Understanding failure in austenitic steels: Key considerations for molten salt storage in CSP applications

Owing to their excellent properties, austenitic stainless steels are extensively used in boilers, furnaces, molten salt tanks, and other applications that are subjected to extreme mechanical loads and high-temperature conditions. Their high corrosion and creep resistance make them suitable for high-temperature operating environments. Additionally, good fatigue resistance and favorable mechanical and visual properties are essential. However, the premature failure of several components at elevated temperatures has been previously reported. Although the failure analysis of components in service is complex, processes such as cold work and welding have been identified as contributing factors to the performance degradation of these steels. This study aims to analyze the various documented failure modes and mechanisms in austenitic steels, including creep, cracking, stress relaxation cracking, and fatigue, to better understand the multi-objective design requirements for these alloys as structural materials for high-temperature molten salt tanks in Concentrating Solar Power (CSP) plants. Stabilized austenitic grades, such as AISI 347H, demonstrate superior resistance to creep and corrosion-related degradation when compared to non-stabilized grades like AISI 316L at temperatures relevant to concentrated solar power (CSP) applications. In contrast, nickel-based alloys offer enhanced corrosion resistance, albeit at a higher cost. This review underscores that creep, stress relaxation cracking, and thermo-mechanical fatigue are the predominant long-term failure risks in CSP hot tanks.

14 SOLAR ENERGY↗

Nano-cavities observed in a 316SS PWR Flux Thimble Tube Irradiated to 33 and 70 dpa

The radiation-induced microstructure of a cold-worked 316SS flux thimble tube from an operating pressurized water reactor (PWR) was examined. Two irradiated conditions, 33 dpa at 290ºC and 70 dpa at 315ºC were examined by transmission electron microscopy. The original dislocation network had completely disappeared and was replaced by fine dispersions of Frank loops and small nano-cavities at high densities. The latter appear to be bubbles containing high levels of helium and hydrogen. An enhanced distribution of these nano-cavities was found at grain boundaries and may play a role in the increased susceptibility of the irradiated 316SS to intergranular failure of specimens from this tube during post-irradiation slow strain rate testing in PWR water conditions.

Edwards, Danny J↗

Helium effects on microstructural evolution in tempered martensitic steels: In situ helium implanter studies in HFIR

Microstructural evolutions in tempered martensitic steels (TMS) under neutron-irradiation, at fusion relevant He/dpa ratios and dpa rates, were characterized using a novel in situ He-implanter technique. F82H-mod3 was irradiated at 500 C in HFIR to a nominal 9 dpa and 190 or 380 appm He in both in the as-tempered (AT) and 20% cold-worked (CW) conditions. In all cases, a high number density of 1-2 nm He-bubbles were observed, along with fewer but larger 10 nm void-like faceted cavities. The He-bubbles form preferentially on dislocations and various interfaces. A slightly larger number of smaller He bubbles were observed in the CW condition. The lower He/dpa ratio produced slightly smaller and fewer He-bubbles. Comparisons of these observations to the results in nano-structured ferritic alloy (NFA) MA957 provide additional evidence that TMS may be susceptible to He-embrittlement as well as void swelling at fusion relevant He concentrations, while NFA are much more resistant to these degradation phenomena.

36 MATERIALS SCIENCE↗

Analysis of Tensile Deformation and Failure in Austenitic Stainless Steels: Part II- Irradiation Dose Dependence

Irradiation effects on stable and unstable deformations and fracture behaviors in irradiated austenitic stainless steels (SSs) have been studied in detail based on the equivalent true stress versus true strain curves. An iterative technique in finite element simulation was used to obtain the equivalent true stress-true strain data from experimental tensile curves. It was shown that the strain hardening rate was retained at a high level on unstable deformation after significant irradiation and was independent of the irradiation dose up to the initiation of a localized necking. The equivalent fracture stress was nearly independent of irradiation dose before the damage (embrittlement) mechanism changed. In low dose range (< ~ 2dpa), the fracture strain and tensile fracture energy decreased rapidly with dose and at higher doses they decreased gradually to saturated levels, which were still high for irradiated materials. It was also found that the fracture properties for EC316LN SS were less sensitive to irradiation dose than those for 316 SS, although their uniform tensile properties showed almost the same dose dependencies. It was confirmed that the dose dependence of tensile fracture properties evaluated by the linear approximation model for nominal stress was accurate enough for practical use without elaborate calculations.

