Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SEM”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,801 records · Page 100

Influence of Oxidation Treatments and Surface Finishing on the Electrochemical Behavior of Ni-20Cr HVOF Coatings

The low-temperature electrochemical behavior of HVOF Ni-20Cr coatings was assessed. The coatings were evaluated in different conditions including as-sprayed, as-ground, and heat-treated in air and argon atmospheres. A detailed analysis of the coatings was carried out by means of XRD, SEM, and EPMA, prior and after the corrosion test. The corrosion rate was analyzed in a NaCl solution saturated with CO{sub 2}. Results demonstrate that the use of a low-oxygen partial pressure favors the formation of a Cr{sub 2}O{sub 3} layer on the surface of the coatings. According to the electrochemical results, the lower corrosion rates were obtained for the heat-treated coatings irrespective of the surface finishing, being the ground and argon heat-treated condition that shows the best corrosion performance. This behavior is due to the synergistic effect of the low-pressure heat treatment and the grinding processes. The grinding promotes a more homogeneous reaction area without surface heterogeneities such as voids, and the pre-oxidation treatment decreases the porosity content of the coating and also allows the growing of a Cr-rich oxide scale which acts as a barrier against the ions of the aqueous solution.

36 MATERIALS SCIENCE↗

Microstructural and Electrochemical Evaluation of Fusion Welded Low-Nickel and 304 SS at Different Heat Input

The present research study investigates the effect of heat input using E 308 electrode (controlled by welding current, i.e., 70, 85 and 100 A) on microstructure, mechanical properties and corrosion behavior of low-nickel and 304 stainless steel (SS) weldments produced by shielded metal arc welding technique. SEM investigation shows that with the higher heat input, δ-ferrite content was reduced. Dendrite and inter-dendritic length is also reduced by lowering the heat input. For all the heat inputs, it is observed that δ-ferrite content was higher in 304 stainless steel (SS) as compared to that of low-nickel austenitic stainless steel (Cr-Mn SS). Considering the heat input for Cr-Mn SS, coarse grains were observed in the heat-affected zone region. For low heat input (LHI), tensile fracture surface has exhibited river-like pattern with dimple appearance. Corrosion studies show better pitting resistance for low heat input (LHI) samples due to higher δ-ferrite present in the weld region. Similarly, higher interphase corrosion resistance is observed in both the SS grades causing more dissolution in the LHI samples.

36 MATERIALS SCIENCE↗

Surface Modification by Friction Stir Processing of Low-Carbon Steel: Microstructure Investigation and Wear Performance

A low-carbon steel sheet with a thickness of 5 mm was subjected to friction stir processing (FSP) by one to four different passes. The microstructures of different regions were characterized using the optical microscopy and electron backscatter diffraction. The Vickers micro-harness was measured at the distance of 200 μm below the processed surfaces. The influence of pass numbers (PNs) on wear resistance was studied in terms of coefficients of friction (CoFs), weight losses and wear rates. SEM topographies of the worn surfaces were also studied to evaluate the wear mechanisms. Microstructure observations showed that Widmänstatten ferrite plates were formed in stir zones (SZs) and heat affected zones. As PN increased, these grains were widened due to the increment of the carbon diffusivity and lengthened because of the high heat input and microstructure anisotropy. Besides, increasing the PN causes increasing of the hardness and wear resistance, simultaneously. Specifically, the wear rate in the SZ was reduced from 2.8 × 10{sup −2} mm{sup 3} m{sup −1} in base metal to 0.3 × 10{sup −2} mm{sup 3} m{sup −1} in sample which was subjected to 4 FSP passes. However, variation in PN had no considerable effect on CoFs. Oxidative wear mechanism was observed on the worn surface of the steel and the FSPed samples while more debris was formed by increasing the PNs.

