Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “INCLUSIONS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Inclusion Characterization in Aluminum-Deoxidized Special Steel with Certain Sulfur Content Under Combined Influences of Slag Refining, Calcium Treatment, and Reoxidation

Inclusions in Al-killed steel with [S] of about 0.0060 to 0.0070 mass pct were characterized and discussed, evaluating the combined effects of basic slag refining and Ca treatment in ladle, together with reoxidation of liquid steel in casting tundish. Inclusions were changed from Al{sub 2}O{sub 3} to MgO-Al{sub 2}O{sub 3} spinel and then to MgO-Al{sub 2}O{sub 3}-CaO during basic slag refining. After Ca treatment, many (MgO-Al{sub 2}O{sub 3}) + CaS inclusions were formed, featuring the coexistence of MgO-Al{sub 2}O{sub 3} and CaS to form a dual-phased structure. In the following Ar blowing, the number density of (MgO-Al{sub 2}O{sub 3}) + CaS inclusions and pure CaS increased obviously, which implied that [Ca] preferentially reacted with [S] rather than [O] in steel. Reoxidation in casting tundish caused the pickup of oxygen in steel, and the rise of total oxygen (T.O) was 0.0002 mass pct; even 55t steel has been poured. As a result, the content of CaO in inclusions increased and MgO-Al{sub 2}O{sub 3}-CaO inclusions were formed again. Thermodynamic calculations revealed that the driving force was strong for the formation of CaS-based inclusions. Higher carbon content in steel would help to reduce oxygen content while enhancing the activity of [S] in steel, which further stabilized the existence of CaS-based inclusions. Therefore, inclusions were mostly the solid (MgO-Al{sub 2}O{sub 3}) + CaS dual-phase ones, without the formation of liquid calcium aluminates. Contents of CaS and CaO in inclusions were affected by the [mass pct S]/[mass pct O] ratio, which was calculated as about 4.58 K and 5.34 K at 1873 K and 1823 K, respectively. This finding implied that lower oxygen was not favorable to prevent the solid inclusions in the calcium treatment of high carbon special steel.

36 MATERIALS SCIENCE↗

Entrapment of Inclusions by Solidified Hooks at the Subsurface of Ultra-Low-Carbon Steel Slab

To understand the mechanism for the entrapment of non-metallic inclusions by curved hooks beneath the surface of continuous casting slabs, the etching of the slab, the observation of hooks and the detection of inclusions on sections vertical and parallel to the slab surface were performed. The location of inclusions and hooks was revealed, and forces acting on the inclusion below a hook were analyzed. Inclusions gathered more below the curved hook than in the overflow zone above the hook. From the observation of hooks and inclusions on sections vertical to the slab surface, the number density of 3 to 5 μm inclusions in the hook zone and no-hook zone was very close, while the number density of > 10 μm inclusions in the hook zone was larger than that in the no-hook zone. From the observation on sections parallel to the slab surface, > 20 μm inclusions were located near the hook line more than in other regions, and the number density of inclusions in the hook zone was more than that in the no-hook zone. The apparent friction coefficient dominated the critical capturing size of inclusions from the solidification front, and the deflection angle, flow velocity, sulfur content and solidification velocity had influences on the size range.

36 MATERIALS SCIENCE↗

Formation of distinct inclusion bodies by inhibition of ubiquitin-proteasome and autophagy-lysosome pathways

