Publisher's Note: Predicted band structures of III-V semiconductors in the wurtzite phase [Phys. Rev. B 81, 155210 (2010)]
No abstract prepared.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
No abstract prepared.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Not provided.
Not Available
Explore the source record for details and available documents.
N/A
Abstract not provided
Abstract not provided
Research in the area of polar semiconductor heterostructures has been growing rapidly, driven in large part by interest in two-dimensional electron gas (2DEG) systems. 2DEGs are known to form at heterojunction interfaces that bear polarization gradients. They can display extremely high electron mobilities, especially at low temperatures, owing to spatial confinement of carrier motions. Recent reports of 2DEG behaviors in Ga{sub 1-x}Al{sub x}N/GaN and Zn{sub 1-x}Mg{sub x}O/ZnO heterostructures have great significance for the development of quantum Hall devices and novel high-electron-mobility transistors (HEMTs). 2DEG structures are usually designed by interfacing a polar semiconductor with its less or more polar alloys in an epitaxial manner. Since the quality of the 2DEG depends critically on interface perfection, as well as the polarization gradient at the heterojunction, understanding compositional and structural details of the parent and alloy semiconductors is an important component in 2DEG design and fabrication. Zn{sub 1-x}Mg{sub x}O/ZnO is one of the most promising heterostructure types for studies of 2DEGs, due to the large polarization of ZnO, the relatively small lattice mismatch, and the large conduction band offsets in the Zn{sub 1-x}Mg{sub x}O/ZnO heterointerface. Although 2DEG formation in Zn{sub 1-x}Mg{sub x}O/ZnO heterostructures have been researched for some time, a clear understanding of the alloy structure of Zn{sub 1-x}Mg{sub x}O is currently lacking. Here, we conduct a detailed and more precise study of the local structure of Zn{sub 1-x}Mg{sub x}O alloys using Raman and solid-state nuclear magnetic resonance (NMR), in conjunction with neutron diffraction techniques.
ScN has attracted great attention for its electronic properties and its ability to enhance polarization of AlN; however, its sister compounds, YN and LaN, remain much less studied. Here, we use first-principles calculations to evaluate YN and LaN in their cubic and hexagonal phases. Rocksalt YN and LaN are semiconductors, although we show that LaN differs from ScN and YN in having a direct band gap, which we attribute to its weaker p-p coupling. Both have low electron effective masses. In addition to their rocksalt structures, we evaluate the layered hexagonal and wurtzite phases of YN and LaN. For YN, the wurtzite phase cannot be stabilized, and hexagonal YN is higher in energy than rocksalt YN. In contrast, for LaN, the wurtzite phase is favored, and it is comparable in energy to rocksalt LaN. Wurtzite LaN has a polarization of 0.608 C/m 2 (referenced to the centrosymmetric layered hexagonal phase), and a high piezoelectric coefficient e 33 = 1.78 C/m 2 . Interestingly, we find that the polarization of wurtzite LaN may be reversible; we find a relatively small switching barrier of 0.06 eV per formula unit, offering the potential for its use as a ferroelectric. Since wurtzite LaN is closely lattice matched to InP, we investigate a heterostructure between (0001) wurtzite LaN and (111) zinc-blende InP, and find the polarization discontinuity would yield a bound charge of 1.3 × 10 14 e/cm 2 , offering the potential for novel electronic applications such as tunnel junctions. Furthermore, our results compare and contrast ScN, YN, and LaN, and highlight the potential of these materials for adoption in electronic and ferroelectric devices.
The structural variation in the x(LiGaO{sub 2}){sub 1/2}(1-x)ZnO alloy system was studied by powder XRD, TEM-SAD and Raman spectroscopy. It was elucidated that the phase varied upon increasing the alloying level was the wurtzite-type for 0{<=}x<0.2, the Zn{sub 2}LiGaO{sub 4}-type for 0.2{<=}x{<=}0.5 and the {beta}-LiGaO{sub 2}-type for 0.8{<=}x{<=}1, and the 0.5<x<0.8 region was the immiscible region of ZnO with LiGaO{sub 2}. The solubility limit of LiGaO{sub 2} in ZnO was explained by the c{sub 0}/a{sub 0} ratio based on the fact that there is no binary wurtzite phase for a c{sub 0}/a{sub 0} less than 1.6. The optical phonons of wurtzite and its derived phase were simply explained by the lattice shrinkage and reduced mass upon reduction the alloying of ZnO with LiGaO{sub 2}. The bowing parameter of the optical band gap of y(Zn{sub 2}LiGaO{sub 4}){sub 1/4}(1-y)ZnO was determined to be 0.67 eV. The value was very low, and it was related to the small lattice and chemical mismatches between the Zn{sub 2}LiGaO{sub 4} and ZnO. - Graphical abstract: The structure of ZnO varied upon alloying with LiGaO{sub 2}. Highlights: Black-Right-Pointing-Pointer We studied structural variation in the x(LiGaO{sub 2}){sub 1/2}(1-x)ZnO alloy system. Black-Right-Pointing-Pointer The wurtzite- and its related Zn{sub 2}LiGaO{sub 4}-type phase appeared for 0{<=}x{<=}0.5. Black-Right-Pointing-Pointer The solubility limit of LiGaO{sub 2} in ZnO was related to the wurtzite c{sub 0}/a{sub 0} ratio. Black-Right-Pointing-Pointer The energy band gap of ZnO was widened up to 4.04 keV by the alloying with LiGaO{sub 2}. Black-Right-Pointing-Pointer The bowing parameter of y(Zn{sub 2}LiGaO{sub 4}){sub 1/4}(1-y)ZnO was determined to be 0.67 eV.
