Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “cracking temperature”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

A predictive modeling tool for damage analysis and design of hydrogen storage composite pressure vessels

In this study, a predictive modeling tool is developed for damage analysis and design of hydrogen (H 2 ) storage composite pressure vessels. It integrates micromechanics of matrix cracking into a continuum damage mechanics (CDM) description for damage evolution, and three-dimensional (3D) finite element (FE) modeling of the vessel structural response. At the scale of the composite layer (mesoscale), the temperature-dependent stiffness reduction law in terms of the damage variable for transverse matrix cracking is computed using an Eshelby-Mori-Tanaka approach for the initial composite thermoelastic properties and a self-consistent model for the stiffness reduction as a function of the damage variable. While transverse matrix cracking obeying a damage evolution relation can progressively evolve from an initiation to a saturation state, fiber failure is predicted by a micromechanical fiber rupture criterion that accounts for the fiber strength and matrix stress. The implementation of this integrated multiscale modeling model into a 3D FE formulation enables damage analysis and design of H 2 storage composite pressure vessels. The developed tool is illustrated through 3D damage analyses of a cryogenically compressed H 2 storage vessel model subjected to thermomechanical loadings to investigate effects of the helical layer fiber orientation and loading scenario on damage development, vessel integrity and burst pressure.

08 HYDROGEN↗

Guidelines for IAEA Small Specimen Test Techniques Master Curve Fracture Toughness Testing

Under the auspices of International Atomic Energy Agency (IAEA), a coordinated research project (CRP) entitled “Towards the Standardization of Small Specimen Test Techniques for Fusion Applications” has started since 2017. The overall objective of the project is to provide a set of guidelines for small specimen test techniques (SSTT) based on commonly agreed best practices on main test techniques including tensile, creep, low cycle fatigue, fracture toughness, and fatigue crack growth rate. This will act as the first step of a full standardization of the SSTT. Fusion structural materials, i.e., reduced activation ferritic/martensitic (RAFM) steels, are used for testing. In addition, the project will create a comprehensive mechanical property database of RAFM steels tested by SSTT. For the fracture toughness task of the CRP, three testing methods including Master Curve, local approach for ductile crack growth and cleavage fracture, and ductile approach at room temperature will be evaluated. This report focuses on developing guidelines for the round-robin Master Curve testing based on the ASTM standard E1921-19b “Standard Test Method for Determination of Reference Temperature, T 0 , for Ferritic Steels in the Transition Range” and commonly agreed best practice from researchers at Oak Ridge National Laboratory (ORNL), Centre for Energy, Environment and Technology (CIEMAT), and UK Atomic Energy Authority (UKAEA).

36 MATERIALS SCIENCE↗

Anisotropic thermal-conductivity degradation in the phase-field method accounting for crack directionality

Dynamic loads applied to metals may lead to brittle or ductile fracture depending on the imposed strain rates, material properties, and specimen geometry. With an increase in the applied velocity, brittle to ductile failure mode transition may also be observed. Furthermore, at high strain rates, ductile fracture may be preceded by shear bands, which are narrow bands of intense plastic deformation, typically accompanied by a significant rise in temperature. Reliable models are needed to predict the response of metals subject to dynamic loads. In particular, capturing the interplay between heat conduction and crack propagation using the phase-field fracture method is still an open research field. To accurately capture the heat transfer physics across crack surfaces, damage models degrading thermal-conductivity are necessary. While isotropic thermal-conductivity degradation models were proposed, they may lead to errors as they are indifferent to crack directionality. In our current work, a new anisotropic approach is proposed in which thermal-conductivity, which depends on the phase-field gradient, is degraded solely across the crack. Here, it is shown that this approach improves the near-field approximation of temperature and heat flux compared with isotropic degradation, when taking the discontinuous crack solutions as reference. Additionally, the anisotropic degradation approach is implemented in a unified dynamic fracture model and a couple of examples demonstrate the viability of this approach.