Research highlights: {yields} Distinct inclusion bodies are developed by inhibition of UPP and ALP. {yields} The inclusion bodies differ in morphology, localization and formation process. {yields} The inclusion bodies are distinguishable by the localization of TSC2. {yields} Inhibition of both UPP and ALP simultaneously induces those inclusion bodies. -- Abstract: Accumulation of misfolded proteins is caused by the impairment of protein quality control systems, such as ubiquitin-proteasome pathway (UPP) and autophagy-lysosome pathway (ALP). In this study, the formation of inclusion bodies was examined after the blockade of UPP and/or ALP in A549 cells. UPP inhibition induced a single and large inclusion body localized in microtubule-organizing center. Interestingly, however, ALP inhibition generated dispersed small inclusion bodies in the cytoplasm. Tuberous sclerosis complex 2 was selectively accumulated in the inclusion bodies of UPP-inhibited cells, but not those of ALP-inhibited cells. Blockade of transcription and translation entirely inhibited the formation of inclusion body induced by UPP inhibition, but partially by ALP inhibition. Moreover, the simultaneous inhibition of two protein catabolic pathways independently developed two distinct inclusion bodies within a single cell. These findings clearly demonstrated that dysfunction of each catabolic pathway induced formation and accumulation of unique inclusion bodies on the basis of morphology, localization and formation process in A549 cells.

60 APPLIED LIFE SCIENCES↗

Fluid Inclusions in Extraterrestrial Samples Fact or Fiction?

Over the years there have been numerous reports of liquid inclusions in meteorites. Roedder reviews the reported occurrences of liquid inclusions in meteorites and states that "silicate-melt inclusions are expectable and apparently ubiquitous, but the presence of actual liquid inclusions (i.e., with moving bubbles at room temperature) would seem almost impossible." The reason for this conclusion is that meteorites (presumably) form in space at high temperatures and very low pressures where liquid water (or carbon dioxide) is not stable. Perhaps the most infamous report of fluid inclusions in meteorites was that of Warner et al. In that study, the authors reported the presence of two-phase, liquid-vapor inclusions in a diogenite from Antarctica. This report of fluid inclusions generated considerable interest in the meteorite community, and caused many to question existing models for the origin of the diogenites. This interest was short-lived however, as later investigations of the same samples showed that the inclusions were most likely artifacts. Rudnick et al. showed that many of the inclusions in meteorites prepared at the Johnson Space Center contained a fluid that fluoresced strongly under the laser beam on the Raman microprobe. They interpreted this to indicate that the inclusions contained Almag oil used in the preparation of thin sections. Presumably, the Almag oil entered empty vesicles along fractures that were opened intermittently during cutting. Here, the occurrence of unambiguous fluid inclusions that could not have been introduced during sample preparation are described in samples from two different extraterrestrial environments. One environment is represented by the SNC (martian) meteorites ALH 84001 and Nakhla. The second environment is represented by the Monahans 1998 meteorite that fell recently in the USA.

Bodnar, R. J.↗

Ceramic Inclusions In Powder Metallurgy Disk Alloys: Characterization and Modeling

Powder metallurgy alloys are increasingly used in gas turbine engines, especially as the material chosen for turbine disks. Although powder metallurgy materials have many advantages over conventionally cast and wrought alloys (higher strength, higher temperature capability, etc.), they suffer from the rare occurrence of ceramic defects (inclusions) that arise from the powder atomization process. These inclusions can have potentially large detrimental effect on the durability of individual components. An inclusion in a high stress location can act as a site for premature crack initiation and thereby considerably reduce the fatigue life. Because these inclusions are exceedingly rare, they usually don't reveal themselves in the process of characterizing the material for a particular application (the cumulative volume of the test bars in a fatigue life characterization is typically on the order of a single actual component). Ceramic inclusions have, however, been found to be the root cause of a number of catastrophic engine failures. To investigate the effect of these inclusions in detail, we have undertaken a study where a known population of ceramic particles, whose composition and morphology are designed to mimic the 'natural' inclusions, are added to the precursor powder. Surface connected inclusions have been found to have a particularly large detrimental effect on fatigue life, therefore the volume of ceramic 'seeds' added is calculated to ensure that a minimum number will occur on the surface of the fatigue test bars. Because the ceramic inclusions are irregularly shaped and have a tendency to break up in the process of extrusion and forging, a method of calculating the probability of occurrence and expected intercepted surface and embedded cross-sectional areas were needed. We have developed a Monte Carlo simulation to determine the distributions of these parameters and have verified the simulated results with observations of ceramic inclusions found in macro slices from extrusions and forgings. The ultimate goal of this study will be to use probabilistic methods to determine the reliability detriment that can be attributed to these ceramic inclusions.