36 MATERIALS SCIENCE↗

Preliminary Evaluation of Cavitation-Erosion Resistance of Ti-Alloys in Mercury for the Spallation Neutron Source

A number of Ti-based alloys in both the mill-annealed and 20% cold-worked conditions were subjected to sonication conditions in Hg using a vibratory horn to assess relative cavitation-erosion resistance. Weight loss as a function of exposure time was roughly proportional to hardness for all alloys/conditions examined, with Ti-6Al-4V (Ti-Grade 5) and Ti-6Al-2Sn-4Zr-2Mo yielding the best resistance to cavitation-erosion as evidenced by low weight losses and little or no tendency to form pits on the exposed surface. Unalloyed Ti (Ti-Grade 4) and Ti-0.12Pd (Ti-Grade 7) exhibited greater weight losses by a factor or about two and about five, respectively, with Ti-0.12Pd particularly prone to pitting development. The mean erosion rates of the best two Ti-alloys examined here were about a factor of three higher than identically tested 316LN stainless steel following a low temperature carburizing treatment, but this difference is considered minor given that the rate for both materials is very low/manageable and represents a through-thickness property for the Ti-alloys. A nitriding surface treatment was also evaluated as a potential method to further increase the cavitation-erosion resistance of these alloys in Hg, but the selected treatment proved largely ineffective. Recommendations for further work to evaluate the efficacy of Ti-based alloys for use in high-powered targets for the Spallation Neutron Source are given.

36 MATERIALS SCIENCE↗

Theoretical investigation of microstructure evolution and deformation of zirconium under neutron irradiation

We studied the radiation growth of zirconium using a reaction–diffusion model which takes into account intra-cascade clustering of self-interstitial atoms and one-dimensional diffusion of interstitial clusters. The observed dose dependence of strain rates is accounted for by accumulation of sessile dislocation loops during irradiation. Moreover, the computational model developed and fitted to available experimental data is applied to study deformation of Zr single crystals under irradiation up to hundred dpa. Finally, the effect of cold work and the reasons for negative prismatic strains and co-existence of vacancy and interstitial loops are elucidated.

36 MATERIALS SCIENCE↗

In situ synchrotron X-ray diffraction study of hydrides in Zircaloy-4 during thermomechanical cycling

The d-spacing evolution of both in-plane and out-of-plane hydrides has been studied using in situ synchrotron radiation X-ray diffraction during thermo-mechanical cycling of cold-worked stress-relieved Zircaloy-4. The structure of the hydride precipitates is such that the δ{111} d-spacing of the planes aligned with the hydride platelet face is greater than the d-spacing of the 111 planes aligned with the platelet edges. Upon heating from room temperature, the δ{111} planes aligned with hydride plate edges exhibit bi-linear thermally-induced expansion. In contrast, the d-spacing of the (111) plane aligned with the hydride plate face initially contracts upon heating. Furthermore, these experimental results can be understood in terms of a reversal of stress state associated with precipitating or dissolving hydride platelets within the α-zirconium matrix.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Swelling resistance of advanced austenitic alloy A709 and its comparison with 316 stainless steel at high damage levels

Alloy A709 is an austenitic alloy developed for power boiler applications in thermal power plants and is being considered as a candidate structural material for Generation IV reactors and fusion reactors, based especially on its increased creep strength over Type 316 stainless steel. However, improved thermal creep properties would not necessarily imply improved radiation resistance, especially with respect to void swelling. Since there are currently no neutron irradiation data on A709 to high fluences, A709 and cold-worked 316 were irradiated in the present study under identical conditions to doses between 100 and 400 peak dpa using irradiation by 3.5 MeV Fe +2 ions. The swelling behavior of 316 is well-known for both neutron and ion irradiation, thus the relative swelling behavior of A709 and 316 under ion irradiation might provide an indication of the swelling behavior of A709 in neutron irradiation environment. Swelling of A709 under ion irradiation was observed over the range of 500-600 ⁰C, peaking at 575 ⁰C. Both A709 and 316 eventually swelled at a rate of ~1 %/dpa under ion irradiation at 575 ⁰C, consistent with the swelling of 316 observed during neutron irradiation. But A709 had a significantly longer transient regime than 316 at any given dpa rate, demonstrating enhanced swelling resistance of A709 over 316 under self-ion irradiation. The swelling levels reached at 400 peak dpa were 55% and 90% for A709 and 316, respectively. The assigned local dpa levels were adjusted both temporally and spatially at each dose for swelling-induced increases in the ion range and concomitant decreases in density. The duration of the transient regimes in each alloy was also observed to increase as the local dpa rate increased, an observation also consistent with neutron irradiation behavior of 316 stainless steel.

