Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “graphitization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Elevated Temperature Graphite Mechanical Testing

High purity graphite will be used for core components within most High Temperature Reactor (HTR) designs. Several "high tech” industries currently utilize synthetic, high-purity, commercially available graphite components to fabricate photovoltaic cells, semi-conductors, optical fibers, and other high value electronic industry products. New advanced HTR designs are also interested in using these graphite grades for long-term, internal core component applications. Consequently, the US Department of Energy, Advanced Reactor Technologies (DOE-ART) program has spent several years testing different high purity graphite grades for potential use within these new nuclear reactor designs. A significant part of that effort has been in the development and improvement of American Society for Testing and Materials (ASTM) test standards specifically for nuclear graphite grades. Nearly all ASTM test standards have either been developed or improved by the DOE-ART program over the past 25 years. The ART program continues to assist in the development of new ASTM test standards in support of the future commercial HTR fleet currently being designed and built in the USA. The newest effort undertaken by ART is the development of high temperature mechanical testing practices that may be acceptable for a future ASTM test standard (or guide) for this critical material property measurement.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

On the thermal oxidation of nuclear graphite relevant to high-temperature gas cooled reactors

Thermal oxidation of nuclear graphite components is highly undesirable because it can cause structural and property degradation that negatively affect a reactor's intended operation. In this work, the body of knowledge of nuclear graphite oxidation is highlighted, including when O 2 , H 2 O, and/or CO 2 are the oxidant. Oxidation conditions relevant to high-temperature gas-cooled reactors (i.e., when oxidation could occur either as an acute or chronic phenomenon) are emphasized. Here, the objective is to summarize graphite oxidation data in a practical and accessible way to inform future research and regulatory requirements. Although each grade of nuclear graphite is different, the oxidation mechanism has underlying commonalities. Although oxidation behavior is grade dependent, the general temperature dependence is well described by a sequence of elementary steps which become rate limiting. Because the regime transition temperature depends on sample microstructure, size, and oxidant supply rate, extrapolating results beyond the experimental range should be done cautiously. Gravimetric oxidation rate measurements generally replicate well. However, caution must be exercised when rates are estimated by other methods or for samples that deviate significantly in size. Air oxidation data for IG-110, NBG-18, and PCEA graphite is critically reviewed to emphasize this point. Despite the amount of experimental data, gaps remain. Sample size and shape effects are not fully explained. Data on the oxidant penetration depth are insufficient. Analytical assessments demonstrate that lower temperature oxidation does not necessarily imply that oxidation is uniform throughout the bulk. Oxidation occurs faster at higher temperature but is more localized to the exposed surface. Paradoxically, at equal mass loss percentage, low temperature oxidation leads to greater property degradation than at high temperature. The isolated effect of oxidation is important; however, a gap remains in the systematic understanding of any potential effect of neutron irradiation on graphite structure and reactivity.

36 MATERIALS SCIENCE↗

Quantification of Inactive Lithium and Solid–Electrolyte Interphase Species on Graphite Electrodes after Fast Charging

Rapid charging of Li-ion batteries is limited by lithium plating on graphite anodes, whereby Li+ ions are reduced to Li metal on the graphite particle surface instead of inserting between graphitic layers, which directly contributes to cell capacity loss because of the low reversibility of the Li plating/stripping process. Furthermore, precisely identifying the onset and amount of Li plating is therefore vital in order to remedy these issues. We demonstrate a titration technique with a detection limit of 20 nmol (5 × 10 –4 mAh) of Li that can be used to quantify inactive Li that remains on the graphite electrode after fast charging. The titration is extended to quantify the total amount of solid carbonate species and lithium acetylide (Li 2 C 2 ) within the solid–electrolyte interphase (SEI), and electrochemical modeling is used to determine the Li plating exchange current density (10 A/m 2 ) and stripping efficiency (65%) of plated Li metal on graphite. These techniques provide a highly accurate measure of the onset of Li plating and quantitative insight into graphite SEI evolution during fast charging.

