Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ARC WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 181 records · Page 10

Effect of Through-Thickness Friction Stir Processing Parameters on Weld Repair and Modification of Fusion-Welded AA6061 Aluminum Alloy

Through-thickness friction stir processing was successfully carried out for microstructure modification and elimination of fusion defects of the gas metal arc welds by applying the process on as-welded joints. Variation in rotational speed from 750 to 1050 rpm and traveling speed from 50 to 200 mm/min resulted in minor changes (approximately 1 µm) in the grain size of nugget zone, while this variation in elongation result was up to 40%. The hardness profile, the width of softening zone, minimum hardness and fracture location also changed for different processing conditions. Furthermore, the defects were vanished efficiently across the welds profile by this method. The results also verified the geometric dynamic recrystallization phenomena as a dominant mechanism of microstructural modification.

36 MATERIALS SCIENCE↗

Hydrogen accelerated fatigue crack growth of friction stir welded X52 steel pipe

Friction stir welded steel pipelines were tested in high pressure hydrogen gas to examine the effects of hydrogen accelerated fatigue crack growth. Fatigue crack growth rate (da/dN) vs. stress-intensity factor range (ΔK) relationships were measured for an X52 friction stir welded pipe tested in 21 MPa hydrogen gas at a frequency of 1 Hz and R = 0.5. Tests were performed on three regions: base metal (BM), center of friction stir weld (FSW), and 15 mm off-center of the weld. For all three material regions, tests in hydrogen exhibited accelerated fatigue crack growth rates that exceeded an order of magnitude compared to companion tests in air. Among tests in hydrogen, fatigue crack growth rates were modestly higher in the FSW than the BM and 15 mm off-center tests. Select regions of the fracture surfaces associated with specified ΔK levels were examined which revealed intergranular fracture in the BM and 15 mm off-center specimens but an absence of intergranular features in the FSW specimens. In conclusion, the X52 friction stir weld and base metal tested in hydrogen exhibited fatigue crack growth rate relationships that are comparable to those for conventional arc welded steel pipeline of similar strength found in the literature.

08 HYDROGEN↗

Real-time Canister Welding Health Monitoring and Prediction System for Spent Fuel Dry Storage

In this report, the salt mist corrosion testing at controlled temperature was carried out successfully on 304L SS submerged arc welded coupons by Unifog Dispersion Tower at ORNL. Corrosion in-situ monitoring system from Intelligent Automation, Inc. (IAI) was setup in the corrosion test and running smoothly to record signals during the corrosion test. Parts and device selection, sensors attachment, and experimental procedures are discussed. There wasn’t any visible corrosion or crack propagation on the weld coupon after about a month of corrosion testing.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A FEASIBILITY STUDY ON CRACK REPAIR IN AUSTENITIC STAINLESS STEEL DRY STORAGE CANISTERS USING ISOTHERMAL FRICTION STIR WELDING

In recent time, solid state crack repair techniques in spent nuclear fuel dry storage canisters (SNF-DSC) have garnered significant interest. Plates of austenitic stainless steels are usually arc welded to fabricate the cylindrical canisters which are prone to chloride-induced stress corrosion cracking. Friction stir welding (FSW) is considered to be a potential candidate for damage repair. In this work, electrical discharge machining was used to simulate cracks in 304L stainless steel plates of 12.7 mm thickness. Subsequently, isothermal FSW was carried out at two different temperatures (725 and 825°C) in order to repair the simulated crack. Microstructure-mechanical property correlations in FSWed plates were studied in detail. Significant grain refinement observed in the stir zone (SZ) was attributed to dynamic recrystallization occurring during FSW. A comparison of Vickers microhardness showed higher hardness and homogeneity in the 725°C SZ than its 825°C counterpart. The fraction of S3 boundary is found to be low in the SZ as compared to base metal (BM). Yield strength of the joints was found to be approximately 100 MPa higher than that of the BM accompanied by a drop in ductility by a factor of 2. Residual stress profile across 825°C weld was measured using x-ray diffraction.