36 MATERIALS SCIENCE↗

Cluster dynamics modeling of irradiation growth in single crystal Zr

Irradiation growth of single-crystal Zr is modeled with a reduced set of cluster dynamics equations. Nucleation and growth of basal and prismatic dislocation loops are both accounted for in the model. Equations are developed for the time evolution of single point defects, a limited number of point defect clusters, interstitial and vacancy loop nucleation rates, as well as for the growth of vacancy loops on basal planes and interstitial loops on prismatic planes. Reduction of the usual infinite hierarchy of cluster dynamics equations to the simple set studied here is justified on the physical basis of the stability of small loops once nucleated. This simplified cluster dynamics model with a small number of adjustable parameters avoids the complexity of explicit representation of higher order point defect clusters. The model shows consistency with experimental observations of the following aspects: (1) the growth rates of Zr crystals along the a- and c-axes; (2) the onset dose for breakaway irradiation growth; (3) the saturation dislocation loop densities of vacancy and interstitial loops; (4) the effects of cold work and temperature on irradiation growth.

36 MATERIALS SCIENCE↗

Heavy ion irradiation response of an additively manufactured 316LN stainless steel

Additive manufacturing has become an appealing technique to fabricate three-dimensional metallic materials and components for nuclear reactors. However, response of additively manufactured alloys to high-dose heavy ion irradiations at elevated temperatures is still not well understood. Here, an additively manufactured 316LN austenitic stainless steel with high-density solidification cells was irradiated using 3.5 MeV Fe ion to a peak dose of 220 dpa at 450 °C. Microscopy studies show a lower Frank loop density and smaller size in the additively manufactured sample compared with its cold worked counterpart, and the cellular structures may largely suppress the formation of perfect loops and dislocation networks and reduce the magnitude of solute segregations comparing with high angle grain boundaries. In conclusion, the present work advances the understanding on the high-temperature irradiation response of additively manufactured steels for nuclear reactor applications.

36 MATERIALS SCIENCE↗

Mechanical and Thermophysical properties of low enriched uranium-10wt% molybdenum rolled foils

In this study, low-enriched (~19.75% 235 U) U-10Mo(wt%) foils were evaluated for both mechanical and thermophysical properties to establish baseline characteristics prior to irradiation testing. Cast U-10Mo ingots were sequentially hot and cold rolled to two different final foil thicknesses, resulting in different levels of cold work being present in the finished foils. The mechanical response of the U-10Mo foils was evaluated in the temperature range of 293–623 K. Increasing test temperatures resulted in decreases of both yield and ultimate tensile strength. Comparison of results to earlier work performed on depleted U-10Mo rolled foils indicates that the material in this study has lower strength and increased ductility. However, a comparison of the two different foil thicknesses in this study found that they were nearly identical in yield and ultimate tensile strength, differing by only 10–20 MPa (<2%). Thermal conductivity was calculated from the measurements of specific heat, linear thermal expansion, and thermal diffusivity from 323 to 1273 K on both thicknesses of the foils. These data were approximately 5–10% lower than previously published data above 573 K and were similar to data for temperature ranges below 573 K. Differences are likely related to differences in grain size and/or impurity content and variation in fabrication history.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

High energy X-ray characterization of the microstructure of PuGa alloy samples at macroscopic depths and non-ambient conditions

