Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Dendritic growth”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Carbon nanotube (CNT) reinforced 316L stainless steel composites made by laser powder bed fusion: Microstructure and wear response

Carbon nanotube (CNT) reinforced 316L stainless steel (SS) composites were fabricated by laser powder bed fusion (LPBF) additive manufacturing (AM). This study focuses on microstructure evolution, hardness, and wear behavior. The wear behavior for AM 316L SS and 1 wt% CNT/316L SS was studied by a dry sliding test under normal loads of 10, 15, and 25 N. The addition of CNT to 316L SS led to the change of solidification mode from cellular/columnar to dendritic growth, producing grain refinement. Nanoscale dendrites were observed. Although TEM characterization confirmed the existence of CNT in cell interior, most CNT were damaged, resulting in carbon material segregation along cellular/dendritic boundaries. The wear rate was found dramatically decreased due to the improved hardness. Compared to the adhesive and abrasive wear in AM 316L SS, the wear mechanism of CNT/316L composite was adhesion and oxidative wear. Furthermore, enhanced cellular/dendritic boundary strengthening by carbon segregation was the main strengthening mechanism of CNT/316L composite.

36 MATERIALS SCIENCE↗

Visualizing Lithium Dendrite Formation within Solid-State Electrolytes

Solid-state electrolyte (SSE) is promising for application in allsolid-state lithium metal batteries because of its reliable safety and longevity. The failure of SSE to suppress dendrite formation of Li metal anodes has been conventionally explained by uneven Li deposition at Li/SSE interfaces and its subsequent dendritic growth. While Li deposition within SSE has been recently proposed as another key cause for SSE failure, little is known regarding the Li growth details inside the SSE itself. In this work, we performed in situ microscopic observation of Li deposition inside the SSE and obtained visualized evidence regarding the dynamic process of Li dendrite formation and growth. Here, Li is seen to directly nucleate and propagate within the SSE, leading to its structural cracking. Such behavior should be caused by the presence of P- and S-based crystalline defects in Li 3 PS 4 SSE, which is consistent with the cryo-transmission electron microscopy observations and theoretical calculations. This observation provides important insights into the growth mechanisms of Li dendrites within a working lithium battery.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Refining Microstructures in Additively Manufactured Al/Cu Gradients Through TiB 2 Inclusions

Here, the additive manufacture of compositionally graded Al/Cu parts by laser engineered net shaping (LENS) is demonstrated. The use of a blue light build laser enabled deposition on a Cu substrate. The thermal gradient and rapid solidification inherent to selective laser melting enabled mass transport of Cu up to 4 mm from a Cu substrate through a pure Al deposition, providing a means of producing gradients with finer step sizes than the printed layer thicknesses. Divorcing gradient continuity from layer or particle size makes LENS a potentially enabling technology for the manufacture of graded density impactors for ramp compression experiments. Printing graded structures with pure Al, however, was prevented by the growth of Al 2 Cu 3 dendrites and acicular grains amid a matrix of Al 2 Cu. A combination of adding TiB 2 grain refining powder and actively varying print layer composition suppressed the dendritic growth mode and produced an equiaxed microstructure in a compositionally graded part. Material phase was characterized for crystal structure and nanoindentation hardness to enable a discussion of phase evolution in the rapidly solidifying melt pool of a LENS print.

36 MATERIALS SCIENCE↗

Disorder to Order in Interface Patterns: Thermal Noise to Limit Cycle Transition in Dendrite Sidebranch Formation