Bonacuse, Pete↗

Experimental Simulation of Shock Reequilibration of Fluid Inclusions During Meteorite Impact

Fluid inclusions are microscopic volumes of fluid trapped within minerals as they precipitate. Fluid inclusions are common in terrestrial minerals formed under a wide array of geological settings from surface evaporite deposits to kimberlite pipes. While fluid inclusions in terrestrial rocks are the rule rather than the exception, only few fluid inclusion-bearing meteorites have been documented. The rarity of fluid inclusions in meteoritic material may be explained in two ways. First, it may reflect the absence of fluids (water?) on meteorite parent bodies. Alternatively, fluids may have been present when the rock formed, but any fluid inclusions originally trapped on the parent body were destroyed by the extreme P-T conditions meteorites often experience during impact events. Distinguishing between these two possibilities can provide significant constraints on the likelihood of life on the parent body. Just as textures, structures, and compositions of mineral phases can be significantly altered by shock metamorphism upon hypervelocity impact, fluid inclusions contained within component minerals may be altered or destroyed due to the high pressures, temperatures, and strain rates associated with impact events. Reequilibration may occur when external pressure-temperature conditions differ significantly from internal fluid isochoric conditions, and result in changes in fluid inclusion properties and/or textures. Shock metamorphism and fluid inclusion reequilibration can affect both the impacted target material and the meteoritic projectile. By examining the effects of shock deformation on fluid inclusion properties and textures we may be able to better constrain the pressure-temperature path experienced by shocked materials and also gain a clearer understanding of why fluid inclusions are rarely found in meteoritic samples.

Madden, M. E. Elwood↗

Simultaneous Modification of Alumina and MgO·Al{sub 2}O{sub 3} Inclusions by Calcium Treatment During Electroslag Remelting of Stainless Tool Steel

Calcium modification of both alumina and MgO·Al{sub 2}O{sub 3} inclusions during protective gas electroslag remelting (P-ESR) of 8Cr17MoV stainless steel and its effect on nitrides and primary carbides were studied by analyzing the transient evolution of oxide and sulfide inclusions in the P-ESR process. The oxide inclusions that were not removed during P-ESR without calcium treatment were found to retain their original state until in as-cast ingot. Calcium treatment modified all MgO·Al{sub 2}O{sub 3} and alumina inclusions that had not been removed in the P-ESR process to liquid/partially liquid CaO-Al{sub 2}O{sub 3}-(MgO) with uniformly distributed elements, in addition to a small proportion of partially modified inclusions of a CaO-MgO-Al{sub 2}O{sub 3} core surrounded by a liquid CaO-Al{sub 2}O{sub 3}. The modification of low-MgO-containing MgO·Al{sub 2}O{sub 3} inclusions involves the preferential reduction of MgO from the MgO·Al{sub 2}O{sub 3} inclusion by calcium and the reaction of calcium with Al{sub 2}O{sub 3} in the inclusion. It is the incomplete/complete reduction of MgO from the spinel by calcium that contributes to the modification of spinels. Alumina inclusions were liquefied by direct reaction with calcium. Calcium treatment during P-ESR refining also provided an effective approach to prevent the formation of nitrides and primary carbides in stainless steel through modifying their preferred nucleation sites (alumina and MgO·Al{sub 2}O{sub 3} inclusions) to calcium aluminates, which made no contribution to improving the steel cleanliness.