Bhattacharyya, Madhumanti↗

RESIDUAL STRESSES IN 3013 CONTAINERS

The DOE Complex is packaging plutonium-bearing materials for storage and eventual disposition or disposal. The materials are handled according to the DOE-STD-3013 which outlines general requirements for stabilization, packaging and long-term storage. The storage vessels for the plutonium-bearing materials are termed 3013 containers. Stress corrosion cracking has been identified as a potential container degradation mode and this work determined that the residual stresses in the containers are sufficient to support such cracking. Sections of the 3013 outer, inner, and convenience containers, in both the as-fabricated condition and the closure welded condition, were evaluated per ASTM standard G-36. The standard requires exposure to a boiling magnesium chloride solution, which is an aggressive testing solution. Tests in a less aggressive 40% calcium chloride solution were also conducted. These tests were used to reveal the relative stress corrosion cracking susceptibility of the as fabricated 3013 containers. Significant cracking was observed in all containers in areas near welds and transitions in the container diameter. Stress corrosion cracks developed in both the lid and the body of gas tungsten arc welded and laser closure welded containers. The development of stress corrosion cracks in the as-fabricated and in the closure welded container samples demonstrates that the residual stresses in the 3013 containers are sufficient to support stress corrosion cracking if the environmental conditions inside the containers do not preclude the cracking process.

42 ENGINEERING↗

Correlation between microstructure and residual stress formation in friction stir welded armor steels characterized by neutron diffraction

Friction stir welding (FSW) is a solid-state joining process that minimizes the heat-affected zone (HAZ) compared with fusion-based arc welding, making it well suited for joining martensitic armor steels where hardness and ballistic resistance are critical. This study investigates residual stress formation in three defect-free FSW butt-joint configurations relevant to armored-vehicle fabrication: similar rolled homogeneous armor (RHA–RHA, Case 1), similar high-hardness armor (HHA–HHA, Case 2), and dissimilar HHA–RHA (Case 3) joints produced under temperature-controlled conditions (770 °C). Neutron diffraction was employed to quantify the magnitude and spatial distribution of residual stresses in the longitudinal, transverse, and normal directions and to correlate them with weld microstructure and hardness. Tensile residual stresses were concentrated in the softened HAZ, reaching approximately 300 MPa for Case 2 and 400 MPa for Case 1 (≈50–70 % of the base-metal yield strength; ∼581 MPa for RHA and ∼566 MPa for HHA), while compressive residual stresses dominated the stir zone. The spatial extent of tensile stresses scaled with the width of the softened HAZ, which was largest in the dissimilar HHA–RHA joint and smallest in the HHA–HHA joint. Full-width-at-half-maximum (FWHM) analysis revealed low microstrain in overtempered HAZ regions and high microstrain in the stir zone associated with severe plastic deformation and fresh martensite formation. This work demonstrates that residual stress evolution in FSW of martensitic armor steels is governed not primarily by peak temperature or thermal contraction, as inferred from fusion-welding analogies, but by the competition between transformation-induced volumetric expansion and tempering-induced stress relaxation. The relative dominance of these mechanisms is shown to depend on alloy hardenability and local thermal history, leading to more extensive HAZ softening and broader tensile stress regions in the lower-hardenability RHA steel. These findings establish a transferable mechanistic framework for optimizing solid-state joining strategies in high-strength steels and other transformation-hardening alloys beyond armor applications.

Friction stir welding↗

Crack growth rates and metallographic examinations of Alloy 600 and Alloy 82/182 from field components and laboratory materials tested in PWR environments.

In light water reactors, components made of nickel-base alloys are susceptible to environmentally assisted cracking. This report summarizes the crack growth rate results and related metallography for field and laboratory-procured Alloy 600 and its weld alloys tested in pressurized water reactor (PWR) environments. The report also presents crack growth rate (CGR) results for a shielded-metal-arc weld of Alloy 182 in a simulated PWR environment as a function of temperature between 290 C and 350 C. These data were used to determine the activation energy for crack growth in Alloy 182 welds. The tests were performed by measuring the changes in the stress corrosion CGR as the temperatures were varied during the test. The difference in electrochemical potential between the specimen and the Ni/NiO line was maintained constant at each temperature by adjusting the hydrogen overpressure on the water supply tank. The CGR data as a function of temperature yielded activation energies of 252 kJ/mol for a double-J weld and 189 kJ/mol for a deep-groove weld. These values are in good agreement with the data reported in the literature. The data reported here and those in the literature suggest that the average activation energy for Alloy 182 welds is on the order of 220-230 kJ/mol, higher than the 130 kJ/mol commonly used for Alloy 600. The consequences of using a larger value of activation energy for SCC CGR data analysis are discussed.

