Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “fracturing materials”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,801 records · Page 100

Basic failure mechanisms in advanced composites

Failure mechanisms in carbon-epoxy composites are identified as a basis for more reliable prediction of the performance of these materials. The approach involves both the study of local fracture events in model specimens containing small groups of filaments and fractographic examination of high fiber content engineering composites. Emphasis is placed on the correlation of model specimen observations with gross fracture modes. The effects of fiber surface treatment, resin modification and fiber content are studied and acoustic emission methods are applied. Some effort is devoted to analysis of the failure process in composite/metal specimens.

Mullin, J. V.↗

Factors affecting the thermal shock resistance of several hafnia based composites containing graphite or tungsten

The thermal shock resistance of hafnia based composites containing graphite powder or tungsten fibers was investigated in terms of material properties which include thermal expansion, thermal conductivity, compressive fracture stress, modulus of elasticity, and phase stability in terms of the processing parameters of hot pressing pressure and/or density, degree of stabilization of the hafnia, and composition. All other parameters were held constant or assumed constant. The thermal shock resistance was directly proportional to the compressive fracture stress to modulus of elasticity ratio and was not affected appreciably by the small thermal expansion or thermal conductivity changes. This ratio was found to vary strongly with the composition and density such that the composites containing graphite had relatively poor thermal shock resistance, while the composites containing tungsten had superior thermal shock resistance.

Lineback, L. D.↗

Kinetic studies of the stress corrosion cracking of D6AC steel

The effect of load interactions on the crack growth velocity of D6AC steel under stress corrosion cracking conditions was determined. The environment was a 3.5 percent salt solution. The modified-wedge opening load specimens were fatigue precracked and subjected to a deadweight loading in creep machines. The effects of load shedding on incubation times and crack growth rates were measured using high-sensitivity compliance measurement techniques. Load shedding results in an incubation time, the length of which depends on the amount of load shed and the baseline stress intensity. The sequence of unloading the specimen also controls the subsequent incubation period. The incubation period is shorter when load shedding passes through zero load than when it does not if the specimen initially had the same baseline stress intensity. The crack growth rates following the incubation period are also different from the steady-state crack growth rate at the operating stress intensity. These data show that the susceptibility of this alloy system to stress corrosion cracking depends on the plane-strain fracture toughness and on the yield strength of the material.

Noronha, P. J.↗

Automated predesign of aircraft

Program uses multistation structural-synthesis to size and design box-beam structures for transport aircraft. Program optimizes static strength and scales up to satisfy fatigue and fracture criteria. It has multimaterial capability and library of materials properties, including advanced composites. Program can be used to evaluate impact on weight of variables such as materials, types of construction, structural configurations, minimum gage limits, applied loads, fatigue lives, crack-growth lives, initial crack sizes, and residual strengths.

Poe, C. C., Jr.↗

Analysis of cracks emanating from a circular hole in unidirectional fiber reinforced composites, part 2

An analytical method is developed for cracks emanating from a circular hole in an off-axis unidirectional fiber-reinforced composite. The method which is formulated by using conservation laws of elasticity and fundamental relationships in anisotropic fracture mechanics, provides a convenient and accurate means to examine the complicated crack behavior, when used in conjunction with a suitable numerical scheme such as the finite element method. The formulation is eventually reduced to a system of linear algebraic equations of mixed-mode stress intensity factors. Fracture parameters, describing crack-tip deformation and fracture in the composite, are obtained explicitly. Effects of material anisotropy and crack/hole geometry are examined also. Of particular interest are the energy release rates associated with crack extension; their values are evaluated for various cases. Results show that mixed-mode stress intensity factors and energy release rates associated with the cracks emanating from a hole change very appreciably with fiber orientation in the composite. K sub 1 and G increase monotonically with increasing theta; but K sub 2 reaches its maximum at theta = 45 deg, and then decreases gradually as theta increases further.

Wang, S. S.↗

Advanced Materials Technology

Composites, polymer science, metallic materials (aluminum, titanium, and superalloys), materials processing technology, materials durability in the aerospace environment, ceramics, fatigue and fracture mechanics, tribology, and nondestructive evaluation (NDE) are discussed. Research and development activities are introduced to the nonaerospace industry. In order to provide a convenient means to help transfer aerospace technology to the commercial mainstream in a systematic manner.

Charles P. Blankenship↗

Interlaminar fracture of composites

Fracture mechanics has been found to be a useful tool for understanding composite delamination. Analyses for calculating strain energy release rates associated with delamination growth have been developed. These analyses successfully characterized delamination onset and growth for particular sources of delamination. Low velocity impact has been found to be the most severe source of composite delamination. A variety of test methods for measuring interlaminar fracture toughness are being developed to identify new composite materials with enhanced delamination resistance.

