Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “REFINING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,801 records · Page 100

Hydrogen atom distribution and hydrogen induced site depopulation for the La{sub 2-x}Mg{sub x}Ni{sub 7}-H system

La{sub 2-x}Mg{sub x}Ni{sub 7} and its hydrides/deuterides were investigated by high resolution synchrotron powder X-ray and neutron diffraction. Upon deuteration the single phase sample of the intermetallic compound with the refined composition La{sub 1.63}Mg{sub 0.37}Ni{sub 7} (space group: P6{sub 3}/mmc) expands isotropically, in contrast to the Mg free phase. The hydrogen uptake, {approx}9 D/f.u., is higher than in La{sub 2}Ni{sub 7}D{sub 6.5}. The refined composition accounts for La{sub 1.63}Mg{sub 0.37}Ni{sub 7}D{sub 8.8} (beta-phase). Rietveld refinements using the neutron and synchrotron diffraction data suggest that deuterium atoms occupy 5 different interstitial sites within both AB{sub 2} and AB{sub 5} slabs, either in an ordered or a disordered way. All determined D sites have an occupancy >50% and the shortest D-D contact is 1.96(3) A. It is supposed that a competition between the tendency to form directional bonds and repulsive D-D (H-H) interactions is the most important factor that influences the distribution of deuterium atoms in this structure. A hitherto unknown second, alpha-phase with composition La{sub 1.63}Mg{sub 0.37}Ni{sub 7}D{sub 0.56}, crystallizing with the same hexagonal symmetry as La{sub 1.63}Mg{sub 0.37}Ni{sub 7}D{sub 8.8}, has been discovered. The unit cell parameters for this D-poor phase differ slightly from those of the intermetallic. Alpha-phase displays only one D site (4f, space group: P6{sub 3}/mmc) occupied >50%, which is not populated in the D-rich beta-phase. This hydrogen/deuterium induced site depopulation can be explained by repulsive D-D (H-H) interactions that are likely to influence non-occupancy of certain interstices in metal lattice when absorbing hydrogen. - Graphical abstract: The detailed D atoms arrangement in La{sub 1.63}Mg{sub 0.37}Ni{sub 7}D{sub 8.8} differs significantly from the previously reported La{sub 1.5}Mg{sub 0.5}Ni{sub 7}D{sub 8.9(9.1)}. The present model consists of only five deuterium sites as opposed to nine proposed for La{sub 1.5}Mg{sub 0.5}Ni{sub 7}D{sub 8.9(9.1)}. The reported four remaining deuterium atom positions in La{sub 1.5}Mg{sub 0.5}Ni{sub 7}D{sub 8.9(9.1)} were not found in the investigated La{sub 1.63}Mg{sub 0.37}Ni{sub 7}D{sub 8.8}. The five Ni atoms have deuterium among their nearest neighbors, which surround them in a way similar to configurations observed in some complex transition metal hydrides and already reported for metallic hydrides. In the presented deuterium-rich phase, deformed tetrahedron, rigid trigonal pyramids as well as disordered and deformed saddle-like configuration are observed. Highlights: Black-Right-Pointing-Pointer Alpha- and beta-phase for La{sub 2-x}Mg{sub x}Ni{sub 7}-H system have been characterized. Black-Right-Pointing-Pointer Five different interstitial sites are occupied by deuterium/hydrogen atoms in the beta-phase. Black-Right-Pointing-Pointer One D/H site has been determined in the alpha-phase. Black-Right-Pointing-Pointer Deuterium/hydrogen induced site depopulation during phase transformation is observed. Black-Right-Pointing-Pointer Ni atoms tend to have tetrahedral-like D/H atom coordination.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of Cu{sup 2+} and Ni{sup 2+} substitution at the Mn site in (La{sub 0.63}Ca{sub 0.37})MnO{sub 3}: A neutron powder diffraction investigation