42 ENGINEERING↗

Complete Optimization of LPBF Ni-Based Alloys Down-Selected from FY23 Candidate Materials Including, Thermodynamic Modeling, Sample Fabrication and Microstructure Characterization

The goal of the Advanced Materials and Manufacturing Technologies (AMMT) program is to accelerate the incorporation of new materials and manufacturing technologies into advanced nuclear-related systems. Although 316H stainless steel fabricated by laser powder bed fusion (LPBF) has already been identified as an alloy that could have a significant effect on various reactor technologies, many other materials and manufacturing techniques are being evaluated. Nickel-based alloys typically offer higher-temperature capabilities compared with advanced stainless steels, and previous reports looked at three Ni-based alloy categories: low-Co alloys with a potential use close to the reactor core; high-temperature, high-strength alloys; and molten salt–compatible alloys. In the first category, alloy 718 was studied in 2023, and creep testing at 600°C and 650°C revealed that the alloy exhibited great creep strength after the appropriate annealing but had low ductility. Advanced characterization was recently conducted to highlight the presence of strengthening γ' and γ" precipitates after creep testing and to show that brittle phases at grain boundaries might explain the low ductility of LPBF 718 compared with wrought 718. For the high-temperature, high-strength alloys, previously purchased powders of alloys 617, 230, and 625 were used to assess the printability of these three solution-strengthened alloys. Hot cracking could not be suppressed for alloy 617 and 230, and it was shown that these cracks, which were elongated along the build direction (BD), had a drastic effect on the ductility of alloy 230 at room temperature when specimens were machined perpendicular to the BD. On the contrary, LPBF printing of crack-free alloy 625 was achieved using similar printing parameters, and the alloy looked like a promising candidate for various reactor technologies. The fabrication of alloy 282 by LPBF, a γ'-strengthened alloy with great creep strength up to 800°C, was performed in 2023, and x-ray computed tomography (XCT) scans of the alloy before and after creep testing at 750°C were carried out to assess the effect of flaws on the alloy’s creep behavior. Correlation between the flaws’ volume fraction, creep ductility, and creep lifetime could be established, and future work on LPBF 625 will take full advantage of in situ printing data and ex situ XCT scans to accelerate the alloy qualification. Finally, single track experiments were performed on the two alloys previously identified as good molten salt–resistant, Ni-based candidates: Hastelloy N and 244. Various laser parameters were considered, and cracking was not observed for either of the two alloys. Wrought 244 offers better creep strength and molten salt compatibility than alloy 625, and future work will aim to establish the alloy LPBF processing window.

36 MATERIALS SCIENCE↗

Fabrication of yttrium hydride for high-temperature moderator application

We report given the superior thermal stability and highly attainable hydrogen density, yttrium hydride is an excellent high-temperature moderator material in advanced thermal neutron spectrum reactors that require small core volumes. Large-scale, crack-free, bulk yttrium hydride is in high demand; however, fabrication of yttrium hydride is challenging and has not been demonstrated for nearly half century. The associated challenges are discussed herein. In response to these challenges, a hydriding system was designed and constructed at Oak Ridge National Laboratory and was used to successfully fabricate crack-free yttrium hydride in complex geometries at large scales. This was accomplished by precisely controlling the hydrogen’s partial pressure and the retort temperature, which was informed by the well-established thermodynamic properties of the binary H–Y system. Hydrogen content in as-fabricated hydride was determined by weight change, an approach which was considered reliable based on the use of ultra–high-purity yttrium, the absence of oxide phases up to levels detectable using x-ray diffraction (XRD), and the significant weight gain. Hydrogen distribution along one yttrium hydride rod was evaluated with XRD analysis on materials extracted from different locations on the rod. The results indicated a relatively homogeneous hydrogen distribution along the hydride rod, with <3% uncertainty in the fraction of the δ-phase hydride. In addition, significant efforts are being dedicated to establish a complete database summarizing the thermomechanical and physical properties of as-fabricated yttrium hydride and the irradiation response to facilitate its deployment as a high-temperature moderator in advanced nuclear reactors.

36 MATERIALS SCIENCE↗

Design rules for 316H nuclear components cladded with nickel or tungsten

The existing Class A metallic materials qualified in the ASME Boiler & Pressure Vessel Code Section III, Division 5 rules for high temperature nuclear reactors are not ideally suited for long term molten salt corrosion resistance in high temperature molten salt reactors. Potentially, corrosion or corrosion driven environmentally assisted cracking could limit the design life of structural components in molten salt reactors. A solution to this limitation is the use of cladded components – overlay the Class A material with a thin layer of some non-qualified, corrosion-resistant material. However, this necessitates the development of design methods for cladded components that do not require long-term testing of clad materials in order to support the near-term deployment of molten salt reactors. This report develops such a methodology along with a complete set of rules presented in a format compatible with an ASME nuclear Code Case. These design rules are for 316H Class A components cladded with either nickel or tungsten. The report also discusses the development of a set of general criteria for selecting clad materials beyond the specific 316H/tungsten and 316H/nickel systems and general acceptance tests for checking the mechanical integrity of the clad/base metal interface. Finally, the report includes a set of fully-documented sample problems detailing the application of the rules to high temperature cladded components