Thin sample directional solidification experiments have been carried out in the model succinonitrile-camphor system to examine the origin of secondary branches in dendrite morphologies. Thermal noise at the dendrite tip creates interface instabilities which amplify to form sidebranches. This is accepted as the primary mode of sidebranching in dendritic growth from an undercooled melt and occurs in directional solidification of dendrites. The proposed limit cycle couples the growth of the tip with the initiation of the sidebranch. Directional solidification of curved interfaces is a driven dissipative system with the potential to form a limit cycle. Two sets of experiments were performed, the first holding velocity constant and evolving the gradient and the second imposing oscillating velocities around the natural period of sidebranching. Both experimental methods were found to characterize a transition from disordered sidebranching induced by thermal noise to ordered sidebranching produced by the limit cycle mechanisms. This is the first quantitative measurement of previously hypothesized limit cycle growth. These experiment sets have been quantitatively analyzed for dynamic behavior seen in limit cycles. High-quality data sets of the tip and instability enable the measurement of the FFT and analysis through a power spectrum. At low gradients, the sidebranches are found to be excited by thermal noise far away from the tip. As the gradient increases and velocity is held constant, the distance between the instability and tip decreases until limit cycle growth is found between the tip of the primary dendrite and the first forming sidebranch. An alternative to the deterministic limit cycles seen in experiments of gradient evolution is a limit cycle actively driven through the square wave oscillation of velocity. Crucial observations of the solidified microstructure conclude that this produced periodic interconnected bridges between the primary dendrites. This is a finding with potentially significant implications for commercial applications.

Trevor Lyons↗

Silicon web process development

Thirty-five (35) furnace runs were carried out during this quarter, of which 25 produced a total of 120 web crystals. The two main thermal models for the dendritic growth process were completed and are being used to assist the design of the thermal geometry of the web growth apparatus. The first model, a finite element representation of the susceptor and crucible, was refined to give greater precision and resolution in the critical central region of the melt. The second thermal model, which describes the dissipation of the latent heat to generate thickness-velocity data, was completed. Dendritic web samples were fabricated into solar cells using a standard configuration and a standard process for a N(+) -P-P(+) configuration. The detailed engineering design was completed for a new dendritic web growth facility of greater width capability than previous facilities.

Duncan, C. S.↗

Data and Modeling of Dendrites Subject to A Step Change in Pressure (TDSE)

There is considerable interest in dendritic solidification because of the influence dendrites have in the determination of microstructure, and thereby in the physical properties of cast metals and alloys. Current theories and models of dendritic growth generally couple diffusion effects in the melt with the physics of the interface. Data and subsequent analysis prior of the tip growth speed and radii of thermal succinonitrile dendrites in the near-convection free, on-orbit, free-fall environment demonstrate that these theories yield predictions that are reasonably in agreement with the results of experiment. However, data and analysis for assessing the interfacial physics component of theory are not sufficiently detailed or definitive. To study fundamental aspects of dendritic interface stability, we are measuring and modeling the kinetics and morphology of dendrites as they evolve from one well-defined steady state at a pre-set supercooling, through a transient stage, to a different well-defined steady state. More specifically, we subject succinonitrile dendrites, growing under steady-state conditions, to a rapid change in pressure. This leads to a rapid change in thermal driving force from the corresponding change in both the equilibrium melting temperature due to the Clapeyron effect, and a change in the far-field temperature due to adiabatic temperature changes in the bulk liquid and solid. Subsequently, we observe transformations from a well-characterized initial state into a new steady-state. Initial data reveal that the dendrite tip velocity changes almost as fast as the pressure charges, while the tip radius changes occur more slowly, taking from 10 60 seconds depending on the size of the step change and the final supercooling. Computer modeling of this process shows both agreements and disagreements with the experimental data. In making these observations and measurements, we are gaining new understandings of interfacial dynamics and state-selection physics.

Koss, Matthew B.↗

Evolution and Control of 2219 Aluminum Microstructural Features Through Electron Beam Freeform Fabrication

The layer-additive nature of the electron beam freeform fabrication (EBF3) process results in a tortuous thermal path producing complex microstructures including: small homogeneous equiaxed grains; dendritic growth contained within larger grains; and/or pervasive dendritic formation in the interpass regions of the deposits. Several process control variables contribute to the formation of these different microstructures, including translation speed, wire feed rate, beam current and accelerating voltage. In electron beam processing, higher accelerating voltages embed the energy deeper below the surface of the substrate. Two EBF3 systems have been established at NASA Langley, one with a low-voltage (10-30kV) and the other a high-voltage (30-60 kV) electron beam gun. Aluminum alloy 2219 was processed over a range of different variables to explore the design space and correlate the resultant microstructures with the processing parameters. This report is specifically exploring the impact of accelerating voltage. Of particular interest is correlating energy to the resultant material characteristics to determine the potential of achieving microstructural control through precise management of the heat flux and cooling rates during deposition.

