At least 181 records · Page 10

Final Technical Report - Recovery Act: Organic Coatings as Encapsulants for Low Cost, High Performance PV Modules

The objective of this project was to evaluate the feasibility of utilizing PPG's commercial organic coatings systems as efficient, modernized encapsulants for low cost, high performance, thin film photovoltaic modules. Our hypothesis was that the combination of an anticorrosive coating with a more traditional barrier topcoat would mitigate many electrochemical processes that are now responsible for the significant portion of photovoltaic (PV) failures, thereby nullifying the extremely high moisture barrier requirements of currently used encapsulation technology. Nine commercially available metal primer coatings and six commercially available top coatings were selected for screening. Twenty-one different primer/top coat combinations were evaluated. The primer coatings were shown to be the major contributor to corrosion inhibition, adhesion, and barrier properties. Two primer coatings and one top coating were downselected for testing on specially-fabricated test modules. The coated test modules passed initial current leakage and insulation testing. Damp Heat testing of control modules showed visible corrosion to the bus bar metal, whereas the coated modules showed none. One of the primer/top coat combinations retained solar power performance after Damp Heat testing despite showing some delamination at the EVA/solar cell interface. Thermal Cycling and Humidity Freeze testing resulted in only one test module retaining its power performance. Failure modes depended on the particular primer/top coating combination used. Overall, this study demonstrated that a relatively thin primer/top coating has the potential to replace the potting film and backsheet in crystalline silicon-based photovoltaic modules. Positive signals were received from commercially available coatings developed for applications having performance requirements different from those required for photovoltaic modules. It is likely that future work to redesign and customize these coatings would result in a coating system meeting the requirements for photovoltaic module encapsulation.

14 SOLAR ENERGY↗

Thermal model to quantify the impact of sub-bandgap reflectance on operating temperature of fielded PV modules

Minimizing module heating is an effective way to increase the lifetime energy output of photovoltaic systems. Maximizing the reflection of light that is unusable for energy conversion is one of the most promising ways to reduce the operating temperature of fielded modules. We derive a model based on a steady-state energy balance to quantify the temperature benefit of cell or module optical modifications aimed at improving reflection of light with photon energies below the photovoltaic cell bandgap energy. This more detailed model is then simplified so that, from outdoor measured data, temperature differences arising from reflectance can be isolated from those arising from irradiance, wind speed, and module standard-test-condition efficiency.

14 SOLAR ENERGY↗

Hotspot testing of glass/backsheet and glass/glass PV modules pre-stressed in extended thermal cycling

This paper investigates the effect of hotspot (HS) stress endurance of two of the latest designs of monocrystalline modules: a half-cell glass/backsheet (G/B) module and a full-cell glass/glass (G/G) module. These modules have already been pre-stressed in extended thermal cycling with 600 cycles per the IEC 61215 standard to represent field-stressed modules. This study differs from the other conventional studies wherein only fresh modules are subjected to hotspot endurance stress. The G/G module reached a maximum temperature of approximately 200 °C at a cell shading of 25 %, 55 °C higher than the maximum hotspot temperature of 145 °C in the G/B module. A significant burn mark, without glass shattering, was observed in the hotspot-stressed cell of the G/G module due to the current mismatch induced by partial shading. Most of the cells in the G/G module appear to be severely damaged (severe dark areas), as observed in the electroluminescence (EL) image, while the dark regions were rarely present in the G/B module. The EL image also illustrates multiple cell cracks that resist current flow and eventually contribute to the full-cell module degradation. About 8.3 % degradation in maximum power was observed for the G/G module and 1.3 % for the G/B module after the sequential stress tests. The lower degradation in the G/B module can potentially be attributed to its design, which comprises of two parallel strings, each having 72-half-cells and benefits from lower heat dissipation. Furthermore, this indicates that the half-cell design could potentially minimize the hotspot degradation and failures in crystalline-silicon modules.

14 SOLAR ENERGY↗

Surface Modification of Backsheets Using Coupling Agents for Roll-To-Roll Processed Thin-Film Solar Photovoltaic (PV) Module Packaging Application

For many flexible electronic and photonic devices, moisture stability is one of the most important factors that affects its short- and long-term performance. To maintain the performance, the device should be packaged in such a way that it hermetically blocks moisture from the device; however, in practice, it is rather difficult to achieve. The more practical solution is to impede the moisture ingress to the device. In optoelectronic devices that will be outdoors like solar cells, the interfacial adhesion strength between the encapsulant layer (adhesive) and a moisture barrier layer is also a critical parameter. This paper presents surface modifications of poly(ethylene terephthalate) (PET) carrier films, one of the layers in the trilayer barrier film that directly adheres to an encapsulant, using chemical, UV/ozone, and both treatments to improve adhesion with the thermoset encapsulant polymer material. Whereas previous studies also utilized treatment methods to increase the wettability characteristics, in this paper, we not only present the results of the adhesion strength upon various techniques to achieve good adhesion but also screen their behavior upon exposure to a damp–heat (60 °C, 90% RH) environment. Here, we found that the combined treatment method increases the adhesion by up to 12.1-fold and demonstrates up to a 200% increase in adhesion strength even upon our severe damp–heat environmental condition.

36 MATERIALS SCIENCE↗

Activation Energy for End-of-Life Solder Bond Degradation: Thermal Cycling of Field-Aged PV Modules

The longevity of solar photovoltaic modules depends on the durability and reliability of their components, one of which is the solder bonds in interconnect ribbons. The solder joints experience stresses from thermal cycling and constant elevated temperatures (40 °C-70 °C) in regular field operation leading to thermo-mechanical fatigue and intermetallic compound formation. To study the end-of-life wear-out mechanisms and to obtain activation energy of solder bond degradation, here two field-aged modules from Arizona-a 21-year-old Solarex MSX60 module (with Sn62Pb36Ag2 at the solder joints) and an 18-year-old Siemens M55 module (with Sn60Pb40 at the solder joints)-underwent 800 and 400 modified thermal cycles, respectively. Using three heating blankets, each module had three temperature zones maintained at 85, 95, and 105 °C during the 15-min hot dwell time of the thermal cycle. Cell-level series resistance data obtained from three temperature zones enabled the calculation of activation energy for solder bond degradation for the MSX60 and the M55 modules to be 0.12 eV and 0.35 eV, respectively. From each temperature zone in both modules, busbar-solder samples were obtained, imaged through SEM, and analyzed with energy-dispersive X-ray spectroscopy. In the MSX60 module with traces of Ag in the solder material, phase segregation and growth were primarily observed at high temperatures. For M55 modules without Ag in the solder material, major phase segregation was observed in all temperature zones. The IMC thickness for both modules increased with increasing module temperature. The beneficial effect of Ag in solder material on mitigating solder bond degradation is presented.

14 SOLAR ENERGY↗

Brief: Daily Performance Changes in Metal Halide Perovskite PV Modules

Metal halide perovskite photovoltaic modules deployed outdoors and held at their maximum power point show daily, reversible, relative changes of up to 30% in efficiency between morning and afternoon. Predicting energy yield and quantifying reliability will require properly handling such daily performance changes.