36 MATERIALS SCIENCE↗

Materials Degradation in Extreme Environments: Novel In-situ Measurements of Cracking in Molten Salt

The safety and reliability of next-gen reactors, i.e. molten salt reactors (MSR), depends on materials performance and longevity in extreme environments, yet no in-situ, validated measurement techniques for environmentally assisted cracking (EAC), one potential degradation mechanism, exist for these conditions. This project combined the use of in-situ direct current potential drop (DCPD) crack growth rate determination applied to a horizontal load frame with high temperature fittings and novel sample geometries to enable evaluation in MSR environments and develop a full in-situ SCC measurement capability for extreme environments (high conductivity and elevated T), necessary to predict materials reliability. A successful demonstration of DCPD measurement in molten NaNO 3 /KNO 3 salts at 340 o C was accomplished and validated through post-test fractography imaging. This is the first ever public example, to the authors knowledge, of an in-situ crack growth rate measurement in a molten salt environment.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Effect of post-weld heat treatment on microstructure and mechanical properties of rotary inertia friction welded dissimilar 422-4140 martensitic steel piston joints

The study investigated how post‐weld heat treatment (PWHT) temperature affects the microstructure and localized deformation/fracture during bend testing of rotary inertia friction welds (RIFW) between AISI 422 stainless steel and AISI 4140 steel. RIFW produced a fully martensitic interface with approximately 550 HV hardness in both the thermo-mechanically affected (TMAZ) and heat‐affected zones (HAZ). Due to differences in temper resistance, the 4140 TMAZ/HAZ softened progressively under PWHT temperatures from 525 °C to 700 °C, while the 422 TMAZ unexpectedly maintained about 550 HV up to 600 °C before significantly softening at temperatures ≥625 °C. This asymmetric softening generated steep hardness gradients across the interface at temperatures ≤600 °C. Furthermore, carbon migration across the interface was minimal up to 600 °C, moderate at 625 °C, and by 700 °C produced a carbide‐rich eutectoid layer in the 422 TMAZ alongside a carbon‐depleted soft ferrite layer in the 4140 TMAZ. Strain during bending was PWHT‐dependent, concentrating on the 4140 side; in as-welded joints, the high hardness led to deformation and crack initiation in the base metals, whereas in PWHT samples, cracking initiated in the softened 4140 TMAZ near the interface. The intermediate PWHT temperature of 625 °C offered the best balance of limited carbon diffusion across the interface, relatively low peak weld hardness and minimized hardness gradients across the interface, more homogenous deformation, and good bend test performance.

4140 low-alloy steel↗

Fission gas retention of densely packed uranium carbonitride tristructural-isotropic fuel particles in a 3D printed SiC matrix

The Transformational Challenge Reactor (TCR) fuel form was designed to contain large, densely packed uranium carbonitride (UCN) tristructural-isotropic (TRISO) fuel particles within a 3D printed SiC matrix, increasing the uranium density compared to conventional TRISO fuel forms and offering full geometric freedom for core design. Here, this work summarizes initial low-burnup, high-power irradiation testing of TCR fuel materials, including loose UCN TRISO particles and integral fuel compacts with ~55% TRISO particles by volume, to evaluate fission gas retention. Fission gasses were fully retained in all loose particle tests and in integral compacts irradiated at low (<250 °C) surface temperatures. Initial testing at higher (~700–750 °C) fuel surface temperatures showed fission gas release (FGR) and complete fracture of three compacts, but no FGR was observed in later high temperature tests (~300–750 °C) of both fueled compacts and loose TRISO particles. Calculated thermal stresses in the failed compacts were far less than the measured strength of the SiC matrix and the stresses in some failed compacts were less than those in compacts that did not show FGR. Thermal stress-induced matrix cracks also would not cause complete fracture because the tensile stresses transition to compression in the higher temperature regions. Therefore, fuel failure was likely not caused by thermal stresses and may have been related to leakage currents from the electrical heaters and erratic fuel surface temperatures that were only observed in the test for which failure was observed. In any case, the matrix cracks propagated through the coatings of TRISO particles located in the high-density matrix regions on the peripheries of the compacts, resulting in measurable fission gas release. The discussion focuses on the importance of understanding matrix density distributions and the particle-matrix interface properties to prevent matrix cracks from causing TRISO particle failures.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Tacky Elastomers to Enable Tear-Resistant and Autonomous Self-Healing Semiconductor Composites