Taminger, Karen M.↗

Evolution and Control of 2219 Aluminum Microstructural Features through Electron Beam Freeform Fabrication

Electron beam freeform fabrication (EBF3) is a new layer-additive process that has been developed for near-net shape fabrication of complex structures. EBF3 uses an electron beam to create a molten pool on the surface of a substrate. Wire is fed into the molten pool and the part translated with respect to the beam to build up a 3-dimensional structure one layer at a time. Unlike many other freeform fabrication processes, the energy coupling of the electron beam is extremely well suited to processing of aluminum alloys. The layer-additive nature of the EBF3 process results in a tortuous thermal path producing complex microstructures including: small homogeneous equiaxed grains; dendritic growth contained within larger grains; and/or pervasive dendritic formation in the interpass regions of the deposits. Several process control variables contribute to the formation of these different microstructures, including translation speed, wire feed rate, beam current and accelerating voltage. In electron beam processing, higher accelerating voltages embed the energy deeper below the surface of the substrate. Two EBF3 systems have been established at NASA Langley, one with a low-voltage (10-30kV) and the other a high-voltage (30-60 kV) electron beam gun. Aluminum alloy 2219 was processed over a range of different variables to explore the design space and correlate the resultant microstructures with the processing parameters. This report is specifically exploring the impact of accelerating voltage. Of particular interest is correlating energy to the resultant material characteristics to determine the potential of achieving microstructural control through precise management of the heat flux and cooling rates during deposition.

Taminger, Karen M.↗

Dendritic solidification in a binary alloy melt: Steady-state versus morphological stability theories

A model for dendritic growth in a binary alloy melt, in the presence of a positive temperature gradient in the liquid, is presented. The model describes satisfactorily the transition from a dendritic interface to a planar interface at very low and very large growth rates. A dendrite tip stability parameter is derived, strictly from steady state considerations, without resorting to a perturbation analysis. The estimates of the parameter agree with those obtained by models based on perturbation analyses.

Laymanan, V.↗

Reactive Carbide‐Based Synthesis and Microstructure of NASICON Sodium Metal All Solid‐State Electrolyte

Reactive carbide precursor-based synthesis of NASICON-type NZSP (Na 1+x Zr 2 Si x P 3-x O 12 ) solid-state electrolyte (SSE) is demonstrated, in contrast to the established oxide-based approach. Exothermic decomposition of ZrC and SiC in air homogenizes microstructure, yielding 98% compact density after conventional sintering at 1200 °C. Quantitative stereology demonstrates that significant microstructural differences are present. Compacts of carbide-derived Carb-NZSP are 98% dense with a secondary zirconium oxide (ZrO 2 ) volume fraction of 0.2% ± 0.3%, versus 93% dense and 3% ± 1% for oxide-derived baseline. For Carb-NZSP, the secondary glassy phosphate phase is agglomerated, while for baseline, it is dispersed and percolated. Electrochemical testing combined with post-mortem analysis demonstrates how microstructural control of secondary phases is critical for dendrite suppression: Carb-NZSP critical current density (CCD) is 3.1 ± 0.8 mA cm −2 at 0.1 mAh cm −2 , versus 1.0 ± 0.7 mA cm −2 at 0.1 mAh cm −2 . Cryogenic focused ion beam (cryo-FIB) analysis demonstrates that in both materials, the porous 2D sheet-like sodium metal dendrites propagate around and subsume NZSP grains, likely following a path enriched with glassy phase and with porosity. Dendrites also flow around isolated zirconia particles. Phase field simulation reveals deflection of dendrites by mechanically tough zirconia, while brittle glassy phase accelerates dendrite growth, especially when finely distributed.

36 MATERIALS SCIENCE↗

Microstructure and stability of melt spun INCONEL 713 LC

The alloy IN-714LC was used in an investigation of the effect of process parameters on the microstructure of a rapidly solidified melt-spun material. The resultant ribbon microstructure consisted of several distinct regions, each of which corresponds to a different thermal history during processing. A chill zone of equiaxed randomly-oriented grains exists in a region of the foil which was in contact with the wheel during casting. This zone develops into a dendritic growth morphology with distance away from the lower ribbon surface. Dendrites inclined in the direction of wheel rotation result from growth into a flowing stream. TEM studies showed that a cell structure formed, the cell size decreasing with increasing wheel speed. Aging studies indicated that the cell structure plays an important role in gamma prime precipitation. Results relating to heat treatments (as would be encountered in compaction and use) and the stability of the melt-spun structure are considered.