25 ENERGY STORAGE↗

Design Criteria of Dilute Ether Electrolytes toward Reversible and Fast Intercalation Chemistry of Graphite Anode in Li-Ion Batteries

To date, dilute ether electrolytes have been believed to be incompatible with graphite in Li-ion batteries due to the detrimental solvent cointercalation and graphite exfoliation. Here, in this paper, we provide design criteria of dilute ether electrolytes for a reversible graphite anode based on tailoring the solvation structures and thermodynamic properties. We clarify that ether solvents can support graphite reversibly by modulating the anion. Our redesigned electrolyte consisting of a single-solvent 1,3-dioxolane (DOL) and 1 M single-salt lithium bis(fluorosulfonyl)imide (LiFSI) shows weakened Li-solvent interaction and results in an inorganic-rich solid-electrolyte interphase. Consequently, we achieved ~99.9% Coulombic efficiency with >96% capacity retention (~350 mAh/g) after 300 cycles at C/5 using natural graphite. The weakly solvated electrolyte maintains desirable transport properties, enabling better rate capability than carbonate electrolytes with an areal capacity of 2–4 mAh/cm 2 . We have demonstrated the potential of dilute ether electrolytes for facile desolvation-based intercalation chemistry in graphite, creating a viable path toward fast-charge Li batteries.

25 ENERGY STORAGE↗

Stabilizing Graphite Anode in Electrolytes with Nanoscale Anion Networking for High-Rate Lithium Storage

Graphite is the preferred anode material in commercial lithium-ion batteries (LIBs), but its limited compatibility with various organic molecules restricts the electrolyte solvent options. The primary challenge is solvent co-intercalation with Li ions, leading to graphite layer exfoliation. As a result, electrolyte selection often relies on ethylene carbonate (EC)-based solvents. Here, in this study, we introduce electrolytes featuring a nanoscale anion network ordering that hinders the liquid-phase exfoliation of graphite. This network, formed from concentrated long-chain lithium salts, traps free dioxolane (DOL) molecules, reducing the interactions between graphite particles and solvents during Li intercalation. Our findings reveal a mechanism that stabilizes graphite in otherwise unstable solvents with concentrated salts like LiTFSI, providing key insights for improving LIB performance by addressing electrolyte limitations on graphite anodes.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Metastability and Ostwald step rule in the crystallisation of diamond and graphite from molten carbon

Abstract Experimental challenges in determining the phase diagram of carbon at temperatures and pressures near the graphite-diamond-liquid triple point are often related to the persistence of metastable crystalline or glassy phases, superheated crystals, or supercooled liquids. A deeper understanding of the crystallisation kinetics of diamond and graphite is crucial for effectively interpreting the outcomes of these experiments. Here, we reveal the microscopic mechanisms of diamond and graphite nucleation from liquid carbon through molecular simulations with first-principles machine learning potentials. Our simulations accurately reproduce the experimental phase diagram of carbon near the triple point and show that liquid carbon crystallises spontaneously upon cooling. Metastable graphite crystallises in the domain of diamond thermodynamic stability at pressures above the triple point. Furthermore, whereas diamond crystallises through a classical nucleation pathway, graphite follows a two-step process in which low-density fluctuations forego ordering. Calculations of the nucleation rates of the two competing phases confirm this result and reveal a manifestation of Ostwald’s step rule, where the strong metastability of graphite hinders the transformation to the stable diamond phase. Our results provide a key to interpreting melting and recrystallisation experiments and shed light on nucleation kinetics in polymorphic materials with deep metastable states.

