DOE OSTI2011
Graphical abstract: Bi{sub 1-y}Sr{sub y}Fe{sub (1-y)(1-x)}Sc{sub (1-y)x}Ti{sub y}O{sub 3} (x = 0-0.2, y = 0.1-0.3) ceramics were obtained by solid-state reaction method. Addition of scandium could simultaneously reduce magnetic coercive field and enhance dielectric properties of prepared samples. Research highlights: {yields} The electrical resistivity of BiFeO{sub 3} is enhanced by forming solid solution with SrTiO{sub 3}. {yields} We further replace Fe{sup 3+} by Sc{sup 3+} in solid solution to reduce H{sub c} and achieve a soft magnet. {yields} Structure-magnetic property relationship has been established by Rietveld refinement. {yields} Sc{sup 3+} substitution can inhibit the dielectric loss effectively. -- Abstract: In this study, bulk ceramics with general formula Bi{sub 1-y}Sr{sub y}Fe{sub (1-y)(1-x)}Sc{sub (1-y)x}Ti{sub y}O{sub 3} (x = 0-0.2, y = 0.1-0.3 mol%) were prepared by traditional solid-state reaction method. As a comparison, bulk BiFeO{sub 3} (BF) was also sintered by rapid sintering method. Their structural, magnetic, dielectric properties were investigated. X-ray diffraction analysis indicated that apart from a small amount of secondary phase detected in BF, all other samples crystallized in pure perovskite structure and maintained original R3c space group. The room temperature M-H curves were obtained. While BF had a coercive magnetic field (H{sub c}) of 150 Oe, Bi{sub 1-y}Sr{sub y}Fe{sub 1-y}Ti{sub y}O{sub 3} solid solutions had a much larger value (for y = 0.1, 0.2, 0.3, H{sub c} were 4537, 5230 and 3578 Oe, respectively). Sc{sup 3+} substitution decreased the H{sub c} values of these solid solutions remarkably, and resulted in soft magnetic properties, as well as a decrease of the dielectric loss. At 1 MHz, the tan {delta} of Bi{sub 0.7}Sr{sub 0.3}Fe{sub 0.7(1-x)}Sc{sub 0.7x}Ti{sub 0.3}O{sub 3} with x = 0.05, 0.1, 0.15, 0.2 were 0.1545, 0.1078, 0.1046 and 0.1701, respectively.