Friction and Wear Characteristics of Cu-4Al Foil Bearing Coating at 25 and 650 degree C

The friction and wear performance of a Cu-4Al top foil coating has been investigated in Generation I foil air bearings. The copper alloy was applied by a novel deposition technique (ion diffusion) and the journal was coated with PS304, a plasma spray deposited high temperature composite solid lubricant coating. The ion diffusion coating process deposits a desirable smooth layer compared to other methods like cathodic arc deposition. The tribological performance of bearings with and without Cu-4Al foil coatings were evaluated through start-stop tests on an air bearing test rig at 25 and 650 C. The results indicate that the Cu-4Al assists during the initial break-in period, gives more stable friction performance with respect to temperature, and appears to prevent top foil wear at high temperature. The measured load capacity coefficient was 0.5, which was comparable to earlier testing of more advanced design Generation III bearings coated with standard cathodic arc deposited Cu-4Al. However, further studies are needed to determine if deeper penetration of the copper alloy into the foil would help make the transition in friction behavior from contact with the Cu-4Al coated foil to contact with the base foil material more gradual. Also, future work is recommended to assess the performance of ion diffusion coatings with different Cu-based alloy compositions and to investigate the effect the coating has on the elastic modulus of the foil material.

Stanford, Malcolm K.↗

Colloidal Platinum–Copper Nanocrystal Alloy Catalysts Surpass Platinum in Low-Temperature Propene Combustion

Low-temperature removal of noxious environmental emissions plays a critical role in minimizing the harmful effects of hydrocarbon fuels. Emission-control catalysts typically consist of large quantities of rare, noble metals (e.g., platinum and palladium), which are expensive and environmentally damaging metals to extract. Alloying with cheaper base metals offers the potential to boost catalytic activity while optimizing the use of noble metals. In this work, we show that Pt x Cu 100–x catalysts prepared from colloidal nanocrystals are more active than the corresponding Pt catalysts for complete propene oxidation. By carefully controlling their composition while maintaining nanocrystal size, alloys with dilute Cu concentrations (15–30% atomic fraction) demonstrate promoted activity compared to pure Pt. Complete propene oxidation was observed at temperatures as low as 150 °C in the presence of steam, and five to ten times higher turnover frequencies were found compared to monometallic Pt catalysts. Additionally, through DFT studies and structural and catalytic characterization, the remarkable activity of dilute Pt x Cu 100–x alloys was related to the tuning of the electronic structure of Pt to reach optimal binding energies of C* and O* intermediates. This work provides a general approach toward investigation of structure–property relationships of alloyed catalysts with efficient and optimized use of noble metals.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Copper-Tin Alloys for the Electrocatalytic Reduction of CO2 in an Imidazolium-Based Non-Aqueous Electrolyte

The ability to synthesize value-added chemicals directly from CO2 will be an important technological advancement for future generations. Using solar energy to drive thermodynamically uphill electrochemical reactions allows for near carbon-neutral processes that can convert CO2 into energy-rich carbon-based fuels. Here, we report on the use of inexpensive CuSn alloys to convert CO2 into CO in an acetonitrile/imidazolium-based electrolyte. Synergistic interactions between the CuSn catalyst and the imidazolium cation enables the electrocatalytic conversion of CO2 into CO at −1.65 V versus the standard calomel electrode (SCE). This catalyst system is characterized by overpotentials for CO2 reduction that are similar to more expensive Au- and Ag-based catalysts, and also shows that the efficacy of the CO2 reduction reaction can be tuned by varying the CuSn ratio.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-Temperature, Low-Cycle Fatigue of Copper-Base Alloys for Rocket Nozzles. Part 1: Data Summary for Materials Tested in Prior Programs

A more detailed analysis of the results obtained in 188 previously reported low-cycle fatigue tests of various candidate materials for regeneratively-cooled, reusable rocket nozzle liners was reported. Plots of load range versus cycles were reported for each test along with a stress-strain hysteresis loop near half-life. In addition, a summary table was provided to compare N5 (cycles to a five percent load range drop) and Nf (cycles to complete specimen separation) values for each test.