08 HYDROGEN↗

Characterization of yttrium-rich precipitates in a titanium alloy weld

The yttrium-rich (Y-rich) precipitates that form in the fusion zone (FZ) of a Ti–5Al–1Sn–1Zr–1V–0.8Mo (wt.%) alloy, or Ti-5111, gas-tungsten arc welds (GTAW) were characterized. The filler metal was modified by a small concentration of Y in order to refine the microstructure and thus improve the FZ ductility. A high number density of nanoscale Y-rich precipitates were characterized in the weld FZ by atom probe tomography (APT) and scanning transmission electron microscopy (STEM). - Highlights: •A high number density of nanoscale precipitates were observed in the FZ matrix. •The nanoscale precipitates are enriched in yttrium. •Oxygen and sulfur are also present in the Y-rich precipitates and their interfaces.

36 MATERIALS SCIENCE↗

Effect of heat input on the microstructure and mechanical properties of tungsten inert gas arc butt-welded AZ61 magnesium alloy plates

In this paper, the effects of heat input on the microstructures and mechanical properties of tungsten inert gas arc butt-welded AZ61 magnesium alloy plates were investigated by microstructural observations, microhardness tests and tensile tests. The results show that with an increase of the heat input, the grains both in the fusion zone and the heat-affected zone coarsen and the width of the heat-affected zone increased. Moreover, an increase of the heat input resulted in a decrease of the continuous {beta}-Mg{sub 17}Al{sub 12} phase and an increase of the granular {beta}-Mg{sub 17}Al{sub 12} phase in both the fusion zone and the heat-affected zone. The ultimate tensile strength of the welded joint increased with an increase of the heat input, while, too high a heat input resulted in a decrease of the ultimate tensile strength of the welded joint. In addition, the average microhardness of the heat-affected zone and fusion zone decreased sharply with an increase of the heat input and then decreased slowly at a relatively high heat input.

36 MATERIALS SCIENCE↗

Monitoring and flaw detection during wire-based directed energy deposition using in-situ acoustic sensing and wavelet graph signal analysis

The goal of this work is to detect flaw formation in the wire-based directed energy deposition (W-DED) process using in-situ sensor data. The W-DED studied in this work is analogous to metal inert gas electric arc welding. The adoption of W-DED in industry is limited because the process is susceptible to stochastic and environmental disturbances that cause instabilities in the electric arc, eventually leading to flaw formation, such as porosity and suboptimal geometric integrity. Moreover, due to the large size of W-DED parts, it is difficult to detect flaws post-process using non-destructive techniques, such as X-ray computed tomography. Accordingly, the objective of this work is to detect flaw formation in W-DED parts using data acquired from an acoustic (sound) sensor installed near the electric arc. To realize this objective, we develop and apply a novel wavelet integrated graph theory approach. The approach extracts a single feature called graph Laplacian Fiedler number from the noise-contaminated acoustic sensor data, which is subsequently tracked in a statistical control chart. Using this approach, the onset of various types of flaws are detected with a false alarm rate less-than 2%. This work demonstrates the potential of using advanced data analytics for in-situ monitoring of W-DED.

42 ENGINEERING↗

Characterization of Mg/Al butt joints welded by gas tungsten arc filling with Zn–29.5Al–0.5Ti filler metal

The multivariate alloying design of a welding joint is used in the Mg to Al welding process. A Zn–29.5Al–0.5Ti alloy is added as filler metal in gas tungsten arc welding of Mg and Al alloy joint based on the analysis of Al and Mg alloy characteristics. The tensile strength, microstructure, and phase constitution of the weld seam are analyzed. The formation of brittle and hard Mg–Al intermetallic compounds is avoided because of the effects of Zn, Al, and Ti. The average tensile strength of the joint is 148 MPa. Al{sub 3}Ti is first precipitated and functions as the nucleus of heterogeneous nucleation during solidification. Moreover, the precipitated Al–MgZn{sub 2} hypoeutectic phase exhibited a feather-like structure, which enhances the property of the Mg–Al dissimilar joint. - Highlights: • Mg alloy AZ31B and Al alloy 6061 are butt welded by fusion welding. • The effect of Ti in filler metal is investigated. • The formation of Mg–Al intermetallic compounds is avoided.