Science & Technology - Other Topics↗

Nano-engineering the material structure of preferentially oriented nano-graphitic carbon for making high-performance electrochemical micro-sensors

Direct synthesis of thin-film carbon nanomaterials on oxide-coated silicon substrates provides a viable pathway for building a dense array of miniaturized (micron-scale) electrochemical sensors with high performance. However, material synthesis generally involves many parameters, making material engineering based on trial and error highly inefficient. Here, we report a two-pronged strategy for producing engineered thin-film carbon nanomaterials that have a nano-graphitic structure. First, we introduce a variant of the metal-induced graphitization technique that generates micron-scale islands of nano-graphitic carbon materials directly on oxide-coated silicon substrates. A novel feature of our material synthesis is that, through substrate engineering, the orientation of graphitic planes within the film aligns preferentially with the silicon substrate. This feature allows us to use the Raman spectroscopy for quantifying structural properties of the sensor surface, where the electrochemical processes occur. Second, we find phenomenological models for predicting the amplitudes of the redox current and the sensor capacitance from the material structure, quantified by Raman. Our results indicate that the key to achieving high-performance micro-sensors from nano-graphitic carbon is to increase both the density of point defects and the size of the graphitic crystallites. Our study offers a viable strategy for building planar electrochemical micro-sensors with high-performance.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Reactor Performance and Safety Characteristics of Beryllium-Based Composite Moderators as Replacements for Graphite in mHTGRs

Here, this study evaluates beryllium-based two-phase composite moderators as an alternative to graphite in an evaluation of reactor performance and safety characteristics. Historically, modular high-temperature gas-cooled reactors (mHTGRs) use graphite as a moderator because of its high moderating ratio and reasonable thermal properties; however, graphite has unfavorable properties under irradiation, which can require component replacement and a significant radioactive waste burden. In this assessment, we explore advanced moderators comprised of magnesium oxide (MgO) as the host matrix and beryllium metal and/or beryllium oxide (Be and/or BeO) as the entrained moderating phase. For the reactor performance and thermal-hydraulic safety analysis, the core design model of the General Atomics mHTGR-350 was used to demonstrate the feasibility of a “drop-in” replacement of graphite using the beryllium-based moderators. We employed the neutronics code Serpent to analyze the moderating behavior of the composite moderators with comparisons drawn to graphite. We performed a scoping analysis of accidents for mHTGRs using RELAP to show that these moderators do not present impediments to safety and are expected to stay within temperature limits. Measured thermophysical properties of the composite moderators are used in the thermal-hydraulic assessments. Our analysis reveals that the two-phase composite MgO-matrix beryllium-based moderators are a suitable replacement for graphite.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Effects of salinity and pH on the spectral induced polarization signals of graphite particles

The electrical property of micrometre-sized graphite particles was investigated under different particle concentration, particle size, fluid conductivity and pH conditions. Due to its large internal electronic conductivity and ability to polarize under external potential field, significant enhancement of its spectral induced polarization (SIP) responses is observed when graphite is included in sand mixtures. While a small amount of graphite inclusion significantly increases the SIP response of its mixtures with sand, further concentration increase does not necessarily lead to a proportional increase of the SIP response. This is shown to be related to the formation of graphite aggregates at higher concentrations. Changes of fluid salinity have a significant effect on graphite's SIP behaviour. This includes a positive impact on normalized chargeability and imaginary conductivity, but a negative impact on chargeability and relaxation time constant. The effect of pH on the SIP response of graphite is small but shows consistent trend, where pH increase leads to a decrease of both the chargeability and relaxation time constant. The underlying cause of this effect is not clear.

58 GEOSCIENCES↗

Fully Bayesian Analysis With Model Inadequacy Correction For Nuclear Graphite Property Models With Hierarchical Variance Structure

Nuclear-grade graphites are extensively utilized in the core designs of various advanced nuclear reactors. Within the reactor environment, graphite is subjected to prolonged exposure to extreme conditions, including high temperatures, radiation, and potentially molten salt and oxygen. Such exposure can induce several degradation mechanisms in graphite, such as nonuniform volumetric strains caused by irradiation and thermal expansion, leading to stresses that may compromise the performance of graphite components. Assessing component integrity, forecasting component performance over the reactor's lifespan, and developing design standards necessitate robust tools for predicting fracture initiation and propagation in graphite structural components within nuclear reactors. This code enables the Bayesian calibration of properties for nuclear-grade graphites. Using a hierarchical Bayesian approach, multiple experimental data sources are combined to develop Gaussian process models for the properties. Using the Kennedy O'Hagan framework, the uncertainties due inadequacies in the model and the inherent spread in the experimental data are quantified.

