Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Coated Clad”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Mechanical creep testing and characterization of Cr coated Zircaloy

Zirconium based cladding has been developed for use in light water reactor fuel applications due to the material’s desirable low neutron scattering cross section. To help improve corrosion resistance in accident conditions, such as a loss of coolant accident (LOCA), a chromium coating can be applied to the outer diameter of the Zircaloy tube. Cladding strength at reactor relevant temperatures is important for the structural performance. Stress relaxation creep testing was performed on Cr coated Zircaloy-4 to measure strain rate as a function of stress for 350 and 650°C. These were performed at both 5 ± 1 % and 7.5 ± 1 % strain. The lower temperature provides results near normal operating temperature, while the higher temperature provides results relevant to off-normal conditions where recrystallization will take place. Characterization was also performed to analyze the structure of the Cr coating and Zircaloy-4 as well as the interface between the two.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Radiation response of Ti 2 AlC MAX phase coated Zircaloy-4 for accident tolerant fuel cladding

A Ti 2 AlC MAX phase material was deposited on Zircaloy-4 substrate using the cold spray process, with the goal of enhancing the accident tolerance of zirconium-alloy fuel cladding in light water reactors. The samples were annealed up to 923 K to study the intermetallic phase formation between the coating and Zircaloy-4 substrate. Three interface compounds, ZrAl 2 , ZrAl, and Zr 3 Al, were identified and the activation energy of the interfacial intermetallic compound growth was determined. The radiation response of the coating material and interfacial intermetallic compounds after 3.5 MeV Zr 2+ ion irradiation was investigated by transmission electron microscopy and nanoindentation. Ion irradiation disrupted the nanolamellar structure of the Ti 2 AlC coating while amorphization was observed some of the intermetallic compounds. Furthermore, nanoindentation revealed overall hardening of the Ti 2 AlC coating and Zr 3 Al phase, with no significant change observed in the ZrAl 2 and ZrAl phases.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

NON-DESTRUCTIVE POST IRRADIATION EXAMINATION OF FIRST CYCLE ACCIDENT TOLERANT AND ADVANCED ZIRCONIUM ALLOY HIGH BURNUP FUEL RODS

Post irradiation examination (PIE) of accident tolerant fuel concepts and high burnup uranium dioxide advanced zirconium alloy clad fuel contribute to near term nuclear industry goals of enhancing light water reactor safety and economics. Westinghouse is developing chromium coated zirconium alloy cladding as an accident tolerant fuel option for current pressurized water reactors. Examination of high burnup fuel further augments the technical foundation for extending the peak rod average burnup limits beyond the current regulatory limit of 62 MWd/kgU. Seven fuel rods were received at the Oak Ridge National Laboratory Irradiated Fuel Examination Facility. This includes three chromium coated zirconium alloy fuel rods and four high burnup advanced zirconium alloy fuel rods. Six of the seven rods were fueled with standard uranium dioxide while one of the chromium coated rods contained Westinghouse’s ADOPT fuel. The overall hot-cell PIE plan and some PIE results have been presented previously. This paper focuses on the additional non-destructive examination and fission gas release. Highlights from visual examination of these rods are presented. The chromium coating showed little to no visual change following irradiation. Observations of the axial burnup trends in the fuel rods are derived from full rod axial gamma-ray scans with additional observations related to local fission product migration. The axial dimensional changes of the seven rods are evaluated. As expected, creep down had not yet occurred in the chromium coated rods, and the maximum diameter strain in the high burnup advanced zirconium alloy cladding was less than 0.5%. Finally, the steady state fission gas release for these rods was measured ranging from 4.1% to 17.6% which matched expectation from literature. These fuel rods now await further destructive examination.

Harp, Jason↗

Effect of PVD-coated chromium on the subcooled flow boiling performance of nuclear reactor cladding materials