36 MATERIALS SCIENCE↗

Investigation of Pt and Pd Modified WO{sub 3} and ZnO Based Thin Film Sensors for Ethanol Sensing

Ethanol sensors based on different WO{sub 3} and ZnO structures are studied in the present work. The XRD and SEM processes are used to characterize the sensing layer’s surface morphology which reveals the presence of nanoparticle in sensing layer. Further reducing the nanoparticle diameter by the addition of palladium (Pd) and platinum (Pt) for both the sensors (ZnO and WO{sub 3}) gives good results on sensitivity, operating temperature, response time and recovery time. Nanoparticle diameter for undoped WO{sub 3}, Pd-modified WO{sub 3} and Pt-modified WO{sub 3} based sensors is 11.8, 6 and 5.4 nm, whereas nanoparticle diameter for undoped, Pd-modified and Pt-modified ZnO based sensors is 20, 14 and 11 nm, respectively. Analysis of dynamic response of the sensors when exposed to different concentrations of ethanol vapour (from 500 to 10,000 ppm) and various temperatures indicate the improvement in sensitivity up to 77.2% for WO{sub 3} and 74.6% for ZnO based sensors.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Electrolytic Synthesis of Ni-W-MWCNT Composite Coating for Alkaline Hydrogen Evolution Reaction

Nickel–tungsten multi-walled carbon nanotube (Ni-W-MWCNT) composite films were fabricated by an electrodeposition technique, and their electrocatalytic activity toward hydrogen evolution reaction (HER) was studied. Ni-W-MWCNT composite films with a homogeneous dispersion of MWCNTs were deposited from an optimal Ni-W plating bath containing functionalized MWCNTs, under galvanostatic condition. The presence of functionalized MWCNT was found to enhance the induced codeposition of the reluctant metal W and resulted in a W-rich composite coating with improved properties. The electrocatalytic behaviors of Ni-W-MWCNT composite coating toward HER were studied by cyclic voltammetry (CV) and chronopotentiometry techniques in 1.0 M KOH medium. Further, Tafel polarization and electrochemical impedance spectroscopy (EIS) studies were carried out to establish the kinetics of HER on the alloy and composite electrodes. The experimental results revealed that the addition of MWCNTs (having a diameter of around 10-15 nm) into the alloy plating bath has a significant effect on the electrocatalytic behavior of Ni-W alloy deposit. The Ni-W-MWCNT composite coating was found to show better HER activity than the conventional Ni-W alloy coating. The enhanced electrocatalytic activity of Ni-W-MWCNT composite coating is attributed to the MWCNT intersticed in the deposit matrix, evidenced by surface morphology, composition and phase structure of the coating through SEM, EDS and XRD analyses, respectively.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Experimental Investigation and Finite Element Analysis on Fatigue Behavior of Aluminum Alloy 7050 Single-Lap Joints

The fatigue behavior of single-lap four-riveted aluminum alloy 7050 joints was investigated by using high-frequency fatigue test and scanning electron microscope (SEM). Stress distributions obtained by finite element (FE) analysis help explain the fatigue performance. The fatigue test results showed that the fatigue lives of the joints depend on cold expansion and applied cyclic loads. FE analysis and fractography indicated that the improved fatigue lives can be attributed to the reduction in maximum stress and evolution of fatigue damage at the critical location. The beneficial effects of strengthening techniques result in tearing ridges or lamellar structure on fracture surface, decrease in fatigue striations spacing, delay of fatigue crack initiation, crack deflection in fatigue crack propagation and plasticity-induced crack closure.