36 MATERIALS SCIENCE↗

Understanding the Thermal Physics and Metallurgy of Metal Big Area Additive Manufacturing

The research goal of this EPSCoR-DOE partnership is to mitigate defects in parts made using a new type of additive manufacturing (AM) process called metal Big Area Additive Manufacturing (m-BAAM). To realize this goal, the PIs will detect and correct defects in the part as it is being printed by combining fundamental knowledge of the thermal physics and metallurgy of m-BAAM with in-process sensor data. Developed at the DOE-funded Manufacturing Demonstration Facility at Oak Ridge National Laboratory, the m-BAAM process involves one or more robots working together to produce a part by fusing metal wire layer-by-layer using arc welding. The process can print large metal parts such as turbine blades, which is not possible using other AM processes. In addition, m-BAAM production rates are more than ten times faster than other AM processes while requiring one-tenth of the material cost. Despite their potential to become a critical force multiplier in the energy generation industry, m-BAAM parts may fail to print accurately due to retention of heat and uneven cooling. Overheating and anomalous cooling rates in turn can cause inconsistencies in the microstructure, leading to sudden failure when used in safety-critical applications. In other words, flaw formation in m-BAAM parts is governed by the thermal history – intensity and spatial distribution of heat inside the part during printing. The thermal history is a complex function of the part shape and process settings such as welding energy, path taken by the welding torch for deposition (tool path), wire feed rate, among others.

36 MATERIALS SCIENCE↗

Interim Report on FY22 ORNL A709 Welding Research and Testing of Production Welds in Support of Developing ASME A709 Code Case Data Package

As part of the Alloy 709 ASME Code Case development effort under the Advanced Reactor Technologies (ART) Program, this work covers the development of the technical basis for weld fabrication and weld qualification of Alloy 709. This report summarizes the Alloy 709 welding research conducted at Oak Ridge National Laboratory (ORNL) in FY 2022. Two new production welds were fabricated on two commercial heats of Alloy 709 of different phosphorus (P) levels using Alloy 709 filler metal with P content less than 20 wppm with gas tungsten arc welding (GTAW). Both production welds successfully passed ASME Section IX weld qualification tests, and this concludes the Alloy 709 welding procedure development to scale up to 2-in thick plates. In FY 2022, we also demonstrated the success in welding of high P commercial Alloy 709 plates with weld wires having higher P content at 30 wppm. A test weld fabricated with the 30 wppm weld wire on the first commercial heat (140 wppm P) passed all weld qualification tests without issues. Additionally, experiment setup and testing procedure of the circular patch weldability test has been developed, for evaluating the P effect in weld wire on solidification cracking susceptibility of Alloy 709 weld, with the preliminary results summarized in this report. Research on further relaxing the P level restriction beyond 30 wppm are planned in FY 2023. The preliminary cross-weld creep tests results continue to show little or no creep strength reduction relative to the base metal.

36 MATERIALS SCIENCE↗

Neutron Residual Stress Mapping of Repaired Spent Nuclear Fuel Welded Stainless-Steel Canisters

Stress corrosion cracking (SCC) caused by atmospheric deposition and deliquescence of aggressive compounds such as chloride-containing salts or oxidized sulfur species may pose a potential issue to the extended service life of spent nuclear fuel (SNF) storage canisters. When a chemically susceptible material is exposed to a hostile environment (e.g., coastal salt air) for a sufficient length of time, SCC may occur at locations on the canister which have undergone high tensile residual stress. These locations are often found in weld zones and the heat-affected zones (HAZ) of welded joints. Ideally, these cracks could be repaired by traditional fusion welding techniques, but the highly localized heat input of the repair welding may introduce additional high tensile residual stress and could increase the risk for future SCCs. This paper presents the results of neutron residual stress mapping of as-welded and repaired stainless steel specimens. The as-welded specimens were provided by Sandia National Laboratories from a canister mock-up manufactured using procedures similar to those used for actual canister production. ASME-qualified gas-tungsten arc welding (GTAW) was used to repair the specimens, and post-repair residual stresses were measured using neutron diffraction at the Oak Ridge National Laboratory (ORNL) High Flux Isotope Reactor (HFIR). As-welded and repaired specimen residual stress distributions are evaluated and compared.