Obrien, T. K.↗

Synthesis and toughness properties of resins and composites

Tensile and shear moduli of four ACEE (Aircraft Energy Efficiency Program) resins are presented along with ACEE composite material modulus predictions based on micromechanics. Compressive strength and fracture toughness of the resins and composites were discussed. In addition, several resin synthesis techniques are reviewed.

Johnston, N. J.↗

Tough Composite Materials

Papers and working group summaries are presented which address composite material behavior and performance improvement. Topic areas include composite fracture toughness and impact characterization, constituent properties and interrelationships, and matrix synthesis and characterization.

Louis F. Vosteen↗

Interlaminar fracture of composites

Fracture mechanics has been found to be a useful tool for understanding composite delamination. Analyses for calculating strain energy release rates associated with delamination growth have been developed. These analyses successfully characterized delamination onset and growth for particular sources of delamination. Low velocity impact has been found to be the most severe source of composite delamination. A variety of test methods for measuring interlaminar fracture toughness are being developed to identify new composite materials with enhanced delamination resistance.

Obrien, T. K.↗

Shock metamorphism of deformed quartz

The effect produced by shock loading (to peak pressures of 12 and 24) on deformed synthetic quartz containing a dislocation and abundant bubbles and small inclusions was investigated, and the relationships between preexisting dislocation density shock lamellae in the target material were examined. The resultant material was found to be inhomogeneously deformed and extremely fractured. Results of TEM examinations indicate that no change in dislocation density was caused by shock loading except in regions containing shock lamellae, where the dislocation density was lowered. The shock-induced defects tend to nucleate on and be controlled by preexisting stress concentrators; shock lamellae, glassy veins, and most curviplanar defects form in tension, presumably during release. An extremely mobile silica fluid is formed and injected into fractures during release, which forcibly removes crystalline fragments from vein walls. It is concluded that shock deformation in quartz is dominated by fracture and melting.

Gratz, Andrew J.↗

High-toughness graphite/epoxy composite material experiment

This experiment was designed to measure the effect of near space exposure on three mechanical properties of specially toughened 5208/T300 graphite/epoxy composite materials. The properties measured are elastic modulus, strength, and fracture toughness. Six toughness specimens and nine tensile specimens were mounted on an external frame during the time of the Long Duration Exposure Facility (LDEF) mission. Three identical sets of specimens were manufactured at the outset: the flight set, a zero time non-flight set, and a total time non-flight set. To date, two toughness specimens and three strength and modulus specimens have been tested from each of the three groups.

Felbeck, David K.↗

The effect of nitric acid exposure on Galileo spacecraft titanium alloy Ti-6Al-4V propellant tanks

The Ti-6Al-4V-constructed retropropulsion-module tanks of the Galileo spacecraft were purged with nitrogen tetroxide in order to wait out a major launch rescheduling; nitric acid is among the residual products of such an operation. A test program was conducted on representative samples to ascertain the fracture toughness and stress corrosion threshold of the tanks' material, in view of Space Shuttle safety and mission-reliability requirements. It was found that the tanks' structural integrity was not degraded by nitric acid exposure.

Hsieh, Cheng↗

Ductility enhancement from interface dislocation sources in a directionally solidified beta + gamma + gamma-prime Ni-Fe-Al composite alloy

A directionally solidified beta + gamma + gamma-prime Ni-Fe-Al in situ composite alloy of composition Ni50Fe30Al20 has been used to investigate the effect of a plastically soft second phase on the mechanical behavior of a B2 ordered intermetallic alloy. This material exhibits extensive plasticity during compressive deformation at room temperature and fails in shear with extensive gamma + gamma-prime lamellar or rod pullout. The material also exhibits about 10 percent tensile elongation to fracture at room temperature, with final fracture that includes substantial necking of the gamma + gamma-prime lamellae or rods. Observation of slip lines and dislocation substructures discloses that the normally brittle beta matrix undergoes extensive plasticity in order to deform compatibly with the more ductile gamma phase. The plasticity of the beta matrix is accomplished by the generation of glissile dislocations into the beta matrix from the beta/gamma interface region and is enhanced because of a favorable beta-gamma orientation relationship for slip transfer. Ductility enhancement from interface-generated mobile dislocations generated from beta-gamma interfaces is compared to that observed in film-coated beta-NiAl single crystals and FeAl polycrystals.