Here we elucidate the separate effect of a thin Cr coating deposited by physical vapor deposition (PVD) on the subcooled flow boiling performance of zircaloy-4. First, we run flow boiling experiments on prototypical zircaloy-4 surfaces mimicking the scratch pattern and surface roughness of nuclear reactor claddings. Then, we PVD-coat a 0.3 µm thick chromium layer on the same exact surface and repeat the same flow boiling investigations. All experiments are run using deionized water at atmospheric pressure, flowing on a 1 × 3 cm 2 rectangular cross section channel at a rate of 1000 kg/m 2 /s and a subcooling of 10 K. We measure the average temperature of the boiling surface at increasing surface heat fluxes, covering a wide range of heat transfer regimes, from single-phase forced convection to the boiling crisis. We also record high-speed videos of the boiling process, which we postprocess to measure bubble nucleation site density, growth time, departure diameter and frequency. The surface analysis reveals that, while the chromium coating does not seem change the surface roughness and morphology, it improves surface wettability. However, it decreases the critical heat flux. The chromium coating causes an increase of nucleation temperature, bubble departure diameter and growth time, and a reduction of the nucleation site density. The concurrence of these observations indicates that a size reduction of the nucleation sites, conformally covered by the chromium coating, may be the cause of the boiling performance deterioration. We confirm this hypothesis repeating the same analysis on a FeCrAl sample prepared and tested using the same protocol as the zircaloy-4 sample, but with a different initial surface texture.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Effects of sample bias on adhesion of magnetron sputtered Cr coatings on SiC

Swelling of SiC at 300 C due to in-service neutron irradiation causes tensile residual stresses in coatings which are expected to adversely affect the performance of coated SiC composite fuel cladding for light water reactors. Matching the coating swelling with the substrate, a solution common for thermal expansion, is not practical in the case of neutron irradiation. Biasing samples during magnetron sputtering deposition induces compressive residual stress which may counteract this. In this study, chromium coatings were deposited on SiC by DC magnetron sputtering with no external heating at bias voltages of –50V, –75V, and –100V. The effects of the bias voltage on morphology, residual stress, microstrain, texture, and adhesion are shown. The low deposition temperature resulted in the coating microstructure evolution following an energetic particle bombardment dominated trend. Additionally, at the two lower bias voltages knock-on implantation dominated increasing the residual stress and microstrain while at the highest bias voltage, thermal spike migration allowed for defect relaxation. When the knock-on induced compressive residual stress exceeded 0.8 GPa microcrack formation in the SiC substrate decreased coating adhesion. While no microcracks formed at the lowest bias voltage, insufficient atomic mobility during coating growth lead to voids forming in the coating. A balance is needed to form void-free coatings that have high compressive residual stress.

36 MATERIALS SCIENCE↗

Zirconium nanoparticle coating development for FCCI diffusion barrier in nuclear cladding

Fuel clad chemical interaction (FCCI) is a pervasive issue for metallic nuclear fuels. FCCI can damage cladding, reduce thermal efficiency, and compromise the structural integrity of the fuel rod. In this study, we evaluated the FCCI mitigation capabilities of electrophoretically-deposited Zr nanoparticle coatings on ferritic-martensitic stainless-steel cladding (HT9). Zr was deposited on the internal surface of 6 mm outer diameter cladding using electrophoretic deposition (EPD). Thickness varied among samples with similar EPD conditions. A uniformly coated sample was selected and sent to the Argonne Tandem Linac Accelerator System (ATLAS) to simulate the coating's behavior under irradiation conditions. Furthermore, the coating prevented FCCI in diffusion couple studies. Results of this study confirm that Zr could potentially make an effective FCCI barrier in metallic fuel rods but the deposition process needs improvement.

36 MATERIALS SCIENCE↗

Advanced surface plasma nitriding for development of corrosion resistant and accident tolerant fuel cladding: Final Report

Although various surface coating techniques have been proposed to increase oxidation and corrosion resistance of fuel cladding materials, the de-bonding of the coating layer with the original cladding matrix under exposure to coolants makes such approaches unsuitable for reactor applications. Furthermore, the feasibility of techniques for large scale processing on cladding tubes remains another technological bottleneck. This project aims to develop a hollow cathode plasma nitriding technique to solve the above issues. Starting with alloys of DOE interest, the team will apply an advanced surface plasma nitriding technique to convert alloy surface layers into nitride layers for better structural integrity and compatibility with both coolants and nuclear fuels. The technique can form uniform nitride layers on both inner and outer surfaces of cylindrical hollow tubes. Both treated and untreated samples will be irradiated by using Fe self ions or dual beams of Fe ions and He ions. Various microstructural characterizations and mechanical property measurements will be performed. For outside surfaces, samples will be tested in high temperature water and liquid molten salt to evaluate their corrosion resistance and compatibility with coolants for LWR and fast reactor applications. For inside surfaces, solid-to-solid diffusion couple experiments will be used to study interface reactions of nitrided samples with uranium, to test whether a nitrided layer can slow down fuel-cladding interactions. The project will impact both the development of advanced methods for manufacturing and the development of advanced reactor in-core structural materials. The proposed technique can form nitride layers on alloys of irregular shapes without an edging effect - an issue encountered in traditional plasma nitriding processes, and is suitable for surface processing of other in-core components.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Particle-modified polymeric cladding on glass optical fibers enhances radial light scattering