High energy (95 keV) X-rays were utilized to characterize the microstructure of eight PuGa alloy samples at room temperature and during cooling to ∼10 K. The samples had different Ga content (nominally 0-3.4 at.%), age, and history. A ninth sample, similarly characterized with neutron diffraction, was included to extend the Ga range to 7 at.%. The samples span the range from single phase α (monoclinic) to δ (face-centered cubic) PuGa, as well as a two-phase α′/δ sample. The crystallographic textures, phase fractions, lattice parameters and dislocation densities of each sample were evaluated through distinct analysis techniques. The textures of the samples were modest. In each case, the dislocation densities were relatively high, comparable to cold worked metals and metals exposed to similar radiation dose. At room temperature, the lattice parameters determined in the predominantly single-phase samples were larger than expected based on the nominal Ga concentration. The observed lattice thermal expansions of the single-phase δ samples to 10 K are self-consistent across the samples and consistent with previous measurements reported in the literature. Significantly larger thermal lattice strain is observed in the δ phase of the two-phase material due to mechanical constraint from the α′ phase, which has a three times larger thermal expansion and is much harder than the δ phase. In conclusion, the results demonstrate the unique value of high-energy X-rays for relatively routine microstructural characterization of Pu alloy samples.

36 MATERIALS SCIENCE↗

Quantification of stress history in type 304L stainless steel using positron annihilation spectroscopy

Five Type 304L stainless steel specimens were subjected to incrementally increasing values of plastic strain. At each value of strain, the associated static stress was recorded and the specimen was subjected to positron annihilation spectroscopy (PAS) using the Doppler Broadening method. A calibration curve for the 'S' parameter as a function of stress was developed based on the five specimens. Seven different specimens (blind specimens labeled B1-B7) of 304L stainless steel were subjected to values of stress inducing plastic deformation. The values of stress ranged from 310 to 517 MPa. The seven specimens were subjected to PAS post-loading using the Doppler Broadening method, and the results were compared against the developed curve from the previous five specimens. It was found that a strong correlation exists between the 'S' parameter, stress, and strain up to a strain value of 15%, corresponding to a stress value of 500 MPa, beyond which saturation of the 'S' parameter occurs. Research Highlights: {yields} Specimens were initially in an annealed/recrystallized condition. {yields} Calibration results indicate positron annihilation measurements yield correlation. {yields} Deformation produced by cold work was likely larger than the maximum strain.

36 MATERIALS SCIENCE↗

Friction surfaced Stellite6 coatings

Solid state Stellite6 coatings were deposited on steel substrate by friction surfacing and compared with Stellite6 cast rod and coatings deposited by gas tungsten arc and plasma transferred arc welding processes. Friction surfaced coatings exhibited finer and uniformly distributed carbides and were characterized by the absence of solidification structure and compositional homogeneity compared to cast rod, gas tungsten arc and plasma transferred coatings. Friction surfaced coating showed relatively higher hardness. X-ray diffraction of samples showed only face centered cubic Co peaks while cold worked coating showed hexagonally close packed Co also. - Highlights: Black-Right-Pointing-Pointer Stellite6 used as coating material for friction surfacing. Black-Right-Pointing-Pointer Friction surfaced (FS) coatings compared with casting, GTA and PTA processes. Black-Right-Pointing-Pointer Finer and uniformly distributed carbides in friction surfaced coatings. Black-Right-Pointing-Pointer Absence of melting results compositional homogeneity in FS Stellite6 coatings.

36 MATERIALS SCIENCE↗

Characterization of alloy 718 subjected to different thermomechanical treatments

Chemical phase and microstructural investigations of alloy 718 solution-annealed and age-hardened were performed in this study. We focused on the effects of solution annealing temperature, aging temperature and holding time, and the amount of intermediate cold work on the alloy. We also studied the formation of secondary phases such as γ’-phase, γ”-phase, and δ-phase, grain sizes, and any deformations of the microstructure with respect to the processed conditions. Statistics such as size and number densities of these precipitates with respect to the processing conditions were evaluated and a discussion on optimum conditions in obtaining finer and higher density of γ’- and γ”-phase precipitates is also presented.