Dhulipala, Som Lakshmi NarasimhaLakshmi Narasimha ↗

Development of a Pulsed Slowing-Down-Time Benchmark of Neutron Thermalization in Graphite

Graphite is a classic neutronic material that has been used as both a reactor reflector and moderator in various nuclear reactor systems. The ability to accurately predict the slowing down and thermalization of neutrons in graphite can have significant implications on the safety and operation of such reactor systems. In reactors, the neutron thermalization process is quantified using the thermal scattering law (TSL) and related cross sections for a given moderator. An ideal approach to assess the validity of TSL data is using benchmark measurement based on the pulsed Slowing-Down-Time technique and its comparison with the appropriate graphite nuclear library. In this work, experimental measurement and computational Monte Carlo simulations were performed to benchmark the slowing down characteristics and thermalization of neutrons in nuclear (reactor-grade) graphite. Given the density of graphite, various graphite libraries were selected for the benchmark analysis.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Progress Report on Graphite-Salt Interaction Studies (FY21)

This report summarizes the activities performed in FY21 to investigate the interactions between nuclear graphite and molten salts, such as FLiNaK. First, building on last year’s achievements, the team improved the procedure for measurements on pressurized salt intrusion in nuclear graphite and performed new experiments at variable pressures with specimens of different sizes and shapes. Additionally, the team actively provided suggestions and comments for ASTM D8091, Standard Guide for Impregnation of Graphite with Molten Salts , which came up for periodic revision in 2021. Second, the team expanded its capabilities to further characterize salt-impregnated graphite by procuring and installing a laser-induced breakdown spectroscopy (LIBS) instrument capable of producing a 3D chemical composition of a surface and subsurface region of specimens. A methodology for accurately analyzing information was developed, and a manuscript was submitted for publication. The LIBS instrument sample cell is sealed in controlled inert atmosphere, which is an advantage for using humidity-sensitive samples and Be-contaminated samples. This aligns with the team’s effort to expand the capabilities of handling FLiBe and Becontaining materials in two newly installed glovebox units. Third, the team performed preliminary tribology tests for pebble graphite wear in contact with stainless steel in dry state and in molten salt at high temperature. These tests are needed to establish the baseline for the wear of pebble graphite by friction against metallic walls. The friction and wear of pebbles in the fluoride salt-cooled hightemperature reactor are expected to generate dust, which is a concern for other components’ properties and safe reactor operation.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Synthesizing Highly Crystalline Graphite Powder from Bulk Polyethylene Waste for Lithium-Ion Battery Anodes

Upcycling plastic waste into graphite can potentially be used, in conjunction with other methods, to manage existing waste materials and diversify graphite supply chains. However, synthesizing large quantities of crystalline graphite powder from plastic waste, particularly polyethylene (PE), remains a challenge because PE decomposes into light gases during thermal processing, and simple methods do not exist at any appreciable size scale to address this challenge. In this work, a method is developed for air processing bulk forms of PE waste to create a stable carbon char that does not readily decompose during high-temperature processing. This method employs solid additives in the form of salts, which are combined with the PE melt during air processing to increase the effective surface area of the melt and improve the oxygen-driven chemistry that stabilizes the PE for high-temperature processing. After removing the solid salt additives from the PE-derived char, it is converted into a highly crystalline bulk graphite powder using a Fe-based low-temperature (<1500 °C) catalytic process. The PE-derived graphite powder showed excellent electrochemical performance as an anode material for lithium-ion batteries (LIBs) with a capacity of up to 302 mAh/g at 0.5 discharge/charge cycles per hour (0.5 C) and capacity retention of 100% after 415 cycles. This method illustrates there are opportunities for upcycling large quantities of PE waste to produce graphite powders.

Huynh, Ngoc Tien [NETL Site Support Contractor, Na↗

Adsorption of carbon monoxide and hydrogen on graphite.

