Effects of Changing Hot Rolling Direction on Microstructure, Texture and Mechanical Properties of Cu-2.7Be Sheets

A hot rolling scheme (cross-rolling and unidirectional rolling) was adopted to process Cu-2.7Be sheets used as multiplier dynodes in photomultiplier. The effects of changing rolling direction on microstructure, texture and mechanical properties were studied by a combination of XRD, EBSD and TEM. It was found that higher copper-type texture and lower brass texture intensity were obtained in the ultimately cross-rolling (CR) sheet compared with the unidirectional rolling (UR) sheet.The EBSD results indicated that the grain orientation from mainly 〈101〉 for UR sample turns to random for CR sample. Great enhancements in YS and UTS after unidirectional rolling were attributed to the massive and polygonal γ precipitates. The CR sample exhibited lower anisotropy, because of the increase of S and γ precipitates with spherical and tiny shape.

36 MATERIALS SCIENCE↗

Mechanical Properties and Interface Evaluation of Al/AZ31 Multilayer Composites Produced by ARB at Different Rolling Temperatures

Many researchers have studied the microstructure and mechanical properties of Al/Mg composites rolled at a unique temperature; however, the effect of rolling temperature, which is one of the more decisive accumulative roll bonding (ARB) parameters, has not been investigated. In this work, laminated Al/Mg composites were fabricated by ARB at different temperatures using AZ31 magnesium alloy and commercially pure aluminum sheets. The microstructure of the layers and the mechanical properties of the rolled Al/AZ31 composites were investigated. Tensile and bending properties of the multilayer materials were examined by tensile and three-point bending tests. The results showed that mechanical bonding of the layers was improved with increasing rolling temperature. As a result, the intermediate rolling temperature (300 °C) indicated the best mechanical properties. Moreover, hot rolling caused an accelerated formation of intermetallic compounds.

36 MATERIALS SCIENCE↗

Effect of Rolling Deformation on the Microstructure and Mechanical Properties of an Extruded Mg-Zn-Ca Alloy

The microstructure and mechanical properties of an as-extruded Mg-4.5Zn-1.1Ca (wt.%) alloy subjected to unidirectional rolling and cross-rolling were compared in the present study. The results indicated that rolling deformation refined the microstructure, dispersed second phases and modified the texture, which resulted in an improvement in the mechanical properties of the as-rolled alloys compared with those of the as-extruded alloy. The yield strength of the Mg-4.5Zn-1.1Ca (wt.%) alloy increased from 173 to 297 MPa after unidirectional rolling. The initial fragmented Ca{sub 2}Mg{sub 6}Zn{sub 3} phases were further refined after rolling deformation, which clearly restricted the grain growth and gave rise to a fine microstructure. It was also found that rolling deformation intensified the basal texture in comparison with the as-extruded alloy, which was related to particle pinning.

36 MATERIALS SCIENCE↗

Annealing of (DU-10Mo)-Zr Co-Rolled Foils

Producing uranium-10wt% molybdenum (DU-10Mo) foils to clad with Al first requires initial bonding of the DU-10Mo foil to zirconium (Zr) by hot rolling, followed by cold rolling to final thickness. Rolling often produces wavy (DU-10Mo)-Zr foils that should be flattened before further processing, as any distortions could affect the final alignment and bonding of the Al cladding to the Zr co-rolled surface layer; this bonding is achieved by a hot isostatic pressing (HIP) process. Distortions in the (DU-10Mo)-Zr foil may cause the fuel foil to press against the Al cladding and thus create thinner or thicker areas in the Al cladding layer during the HIP cycle. Post machining is difficult and risky at this stage in the process since there is a chance of hitting the DU-10Mo. Therefore, it is very important to establish a process to flatten and remove any waviness. This study was conducted to determine if a simple annealing treatment could flatten wavy foils. Using the same starting material (i.e. DU-10Mo coupons of the same thickness), five different levels of hot rolling and cold rolling, combined with five different annealing treatments, were performed to determine the effect of these processing variables on flatness, bonding of layers, annealing response, microstructure, and hardness. The same final thickness was reached in all cases. Micrographs, textures, and hardness measurements were obtained for the various processing combinations. Based on these results, it was concluded that annealing at 650°C or higher is an effective treatment to appreciably reduce foil waviness.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Measurement method for roll angular displacement with a high resolution by using diffraction gratings and a heterodyne interferometer