36 MATERIALS SCIENCE↗

Dendritic Zinc Growth in Acid Electrolyte: Effect of the pH

In this paper, dendritic growth at the edges of electrogalvanized steel strip has been studied using a specially designed rotating washer electrode which simulates the fluid dynamic conditions and the current density distribution at the steel strip edge found in a production line. The effect of electrolyte pH and current density on dendritic growth in an acidic zinc plating bath (ZnSO{sub 4} and H{sub 2}SO{sub 4}) was addressed. The temperature was kept constant at 60 °C. Solution pH was adjusted to 1, 2 or 3 using different amounts of H{sub 2}SO{sub 4}. In addition, the influence of temperature on the pH of the solution was determined. The current density was set at 40 or 60 A/dm{sup 2}, similar to that used in the industry. Deposits were characterized using SEM and XRD. The results showed that pH strongly affects dendrites shape, length and texture. Furthermore, the morphology of dendrites at the washer edge and of deposits on the flat portion of the washer changed considerably as solution pH was increased from 1 to 3. It was found that the morphology of dendrites at the washer edge stems from the morphology of the deposit on its flat portion, which in turn determines their shape.

36 MATERIALS SCIENCE↗

Characterization of Microstructure and Wear Resistance of PEO Coatings Containing Various Microparticles on Ti6Al4V Alloy

Titania-based composite coatings were prepared by plasma electrolytic oxidation (PEO) treatment of Ti6Al4V alloy in electrolyte with α-Al{sub 2}O{sub 3}, Cr{sub 2}O{sub 3} or h-BN microparticles in suspension. The microstructure, composition of PEO composite coatings were analyzed by SEM, EDS and XRD. The wear resistance of composite ceramic coatings was studied by ball-on-disk wear test at ambient temperature and 300 °C. The results showed that the addition of microparticles accelerated the growth rate of PEO coating and changed the microstructure and composition of PEO coating. PEO coating was porous and mainly composed of rutile-TiO{sub 2}, anatase-TiO{sub 2} and Al{sub 2}TiO{sub 5}. PEO/α-Al{sub 2}O{sub 3} (Cr{sub 2}O{sub 3} or h-BN) composite coating only had small micropores and appeared some α-Al{sub 2}O{sub 3} (Cr{sub 2}O{sub 3} or h-BN) phase. Besides, the addition of α-Al{sub 2}O{sub 3} (Cr{sub 2}O{sub 3} or h-BN) microparticles greatly improved the wear resistance of PEO coating. At ambient temperature, abrasive wear dominated the wear behavior of PEO coating, but abrasive wear and adhesive peel simultaneously happened at 300 °C. Whether at ambient temperature or 300 °C, PEO composite coating had better wear resistance than PEO coating. Besides, PEO/h-BN composite coating outperformed other composite coatings regardless of the temperature.

36 MATERIALS SCIENCE↗

Tribological Performance of Duplex-Annealed Ti-6Al-2Sn-4Zr-2Mo Titanium Alloy at Elevated Temperatures Under Dry Sliding Condition

Ti-6Al-2Sn-4Zr-2Mo (Ti-6-2-4-2) is a typical near-α titanium alloy developed for high-temperature applications. It offers numerous enhanced properties like an outstanding strength-to-weight ratio, a low Young’s modulus and exceptional creep and corrosion resistance. On the other hand, titanium alloys are known for their weak resistance to wear. Ti-6-2-4-2 is mainly applied in aero engine component parts, which are exposed to temperatures up to 565 °C. Through an increasing demand on efficiency, engine components are exposed to higher combustion pressures and temperatures. Elevated temperature tribology tests were conducted on a pin-on-disk tribometer equipped with a heating chamber. The tests were carried out under dry conditions with a constant sliding distance of 600 m with a speed of 0.16 m/s at the ball point. The sliding partner was AISI E52100 steel ball with the hardness of 58HRC. The varied input variables are normal load and temperature. It can be concluded that the coefficient of friction (CoF) increases with increasing temperature, while the wear rate decreases to its minimum at 600 °C due to increasing adhesion and oxidation mechanisms. Wear track observations using a scanning electron microscope (SEM) including energy-dispersive x-ray spectroscopy (EDS) were used to determine the occurring wear mechanisms.