The crystal and magnetic structures of the (La{sub 0.63}Ca{sub 0.37})(Mn{sub 1−x}TM{sub x})O{sub 3} compounds (x=0.00, 0.03, 0.08; TM=Cu{sup 2+}, Ni{sup 2+}) were investigated between 5 K and 300 K by means of dc magnetic measurements and neutron powder diffraction analysis followed by Rietveld refinement. Both substituting cations lead to a reduction of the long range ferromagnetic ordering temperature; ferromagnetism is strongly suppressed in the 8% Cu-substituted sample, where long- and short-range FM magnetic orders coexist together with short-range A-type AFM order. This particular feature can be related to the Jahn–Teller character of Cu{sup 2+}, absent in Ni{sup 2+}, and suggests the occurrence of a quantum critical point in the (La{sub 0.63}Ca{sub 0.37})(Mn{sub 1−x}Cu{sub x})O{sub 3} system. - Graphical abstract: Rietveld refinement plot of (La{sub 0.63}Ca{sub 0.37})(Mn{sub 0.92}Cu{sub 0.08})O{sub 3} showing in the inset the coexistence of broad A-type AFM peaks with FM ones. Highlights: ► (La{sub 0.63}Ca{sub 0.37})MnO{sub 3} was substituted with Ni and Cu. ► Neutron powder diffraction and Rietveld refinement were carried out. ► A quantum critical point possibly occurs in the (La{sub 0.63}Ca{sub 0.37})(Mn{sub 1−x}Cu{sub x})O{sub 3} system.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A new member of “114” family Ca{sub 1−x}Eu{sub x}BaZn{sub 2+x}Ga{sub 2−x}O{sub 7} (x≤0.24): Structure and luminescence

New “114” oxides Ca{sub 1−x}Eu{sub x}BaZn{sub 2+x}Ga{sub 2−x}O{sub 7} (x≤0.24) were synthesized by solid state reaction. Rietveld refinements were performed on high quality powder XRD data in the space group P6{sub 3}mc. Zn{sup 2+} and Ga{sup 3+} co-occupy T1 and T2 positions, which are both in tetrahedral coordinated environment. Comparing the host compound, O3 moves towards T2 cation as much as 0.08 Å when x=0.24. It is the most observable structural change during the substitution. By comparing the structures of CaBaZn{sub 2}Ga{sub 2}O{sub 7} (P6{sub 3}mc) and CaBaCo{sub 4}O{sub 7} (Pbn2{sub 1}), we find that smaller cations in tetrahedral sites would lead to a lower symmetry in “114” oxides. Luminescent spectra show the noncentrosymmetric coordination of Eu{sup 3+}, and the f–f excitations are comparable to CT-excitation. No concentration quenching was observed up to x=0.24. The optical band gaps were estimated to be 3.8 eV for Ca{sub 1−x}Eu{sub x}BaZn{sub 2+x}Ga{sub 2−x}O{sub 7} (x=0, 0.16). - Graphical abstract: Reitveld refinements show Ca{sub 1−x}Eu{sub x}BaZn{sub 2+x}Ga{sub 2−x}O{sub 7} all crystallize in P6{sub 3}mc. By Eu{sup 3+}-doping, O3 show the most obvious movement (∼0.08 Å) along the c-axis. Display Omitted - Highlights: • Ca{sub 1−x}Eu{sub x}BaZn{sub 2+x}Ga{sub 2−x}O{sub 7} (x≤0.24) solid solutions were synthesized in air. • Rietveld refinements of high quality powder XRD show good convergences. • Ca{sub 1−x}Eu{sub x}BaZn{sub 2+x}Ga{sub 2−x}O{sub 7} all crystallize in the space group P6{sub 3}mc. • Luminescent spectra of Eu{sup 3+} show no quenching effect up to x=0.24. • Optical band gaps for CaBaZn{sub 2}Ga{sub 2}O{sub 7} are estimated to be 3.8 eV.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Structure of β-AgGaO{sub 2}; ternary I–III–VI{sub 2} oxide semiconductor with a wurtzite-derived structure