36 MATERIALS SCIENCE↗

Investigation of RE-O-S-As Inclusions in High Carbon Steels

The formation of RE-O-S-As inclusions is an inevitable issue when rare earth (RE) elements are used to modify the existing state of residual element arsenic. The evolution process of La-O-S-As inclusions in high carbon steels was investigated under conditions of different La contents. An in-situ sample preparation method was used to prepare film samples. The results show that it is practical to add RE elements to stabilize arsenic by generating As-bearing RE inclusions. A new type of As-bearing RE inclusion was discovered and identified as LaAsO{sub 4}. As La content increased from 0.003 to 0.089 wt pct, the dominant inclusions of the La-O-S-As system changed from La{sub 2}O{sub 3} to La{sub 2}O{sub 2}S, then to La{sub 2}O{sub 2}S-LaAsO{sub 4}, and finally to LaAsO{sub 4}. A full model of the inclusion formation of the RE-O-S-As system was also established to describe what kind of inclusion to form in conditions of different atomic ratios of RE/O and RE/S. The first As-bearing RE inclusion is RE-O-As or RE-S-As, and RE-O-S-As inclusions can be controlled to form certain inclusions that make O and S useful to modify the existing state of arsenic.

36 MATERIALS SCIENCE↗

Automated Classification and Analysis of Non-metallic Inclusion Data Sets

The aim of this study is to utilize principal component analysis (PCA), clustering methods, and correlation analysis to condense and examine large, multivariate data sets produced from automated analysis of non-metallic inclusions. Non-metallic inclusions play a major role in defining the properties of steel and their examination has been greatly aided by automated analysis in scanning electron microscopes equipped with energy dispersive X-ray spectroscopy. The methods were applied to analyze inclusions on two sets of samples: two laboratory-scale samples and four industrial samples from a near-finished 4140 alloy steel components with varying machinability. The laboratory samples had well-defined inclusions chemistries, composed of MgO-Al{sub 2}O{sub 3}-CaO, spinel (MgO-Al{sub 2}O{sub 3}), and calcium aluminate inclusions. The industrial samples contained MnS inclusions as well as (Ca,Mn)S + calcium aluminate oxide inclusions. PCA could be used to reduce inclusion chemistry variables to a 2D plot, which revealed inclusion chemistry groupings in the samples. Clustering methods were used to automatically classify inclusion chemistry measurements into groups, i.e., no user-defined rules were required.

36 MATERIALS SCIENCE↗

Study on Formation Mechanism of CaO-SiO{sub 2}-Based Inclusions in Saw Wire Steel

Attempts were made to elucidate the formation mechanism of CaO-SiO{sub 2}-based inclusions in saw wires by both laboratory experiments and industrial trials. The key point was to make clear the origin of CaO in such oxide inclusions. Probable origins of [Ca] in steel were first discussed, which can be taken into steel from the steel-slag reaction or ferrous alloy. As a result, slag-steel chemical reaction equilibrium was carefully evaluated at 1873 K (1600 °C) to classify the changes of dissolved aluminum ([Al]), total magnesium (Mg), and total calcium (Ca) in steel and the caused composition variations of inclusions. With the rise of slag basicity from 0.5 to 1.8, [Al] was remarkably increased from 0.00045 to 0.00139 mass pct, whereas Mg varied in the range of 0.00038 to 0.00048 mass pct. By contrast, Ca was constantly kept below 0.00003 mass pct. Accordingly, Al{sub 2}O{sub 3} and MgO in inclusions witnessed obvious rises from 5 to 23 mass pct and from 2 to 8 mass pct, respectively. By contrast, inclusions were free of CaO when slag basicity was below 1.5. With slag basicity further increased to 1.8, CaO witnessed a negligible rise to only 1.0 mass pct on average. This phenomenon agreed well with thermodynamic calculations, which revealed that chemical reaction between steel and CaO in slag (for example, between [Si] and CaO) was weak to hardly supplying sufficient [Ca] to steel to increase CaO in inclusions. Ca contained in ferrous alloys as contaminations was not the cause of CaO-SiO{sub 2}-based inclusions, either. The industrial trial results indicated that CaO-SiO{sub 2}-based inclusions have been readily produced in short time just after BOF tapping. Also, a percentage of them changed slightly with the proceeding of refining. Based on the good agreement of laboratory, industrial, and thermodynamics calculations results, it can be reasonably concluded that CaO-SiO{sub 2}-based inclusions in saw wire were exogenous particles from entrapped/emulsified top slag, but not products of slag-steel-inclusion chemical reactions.