Mechanical failure of π-conjugated polymer thin films is unavoidable under cyclic loading conditions, due to intrinsic defects and poor resistance to crack propagation. Here, the first tear-resistant and room-temperature self-healable semiconducting composite is presented, consisting of conjugated polymers and butyl rubber elastomers. This new composite displays both a record-low elastic modulus (<1 MPa) and ultrahigh deformability with fracture strain above 800%. More importantly, failure behavior is not sensitive to precut notches under deformation. Autonomous self-healing at room temperature, both mechanical and electronic, is demonstrated through the physical contact of two separate films. The composite film also shows device stability in the ambient environment over 5 months due to much-improved barrier property to both oxygen and water. Butyl rubber is broadly applicable to various p-type and n-type semiconducting polymers for fabricating self-healable electronics to provide new resilient electronics that mimic the tear resistance and healable property of human skin.

36 MATERIALS SCIENCE↗

Joining of High Strength Low Ductility AA7055 by Friction Self-piercing Rivet

High strength aluminum (Al) alloy is one of higher specific strength materials for decarbonization in transportation industries. Because of low ductility at room temperature, conventional mechanical fastening such as self-piercing riveting produces cracks at the joint. In this work, we applied friction self-piercing riveting to join Al alloy (AA) 7055. No cracks were observed in the joints because of the improved local ductility of Al alloy by the generated frictional heat during joining step. Numerical modeling of joining process was applied to guide rivet geometry design and rivet material strength. Mechanical integrity of the AA7055 joints was assessed by lap shear tensile and cross-tension testing. Metallurgical characterizations revealed solid-state bonding formed not only between the rivet and surround Al materials, but also upper and lower Al sheets at the joint interface. Both solid-state bonding and mechanical interlocking between the flared rivet and bottom AA7055 sheet were the major joint mechanisms.

Lim, Yong Chae↗

The role of catalyst acidity and microstructure on light olefin selectivity in polyethylene deconstruction in short contact time pulse Joule-heated reactors

The growing volume of plastics waste, compounded with a low recycling rate, has led to an alarming amount of plastics ending up in landfills or being incinerated. While pyrolysis offers a route for plastic waste deconstruction, its product distribution is often broad and poorly controlled due to unselective radical chemistry at high temperatures. We recently demonstrated that rapid pulse Joule-heated catalytic cracking over HZSM-5, combined with small fractions of steam, can achieve high selectivity (>80 %) toward C 2 -C 4 olefins, while significantly reducing coking compared to continuous Joule heating. Here, we investigate how acid catalyst properties, such as silica/alumina ratio, zeolite topology, and catalyst porosity, influence light olefin selectivity during polyethylene deconstruction via rapid pulse Joule heating. We demonstrate that silica-to-alumina ratios of ∼30 yield high light olefin selectivity, and small-pore zeolites favor light olefins at the expense of increased coke formation. To mitigate coking, we synthesize HZSM-5 nanosheets and hierarchical zeolites (MFI, FAU, and CHA). Furthermore, these catalysts achieve an ethylene selectivity of approximately 35 %, a twofold increase over prior catalytic pyrolysis. Additionally, co-feeding steam and incorporating hierarchical porosity reduce coke formation and enhance catalyst stability.

Catalytic cracking↗

Design and development of a high-performance Ni-based superalloy WSU 150 for additive manufacturing

This work proposes a design and development strategy of a new nickel-based superalloy for additive manufacturing. A new Ni-based superalloy has been developed by the application of the combinatorial alloy development technique coupled with CALPHAD based solidification modeling by effectively suppressing the precipitation kinetics. The suppression of precipitation during processing paved a way for prevention of cracks during deposition. The new alloy "WSU 150" revealed excellent room temperature mechanical properties with a yield strength of 867 MPa, an ultimate tensile strength of 1188 MPa, and an elongation of 27.9% in the as-deposited condition. The mechanical properties of the heat-treated alloy were improved significantly to 1114 MPa yield strength, 1396 MPa ultimate tensile strength, and an elongation of 16.1%. Improvement in the mechanical properties is attributed to the additional precipitation and coarsening of γ' and carbides during heat-treatment. Microstructural investigation of the alloy revealed spherical γ' with a rippled size distribution from the center to the interdendritic region. The average size of the γ' particles in the as-deposited condition was found to be around 48 nm in the interdendritic region. Heat-treatment promoted the coarsening of γ' which is explained in the paper.