The structure of the wurtzite-derived β-AgGaO{sub 2} was refined by Rietveld analysis of high-resolution powder diffraction data obtained using synchrotron X-ray radiation. The space group of the crystal is Pna2{sub 1} with lattice parameters of a{sub 0}=5.56175 Å, b{sub 0}=7.14749 Å, and c{sub 0}=5.46875 Å. The deviation of O–Ag–O and M–O–M bond angles from the regular tetrahedral angle of 109.5° was very large at ∼8° and ∼11°, respectively. The electronic structure of β-AgGaO{sub 2} is discussed based on its structure, and the indirect band gap of β-AgGaO{sub 2} was related to significant tetrahedral distortion. Although β-AgGaO{sub 2} decomposes into metallic silver and Ga{sub 2}O{sub 3} at a high temperature in any atmosphere, β-AgGaO{sub 2} is stable up to 690 °C under an O{sub 2} atmosphere. No direct transformation from the wurtzite-derived phase to a delafossite phase occurs in β-AgGaO{sub 2}. - Graphical abstract: Crystal structure of β-AgGaO{sub 2} was refined by Rietveld analysis. AgO{sub 4} and O(Ag,Ga){sub 4} tetrahedra are significantly distorted from ideal tetrahedron. - Highlights: • Orthorhombic β-AgGaO{sub 2} with a wurtzite-derived β-NaFeO{sub 2} structure was synthesized. • Its structure was refined by Rietveld analysis of high-resolution XRD data. • Silver and oxygen tetrahedra are significantly distorted from an ideal tetrahedron. • The extent of this tetrahedral distortion is related to the band gap nature. • β-AgGaO{sub 2} is a metastable phase but is stable up to 690 °C in an O{sub 2} atmosphere.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microwave sol–gel synthesis and upconversion photoluminescence properties of CaGd{sub 2}(WO{sub 4}){sub 4}:Er{sup 3+}/Yb{sup 3+} phosphors with incommensurately modulated structure

CaGd{sub 2−x}(WO{sub 4}){sub 4}:Er{sup 3+}/Yb{sup 3+} phosphors with the doping concentrations of Er{sup 3+} and Yb{sup 3+} (x=Er{sup 3+}+Yb{sup 3+}, Er{sup 3+}=0.05, 0.1, 0.2 and Yb{sup 3+}=0.2, 0.45) have been successfully synthesized by the microwave sol–gel method. The crystal structure of CaGd{sub 2−x}(WO{sub 4}){sub 4}:Er{sup 3+}/Yb{sup 3+} tungstates have been refined, and upconversion photoluminescence properties have been investigated. The synthesized particles, being formed after the heat-treatment at 900 °C for 16 h, showed a well crystallized morphology. Under the excitation at 980 nm, CaGd{sub 2}(WO{sub 4}){sub 4}:Er{sup 3+}/Yb{sup 3+} particles exhibited a strong 525-nm and a weak 550-nm emission bands in the green region and a very weak 655-nm emission band in the red region. The Raman spectrum of undoped CaGd{sub 2}(WO{sub 4}){sub 4} revealed about 12 narrow lines. The strongest band observed at 903 cm{sup −1} was assigned to the ν{sub 1} symmetric stretching vibration of WO{sub 4} tetrahedrons. The spectra of the samples doped with Er and Yb obtained under the 514.5 nm excitation were dominated by Er{sup 3+} luminescence preventing the recording of these samples Raman spectra. Concentration quenching of the erbium luminescence at {sup 2}H{sub 11/2}→{sup 4}I{sub 15/2} transition is weak in the range of erbium doping level x{sub Er}=0.05–0.2, while, for transition {sup 4}S{sub 3/2}→{sup 4}I{sub 15/2}, the signs of concentration quenching become pronounced at x{sub Er}=0.2. - Graphical abstract: CaGd{sub 2−x}(WO{sub 4}){sub 4}:Er{sup 3+}/Yb{sup 3+} phosphors with the doping concentrations of Er{sup 3+} and Yb{sup 3+} (x=Er{sup 3+}+Yb{sup 3+}, Er{sup 3+}=0.05, 0.1, 0.2 and Yb{sup 3+}=0.2, 0.45) have been successfully synthesized by the microwave sol–gel method and the crystal structure refinement, and upconversion photoluminescence properties have been investigated. - Highlights: • CaGd{sub 2−x}(WO{sub 4}){sub 4}:Er{sup 3+}/Yb{sup 3+} phosphors have been synthesized by the microwave sol–gel method. • The crystal structure of CaGd{sub 2−x}(WO{sub 4}){sub 4}:Er{sup 3+}/Yb{sup 3+} tungstates have been refined. • The upconversion photoluminescence properties have been investigated.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