36 MATERIALS SCIENCE↗

Effects of Reoxidation of Liquid Steel and Slag Composition on the Chemistry Evolution of Inclusions During Electroslag Remelting

Electroslag remelting (ESR) is increasingly used to produce some varieties of special steels and alloys, mainly because of its ability to provide extreme cleanliness and an excellent solidification structure simultaneously. In the present study, the combined effects of varying SiO{sub 2} contents in slag and reoxidation of liquid steel on the chemistry evolution of inclusions and the alloying element content in steel during ESR were investigated. The inclusions in the steel before ESR refining were found to be oxysulfides of patch-type (Ca,Mn)S adhering to a CaO-Al{sub 2}O{sub 3}-SiO{sub 2}-MgO inclusion. The oxide inclusions in both the liquid metal pool and remelted ingots are CaO-Al{sub 2}O{sub 3}-MgO and MgAl{sub 2}O{sub 4} together with CaO-Al{sub 2}O{sub 3}-SiO{sub 2}-MgO inclusions (slightly less than 30 pct of the total inclusions), which were confirmed to originate from the reduction of SiO{sub 2} from the original oxide inclusions by dissolved Al in liquid steel during ESR. CaO-Al{sub 2}O{sub 3}-MgO and MgAl{sub 2}O{sub 4} are newly formed inclusions resulting from the reactions taking place inside liquid steel in the liquid metal pool caused by reoxidation of liquid steel during ESR. Increasing the SiO{sub 2} content in slag not only considerably reduced aluminum pickup in parallel with silicon loss during ESR, but also suppressed the decrease in SiO{sub 2} content in oxide inclusions. (Ca,Mn)S inclusions were fully removed before liquid metal droplets collected in the liquid metal pool.

36 MATERIALS SCIENCE↗

Evolution of Oxide–Sulfide Complex Inclusions and Its Correlation with Steel Cleanliness During Electroslag Rapid Remelting (ESRR) of Tool Steel

The evolution of CaO-Al{sub 2}O{sub 3}-MgO-(SiO{sub 2}) inclusions associated with CaS during electroslag rapid remelting (ESRR) of the tool steel with ultra low oxygen (8 ppm) under protective atmosphere was investigated. Thermodynamic calculation was performed to evaluate the oxygen level of liquid steel and the inclusion evolution during ESRR with the help of FactSage software (CON2 database). The results demonstrated that the reoxidation of liquid steel took place during industrial ESRR, resulting in the oxygen pickup of approximately double content. The oxygen level in the steel was determined by [Al]-[O] equilibrium during ESRR, whereas FeO in the slag transferred oxygen into the liquid steel, as indicated by the significant oxygen pickup. The inclusions in the steel electrode are oxide–sulfide type of CaO-Al{sub 2}O{sub 3}-MgO partially wrapped with CaS. The original oxide inclusions that had not been removed in ESRR process were transformed to liquid CaO-Al{sub 2}O{sub 3}-SiO{sub 2}-MgO inclusions through reacting with the dissolved oxygen supplied from the reoxidation of liquid steel and concerned elements in liquid steel during ESRR. These CaO-Al{sub 2}O{sub 3}-SiO{sub 2}-MgO inclusions were invariably associated with patch-type or shell-type CaS, which hold different formation mechanisms. The inclusions ranging from 2 to 4 µm take up a dominant proportion (a little more than 50 pct of the total inclusions) in the remelted ingots, and those larger than 8 µm account for about 3 pct. Melting rates of ESRR not only exerted a negligible effect on the steel cleanliness and the removal efficiency of oxide inclusions, but also on the inclusion size distribution.