Antolovich, S. D.↗

Pressure-Tolerant 3D Anodes Enable Short-Circuit Prevention and Low Heat Generation in Argyrodite Solid-State Batteries

Solid-state batteries (SSBs) offer a safer, higher-energy-density alternative to lithium-ion batteries, yet commercialization is hindered by incompatibility with lithium metal. Here, to overcome these challenges, we developed a cost-effective, commercially available prelithiated micro carbon fiber framework (Li-Cf) anode featuring a high-pressure-tolerance, for use with argyrodite solid-state electrolytes (SSEs). This 3D structure accommodates uniform lithium deposition, simplifies cell assembly under elevated pressure, inhibits dendrite growth toward SSEs, reduces heat generation, and enhances overall compatibility. Notably, our architecture enables the cell to tolerate pressures up to 400 MPa without short-circuiting during assembly. Meanwhile, the 3D framework serves as a preferential pathway for lithium deposition, thereby reducing lithium growth toward the SSEs and mitigating the risk of dendrite formation in SSEs. Operando calorimetry and distribution of relaxation times analysis reveal that lithium morphology degradation at the interface with the SSEs is a key failure mechanism in lithium metal argyrodite SSBs, leading to increased diffusion resistance and heat generation. In contrast, the Li-Cf anode mitigates these issues by reducing both heat flux and charge transfer resistance. Full cells with LiNi 0.8 Co 0.1 Mn 0.1 O 2 /Li 6 PS 5 Cl/Li-Cf retain ~79% capacity after 600 cycles, demonstrating significantly improved cycling stability and strong potential for practical energy storage applications.

25 ENERGY STORAGE↗

Primary arm spacing in chill block melt spun Ni-Mo alloys

Chill block melt spun ribbons of Ni-Mo binary alloys containing 8.0 to 41.8 wt % Mo have been prepared under carefully controlled processing conditions. The growth velocity has been determined as a function of distance from the quench surface from the observed ribbon thickness dependence on the melt puddle residence time. Primary arm spacings measured at the midribbon thickness locations show a dependence on growth velocity and alloy composition which is expected from dendritic growth models for binary alloys directionally solidified in a positive temperature gradient.

Tewari, S. N.↗

Cellular microstructure of chill block melt spun Ni-Mo alloys

Chill block melt spun ribbons of Ni-Mo binary alloys containing 8.0 to 41.8 wt pct Mo have been prepared under carefully controlled processing conditions. The growth velocity has been determined as a function of distance from the quench surface from the observed ribbon thickness dependence on the melt puddle residence time. Primary arm spacings measured at the midribbon thickness locations show a dependence on growth velocity and alloy composition which is expected from dendritic growth models for binary alloys directionally solidified in a positive temperature gradient. Microsegregation across cells and its variation with distance from the quench surface and alloy composition have been examined and compared with theoretical predictions.

Tewari, S. N.↗

Primary arm spacing in chill block melt spun Ni-Mo alloys

Chill block melt spun ribbons of Ni-Mo binary alloys containing 8.0 to 41.8 wt pct Mo have been prepared under carefully controlled processing conditions. The growth velocity has been determined as a function of distance from the quench surface from the observed ribbon thickness dependence on the melt puddle residence time. Primary arm spacing measured at the midribbon thickness locations show a dependence on growth velocity and alloy composition which is expected from dendritic growth models for binary alloys directionally solidified in a positive temperature gradient.