Conway, J. B.↗

High temperature low cycle fatigue mechanisms for nickel base and a copper base alloy

Damage mechanisms were studied in Rene' 95 and NARloy Z, using optical, scanning and transmission in microscopy. In necklace Rene' 95, crack initiation was mainly associated with cracking of surface MC carbides, except for hold time tests at higher strain ranges where initiation was associated more with a grain boundary mechanism. A mixed mode of propagation with a faceted fracture morphology was typical for all cycle characters. The dependence of life on maximum tensile stress can be demonstrated by the data falling onto three lines corresponding to the three tensile hold times, in the life against maximum tensile stress plot. In NARloy Z, crack initiation was always at the grain boundaries. The mode of crack propagation depended on the cycle character. The life decreased with decreasing strain rate and with tensile holds. In terms of damage mode, different life prediction laws may be applicable to different cycle characters.

Shih, C. I.↗

On Heat-Treatable Copper-Chromium Alloy, 1

A mother alloy of 10% Cr and 90% Cu was prepared by sintering. This was alloyed with the Cu melt and Cu-Cr alloys containing about 0.5% Cr was obtained. These alloys could be deformed easily in both the hot and cold states. By measuring the hardness change, age-hardening properties of cast alloys were studied, which were quenched from 950 deg and aged at 300 to 700 deg for 1 hour. The maximum hardness was obtained with the tempering temperature of 500 deg. For the temperature of solution-treatment, 950 deg was insufficient and that above 1000 deg necessary. For the tempering time, a treatment at 500 deg for 1 hr. or at 450 deg for 3 hrs. yielded the maximum hardness. As for the properties for electrical conductors, 3 kinds of wires (diam. 2 mm.) were made: (1) after cold-drawn to 2 mm., solution-treated, quenched, and then tempered (500 deg, 1 hr.); (2) after quenching, cold-drawn (75% reduction) to 2 mm. and tempered (500 deg, 1 hr.); and (3) after quenching, cold-drawn (81%) to intermediate diameter, tempered (500 deg, 1 hr.) and then cold-drawn (88%) again. Properties obtained for the 3 kinds, respectively, were as follows: conductivity 91, 90, and 86%. Tensile strength and strength for electrical conductivity are given.

Koda, S.↗

Initial aging phenomena in copper-chromium alloys

The effects of quenching and aging temperatures on the initial aging curves of Cu-Cr alloy were examined mainly by means of electrical resistivity measurements. Three Cu-Cr alloy specimens having 0.24, 0.74, and 1.0% Cr were solution-treated at 950-1050 C, quenched into ice-water, and subsequently aged at 300-500 C. The results were as follows: (1) At the very early stage of aging (within about 30 sec), an abrupt decrease of resistivity with lowering aging tempratures. (T sub A) and rising solution temperatures (T sub S) was observed at (T sub A) up to about 400 C. In contrast, a transient increase of resistivity with rising T sub A and lowering T sub S was observed at T sub A from about 450 to 500 C. These phenomena seem to be caused by a rapid formation of solute clusters and the reversion of clusters formed during quenching, which are enhanced by quenched-in vacancies, respectively. (2) The amount of precipitation increased at the latter stage of aging with rising T sub S and T sub A as generally expected, where T sub S was not so high as to form secondary defects. (3) As a result, the initial aging phenomena in Cr-Cr alloy were revealed to be complicated against expectations. This was considered to be due to the migration energy of vacancies so larger in Cu-base.

Suzuki, H.↗

Lifing of Engine Components

The successful development of advanced aerospace engines depends greatly on the capabilities of high performance materials and structures. Advanced materials, such as nickel based single crystal alloys, metal foam, advanced copper alloys, and ceramics matrix composites, have been engineered to provide higher engine temperature and stress capabilities. Thermal barrier coatings have been developed to improve component durability and fuel efficiency, by reducing the substrate hot wall metal temperature and protecting against oxidation and blanching. However, these coatings are prone to oxidation and delamination failures. In order to implement the use of these materials in advanced engines, it is necessary to understand and model the evolution of damage of the metal substrate as well as the coating under actual engine conditions. The models and the understanding of material behavior are utilized in the development of a life prediction methodology for hot section components. The research activities were focused on determining the stress and strain fields in an engine environment under combined thermo-mechanical loads to develop life prediction methodologies consistent with the observed damage formation of the coating and the substrates.