The roll angle measurement is difficult to be achieved directly using a typical commercial interferometer due to its low sensitivity in axial direction, where the axial direction is orthogonal to the plane of the roll angular displacement. A roll angle measurement method combined diffraction gratings with a laser heterodyne interferometer is discussed in this paper. The diffraction grating placed in the plane of a roll angular displacement and the interferometer arranged in the plane's orthogonal direction, constitute the measurement pattern for the roll angle with high resolution. The roll angular displacement, considered as the linear, can be tested precisely when the corresponding angle is very small. Using the proposed method, the angle roll measurement obtains the high resolution of 0.002{sup ″}. Experiment has proved its feasibility and practicability.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Inflation with a constant rate of roll

We consider an inflationary scenario where the rate of inflaton roll defined by {sup ··}φ/H φ-dot remains constant. The rate of roll is small for slow-roll inflation, while a generic rate of roll leads to the interesting case of 'constant-roll' inflation. We find a general exact solution for the inflaton potential required for such inflaton behaviour. In this model, due to non-slow evolution of background, the would-be decaying mode of linear scalar (curvature) perturbations may not be neglected. It can even grow for some values of the model parameter, while the other mode always remains constant. However, this always occurs for unstable solutions which are not attractors for the given potential. The most interesting particular cases of constant-roll inflation remaining viable with the most recent observational data are quadratic hilltop inflation (with cutoff) and natural inflation (with an additional negative cosmological constant). In these cases even-order slow-roll parameters approach non-negligible constants while the odd ones are asymptotically vanishing in the quasi-de Sitter regime.

79 ASTRONOMY AND ASTROPHYSICS↗

Large slow roll parameters in single field inflation

We initially consider two simple situations where inflationary slow roll parameters are large and modes no longer freeze out shortly after exiting the horizon, treating both cases analytically. By modes, we refer to the comoving curvature perturbation R. We then consider applications to transient phases where the slow roll parameters can become large, especially in the context of the common 'fast-roll' inflation frequently used as a mechanism to explain the anomalously low scalar power at low l in the CMB. These transient cases we treat numerically. We find when ε, the first slow roll parameter, and only ε is large, modes decay outside the horizon, and when δ, the second slow roll parameter, is large, modes grow outside the horizon. When multiple slow roll parameters are large the behavior in general is more complicated, but we nevertheless show in the 'fast-roll' inflation case, modes grow outside the horizon.

79 ASTRONOMY AND ASTROPHYSICS↗

Effects of Grain Size and Interstitial Content on Recrystallization in Nb after Cold Rolling

A fully recrystallized microstructure with a fine grain size can improve the performance of superconducting radio-frequency (SRF) cavities produced from high-purity Nb (ASTM B393–18 Type 5 Nb) while providing mechanical strength. Recrystallization depends on impurity content, initial microstructure, deformation state, and annealing conditions. To better understand how fine-grained, fully recrystallized microstructures may be produced, the recrystallization behaviors of Type 5 and Type 2 Nb materials were studied. Type 5 Nb specimens were produced with both fine and coarse initial grain sizes. All were cold rolled and then annealed under vacuum for one hour to determine the rolling reductions and temperatures required for recrystallization. The recrystallized fraction exceeded 95% in fine-grained Type 5 Nb rolled to a 30% or greater thickness reduction and then annealed at 800 °C or higher. The coarse grained Type 5 Nb required greater rolling reductions to produce any recrystallized grains at 800 °C. The higher interstitial content of the Type 2 Nb required a temperature of 1000 °C or higher to reach a recrystallized fraction greater than 95% in specimens rolled to a 60% reduction. Recrystallization is more easily achieved during annealing at a given temperature for a set time by increasing rolling reduction, decreasing interstitial content, and decreasing initial grain size prior to cold rolling. In conclusion, to avoid grain growth following recrystallization, which increases grain size, the minimum time and temperature necessary for complete recrystallization should be applied.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Recrystallization Behavior and Super-Elasticity of a Metastable β-Type Ti-21Nb-7Mo-4Sn Alloy During Cold Rolling and Annealing

