Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Life”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

PEDOT-PSS coated ZnO/C hierarchical porous nanorods as ultralong-life anode material for lithium ion batteries

ZnO/C hierarchical porous nanorods were synthesized through one-pot wet-chemical reaction followed by thermal calcination. It was found that ZnO/C porous nanorods are composed of numerous nanograins, exhibiting a hierarchical micro/nanostructure. In-situ synchrotron high energy X-ray diffraction study revealed that ZnO/C hierarchical porous nanorods involve a two-step reversible lithiation mechanism during charge/discharge; and part of ZnO and Zn remains at the end of the first discharge and charge process, respectively, leading to a low coulombic efficiency in the initial few cycles. The electrochemical test demonstrated that the reversible capacity and the rate performance of ZnO/C hierarchical porous nanorods anode have been greatly improved by PEDOT-PSS coating, which could maintain a reversible capacity of 623.94 mA h g(-1) after 1500 cycles at 1 C. Its excellent high rate capability and long cycle stability were attributed to the high electronic conductivity of PEDOT-PSS coating layer and the hierarchical structures of ZnO/C porous nanorods. (C) 2015 Elsevier Ltd. All rights reserved.

anode↗

Mechanical Reliability and Life Prediction of Coated Metallic Interconnects within Solid Oxide Fuel Cells

Metallic cell interconnects (IC) made of ferritic stainless steels, i.e., iron-based alloys, have been increasingly favored in the recent development of planar solid oxide fuel cells (SOFCs) because of their advantages in excellent imperviousness, low electrical resistance, ease in fabrication, and cost effectiveness [1]. Typical SOFC operating conditions inevitably lead to the formation of oxide scales on the surface of ferritic stainless steel, which could cause delamination, buckling, and spallation resulting from the mismatch of the coefficient of thermal expansion and eventually reduce the lifetime of the interconnect components. Various protective coating techniques have been applied to alleviate these drawbacks [2]. In the present work, a fracture-mechanics-based quantitative modeling framework has been established to predict the mechanical reliability and lifetime of the spinel-coated, surface-modified specimens under an isothermal cooling cycle. Analytical solutions have been formulated to evaluate the scale/substrate interfacial strength and determine the critical oxide thickness in terms of a variety of design factors, such as coating thickness, material properties, and uncertainties. The findings then are correlated with the experimentally measured oxide scale growth kinetics to quantify the predicted lifetime of the metallic interconnects.

Solid oxide fuel cell (SOFC), Ferritic stainless s↗

Enzymes as parts in need of replacement - and how to extend their working life

Enzymes catalyze reactions in vivo at different rates and each enzyme molecule has a lifetime limit before it is degraded and replaced to enable catalysis to continue. Considering these rates together as a unitless ratio of catalytic cycles until replacement (CCR) provides a new quantitative tool to assess the replacement schedule of and energy investment into enzymes as they relate to function. Here, we outline the challenges of determining CCRs and new approaches to overcome them and then assess the CCRs of selected enzymes in bacteria and plants to reveal a range of seven orders of magnitude for this ratio. Modifying CCRs in plants holds promise to lower cellular costs, to tailor enzymes for particular environments, and to breed enzyme improvements for crop productivity.

Catalytic rate↗

Long-Life, Ultrahigh-Nickel Cathodes with Excellent Air Storage Stability for High-Energy Density Lithium-Based Batteries

With increased energy density and cost advantage, ultrahigh-nickel layered oxides (LiNi x M 1-x O 2 , x = 0.9 - 1.0) are becoming front-runner as cathodes for next-generation lithium-based batteries, yet their commercialization is blocked both by severe capacity fade and exponentially aggravated air degradation. Thus, it is imperative to find effective solutions to address these issues simultaneously. Here, a significant enhancement in both the cycling and air storage stability of the ultrahigh-Ni cathode LiNi 0.94 Co 0.06 O 2 is achieved via a distinctive phosphoric acid treatment strategy. The modified cathode displays remarkably improved capacity retention (from 36 % to 80 % after 1,000 cycles) and rate capability (from 0 to 105 mA h g -1 at 30C rate) in pouch cells. Impressively, the modified cathode, after air storage for 450 days, maintains the morphology and 92% of the initial capacity of the fresh sample with excellent cyclability. Comprehensive interphase and structural analyses reveal that the enhanced electrochemical performance is due to a highly stabilized electrode/electrolyte interphase that suppresses electrode corrosion and lattice reconstruction. The excellent air stability results from an adsorption-buffering effect enabled by phosphoric acid to air attack. Finally, the study demonstrates an engineering pathway to improve the cycling and air stability, facilitating the practical viability of high-capacity, affordable, ultrahigh-Ni cathodes in lithium-based batteries.

25 ENERGY STORAGE↗

Unraveling the Complex Delithiation Mechanisms of Olivine-Type Cathode Materials, LiFe x Co 1– x PO 4

The delithiation mechanisms occurring within the olivine-type class of cathode materials for Li-ion batteries have received considerable attention owing to the good capacity retention at high rates for LiFePO4. A comprehensive mechanistic study of the (de)lithiation reactions that occur when the substituted olivine-type cathode materials LiFexCo1-xPO4 (x = 0, 0.05, 0.125, 0.25, 0.5, 0.75, 0.875, 0.95 and 1) are electrochemically cycled is reported here, using in situ X-ray diffraction (XRD) data. On the first charge, two intermediate phases are observed and identified: Li1-x(Fe3+)x(Co2+)1- xPO4 for 0 < x < 1 (i.e. after oxidation of Fe2+ => Fe3+) and Li2/3FexCo1-xPO4 for 0 ≤ x ≤ 0.5 (i.e. the Co-majority materials). For the Fe-rich materials, we study how nonequilibrium, single-phase mechanisms that occur discretely in single particles, as observed for LiFePO4 at high rates, is affected by Co substitution. In the Co-majority materials, a two-phase mechanism with a coherent interface is observed, as was seen in LiCoPO4, and we discuss how it is manifested in the XRD patterns. We then compare the nonequilibrium, single-phase mechanism with the bulk single-phase and the coherent interface two-phase mechanisms. Despite the apparent differences between these mechanisms, we discuss how they are related and interconverted as a function of Fe/Co substitution and the potential implications for the electrochemistry of this system.

36 MATERIALS SCIENCE↗