Larsen, M.↗

High-toughness graphite/epoxy composite material experiment

This experiment was designed to measure the effect of near-earth space exposure on three mechanical properties of specially toughened 5208/T300 graphite/epoxy composite materials. The properties measured are elastic modulus, strength, and fracture toughness. Six toughness specimens and nine tensile specimens were mounted on an external frame during the 5.8-year orbit of the Long Duration Exposure Facility (LDEF). Three identical sets of specimens were manufactured at the outset: the flight set, a zero-time non-flight set, and a total-time non-flight set.

Felbeck, David K.↗

Instrumented Materials Testing

This presentation starts with an introduction to the need for materials testing. Classic failures (such as brittle ship hull fractures) are discussed before fundamental discoveries in fracture analysis (Griffith, Westergaard, and Irwin). Next standard tests are identified, followed by a look at brittle versus ductile failure. Griffith's result (the composite paradigm) that smaller composite specimens are stronger because they have smaller flaws, is covered. This leads into composite tests. And finally, stress waves are shown as an example that will initiate damage.

Mackin, Thomas J.↗

Dog-Bone Horns for Piezoelectric Ultrasonic/Sonic Actuators

A shape reminiscent of a dog bone has been found to be superior to other shapes for mechanical-amplification horns that are components of piezoelectrically driven actuators used in a series of related devices denoted generally as ultrasonic/sonic drill/corers (USDCs). The first of these devices was reported in Ultrasonic/Sonic Drill/Corers With Integrated Sensors (NPO-20856), NASA Tech Briefs, Vol. 25, No. 1 (January 2001), page 38. The dog-bone shape was conceived especially for use in a more recent device in the series, denoted an ultrasonic/ sonic gopher, that was described in Ultrasonic/Sonic Mechanisms for Drilling and Coring (NPO-30291), NASA Tech Briefs, Vol. 27, No. 9 (September 2003), page 65. The figure shows an example of a dog-bone-shaped horn and other components of an ultrasonic gopher. Prerequisite to a meaningful description of this development is an unavoidably lengthy recapitulation of the principle of operation of a USDC and, more specifically, of the ultrasonic/sonic gopher as described previously in NASA Tech Briefs. The ultrasonic actuator includes a stack of piezoelectric rings, the horn, a metal backing, and a bolt that connects the aforementioned parts and provides compressive pre-strain to the piezoelectric stack to prevent breakage of the rings during extension. The stack of piezoelectric rings is excited at the resonance frequency of the overall ultrasonic actuator. Through mechanical amplification by the horn, the displacement in the ultrasonic vibration reaches tens of microns at the tip of the horn. The horn hammers an object that is denoted the free mass because it is free to move longitudinally over a limited distance between hard stops: The free mass bounces back and forth between the ultrasonic horn and a tool bit (a drill bit or a corer). Because the longitudinal speed of the free mass is smaller than the longitudinal speed of vibration of the tip of the horn, contact between the free mass and the horn tip usually occurs at a phase of the vibration favorable to transfer of momentum from the horn to the free mass. Therefore, the free mass picks up momentum and is accelerated back to the tool bit. Upon impact of the free mass on the tool bit, momentum is transferred to the tool bit. The impacts of the free mass on the tool bit repeat at a sonic frequency that can range from tens of hertz to about 1 kHz. The shock waves caused by the impacts of the free mass propagate to the interface between the tool bit and the medium (typically, rock, ice, or other brittle material) to be drilled or cored. The medium becomes fractured when its ultimate strain is exceeded at the medium/tool-bit interface. This concludes the description of the principle of operation.

Sherrit, Stewart↗

Design and Manufacturing Considerations for Shockproof and Corrosion-Immune Superelastic Nickel-Titanium Bearings for a Space Station Application

An intermetallic nickel-titanium alloy, 60NiTi (60wt%Ni, 40wt%Ti), is a promising tribological material for space mechanisms. 60NiTi offers a broad combination of physical properties that make it unique among bearing materials. 60NiTi is hard, electrically conductive, highly corrosion resistant, readily machined prior to final heat treatment, easily lubricated and is non-magnetic. It also falls within the class of superelastic alloys and can elastically endure large strains (beyond 5 percent) making it highly resistant to excessive and unexpected (shock) loads. Key material properties and characteristics such as elastic modulus, tensile fracture sensitivity and residual stress behavior, however, differ from conventional alloys such as steel and this significantly affects bearing design and manufacturing. In this paper, the preliminary design and manufacture of ball bearings made from 60NiTi are considered for a highly corrosive, lightly loaded, low speed bearing application found inside the International Space Station s water recycling system. The information presented is expected to help guide more widespread commercialization of this new technology into space mechanism and other applications.

DellaCorte, Christopher↗

Refine your search to explore more results.