Source record↗

Experimental Investigations on Pulsed Nd:YAG Laser Welding of C17300 Copper-Beryllium and 49Ni-Fe Soft Magnetic Alloys

Copper-beryllium and soft magnetic alloys must be joined in electrical and electro-mechanical applications. There is a high difference in melting temperatures of these alloys which cause to make the joining process very difficult. In addition, copper-beryllium alloys are of age hardenable alloys and precipitations can brittle the weld. 49Ni-Fe alloy is very hot crack sensitive. Moreover, these alloys have different heat transfer coefficients and reflection of laser beam in laser welding process. Therefore, the control of welding parameters on the formation of adequate weld puddle composition is very difficult. Laser welding is an advanced technique for joining of dissimilar materials since it can precisely control and adjust the welding parameters. In this study, a 100W Nd:YAG pulsed laser machine was used for joining 49Ni-Fe soft magnetic to C17300 copper-beryllium alloys. Welding of samples was carried out autogenously by changing the pulse duration, diameter of beam, welding speed, voltage and frequency. The spacing between samples was set to almost zero. The ample were butt welded. It was required to apply high voltage in this study due to high reflection coefficient of copper alloys. Metallography, SEM analysis, XRD and microhardness measurement was used for survey of results. The results show that the weld strength depends upon the chemical composition of the joints. To change the wells composition and heat input of the welds, it was attempted to deviate the laser focus away from the weld centerline. The best strength was achieved by deviation of the laser beam away about 0.1mm from the weld centerline. The result shows no intermetallic compounds if the laser beam is deviated away from the joint.

36 MATERIALS SCIENCE↗

Structural-Phase Features of Low-Stability Pre-Transitional States of BCC-Alloys with Complexes of Planar Defects (Antiphase Boundaries)

Using the Monte Carlo method, the influence of the complexes of antiphase boundaries (APBs) (a pair of shear APBs and a pair of thermal APBs) on the low-stability, pre-transitional states of BCC-alloys is considered by the example of a conventional copper alloy CuZn and an intermetallic compound NiAl. It is shown that in the region of low-stability structural-phase states the energy of formation of a complex of thermal APBs is higher than that of shear APBs. The contribution of APBs into disordering is appreciable up to the structural-phase transition temperature. The most significant factor in terms of the long-range order is the formation of the defect itself; the differences in the APB type or the plane of their occurrence do not so much affect the longrange order behavior with the temperature variation. The type of APBs however appreciably affects the structural-energy characteristics of the system at the temperatures below the phase transformation temperature. Logically, a system with structural defects is less ordered than a defect-free system. The presence of a defect favors the onset of disordering at lower temperatures: it starts at lower temperatures in the case of thermal APBs (TAPBs) compared to shear APBs (TAPBs). In a BCC-system with a complex of TAPBs the first signs of disordering invariably appear near the phase boundary in the neighborhood of large atoms (Zn–Zn in the CuZn alloy or Al–Al in the NiAl intermetallide). In the alloy with a complex of shear APBs the distortion of ordering at low temperatures is observed in the regions where the boundaries cross. The presence of antiphase boundaries affects the alloy stability under heating. It is shown that disordering is accompanied by smearing of the boundaries and their faceting. It follows from a comparative analysis of the peculiarities of disordering in the BCC-system under study (classical alloy CuZn and intermetallide NiAl) under conditions of higher temperatures in the region of low-stability, pre-transitional states that the order – disorder phase transition in the CuZn alloy takes place as a result of disordering of the system, while in the intermetallide NiAl the change of long-range order results from the structural-phase transition.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