36 MATERIALS SCIENCE↗

Formation Mechanism of Al{sub 2}O{sub 3}-Containing Inclusions in Al-Deoxidized Spring Steel

The source, characteristics, and mechanism of Al{sub 2}O{sub 3}-containing inclusions in Al-deoxidized spring steel were investigated using electron-probe X-ray microanalysis (EPMA). Spring samples were collected during vacuum degassing (VD) refining, in a tundish ladle, and after hot rolling, respectively. Based on primary inclusion components, seven types of inclusions were observed through the manufacturing process: Al{sub 2}O{sub 3}, Al{sub 2}O{sub 3}-SiO{sub 2}, Al{sub 2}O{sub 3}-CaO, Al{sub 2}O{sub 3}-MgO, Al{sub 2}O{sub 3}-MgO-CaO, Al{sub 2}O{sub 3}-SiO{sub 2}-MnO, and Al{sub 2}O{sub 3}-SiO{sub 2}-CaO. The Al{sub 2}O{sub 3} and Al{sub 2}O{sub 3}-SiO{sub 2} inclusions were mainly attributed to deoxidization products, less than 15 μm in diameter and with liquidus temperatures exceeding 1600 °C. For Al{sub 2}O{sub 3}-CaO inclusions, which were considered to be formed by the reduction of entrapped slag by Al dissolved in the steel, the Al{sub 2}O{sub 3}/CaO ratio obviously decreased with the increase of inclusion sizes. Most Al{sub 2}O{sub 3}-SiO{sub 2}-CaO inclusions were less than 15 μm in diameter, with their composition close to that of the refining slag and a liquidus temperature near 1500 °C. The Al{sub 2}O{sub 3}-MgO and Al{sub 2}O{sub 3}-SiO{sub 2}-MnO inclusions originated from inherent reactions between dissolved [Al], [Si], [Mn], [Mg], and [O] in the steel. Al{sub 2}O{sub 3}-MgO-CaO inclusions resulted from coalescence between Al{sub 2}O{sub 3}-MgO and Al{sub 2}O{sub 3}-CaO inclusions.

36 MATERIALS SCIENCE↗

The crack-inclusion interaction problem

The general plane elastostatic problem of interaction between a crack and an inclusion is considered. The Green's functions for a pair of dislocations and a pair of concentrated body forces are used to generate the crack and the inclusion. Integral equations are obtained for a line crack and an elastic line inclusion having an arbitrary relative orientation and size. The nature of stress singularity around the end points of rigid and elastic inclusions is described and three special cases of this intersection problem are studied. The problem is solved for an arbitrary uniform stress state away from the crack-inclusion region. The nonintersecting crack-inclusion problem is considered for various relative size, orientation, and stiffness parameters, and the stress intensity factors at the ends of the inclusion and the crack are calculated. For the crack-inclusion intersection case, special stress intensity factors are defined and are calculated for various values of the parameters defining the relative size and orientation of the crack and the inclusion and the stiffness of the inclusion.

Xue-Hui, L.↗

The crack-inclusion interaction problem

The general plane elastostatic problem of interaction between a crack and an inclusion is considered. The Green's functions for a pair of dislocations and a pair of concentrated body forces are used to generate the crack and the inclusion. Integral equations are obtained for a line crack and an elastic line inclusion having an arbitrary relative orientation and size. The nature of stress singularity around the end points of rigid and elastic inclusions is described and three special cases of this intersection problem are studied. The problem is solved for an arbitrary uniform stress state away from the crack-inclusion region. The nonintersecting crack-inclusion problem is considered for various relative size, orientation, and stiffness parameters, and the stress intensity factors at the ends of the inclusion and the crack are calculated. For the crack-inclusion intersection case, special stress intensity factors are defined and are calculated for various values of the parameters defining the relative size and orientation of the crack and the inclusion and the stiffness of the inclusion.