Based on the d-electron alloy design theory, a new metastable β-type titanium alloy for biomedical applications, Ti-21Nb-7Mo-4Sn (wt.%) was designed in this article. This theory predicted this alloy was a metastable single β-type titanium alloy with low elastic modulus at room temperature, and the β-phase transition (β to α″) would be easy to occur during the cold rolling. The evolution of microstructure and mechanical properties of this alloy during cold rolling plus annealing were investigated by means of x-ray diffraction, optical microscope, transmission electron microscope and mechanical properties test. The results indicate that only β phase can be identified in this alloy before cold rolling, while a large amount of lath martensite (α″ phase) appears after cold rolling due to stress-induced martensitic transformation, which is in accordance with the prediction of the d-electron alloy design theory. The recrystallization nucleation occurs preferentially in the martensite lath region during the subsequent annealing process, and this region forms a large number of nano-crystals and microcrystals, showing that cold rolling plus annealing can become a new process for refining grains. Compared with casting and cold rolling samples, the annealing materials at 923 K for 10 min have excellent comprehensive mechanical properties with lower elastic modulus (58 GPa) and higher elastic recovery rate (35.39%).

36 MATERIALS SCIENCE↗

Microstructural Analysis and Texture Evolution of the CVCEDed AZ31 Magnesium Alloy by Hot Rolling

Grain refinement is one of the important methods to improve the performance of magnesium alloy sheets. This paper attempts to prepare the billets of AZ31 magnesium alloy sheets by continuous variable cross-section direct extrusion (CVCDE) and then prepare sheets by rolling. The results show that the average grain size of the sheets rolled from extruded products by CVCDE with 2 interim dies reduced by 30% and the tensile strength increased by 12.6% compared with the sheets rolled from extruded products by traditional extrusion (CE), which is related to the dislocation multiplication in the corresponding conditions. The high dislocation density hinders the plastic deformation of the material, which is one of the internal factors that cause the increase in the strength of the material and the decrease in the plasticity. In addition, the basal surface of a lot of grains of the sheets rolled from extruded products by CVCDE with 2 interim dies is parallel to the RD-TD plane and the strength of texture is high. Meanwhile, the value of average Schmid factor of the sheets rolled from extruded products by CVCDE with 2 interim dies along the rolling direction is lowest, which result in lower plasticity. The above research provides a new idea for the development of high-performance magnesium alloy sheets.

36 MATERIALS SCIENCE↗

Contradictory Feature Size Effects in the Tensile Yield Strength of Cu Sheets Produced Using Different Sequences Involving Annealing, Rolling, and Grinding

The feature size effect is significant research interest in the field of microforming. It is assumed that the size effect is influenced by the material preparation process. To verify this, the feature size effects associated with the tensile yield strength of Cu sheets with thicknesses ranging from 100 to 200 μm, produced using different sequences involving annealing, rolling, and grinding, were studied. Differing feature size effects were observed in the Cu specimens, and it was confirmed that the size effect was indeed influenced by the specimen preparation sequence. The tensile yield strengths of the annealed–ground–rolled and annealed–rolled specimens increased as the specimen thicknesses decreased. However, an opposing size effect was observed in the case of the annealed–rolled–annealed, annealed–ground, and annealed–rolled–ground specimens. The reduction ratio did not alter the trend associated with the size effect, but influenced the intensity of the size effect. It is believed that the reinforcement and erosion of the surface-hardened layer introduced during rolling resulted in the contradictory results.

36 MATERIALS SCIENCE↗

The Mechanical and Corrosion Properties of Hot-Rolled TiB{sub 2}/Ni Composites

To quickly prepare TiB{sub 2}/Ni composites at low temperatures, a method combining spark plasma sintering and hot rolling was used. This paper presents the preparation, microstructural and mechanical properties, strengthening mechanism and corrosion properties of TiB{sub 2}/Ni composites in detail. X-ray diffraction analysis shows that the texture degree of the TiB{sub 2}/Ni composites after hot rolling greatly differed from that of the as-rolled pure Ni samples. The addition of TiB{sub 2} particles limited grain growth in the Ni matrix and led to grain refinement. Dislocation strengthening, grain refinement strengthening and load transfer strengthening contributed to a 30% increase in the tensile strength compared to that of the as-rolled pure Ni. In addition, the strengthening mechanism of the mechanical property reinforcement was analyzed. The electrochemical test results demonstrate that the as-rolled pure Ni exhibited a lower corrosion current density and corrosion resistance than the other as-rolled TiB{sub 2}/Ni composites fabricated in this paper. This work demonstrates a new approach for fabricating composites in less time at lower preparation temperatures than conventional methods.