HPHT synthesis, structure and electrical properties of type-I clathrates Ba{sub 8}Al{sub x}Si{sub 46−x}

Clathrate compounds Ba{sub 8}Al{sub x}Si{sub 46−x} were successfully synthesized using the method of high-pressure and high-temperature (HPHT). In this process, we used BaSi{sub 2} as one of the starting materials in place of Ba metals, which reduces the complexity of the program caused by the extremely high chemical reactivity. By using this method, the processing time was reduced from few days to an hour. X-ray diffraction and structural refinement indicated this composition crystallized in type-I clathrate phase. Bond length analysis showed the Ba atoms in small dodecahedron had spherical thermal ellipsoids while those in large tetrakaidecahedron displayed anisotropic thermal ellipsoids. The negative Seebeck coefficient indicated transport processes were dominated by electrons as carriers, and increased with the increasing temperature. The electrical properties, including Seebeck coefficient and Power factor, were greatly enhanced by Al substitution. - Graphical abstract: Left: The cavity structure diagram of a China-type large volume cubic high-pressure apparatus, and the Type-I clathrate structure of sample synthesized using HPHT. Middle: X-ray Rietveld refinement profile for Ba{sub 8}Si{sub 46} and element mapping for Ba{sub 8}Al{sub 16}Si{sub 30}. Right: Temperature dependence of Seebeck coefficient for Ba{sub 8}Al{sub x}Si{sub 46−x} prepared by HPHT. - Highlights: • HPHT is a simple and rapid synthetic approach. • We use BaSi{sub 2} as one of the starting materials replacing Ba metals. • The processing time reduces from few days to an hour. • Structure determination is refined by Rietveld analysis of XRD data. • Variable temperature electrical properties are characterized.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Hydrogenation studies on NdScSi and NdScGe

NdScSi and NdScGe were synthesized from the elements via arc-melting and subsequent annealing. Their ordered La{sub 2}Sb type structures, with space group I4/mmm, were refined from single crystal X-ray diffractometer data: a=428.94(6) and b=1570.5(3) pm, wR2=0.0395, 309 F{sup 2} values for NdScSi and a=431.2(1) and c=1581.3(5) pm, wR2=0.1220, 227 F{sup 2} values for NdScGe, with 11 variables per refinement. Hydrogen insertion was performed on both Nd-based intermetallics by solid/gas reaction. Hydrogen uptake keeps the pristine compound space group but yields an anisotropic expansion of the unit cell with a large increase of c (≈+7%) and a slight decrease of a (≈−1.7%) parameters. Hydrogen absorption at 350 °C and under 5 bar of H{sub 2} pressure shows that the hydride NdScSiH{sub 1.48(5)} is formed. An in-situ neutron diffraction study during the deuteration of NdScSi reveals for the first time in a CeScSi-type compound, the possibility to fill two interstitial sites with deuterium atoms, leading to the composition NdScSiD{sub 1.5} for the deuteride adopting then the La{sub 2}Fe{sub 2}Se{sub 2}O{sub 3}-type structure. From magnetization measurements, we evidence that hydrogenation strongly reduces the Curie temperature of NdScSi (T{sub C}=175 K) and NdScGe (T{sub C}=194 K) since NdScSiH{sub 1.5} and NdScGeH{sub x} undergo a magnetic transition at 4 K and around 2 K, respectively. - Highlights: • Crystal structures of NdScSi and NdScGe were refined from single crystal XRD data. • The hydrogenation of NdScSi leads to the formation of the NdScSiH{sub 1.5} hydride. • NdScSiD{sub 1.5} adopts the La{sub 2}Fe{sub 2}Se{sub 2}O{sub 3}-type structure. • Hydrogenation strongly reduces the ordering temperature of both intermetallics.