Radially light-emitting optical fibers are of increasing interest for applications in medicine, visible aesthetics, and environmental remediation. Optical fibers contain a light guiding core coated by protective polymer layers (cladding and coating), which assure both the strength and flexibility of the optical fiber. This paper examines the feasibility of scattering light radially from fibers by loading the fiber cladding with particle scattering centers during the optical fiber fabrication process. This work uses an in-line full-scale scalable facility to coat the fibers and control the polymer cladding and silica sphere. Loadings up to 2.0 wt. % of 500 nm silica particles on the cladding of the optical fiber led to an average of 80 times higher scattering for visible light and up to 30 times higher in the UVA wavelength range compared against cladding without particle modifications. We report this study illustrated the feasibility of fabricating broadband light scattering optical fibers for use with modified polymeric cladding.

47 OTHER INSTRUMENTATION↗

High-resolution characterization of ceramic-metal interface of TiN coating on ferritic-steels for nuclear application

Advanced fuel cladding is critical for fast reactors, offering sufficient thermal conductivity, mechanical and dimensional stability and radiation tolerance of the cladding base material. Additionally, it must provide corrosion resistance and high temperature coolant compatibility on the cladding outer surface, as well as chemical stability on the cladding inner wall against fuel cladding chemical interaction (FCCI). TiN ceramic coating has been considered an effective diffusion barrier for inner and outer cladding-walls for enhanced performance. The TiN-metal interface microstructure and chemistry play a critical role in coating bond strength and integrity under harsh conditions. High-resolution transmission electron microscopy characterization of ceramic-metal interface at atomic resolution in unirradiated, irradiated and thermal cycled conditions were performed. The interface remained intact after irradiation up to 200 dpa or thermal cycling five times up to 550 °C. In conclusion, this work discusses the potential impact of these results on coating performance and design for advanced claddings.

36 - MATERIALS SCIENCE↗

Single Rod Reflood Quenching Experiments with Simulated Decay Heat for Accident-Tolerant Fuel Claddings

The Loss-of-Coolant Accident (LOCA) is a hypothetical situation which includes a sudden loss of coolant, overheating of fuel rods, and emergency coolant injection. This situation could be modeled as a quenching process of cladding material into the coolants, a reverse process of boiling the coolants. The KAERI have been developing a CrAl-coating type Accident-Tolerant Fuel (ATF) claddings to enhance safety margin in such severe accident situations and evaluations for the performance in various aspects are on process. We established a single-rod type reflood quenching experiment setup to simulate the LOCA process. Unlike other conventional quenching experiment setup, our experiment setup is capable of heating during the reflooding process, simulating the decay heat in the real core. We installed heaters and thermocouples (TC) inside the cladding specimens to minimize any disturbances on the interfacial layer during the experiment. Currently the setup is on test run and we present experiment data and verification with conventional Zircaloy-4 claddings. We are going to conduct the reflood quenching experiment with KAERI's CrAl-coated ATF claddings to evaluate the cooling performances.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of ATF Cr-coated-Zircaloy on BWR In-vessel Accident Progression during a Station Blackout

The deposition of protective coatings on nuclear fuel cladding has been considered as a near-term Accident Tolerant Fuel (ATF) concept that will reduce the high-temperature oxidation rate and enhance accident tolerance of the cladding while providing additional benefits during normal and transient. In this study, the performance of the proposed ATF concept of Cr-coated-Zircaloy is assessed using a generic Boiling Water Reactor MELCOR plant model considering a Short-term Station Blackout (STSBO) scenario. Simulation results indicate that the use of Cr-coated-Zircaloy as cladding and canister material mitigates the core degradation process as compared to the traditional Zircaloy cladding and canister design. The onset of fuel degradation and collapse is delayed by over thirty minutes, and the extent of fuel degradation is reduced. Specifically, the gross in-vessel hydrogen generation decreased by almost a factor of three. Although the eutectic reaction between Cr-coating and Zircaloy could cause an early failure of the coating, the improvement in the delay of fuel degradation is still notable. In addition, a thicker coating is found helpful to obtain additional coping time and to decrease hydrogen generation. In addition to the eutectic formation that may compromise Cr-coated Zr, a different failure mode is identified for the Cr-coated-Zr when compared to Zircaloy; i.e., a complete melt of base material leads to component collapse before the coating is oxidized and consumed. These findings can help the industry focus on productive areas of research and development for accident-tolerant fuel concepts and enhancement of core safety margins.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Modifications to MELCOR 1.8.6 for modeling Accident Tolerant Fuel in Boiling Water Reactors