Adsorption of carbon monoxide and hydrogen was investigated on three graphites: a high-density pyrolytic graphite, a small-grain extruded graphite, and a processed pyrolytic graphite tape. The sticking probability of CO was found to decrease rapidly as the average surface coverage approached 0.01 monolayer. Lower sticking probabilities were observed on the highly oriented pyrolytic graphite which indicated that adsorption occurs principally on the edge atoms. There is negligible adsorption of molecular hydrogen on graphite that has been heated to 2400 K in vacuo.

Beitel, G. A.↗

The action of macrosounds on graphite ore and derived products

A suspension of graphite ore, floated graphite, and the gangue left over from flotation were subjected to the action of macrosounds under determinant conditions. The following was found: (1) The graphite ore undergoes an efficient settling action. (2) The floated graphite is strongly crushed down to the dimensions of colloidal graphite. (3) The gangue left over from flotation can be further processed to recuperate graphite from its nuclei.

Bradeteanu, C.↗

Friction and wear of metals in contact with pyrolytic graphite

Sliding friction experiments were conducted with gold, iron, and tantalum single crystals sliding on prismatic and basal orientations of pyrolytic graphite in various environments, including vacuum, oxygen, water vapor, nitrogen, and hydrogen bromide. Surfaces were examined in the clean state and with various adsorbates present on the graphite surfaces. Auger and LEED spectroscopy, SEM, and EDXA were used to characterize the graphite surfaces. Results indicate that the prismatic and basal orientations do not contain nor do they chemisorb oxygen, water vapor, acetylene, or hydrogen bromide. All three metals exhibited higher friction on the prismatic than on the basal orientation and these metals transferred to the atomically clean prismatic orientation of pyrolytic graphite. No metal transfer to the graphite was observed in the presence of adsorbates at 760 torr. Ion bombardment of the graphite surface with nitrogen ions resulted in the adherence of nitrogen to the surface.

Buckley, D. H.↗

Graphite and ablative material response to CO2 laser, carbon-arc, and xenon-arc radiation

The behavior was investigated of graphite and several charring ablators in a variety of high-radiative heat-flux environments. A commercial-grade graphite and nine state-of-the-art charring ablators were subjected to various radiative environments produced by a CO2 laser and a carbon arc. Graphite was also tested in xenon-arc radiation. Heat-flux levels ranged from 10 to 47 MW/sq m. Tests were conducted in air, nitrogen, helium, and a CO2-N2 mixture which simulated the Venus atmosphere. The experimental results were compared with theoretical results obtained with a one-dimensional charring-ablator analysis and a two-dimensional subliming-ablator analysis. Neither the graphite nor the charring ablators showed significant differences in appearance or microstructure after testing in the different radiative environments. The performance of phenolic nylon and graphite was predicted satisfactorily with existing analyses and published material property data. Good agreement between experimental and analytical results was obtained by using sublimation parameters from a chemical nonequilibrium analysis of graphite sublimation. Some charring ablators performed reasonably well and could withstand radiative fluxes of the level encountered in certain planetary entries. Other materials showed excessive surface recession and/or large amounts of cracking and spalling, and appear to be unsuitable for severe radiative environments.

Brewer, W. D.↗

Mechanisms of graphite fluoride /CFx/n lubrication

Friction, wear and wear life results were compared with optical microscope observations as a function of sliding distance for graphite fluoride rubbed films applied to three surface finishes - polished, sanded and sandblasted. The lubricating process consisted of the plastic flow of thin films of graphite fluoride between flat areas on the rider and on the metallic substrate. If the substrate was rough, flat areas were created during run-in, and the graphite fluoride (CFx)n flowed across them. Wear life was enhanced by restricting radial (or transverse) flow of the graphite fluoride from the contact region by increasing surface roughness. Valleys in the roughened substrate surface served as a reservoir for graphite fluoride and as a deposit site for wear debris. Failure resulted from the gradual depletion of graphite fluoride from the contact region with the subsequent formation of powdery metallic debris that covered both rider and disk surfaces

Fusaro, R. L.↗