36 MATERIALS SCIENCE↗

Structure resolution by electron diffraction tomography of the complex layered iron-rich Fe-2234-type Sr{sub 5}Fe{sub 6}O{sub 15.4}

The crystal structure of the strontium ferrite Sr{sub 5}Fe{sub 6}O{sub 15.4}, was solved by direct methods on electron diffraction tomography data acquired on a transmission electron microscope. The refined cell parameters are a=27.4047(3) Å, b=5.48590(7) Å and c=42.7442(4) Å in Fm2m symmetry. Its structure is built up from the intergrowth sequence between a quadruple perovskite-type layer with a complex rock-salt (RS)-type block. In the latter iron atoms are found in two different environments : tetragonal pyramid and tetrahedron. The structural model was refined by Rietveld method based on the powder X-ray diffraction pattern. - Highlights: • Complex structure of Sr{sub 5}Fe{sub 6}O{sub 15.4} solved by electron diffraction tomography. • Observed Fourier maps allow determining missing oxygen atoms in the structure. • Structural model refined from powder X-ray diffraction data. • Intergrowth between quadruple perovskite layer with double rock-salt-type layer.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Phase equilibria in the NaF-CdO-NaPO{sub 3} system at 873 K and crystal structure and physico-chemical characterizations of the new Na{sub 2}CdPO{sub 4}F fluorophosphate

Isothermal sections of the diagram representing phase relationships in the NaF-CdO-NaPO{sub 3} system have been investigated by solid state reactions and powder X-ray diffraction. This phase diagram investigation confirms the polymorphism of the NaCdPO{sub 4} side component and the structure of the ß high temperature polymorph (orthorhombic, space group Pnma and unit cell parameters a=9.3118(2), b=7.0459(1), c=5.1849(1) Å has been refined. A new fluorophosphate, Na{sub 2}CdPO{sub 4}F, has been discovered and its crystal structure determined and refined from powder X-ray diffraction data. It exhibits a new 3D structure with orthorhombic symmetry, space group Pnma and unit cell parameters a=5.3731(1), b=6.8530(1), c=12.2691(2) Å. The structure is closely related to those of the high temperature polymorph of the nacaphite Na{sub 2}CaPO{sub 4}F and the fluorosilicate Ca{sub 2}NaSiO{sub 4}F but differs essentially in the cationic repartition since the structure is fully ordered with one Na site (8d) and one Cd site (4c). Relationships with other Na{sub 2}M{sup II}PO{sub 4}F (M{sup II}=Mg, Ca, Mn, Fe, Co, Ni) have been examined and the crystal-chemical and topographical analysis of these fluorophosphates is briefly reviewed. IR, Raman, optical and {sup 19}F, {sup 23}Na, {sup 31}P MAS NMR characterizations of Na{sub 2}CdPO{sub 4}F have been investigated. - Graphical abstract: The structure of the compound Na{sub 2}CdPO{sub 4}F, discovered during the study of the phase relationships in the NaF-CdO-NaPO{sub 3} system, has been determined and compared with other Na{sub 2}M{sup II}PO{sub 4}F fluorophosphates. - Highlights: • XRD analysis of the isothermal section of the NaF-CdO-NaPO{sub 3} system at 923 K. • Rietveld refinement of the high temperature polymorph β-NaCdPO{sub 4}. • Crystal structure of the new Na{sub 2}CdPO{sub 4}F fluorophosphate determined from powder XRD. • Crystal structure - composition relationships of Na{sub 2}M{sup II}PO{sub 4}F compounds are reviewed. • IR, Raman, optical and {sup 19}F, {sup 23}Na, {sup 31}P MAS NMR characterizations of Na{sub 2}CdPO{sub 4}F.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microstructures in the 6060 aluminium alloy after various severe plastic deformation treatments