ZnSe nanowires with a dominant wurtzite structure have been grown at low temperature (300 °C) by molecular beam epitaxy assisted by solid Au nanoparticles. The nanowires emission is polarized perpendicularly to their axis in agreement with the wurtzite selection rules. Alternations of wurtzite and zinc-blende regions have been observed by transmission electron microscopy, and their impact on the nanowires optical properties has been studied by microphotoluminescence. The nanowires show a dominant intense near-band-edge emission as well as the ZnSe wurtzite free exciton line. A type II band alignment between zinc-blende and wurtzite ZnSe is evidenced by time-resolved photoluminescence. From this measurement, we deduce values for the conduction and valence band offsets of 98 and 50 meV, respectively.
We reported long-range ferromagnetic interactions in La doped Zn{sub 0.95}Fe{sub 0.05}O nanoparticles that mediated through lattice defects or vacancies. Zn{sub 0.92}Fe{sub 0.05}La{sub 0.03}O (ZFLaO53) nanoparticles were synthesized by a sol–gel process. X-ray fluorescence spectrum of ZFLaO53 detects the weight percentage of Zn, Fe, La and O. X-ray diffraction shows the hexagonal Wurtzite ZnO phase. The Rietveld refinement has been used to calculate the lattice parameters and the position of Zn, Fe, La and O atoms in the Wurtzite unit cell. The average size of ZFLaO53 nanoparticles is 99 nm. The agglomeration type product due to OH ions with La results into ZnO nanoparticles than nanorods that found in pure ZnO and Zn{sub 0.95}Fe{sub 0.05}O sample. The effect of doping concentration to induce Wurtzite ZnO structure and lattice defects has been analyzed by Raman active vibrational modes. Photoluminescence spectra show an abnormal emission in both UV and visible region, and a blue shift at near band edge is formed with doping. The room temperature magnetic measurement result into weak ferromagnetism but pure ZnO is diamagnetic. However, the temperature dependent magnetic measurement using zero-field and field cooling at dc magnetizing field 500 Oe induces long-range ferromagnetic ordering. It results into antiferromagnetic Neel temperature of ZFLaO53 at around 42 K. The magnetic hysteresis is also measured at 200, 100, 50 and 10 K measurement that indicate enhancement in ferromagnetism at low temperature. Overall, the La doping into Zn{sub 0.95}Fe{sub 0.05}O results into enhanced antiferromagnetic interaction as well as lattice defects/vacancies. The role of the oxygen vacancy as the dominant defects in doped ZnO must form Bound magnetic polarons has been described. - Graphical abstract: The long-range ferromagnetic order in Zn{sub 0.92}Fe{sub 0.05}La{sub 0.03}O nanoparticles at low temperature measurements involves oxygen vacancy as the medium of magnetic interactions. - Highlights: • The La and Fe doping into ZnO nanoparticles induce defects in terms of oxygen vacancy. • The La ions in Fe substituted ZnO formed nanoparticles than nanorods. • Antiferromagnetic interactions are observed at room temperature magnetic measurement. • Rietveld analysis evaluated structural deformation in the Wurtzite ZnO lattice.
Future spintronics technologies based on diluted magnetic semiconductors (DMS) will rely heavily on a sound understanding of the microscopic origins of ferromagnetism in such materials. It remains unclear, however, whether the ferromagnetism in DMS is intrinsic - a precondition for spintronics - or due to dopant clustering. For this, we include a simultaneous doping from transition metal (Ni, Cu) and rare earth (Ce) ions in ZnO nanoparticles that increase the antiferromagnetic ordering to achieve high-T{sub c} ferromagnetism. Rietveld refinement of XRD patterns indicate that the dopant ions in ZnO had a wurtzite structure and the dopants, Ni{sup 2+}, Cu{sup 2+}, Ce{sup 3+} ions, are highly influenced the lattice constants to induce lattice defects. The Ni, Cu, Ce ions in ZnO have nanoparticles formation than nanorods was observed in pure sample. FTIR involve some organic groups to induce lattice defects and the metal-oxygen bonding of Zn, Ni, Cu, Ce and O atoms to confirm wurtzite structure. Raman analysis evaluates the crystalline quality, structural disorder and defects in ZnO lattice with doping. Photoluminescence spectra have strong near-band-edge emission and visible emission bands responsible for defects due to oxygen vacancies. The energy band gap is calculated using Tauc relation. Room temperature ferromagnetism has been described due to bound magnetic polarons formation with Ni{sup 2+}, Cu{sup 2+}, Ce{sup 3+} ions in ZnO via oxygen vacancies. The zero field and field cooling SQUID measurement confirm the strength of antiferromagnetism in ZnO. The field cooling magnetization is studied by Curie-Weiss law that include antiferromagnetic interactions up to low temperature. The XPS spectra have involve +3/+4 oxidation states of Ce ions to influence the observed ferromagnetism. - Graphical abstract: The lattice defects/vacancies attributed by Ni and Ce ions in the wurtzite ZnO structure are responsible in high T{sub c} -ferromagnetism due to long-range magnetic interactions with cluster and spin-glass type growth. - Highlights: • Lattice defects/vacancies attributed high T{sub c} –ferromagnetism. • Transition metal and rare earth ions deform the wurtzite ZnO lattice to induce defects. • Oxygen vacancies are more favorable than Zn with Ni, Cu, Ce into ZnO. • Defects assisted long-range ferromagnetism of doped ZnO include cluster and spin-glass growth.