This work describes further modifications made to a previously implemented User-Defined Generalized Coating (UDGC) model in MELCOR 1.8.6. The UDGC version of the code allows for the modeling of cladding and canister materials other than Zircaloy (without overwriting Zircaloy properties) as well as coated Zircaloy cladding and canisters, with the thermophysical and oxidation properties of the clad or coating material specified by the user. Specific changes outlined in this report are the extension of the UDGC models to BWR canisters, and generalization of the oxidation model for all UDGC components to accommodate different oxidation rate correlations in two different temperature ranges. User input requirements are specified and an example case is described that illustrates the potential impact of model assumptions.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Formation of Ti-Al intermetallics on a surface of titanium by non-vacuum electron beam treatment

Highlights: • Electron beam cladding allows fabricating thick intermetallic coatings on Ti surface. • By variation of Ti:Al ratio the phase composition of the coatings can be controlled. • Oxidation resistance of clads increase with increase of Al content. • Single-phase Ti{sub 3}Al coating provides the highest microhardness and wear resistance. - Abstract: Titanium and titanium alloys are highly important structural materials for many industries where low density in combination with high mechanical strength and corrosion resistance are required. However, titanium is not applicable for tribological or high temperatures purposes due to its interaction with atmospheric gases and friction seizure during the contact with most metallic materials. To protect the surface of titanium and improve its wear resistance intermetallic coatings can be applied. In this study, the Ti-Al intermetallic layers were fabricated on Ti surface by electron beam melting of Al and Ti powders. By variation of Al/Ti ratio in the initial powders it was possible to control elemental and phase composition of the layers. The formation of TiAl, Al{sub 2}Ti and Ti{sub 3}Al phases was observed in the layers. Independently on Al content the layers had lamellar type of structure. Microhardness, wear resistance and oxidation resistance were measured to evaluate the quality of the layers. The microhardness and wear resistance were in good agreement with each other. The coating, consisted of pure Ti{sub 3}Al phase, demonstrated the highest level of these properties. Oxidation resistance of the coatings increased proportionally to the aluminium content due to formation of alumina in oxide scale.

36 MATERIALS SCIENCE↗

Steam oxidation of chromium corrosion barrier coatings for sic-based accident tolerant fuel cladding

SiC-based materials are currently being considered for accident tolerant fuel (ATF) cladding, however, there are concerns regarding hydrothermal corrosion rates and hermeticity. These issues may be addressed with the utilization of a Cr corrosion barrier coating (CBC) but the interaction of Cr with SiC under loss of coolant accident (LOCA) conditions needs to be investigated. In the present work, Cr coatings were deposited onto chemically vapor deposited (CVD) SiC with either high power impulse magnetron sputtering (HiPIMS), cathodic arc (CA), or a combination of both. Annealing and steam thermogravimetric analysis (TGA) was used to study reaction product formation with and without oxidation. Additionally, after 1200 °C annealing, formation of a Cr x C y carbide layer at the ambient interface and a Cr x Si y C z silicide layer at the SiC interface was observed. After 1200 °C TGA exposure, similar carbide and silicide layers were observed but with a Cr 2 O 3 outer reaction layer and a Si and O rich interfacial layer forming between the carbide and silicide layers. Initial mass gain of the coatings during the 1200 °C TGA exposure was parabolic and were similar to reported rates of chromia formation. Mass gain behavior and observed transitions in chromia microstructure indicate that metallic Cr may be consumed within the first ~1 h at 1200 °C and that subsequent chromia formation occurs at the expense of the underlying Cr carbide layer. Overall, the results show no detrimental impact of Cr coatings on the steam oxidation resistance of SiC up to 4 h at 1200 °C.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