This paper presents the results concerning the microstructural refinement of the industrial 6060 aluminium alloy processed by severe plastic deformation (SPD). The high level of plastic deformation was achieved using the three methods: hydrostatic extrusion (HE), equal channel angular extrusion (ECAE) and extrusion torsion (ET), which differed in the dynamics of the loading, intensity and homogeneity of the plastic strain field. Microstructure analyses were performed before and after SPD deformation using a transmission (TEM) and a scanning electron microscope (SEM). The refined microstructures were examined qualitatively and quantitatively by the stereological methods and computer image analyses. The microstructure of the industrial 6060 aluminium alloy after deformation was characterized by an average grain size of about 0.4 {mu}m. The results show that the precipitates strongly affect the degree of refinement and the mechanism of microstructural transformations. During the SPD, the second phase particles break apart and homogenize. The HE method generates the largest increase of the volume fraction of the small primary particles. Moreover, the HE process is most effective in reducing the primary particle size. During HE and ECAE processes the second phase precipitates dissolve partially and change their shape. - Research Highlights: {yields} SPD results in a significant increase in the density of the small primary particles. {yields} SPD homogenizes the particle size distribution. {yields} HE and ECAE processes bring nano-grains in the vicinity of the primary particles. {yields} HE and ECAE processing results in the {beta}' precipitates partial dissolutions. {yields} During HE and ECAE processes the {beta}' particles change their shape.

36 MATERIALS SCIENCE↗

Microstructural characterization of high-manganese austenitic steels with different stacking fault energies

Microstructures of tensile-deformed high-manganese austenitic steels exhibiting twinning-induced plasticity were analyzed by electron backscatter diffraction pattern observation and X-ray diffraction measurement to examine the influence of differences in their stacking fault energies on twinning activity during deformation. The steel specimen with the low stacking fault energy of 15 mJ/m{sup 2} had a microstructure with a high population of mechanical twins than the steel specimen with the high stacking fault energy (25 mJ/m{sup 2}). The <111> and <100> fibers developed along the tensile axis, and mechanical twinning occurred preferentially in the <111> fiber. The Schmid factors for slip and twinning deformations can explain the origin of higher twinning activity in the <111> fiber. However, the high stacking fault energy suppresses the twinning activity even in the <111> fiber. A line profile analysis based on the X-ray diffraction data revealed the relationship between the characteristics of the deformed microstructures and the stacking fault energies of the steel specimens. Although the variation in dislocation density with the tensile deformation is not affected by the stacking fault energies, the effect of the stacking fault energies on the crystallite size refinement becomes significant with a decrease in the stacking fault energies. Moreover, the stacking fault probability, which was estimated from a peak-shift analysis of the 111 and 200 diffractions, was high for the specimen with low stacking fault energy. Regardless of the difference in the stacking fault energies of the steel specimens, the refined crystallite size has a certain correlation with the stacking fault probability, indicating that whether the deformation-induced crystallite-size refinement occurs depends directly on the stacking fault probability rather than on the stacking fault energies in the present steel specimens. - Highlights: {yields} We studied effects of stacking fault energies on deformed microstructures of steels. {yields} Correlations between texture and occurrence of mechanical twinning are discussed. {yields} Evolutions of dislocations and crystallite are analyzed by line profile analysis.

36 MATERIALS SCIENCE↗

Modification of Mg{sub 2}Si in Mg–Si alloys with gadolinium

The modification effect of gadolinium (Gd) on Mg{sub 2}Si in the hypereutectic Mg–3 wt.% Si alloy has been investigated using optical microscope, scanning electron microscope, X-ray diffraction and hardness measurements. The results indicate that the morphology of the primary Mg{sub 2}Si is changed from coarse dendrite into fine polygon with the increasing Gd content. The average size of the primary Mg{sub 2}Si significantly decreases with increasing Gd content up to 1.0 wt.%, and then slowly increases. Interestingly, when the Gd content is increased to 4.0 and 8.0 wt.%, the primary and eutectic Mg{sub 2}Si evidently decrease and even disappear. The modification and refinement of the primary Mg{sub 2}Si is mainly attributed to the poisoning effect. The GdMg{sub 2} phase in the primary Mg{sub 2}Si is obviously coarsened as the Gd content exceeds 2.0 wt.%. While the decrease and disappearance of the primary and eutectic Mg{sub 2}Si are ascribed to the formation of vast GdSi compound. Therefore, it is reasonable to conclude that proper Gd (1.0 wt.%) addition can effectively modify and refine the primary Mg{sub 2}Si. - Highlights: ► Proper Gd (1.0 wt.%) addition can effectively modify and refine the primary Mg{sub 2}Si. ► We studied the reaction feasibility between Mg and Si, Gd and Si in Mg–Gd–Si system. ► We explored the modification mechanism of Gd modifier on Mg{sub 2}Si.