36 MATERIALS SCIENCE↗

Hydrogen influences thermal activation parameters for dislocation glide during low cycle fatigue of 316L stainless steel

Measurements of activation areas are used to investigate the effect of hydrogen on the kinetics of dislocation glide during cyclic deformation in cold-worked 316L stainless steel. Non-charged and hydrogen-precharged (H-precharged) specimens were tested in low cycle fatigue (LCF) under plastic strain control. A series of plastic strain rate changes was performed periodically at the peak true plastic strain from the first cycle to half-life, and at various plastic strain values around stable hysteresis loops near half-life to determine the operational activation area, Δ a ∗. Both material conditions demonstrate a rapid increase in Δ a ∗ during the initial rapid softening followed by a region of approximately constant values coinciding with a reduced rate of softening. Near half-life, hydrogen reduces Δ a ∗ at a given true stress due to its effect on the activation distance and obstacle spacing. The magnitudes of Δ a ∗ reveal that bypassing solutes, cutting forest dislocations, and initiating cross slip are important mechanisms of thermally activated dislocation glide at all amplitudes, except hydrogen suppresses cross slip at the lowest plastic strain amplitudes. These results are supported by electron microscopy characterization of deformed microstructures. A Haasen plot analysis indicates that forest dislocations control the kinetics of deformation in both material conditions. It also reveals the presence of athermal obstacles in both non-charged and H-precharged conditions, likely dense dislocation tangles and cell walls. Additionally, the effect of hydrogen on microstructure evolution (by reducing the propensity for cross slip) leads to a dependence of athermal stress on plastic strain amplitude.

Activation area↗

Recrystallization driven softening and heating rate dependencies of FeCrAl nuclear fuel cladding during accident transients

A refined understanding of FeCrAl cladding behavior during rapid transients is critical for its potential deployment in light-water reactors. Current assessments focus on transient burst testing metrics such as balloon geometry, burst temperature, and hoop stress, often used as proxies for simpler conventional tensile properties. However, directly correlating isothermal tensile and creep data with accident transient scenarios remains a challenge, although it is essential for high fidelity model development. Recent modeling based on tensile tests up to 800 °C, conducted with both immediate loading and a 10-minute soak, showed that immediate loading better predicts experimental burst temperatures, indicating a thermal softening effect. Building upon this observation, the current study connects transient performance, microstructural evolution, and high-temperature tensile properties by leveraging results from C26M claddings burst tests performed at heating rates of 1–50 °C/s and hoop stresses from 25 to 100 MPa. At 25 MPa, rupture temperatures varied by only 6 °C, but at 100 MPa, the difference reached 116 °C, with faster heating yielding higher burst temperatures. Microstructural analysis identified recrystallization as the primary cause of heating rate-dependent softening, eliminating prior cold-working. In-situ thermomechanical data linked ballooning onset to localized instabilities, similar to ultimate tensile strength behavior in conventional tensile tests. High heating rates correlated with immediate loading tensile data, while lower rates matched soaked data. Furthermore, by linking burst performance to microstructural evolution and tensile properties, this work provides a foundation for more accurate modeling of FeCrAl claddings and potentially other Fe-based materials under accident conditions.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Lifetime estimation of a BWR core shroud in terms of IGSCC

The continued operation of aging Boiling Water Reactors (BWRs) worldwide requires gradually increasing cost of inspection, maintenance, and repair. Intergranular Stress Corrosion Cracking (IGSCC) in sensitized austenitic stainless steel piping first became a major issue for BWRs in the 1980s, resulting in recognition of the susceptibility of reactor internals to IGSCC. Shroud cracking identified in 1993–1994 confirmed that IGSCC of internals is a significant issue for BWRs. IGSCC is a time-dependent, material degradation process, which is caused and accelerated by the presence of residual stresses, material sensitization, irradiation, cold work, elevated temperature, and corrosive environments. This paper emphasizes the importance of accounting for corrosive environments, or more exactly, electrochemical phenomena in modelling IGSCC and predicting the service life of BWR in-vessel components, and stresses the necessity of performing such modeling not just for a single state point under full power conditions, but for the whole operating history of the reactor, including startups and shutdowns. Overall, this paper demonstrates that ignoring electrochemical considerations may result in underestimating component lifetime and lead to unnecessary expenses for inspection and repair.