87% confinement of plasticity in the irradiated material. Cr has little effect on the irradiation-induced changes in pile-up topography and deformation fields, suggesting it has limited impact on retaining strain hardening capacity and reducing irradiation-induced embrittlement.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