36 MATERIALS SCIENCE↗

Microstructural evolution in an ultra-fine YAl{sub 2p} reinforced Mg–14Li–3Al composite during warm-rolling

The YAl{sub 2p}/MgLiAl composite prepared by stir casting was initially forged and then rolled at 200 °C to different thicknesses. The microstructural evolution in the composite during warm rolling was investigated by using transmission electron microscope (TEM). It is found that increasing rolling reduction is conducive to the uniform distribution and refinement of the YAl{sub 2} particles. The rolling deformation promoted the precipitation of an α phase, and the α precipitate is semi-coherent to the matrix with an orientation relationship to the β matrix as: (0002){sub α}‖(110){sub β}. In addition, many nano-sized YAl particles with a cubic shape were found in the matrix of the composite with a high rolling reduction due to the diffusion of Y from YAl{sub 2} to the matrix, which reacted with the Al in the matrix during warm rolling. - Highlights: • The reinforcement YAl{sub 2} particles were distributed more uniformly in the matrix and refined with increasing rolling reduction. • The rolling deformation promoted and refined the precipitation of an α phase with increasing rolling reduction. • Many nano-sized YAl phases were produced and distributed in the matrix of the composite at a high rolling reduction.

36 MATERIALS SCIENCE↗

Improved the microstructures and properties of M3:2 high-speed steel by spray forming and niobium alloying

The microstructures and properties of spray formed (SF) high-speed steels (HSSs) with or without niobium (Nb) addition were studied. Particular emphasis was placed on the effect of Nb on the solidification microstructures, decomposition of M{sub 2}C carbides, thermal stability and mechanical properties. The results show that spray forming can refine the cell size of eutectic carbides due to the rapid cooling effect during atomization. With Nb addition, further refinement of the eutectic carbides and primary austenite grains are obtained. Moreover, the Nb addition can accelerate the decomposition of M{sub 2}C carbides and increase the thermal stability of high-speed steel, and also can improve the hardness and bending strength with slightly decrease the impact toughness. The high-speed steel made by spray forming and Nb alloying can give a better tool performance compared with powder metallurgy M3:2 and commercial AISI M2 high-speed steels. - Highlights: • Spray forming can effectively refine the microstructure of M3:2 steel. • Niobium accelerates the decomposition of M{sub 2}C carbides. • Niobium increases the hardness and bending strength of spray formed M3:2 steel. • Spray-formed niobium-containing M3:2 steel has the best tool performance.

36 MATERIALS SCIENCE↗

Improving precipitation hardening behavior of Mg−Zn based alloys with Ce−Ca microalloying additions

The precipitation hardening behavior of newly developed Mg−Zn−Ca−Ce alloys, with modified texture and improved ductility, is studied to delineate the microstructural characteristics that lead to effective hardening upon ageing treatments. Advanced electron microscopy and atom probe techniques are used to analyze the structural characteristics in relevance to the hardening potential. It has been found that the formation of a new basal precipitate phase, which evolves from a single atomic layer GP zone, and is finely distributed in both under-aged and peak-aged microstructures, has a significant impact in the improvement of the hardening response compared with the base Mg−Zn alloys. It has also been found that the β′{sub 1} rod precipitates, commonly formed during ageing treatments of Mg−Zn alloys, have their size and distribution significantly refined in the Ca−Ce containing alloys. The role of alloy chemistry in the formation of the fine basal plate GP zones and the refinement in β′{sub 1} precipitation and their relationships to the hardening behavior are discussed. It is proposed that Ca microalloying governs the formation of the GP zones and the enhancement of hardening, particularly in the under-aged conditions, but that this is aided by a beneficial effect from Ce. - Highlights: • Ce−Ca microalloying additions improve hardening in Mg−Zn, over Ce or Ca alone. • Improved hardening is due to refined β′{sub 1} rods, and fine basal plate precipitates. • Atom probe tomography identifies Ca in both β′{sub 1} and the fine basal plates. • The fine basal plates originate as ordered monolayer GP zones with 1:1 Zn:Ca (at.%). • With ageing GP zones become more Zn-rich and transform to the fine basal plates.