36 MATERIALS SCIENCE↗

Dynamic Analysis of Recalescence Process and Interface Growth of Eutectic Fe{sub 82}B{sub 17}Si{sub 1} Alloy

By employing the glass fluxing technique in combination with cyclical superheating, the microstructural evolution of the undercooled Fe{sub 82}B{sub 17}Si{sub 1} alloy in the obtained undercooling range was studied. With increase in undercooling, a transition of cooling curves was detected from one recalescence to two recalescences, followed by one recalescence. The two types of cooling curves were fitted by the break equation and the Johnson–Mehl–Avrami–Kolmogorov model. Based on the cooling curves at different undercoolings, the recalescence rate was calculated by the multi-logistic growth model and the Boettinger–Coriel–Trivedi model. Both the recalescence features and the interface growth kinetics of the eutectic Fe{sub 82}B{sub 17}Si{sub 1} alloy were explored. The fitting results that were obtained using TEM (SAED), SEM and XRD were consistent with the changing rule of microstructures. Finally, the relationship between the microstructure and hardness was also investigated.

36 MATERIALS SCIENCE↗

Effect of the As-Forged and Heat-Treated Microstructure on the Room Temperature Anisotropic Ductile Fracture of Inconel 718

The purpose of the present work was to investigate the effect of primary carbides and the δ-phase on the anisotropic ductile fracture of Inconel 718 in the forging process. Inconel 718 alloys were prepared by VIM + VAR processes with various carbon contents (0.009 and 0.027 wt.%). Then, the alloys were forged and annealed at temperatures of 980 and 1030 °C. The room temperature mechanical anisotropy of the alloys was evaluated at the longitudinal direction (LD) and transverse direction (TD). Tensile and impact tests were used to characterize the mechanical properties of the specimens. The microstructural characterization and the fractography of the alloys were carried out by FE-SEM. The obtained results showed that the fracture strain and the impact energy in the TD were 30-50% lower than the LD. The fracture was accelerated by the δ-phase, leading to the reduction of impact energy in the longitudinal and the lateral directions up to 50%. The low-carbon alloy indicated similar characteristics in both the LD and the TD. Aligned carbides changed the fracture path from a zigzag path in the LD to a fibrous path in the TD, while the δ-phase created a flat fracture path. The shear lip area ratio in the tensile fracture cross section was decreased by reducing ductility.

36 MATERIALS SCIENCE↗

The Effect of Prestrain Temperature on Kinetics of Static Recrystallization, Microstructure Evolution, and Mechanical Properties of Low Carbon Steel

In this research, the samples of a low carbon steel sheet were rolled up to a thickness prestrain of 67% at three different temperatures consisted of room, blue brittleness, and subzero temperature. Microhardness, SEM, and tensile tests were carried out to evaluate the static recrystallization kinetics defined by the Avrami equation, microstructural evolution, and mechanical properties. It was found that the Avrami exponent is altered with change in prestrain temperature and it achieves the value of 1 to 1. 5. Moreover, it was indicated that prestraining at subzero temperature followed by annealing at 600 °C leads to considerable enhancement in tensile properties and kinetics of static recrystallization compared to room and blue brittleness temperatures. The prestraining at blue brittleness temperature followed by annealing treatment caused, however, a higher strength and faster kinetics compared with that at room temperature. It was concluded that although from the steel ductility point of view, the blue brittleness temperature is called an unsuitable temperature, but it can be used as prestraining temperature to develop noticeable combination of strength and ductility in low carbon steel.

36 MATERIALS SCIENCE↗

Investigation of Mechanical and Electromagnetic Interference Shielding Properties of Nickel–CFRP Textile Composites