36 MATERIALS SCIENCE↗

Residual Stress Modeling and Advanced Diffraction Measurements of 347H Steel Weldments

The 347H stainless steel is a primary high-temperature material for many energy and power generation industries. Stress relief cracking (SRC) has been a particular concern in welding of this material. The residual stress induced by welding and its evolution during post-welding heat treatment (PWHT) and subsequent operating and service conditions is one of the primary factors contributing to SRC. The lifetime of welded structure components is also controlled by the precipitation kinetics that accompanies PWHT, stress relaxation process, and long-term aging and complex synergistic factors. Various theories have been proposed in the past to explain SRC. However, a widely accepted approach to predicting the entire damage evolution and the resulting performance reduction is still lacking. This study is to demonstrate a reliable solution for two critical issues that affect the predictions. First, the residual stress distribution obtained from both simulation and neutron diffraction is compared, which increases the accuracy of mechanical analysis simulation model and therefore builds a solid basis for the lifetime prediction model. Second, the generation, evolution, and annihilation of precipitates are monitored by the synchrotron diffraction experiment. Preliminary results demonstrate the critical importance of precipitation kinetics on the residual stress distribution/redistribution during heat treatments.

Yang, Yi↗

Multiphase representation of hotspot formation and growth

Multiphase reacting flow approach has been adopted for modeling of hotspot formation and growth on sub-zonal scale. Mechanical response of the high explosive (HE) is modeled by the Visco-Plastic SCRAM model which includes plastic work, crack growth, and frictional heating along the cracks. In this work a sub-zonal regions with high temperature, hotspots, are modeled as a new phase. Formation and growth of the hotspot phase from the cold phase is modeled as a phase change. Each phase has its own temperature and pressure. Chemical reactions also progress in both phases. The growth of hotspots are determined by the solution of the heat conduction equation with appropriate heat sources due to friction and plastic heating. Sample calculations using the BABBO code show successful detonation calculations with hotspot formation and growth.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Feasibility of an Accelerometer-Based Structural Health Monitoring System for the LANL Blast Tube

A modeling- and simulation-based study was conducted on the feasibility of implementing an accelerometer-based SHM system on the Los Alamos National Laboratory blast tube. A blast tube experiment was modeled using the Abaqus explicit finite element solver. A custom user subroutine was written to apply test-like pressure loading to the inside surface of the blast tube. The subroutine applies analytically defined pressure loads derived from tracer output taken from a Compressible Flow Computational Fluid Dynamics Solver model of the blast tube. Five unique versions of the model were created: an undamaged reference model at 65°F was used as the baseline and compared to equivalent models at 10°F and 100°F. These three models were compared to models with small damage at the reference temperature. The two types of damage considered were a radial (circumferential) crack in the main tube body and a longitudinal crack in the supports. Acceleration outputs were extracted from accelerometer bodies included in the model and were post processed using a variety of standard SHM techniques. Different potential features signaling failure were extracted and compared using statistical methods in the time and frequency domains. A method was identified that clearly shows that differences in structural response resulting from the modeled damage can be differentiated from the structural response resulting from changing environmental conditions. However, the amount of damage applied to create observable differences in the accelerometer data was so large that simpler methods of damage detection would be more cost effective in locating damage.

42 ENGINEERING↗

THE DESIGN OF LAYER TIME OPTIMIZATION IN LARGE SCALE ADDITIVE MANUFACTURING WITH FIBER REINFORCED POLYMER COMPOSITES

In this study, we have developed a method to optimize a layer deposition time (a.k.a. layer time) for large-scale additive manufacturing (AM) via physics-based simulations. A long layer time leads to an over-cooled surface on which a new layer is deposited, and therefore, it may result in a weak bonding or debonding between layers, cracking, or warping. A short layer time leads to a high temperature of the structure due to insufficient cooling, and therefore, the structure may not be stiff enough and may collapse during manufacturing. Therefore, it is important to estimate the optimal layer time in additive manufacturing for a high-quality product. The temperature of a top layer right before deposition is recommended to be slightly higher than the glass temperature of the material. A temperature cooling was approximated to an exponential function of time, and the optimized layer time was obtained based on a target temperature while maintaining a minimal printing time. The material used is carbon fiber-reinforced polycarbonate (CF/PC), and the large-scale deposition system used is LSAM TM from Thermwood Corporation. Three different layer time cases were used for experiments, and a series of thermal images were obtained via an infra-red (IR) camera during the entire AM processes. AM process simulations were performed using a finite element method and the temperature profiles from the simulation were in good agreement with those from experiments. The layer time optimization was performed based on the temperature profiles from the simulations. A layer temperature with the optimal layer time was confirmed as the target temperature through simulation.

Jo, Eonyeon↗