Liu, X.-H.↗

Chemical compositions of refractory inclusions from the Vigarano and Leoville carbonaceous chondrites

The contents of the major and the trace elements of three refractory inclusions from Leoville and two hibonite-rich refractory inclusions and a dark clast from Vigarano were investigated using INAA technique, and the results were compared with results reported for an Allende inclusion. It was found that two out of the three refractory inclusions from Leoville and both inclusions from Vigarano have lower Na and Au contents than the coarse-grained inclusion from Allende. It is shown that the concentrations of all volatile elements in refractory inclusions in the Leoville and Vigarano meteorites tend to be either below or at the low end of their concentration ranges in Allende coarse-grained inclusions. This is considered to be due to the fact that the former were altered in parts of the solar nebula where grain-bias separation processes removed the inclusions from chemical communication with the gas at a higher temperature or after a shorter time than for the inclusions from Allende.

Mao, Xue-Ying↗

Distribution of Inclusion-Initiated Fatigue Cracking in Powder Metallurgy Udimet 720 Characterized

In the absence of extrinsic surface damage, the fatigue life of metals is often dictated by the distribution of intrinsic defects. In powder metallurgy (PM) alloys, relatively large defects occur rarely enough that a typical characterization with a limited number of small volume fatigue test specimens will not adequately sample inclusion-initiated damage. Counterintuitively, inclusion-initiated failure has a greater impact on the distribution in PM alloy fatigue lives because they tend to have fewer defects than their cast and wrought counterparts. Although the relative paucity of defects in PM alloys leads to higher mean fatigue lives, the distribution in observed lives tends to be broader. In order to study this important failure initiation mechanism without expending an inordinate number of specimens, a study was undertaken at the NASA Glenn Research Center where known populations of artificial inclusions (seeds) were introduced to production powder. Fatigue specimens were machined from forgings produced from the seeded powder. Considerable effort has been expended in characterizing the crack growth rate from inclusion-initiated cracks in seeded PM alloys. A rotating and translating positioning system, with associated software, was devised to map the surface inclusions in low-cycle fatigue (LCF) test bars and to monitor the crack growth from these inclusions. The preceding graph illustrates the measured extension in fatigue cracks from inclusions on a seeded LCF test bar subjected to cyclic loading at a strain range of 0.8 percent and a strain ratio (max/min) of zero. Notice that the observed inclusions fall into three categories: some do not propagate at all (arrest), some propagate with a decreasing crack growth rate, and a few propagate at increasing rates that can be modeled by fracture mechanics. The following graph shows the measured inclusion-initiated crack growth rates from 10 interrupted LCF tests plotted against stress intensities calculated for semi-elliptical cracks with the observed surface lengths. The expected scatter in the crack growth rates for stress intensity ranges near threshold is observed. These data will be used to help determine the distribution in growth rates of cracks emanating from inclusions as well as the proportion of cracks that arrest under various loading conditions.

Bonacuse, Peter J.↗

Effectiveness of Shot Peening In Suppressing Fatigue Cracking At Non-Metallic Inclusions In Udimet(Registered Trademark)720

The fatigue lives of modern powder metallurgy disk alloys can be reduced over an order of magnitude by cracking at inherent non-metallic inclusions. The objective of this work was to study the effectiveness of shot peening in suppressing LCF crack initiation and growth at surface nonmetallic inclusions. Inclusions were carefully introduced at elevated levels during powder metallurgy processing of the nickel-base disk superalloy Udimet 720. Multiple strain-controlled fatigue tests were then performed on machined specimens with and without shot peened test sections at 427 C and 650 C. The low cycle fatigue lives and failure initiation sites varied as functions of inclusion content, shot peening, and fatigue conditions. A large majority of the failures in as-machined specimens with the introduced inclusions occurred at cracks initiating from inclusions intersecting the specimen surface. These inclusions reduced fatigue life by up to 100X, when compared to lives of material without inclusions residing at specimen surface. Large inclusions produced the greatest reductions in life for tests at low strain ranges and high strain ratios. Shot peening improved life in many cases by reducing the most severe effects of inclusions.

Barrie, Robert L.↗