Tewari, S. N.↗

Minimizing Segregation during the Controlled Directional Solidification of Dendric Alloys

Gravity-driven convection induced in the liquid by density gradients of temperature or composition disrupts uniform dendritic growth during controlled directional solidification and promotes severe macrosegregation. The solute-rich region about the dendrite tip appears to play a pivotal role in channel initiation. Allen and Hunt referred to this region as an "initial transient" or dynamic region constituting steep concentration gradients. Experimental investigation also point to the role the tip region plays in developing microstructure. Hellawell and co-workers showed that flow-through dendritic channels could be effectively disrupted, and segregation minimized, during the gradient freezing of bulk castings by rotating the melt through a slight angle with respect to Earth's gravity vector. Adapting this principle to controlled directional solidification, it has been shown" that segregation in dendritic alloys can be minimized, and properties improved, by processing the sample near horizontal in conjunction with a slow axial rotation of the crucible. It is postulated that the observed microstructural uniformity arises by maintaining the developing solute field about the dendrite tip. Solute rejected during vertical directional solidification will rise or sink parallel to the primary dendrite arms during axial rotation setting the stage for accumulation, instabilities, and segregation. In contrast, during horizontal growth, the rejected solute will sink or rise perpendicular to the primary dendrite. Now, in the presence of a slight axial rotation, solute that was initially sinking (or rising) will find itself above (or below) its parent dendrite, i.e., still about the tip region. The following is intended to experimentally demonstrate the viability of this concept in coordination with a model that gives predictive insight regarding solute distribution about growing dendrites. Alloys based on the lead-tin eutectic system were used in this study. The system is well characterized, the constituent metals are available in a very pure form, and the thermophysical properties are well known. During solidification of hypoeutectic alloys, e.g., 55 wt pct Pb, the primary dendrites reject the less dense tin, and for the hypereutectic alloys, e.g., 75 wt pct Sn, the primary dendrites reject denser lead. Alloys were prepared by melting appropriate amounts of lead and tin in a glass crucible after which the homogeneous liquid was sucked directly into 5-mm i.d. glass tubes. The sample tube, containing approximately 30 cm of alloy, was then mechanically driven into the directional solidification furnace assembly and positioned such that approx. 20 cm of the sample was remelted. Subsequently, directional solidification was initiated by withdrawing the sample through a water-cooled jacket at a constant growth velocity of 2 ,microns/s. After 5 to 6 cm of growth, the sample was quickly removed from the furnace and quenched in a water bath to preserve the solid-liquid interface. Samples were directionally solidified vertically upward, nearly horizontally, and some in conjunction with an applied axial rotation of the crucible. Temperature gradients at the solid-liquid interface were measured with an in-siru K-type thermocouple. Solidified samples were cut perpendicular and parallel to the growth direction and conventionally prepared for microscopic examination.

Grugel, Richard N.↗

Microsegregation during directional solidification

During the directional solidification of alloys, solute inhomogeneities transverse to the growth direction arise due to morphological instabilities (leading to cellular or dendritic growth) and/or due to convection in the melt. In the absence of convection, the conditions for the onset of morphological instability are given by the linear stability analysis of Mullins and Sekerka. For ordinary solidification rates, the predictions of linear stability analysis are similar to the constitutional supercooling criterion. However, at very rapid solidification rates, linear stability analysis predicts a vast increase in stabilization in comparison to constitutional supercooling.

Coriell, S. R.↗

Preliminary flight results from the second U.S. Microgravity Payload (USMP-2)

The second U.S. Microgravity Payload (USMP-2) was flown on the Space Shuttle in March 1994. It carried four major microgravity experiments plus a sophisticated accelerometer system to record the microgravity environment during USMP-2 operations. The USMP program is designed to accommodate experiments requiring extensive resources short of a full Spacelab mission, and the experiments are remotely operated and monitored. Results are reviewed from the four experiments: the Advanced Automated Directional Solidification Facility (AADSF), the Isothermal Dendrite Growth Experiment (IDGE), the Materiel por Etude des Phenomenes Interessant la Soldification sur Terre et en Orbite (MEPHISTO), and the Critical Fluid Light Scattering Experiment (Zeno). AASDF grew what is expected to be the largest steady-state sample ever of HgCdTe during 240 hours of operation. IDGE provided 60 growth cycles over a wide range of supercooling conditions studying the dendritic solidification of succinonitrile. MEPHISTO achieved 55 melt-solidify cycles and grew over 1 m of Bi/Sn alloy. Zeno located the critical point temperature for liquid Xe to 0.00001 K. IDGE and Zeno also provided the most extensive demonstrations to date of telescience.

Curreri, Peter↗