36 MATERIALS SCIENCE↗

The effects of asymmetrical cold rolling on kinetics, grain size and texture in IF steels

Asymmetrical rolling is a promising way to achieve high rolling reductions and potentially grain refinement. However in steels the effect of asymmetrical rolling is not thoroughly quantified. In this paper the impact of cold asymmetrical rolling obtained by changing the roll velocity ratio (from 1.1 to 1.45) on the deformation and recrystallization features has been finely investigated by Electron Back-Scattering Diffraction in a Scanning Electron Microscope. In the investigated conditions (with low thickness reduction), it is found that asymmetrical rolling induces grain refinement and more homogeneous gamma fiber texture.

36 MATERIALS SCIENCE↗

Reinforcement of the Cube texture during recrystallization of a 1050 aluminum alloy partially recrystallized and 10% cold-rolled

In high purity Aluminum, very strong {l_brace}100{r_brace}<001> recrystallization texture is developed after 98% cold rolling and annealing at 500 Degree-Sign C. On the contrary, in Aluminum alloys of commercial purity, the Cube component hardly exceeds 30% after complete recrystallization. Parameters controlling Cube orientation development are mainly the solute dragging due to impurities in solid solution and the stored deformation energy. In the present study, besides the 85% cold rolling, two extra annealings and a slight cold rolling are introduced in the processing route to increase the Cube volume fraction. The Cube development was analyzed by X-ray diffraction and Electron BackScattered Diffraction (EBSD). The nucleation and growth mechanisms responsible for the large Cube growth were investigated using FEG/EBSD in-situ heating experiments. Continuous recrystallization was observed in Cube oriented grains and competed with SIBM (Strain Induced Boundary Migration) mechanism. This latter was favored by the stored energy gap introduced during the additional cold-rolling between the Cube grains and their neighbors. Finally, a Cube volume fraction of 65% was reached after final recrystallization. - Highlights: Black-Right-Pointing-Pointer EBSD in-situ heating experiments of aluminum alloy of commercial purity. Black-Right-Pointing-Pointer A 10% cold-rolling after a partial recrystallization improved Cube nucleation and growth. Black-Right-Pointing-Pointer Annealing before cold-rolling limited the solute drag effect and permitted a large Cube growth. Black-Right-Pointing-Pointer Cube development is enhanced by continuous recrystallization of Cube sub-grains. Black-Right-Pointing-Pointer The preferential Cube growth occurs by SIBM of small Cube grains.

36 MATERIALS SCIENCE↗

Characterization of microstructure, texture and magnetic properties in twin-roll casting high silicon non-oriented electrical steel

An Fe-6.5 wt.% Si-0.3 wt.% Al as-cast sheet was produced by twin-roll strip casting process, then treated with hot rolling, warm rolling and annealing. A detailed study of the microstructure and texture evolution at different processing stages was carried out by optical microscopy, X-ray diffraction and electron backscattered diffraction analysis. The initial as-cast strip showed strong columnar grains and pronounced < 001 >//ND texture. The hot rolled and warm rolled sheets were characterized by large amounts of shear bands distributed through the thickness together with strong < 110 >//RD texture and weak < 111 >//ND texture. After annealing, detrimental < 111 >//ND texture almost disappeared while beneficial (001)<210 >, (001)<010 >, (115)<5 − 10 1 > and (410) < 001 > recrystallization textures were formed, thus the magnetic induction of the annealed sheet was significantly improved. The recrystallization texture in the present study could be explained by preferred nucleation and grain growth mechanism. - Highlights: • A high silicon as-cast strip with columnar structure was produced. • A thin warm rolled sheet without large edge cracks was obtained. • Microstructure and texture evolution at each stage were investigated. • Beneficial (001)<210 >, (001)<010 >, (410)<001 > recrystallization textures were formed. • The magnetic induction of annealed sheet was significantly improved.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties development of micro channel tubes in extrusion, rolling and brazing