The most common materials used for electromagnetic interference shielding are metals and their alloys. However, those materials are heavy and highly reflective. In order to eliminate or reduce the intensity of wave radiation in their working environment, lightweight materials that have interference shielding properties are needed. In this paper, nickel wire mesh yarns (warps) were woven into carbon fibers-reinforced plastic yarns (wefts) to produce metal–carbon textile composite materials. The plain weave and 2/2 twill weave techniques were used, and the woven fabrics were laminated to manufacture experimental test samples. The nickel, which has high magnetic permeability and good electric conductivity, and carbon fibers, which have good electrical, thermal and mechanical properties, were used together to achieve the desired properties. The shielding effectiveness of each sample was investigated using a network analyzer connected with coaxial transmission line test in accordance with ASTM 4935-99 standard, with the frequencies ranging from 500 MHz to 1.5 GHz. Here, the plain weave structure showed higher shielding effectiveness than twill weave. The absorption losses for both materials were relatively greater than reflection losses. In reference to the orientation of wire mesh yarns about the loading axis, the tensile strengths in the transversal direction were 19.04 and 16.34% higher than the tensile strengths in longitudinal direction for plain weave and twill weave, respectively. The fractography analysis with SEM showed a ductile fracture of wire mesh and brittle fracture of epoxy matrix and carbon fibers.

36 MATERIALS SCIENCE↗

The Effect of Titanium Dioxide (TiO{sub 2}) Nanoparticles on Hydroxyapatite (HA)/TiO{sub 2} Composite Coating Fabricated by Electrophoretic Deposition (EPD)

Composite coatings of Hydroxyapatite (HA) with ceramics, polymers and metals are used to modify the surface structure of implants. In this research, HA/TiO{sub 2} composite coating was fabricated by electrophoretic deposition (EPD) on 316 stainless steel substrate. HA/TiO{sub 2} composite coatings with 5, 10 and 20 wt.% of TiO{sub 2}, deposited at 40 V and 90 s as an optimum condition. The samples coated at this condition led to an adherent, continuous and crack-free coating. The influence of TiO{sub 2} content was studied by performing different characterization methods such as scanning electron microscopy (SEM), energy dispersive x-ray spectroscopy (EDS), corrosion resistance in simulated body fluid (SBF), coating’s dissolution rate in physiological solution and bond strength to the substrate. The results showed that the higher amount of TiO{sub 2} in the composite coating led to increase in bond strength of coating to stainless steel substrate from 3 MPa for HA coating to 5.5 MPa for HA-20 wt.% TiO{sub 2} composite coating. In addition, it caused to reduction of corrosion current density of samples in the SBF solution from 18.92 μA/cm{sup 2} for HA coating to 6.35 μA/cm{sup 2} for HA-20 wt.% TiO{sub 2} composite coating.

36 MATERIALS SCIENCE↗

Microstructural Evolution of NiCrBSi Coatings Fabricated by Stationary Local Induction Cladding

The development of induction cladding has been restricted by the complicated geometric characteristics of workpieces and the large heat-affected zone in the cladded workpieces. In this paper, three-dimensional continual local induction cladding (3D-CLIC) was proposed as a potential process to clad coating over a substrate with curved surface, and a stationary local induction cladding (SLIC) experiment was conducted as an exploratory study of 3D-CLIC. The microstructures and microhardness in the coatings were measured by SEM, EDS, XRD and microsclerometer, respectively. The results indicate that the coating is metallurgically bonded with the substrate without any defects. A compositional gradient exists in the diffusion transfer belt (DTB), and it decreases with the increase in induction heating time. The coating is mainly composed of (Fe, Ni), CrB, M{sub 7}C{sub 3}, Ni{sub 3}B, Ni{sub 3}Si and M{sub 23}C{sub 6} (M = Cr, Ni, Fe). Among the carbides, M{sub 7}C{sub 3} presents several morphologies and M{sub 23}C{sub 6} is always attached to the DTB. A special phenomenon of texture was found in the SLIC coatings. The preferred orientation in (200) crystal plane or the restrained orientation in (111) (200) crystal plane becomes more obvious as the scanning speed increases. The maximum average microhardness is 721 HV when the coating is heated for 5 s. The wear loss of different samples increases with increasing induction heating time. The longer heating time would result in higher dilution in the SLIC coatings due to the complete mixing with the substrate, thus leading to the decrease in microhardness and wear loss.