36 MATERIALS SCIENCE↗

Effect of gadolinium addition on microstructural evolution and solidification characteristics of Al-15%Mg2Si in-situ composite

Highlights: • The Al{sub 3}Gd is the heterogeneous nucleation of primary Mg{sub 2}Si in Al-15%Mg{sub 2}Si composite. • Addition of Gd to Al-15%Mg{sub 2}Si resulted in the formation of Al{sub 2}Si{sub 2}Gd and AlSiGd intermetallic compounds. • Absorption of Gd atoms preferentially on {100} facets of Mg{sub 2}Si crystals changed its growth manners. • Primary Mg{sub 2}Si transformed from coarse-dendritic to perfect truncated octahedral shape after treating with 1.0 wt% Gd. • Gd addition increased the nucleation and growth temperatures of primary Mg{sub 2}Si. - Abstract: The current study investigated the effects of gadolinium (Gd) addition (0, 0.3, 0.5, 1.0, and 2.0 wt%) on microstructural development and solidification characteristics of hypereutectic Al-15%Mg{sub 2}Si in-situ composite. Microstructural examinations were carried out via optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), transmission electron microscopy (TEM), and electron backscattered diffraction (EBSD). The results showed that an addition of 1.0 wt% Gd, changed the morphology of primary Mg{sub 2}Si from coarse dendritic to fine truncated octahedral shape. Furthermore, the average size of primary Mg{sub 2}Si particles decreased from 40 μm to 20 μm and density increased from 495 to 1167 particles/mm{sup 2}. Besides that, cooling curve thermal analysis (CCTA) technique revealed that Gd addition increased nucleation and growth temperatures of primary Mg{sub 2}Si phase. It is proposed that modification and refinement mechanism of Gd addition are mainly attributed to formation of tiny Al{sub 3}Gd particles as the heterogeneous nucleation substrates for primary Mg{sub 2}Si, which results in a refined distribution of these particles and poisoning effect by adsorbing Gd atoms, preferentially on {100} facets of Mg{sub 2}Si crystals. Moreover, it is believed that formation of Gd intermetallic compounds is responsible for refinement of primary Mg{sub 2}Si particles.

36 MATERIALS SCIENCE↗

Grinding-induced metallurgical alterations in the binder phase of WC-Co cemented carbides

The metallic binder phase dictates the toughening behavior of WC-Co cemented carbides (hardmetals), even though it occupies a relative small fraction of the composite. Studies on deformation and phase transformation of the binder constituent are scarce. Grinding represents a key manufacturing step in machining of hardmetal tools, and is well-recognized to induce surface integrity alterations. In this work, metallurgical alterations of the binder phase in ground WC-Co cemented carbides have been assessed by a combination of electron back scattered diffraction and transmission electron microscopy techniques. The Co-base binder experiences a martensitic phase transformation from fcc to hcp crystal structure, predominantly in the first 5 μm below the surface. The hcp fraction decreases gradually along a depth of 10 μm. Surface Co displays severe plastic deformation under the highest strain, resulting in formation of nanocrystalline grains in the first micrometer below the surface. Microstructural refinement within the binder phase is observed even at greater depth. Stacking faults were detected in most of the refined grains. The metallurgical alterations of the binder phase modify the local stress distribution during grinding, which affects the discerned subsurface microcracking. The resulting residual stress profile is the sum of multiple subsurface changes, such as phase transformation, severe plastic deformation and grain refinement, where it is discerned that the depth profile of the transformed hcp-Co fraction coincides with the grinding-induced residual stress profile.

36 MATERIALS SCIENCE↗

Refine your search to explore more results.