Highlights: • Rolling and brazing greatly affect the properties of micro-channel tubes (MCTs). • The properties of MCTs are investigated by the evolution of the microstructure. • Strength is decreased by 47% at 5%-rolling reduction ratio and 3-minute brazing. • Ductile fracture mode is observed by OM at failure of MCTs under inner pressure. - Abstract: In addition to extrusion, the post-processing of rolling and brazing has significant effect on the mechanical properties of multi-port tubes. The aluminum micro channel tubes, especially the seam welding zone in the internal webs, are investigated in terms of mechanical tests, microstructure characterization, and finite element analysis. The effect of the post-process of rolling are quantified by varying amount of rolling reduction ratios. Tensile strength and pressure bearing capacity are determined by tensile tests and burst pressure tests, respectively. The evolution of the microstructure within the seam wielding zone is characterized by Electron backscattered diffraction (EBSD) and optical microscopy (OM). The fracture profile observed by OM indicates ductile fracture mode. The pressure bearing capacity is reduced by ~47% at 5% reduction ratio of rolling followed by 3-minute brazing, where largest grains are obtained due to abnormal grain growth.

36 MATERIALS SCIENCE↗

Surface Strength of Silicon Nitride in Relation to Rolling Contact Performance Measured on Ball-on-Rod and Modified Four-Ball Tests

Silicon nitride (Si{sub 3}N{sub 4}) has been used in various rolling contact applications in turbomachinery, automotive and power industry. It is favoured to replace conventional steel due to its low density, low friction, corrosion resistance and good performance under extreme condition. However, a major limitation of its wider application is its high material and machining cost, especially the cost associated with the finishing process. In the present study, a low cost sintered and reaction bonded silicon nitride (SRBSN) is used to study the surface machining effects on its rolling contact performance. Attempt has been made to link the surface strengths of Si{sub 3}N{sub 4} derived from half-rod and C-sphere flexure strength specimens to the rolling contact lifetimes of Si{sub 3}N{sub 4} rod and ball specimens. The rolling contact fatigue tests are carried out on ball-on-rod and modified four ball machines. Three types of surfaces with coarse, fine and conventional finishing conditions are examined. Flexure strength tests on half-rod and C-sphere show an increasing surface strength from specimens with coarse, fine to conventionally machined conditions. During rolling contact fatigue test of as-machined specimens, there are no failures observed on both ball-on-rod and four ball tests after 100 million stress cycles. However, there is a trend of decreasing wear volumes measured on the contact path of rods and balls with coarse, fine and conventional conditions. In four ball test, spall failures are observed on pre-crack specimens. There is a trend of increasing rolling contact fatigue lifetime from pre-cracked specimens with coarse, fine to conventional machining conditions.

36 MATERIALS SCIENCE↗

Strip edge cracking simulation in cold rolling

This research work focuses on a specific defect which occurs during cold rolling of steel strips: edge-serration. Investigations on the industrial processes have led to the conclusion that this defect is the result of the edge-trimming and cold rolling sequences. The aim of this research work is to analyze the effect of the cutting process and the cold rolling on cracks occurrence, especially on strip edges.This study is performed using an experimental testing stand called Upsetting Rolling Test (URT). It allows to reproduce cold rolling contact parameters such as forward slip, reduction ratio and friction coefficients. Specimens sampled near trimmed industrial strip edges are deformed using the URT stand. Two sets of specimens with different stress states, obtained by annealing, are submitted to two reduction passes with extreme forward slips.Scanning electron microscopy observations added to 3D optical surface profiler topographies show that on one hand, forward slip has a major effect on cracks opening. On the other hand, cracks opening decreases according to high roll strip speed gradient. Concerning the heat-treated specimens, no crack appeared after all reduction passes, showing a large influence of the cutting process and consequently of the local stress state in the vicinity of the burnish and fracture regions.

36 MATERIALS SCIENCE↗