36 MATERIALS SCIENCE↗

Electrodeposition and Characterization of Ni-Al{sub 2}O{sub 3} Nanocomposite Coatings on Steel

Monodispersed alumina particles were synthesized by the homogeneous precipitation under reflux boiling. The particles were employed as reinforcement additives in the electrodeposited Ni-Al{sub 2}O{sub 3} composite coatings on steel. The deposited pure Ni and Ni-Al{sub 2}O{sub 3} composite coatings were analyzed by SEM, XRD, and microhardness tester. The wear resistance and friction coefficient of the coated samples were determined by using a ball-on-disk tribometer. Furthermore, XRD analysis showed that coating temperature and the presence of particles in the deposited coatings had a noticeable effect on the preferred orientation of the crystalline faces of the nickel grains. Significant differences were noted in the texture coefficient of the pure Ni and Ni-Al{sub 2}O{sub 3} composite coatings produced at different temperatures. These differences were attributed to the changes in the microstructure of the matrix caused by the embedded Al{sub 2}O{sub 3} particles. Results revealed that wear resistance and the friction coefficient were turned out to be higher and smaller, respectively, for the composite coatings as compared to pure Ni coating at a given sliding distance. It was noted that the corrosion resistance of these specimens increased in the following order: bare substrate < pure Ni coating < Ni-Al{sub 2}O{sub 3} nanocomposite coatings.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Enhanced Hot Tensile Ductility of Mg-3Al-1Zn Alloy Thin-Walled Tubes Processed Via a Combined Severe Plastic Deformation

In the current study, combined parallel tubular channel angular pressing (PTCAP) and tube backward extrusion (TBE), as a recently developed severe plastic deformation (SPD) method, were applied at 300 °C on a commercial Mg-3Al-1Zn alloy tubes to achieve an ultrafine grained structure. Then, the microstructure, hardness, tensile properties, and fractography evaluations were done at room temperature on the SPD-processed samples. Also, to study the hot tensile ductility of the SPD-processed samples, tensile testing was performed at an elevated temperature of 400 °C, and then, the fractured surface of the tensile samples was studied. It was observed that a bimodal microstructure, with large gains surrounded by many tiny ones, was created in the sample processed by PTCAP followed by TBE. This microstructure led to reach higher hardness and higher strength at room temperature and also led to reach very high elongation to failure (~ 181%) at 400 °C. Also, the value of elongation to failure for this sample was ~ 14.1% at room temperature. The fractographic SEM images showed the occurrence of predominately ductile fracture in the samples pulled at 400 °C. This was mostly due to the nucleation of microvoids and their subsequent growth and coalescence with each other.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment on the Properties of CoCrMo Alloy Manufactured by Selective Laser Melting

To obtain medical implants with better mechanical properties, it is necessary to conduct studies on the heat treatment process of the selective laser melting (SLM) manufacturing parts. The differential scanning calorimetry method was used to study the heat treatment process of the phase transition of SLM CoCrMo alloy parts. The tensile properties were tested with a tensile test machine, the quantity of carbide precipitated after heat treatment was measured by energy-dispersive x-ray spectroscopy, and the tensile fracture morphology of the parts was investigated using SEM. The obtained results were: Mechanical properties in terms of elongation and tensile strength of CoCrMo alloy manufactured by SLM that had been heat-treated at 1200 °C for 2 h followed by cooling with water were not only higher than the national standard but also higher than the experimental results of the same batch of castings. The mechanism of fracture of parts manufactured by SLM without heat treatment was brittle fracture, whereas parts which had been heat-treated at 1200 °C for 2 h combined with water cooling and at 1200 °C for 1 h with furnace cooling suffered ductile fracture. This study provides the basis for defining the applications for which CoCrMo alloys manufactured by SLM are suitable within the field of medical implants.

36 MATERIALS SCIENCE↗

Refine your search to explore more results.