Chatzidakis, Stylianos↗

ER4047 Filler Wire Development - Initial Studies

This report describes the results of bead on pipe welding trials for the purpose of evaluating commercial off the shelf (COTS) 0.047” ER4047 filler material vendors for down selection of the of best candidate filler material for future Gas-metal Arc Welding (GMAW) development efforts. Four candidate COTS ER4047 filler wires were evaluated during this work - Astrolite, Alcotec, Hobart, and Lincoln. The storage condition of each of these filler wires was documented and visual inspection was performed.

36 MATERIALS SCIENCE↗

Upgraded HFIR Fuel Element Welding System

The welding of aluminum-clad fuel plates into aluminum alloy 6061 side plate tubing is a unique design feature of the High Flux Isotope Reactor (HFIR) fuel assemblies as 101 full-penetration circumferential gas metal arc welds (GMAW) are required in the fabrication of each assembly. In a HFIR fuel assembly, 540 aluminum-clad fuel plates are assembled into two nested annular fuel elements 610 mm (24-inches) long. The welding process for the HFIR fuel elements was developed in the early 1960 s and about 450 HFIR fuel assemblies have been successfully welded using the GMAW process qualified in the 1960 s. In recent years because of the degradation of the electronic and mechanical components in the old HFIR welding system, reportable defects in plate attachment or adapter welds have been present in almost all completed fuel assemblies. In October 2008, a contract was awarded to AMET, Inc., of Rexburg, Idaho, to replace the old welding equipment with standard commercially available welding components to the maximum extent possible while maintaining the qualified HFIR welding process. The upgraded HFIR welding system represents a major improvement in the welding system used in welding HFIR fuel elements for the previous 40 years. In this upgrade, the new inner GMAW torch is a significant advancement over the original inner GMAW torch previously used. The innovative breakthrough in the new inner welding torch design is the way the direction of the cast in the 0.762 mm (0.030-inch) diameter aluminum weld wire is changed so that the weld wire emerging from the contact tip is straight in the plane perpendicular to the welding direction without creating any significant drag resistance in the feeding of the weld wire.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Fusion welding of refractory metals and ZrB 2 -SiC-ZrC ceramics

Molybdenum and a molybdenum alloy were fusion welded to ZrB2-based ceramics to determine if the electrical and thermal properties of the metals and ceramics affected their weldability. Commercial ceramic powders were hot pressed, machined into coupons, and preheated to 1600 °C before joining the ceramics to commercial metals using plasma arc welding. Weldability varied as indicated by the range of porosity observed within the fusion zones. Measured thermal and electrical properties appeared to have little to no effect on the weldability of metal-ceramic welds despite the large range of values measured across each property. Differences in melting temperatures between metal and ceramic coupons did affect weldability by changing the weld penetration depth into ceramic coupons. Finally, future studies on metal-ceramic welds are suggested to investigate the effect that work function, melt viscosity, wetting, or other properties have on weldability.

36 MATERIALS SCIENCE↗

Fabrication and Testing of DOE Standard Canister Closure Leak Test Assembly

DOE manages over 300 types of spent nuclear fuel (SNF), many of which are located at the Idaho National Laboratory (INL) site. Managing this large variety of SNF for storage, transportation, and disposal poses a challenge to DOE. The Idaho Cleanup Project and INL are collaborating on the DOE SNF Road-Ready Demonstration (“Road-Ready Demonstration”), which will develop and demonstrate the designs, technology, processes, and regulatory framework for packaging DOE-managed SNF for “road-ready dry storage.” Road-ready dry storage is an SNF management concept in which SNF is packaged into dry, sealed canisters that are then placed in onsite storage in anticipation of later transport and disposition. The forward-looking goal of the Road-Ready Demonstration is to establish the foundation for a large-scale road-ready dry storage program at the INL site. In support of establishing a large-scale road-ready dry storage program at the INL site, the Road-Ready Demonstration will first package Fort St. Vrain SNF currently in dry storage at INL into several DOE Standard Canisters (DOESCs). These DOESCs will in turn be loaded into another containment similar to commercial multi-purpose canisters. This multi-purpose canister will then be compatible with a transportation or storage system, such as a storage cask for interim storage or transportation package for offsite transport. These DOESCs will remain sealed over the course of their storage, transportation, and applicable disposal functions. The closure process for the DOESC will include fuel and basket loading, welding, inspection, leak testing, and, if needed, repair. As a follow-up to previous discussions on the design of the DOE Closure Leak Test Assembly (LTA), this report describes recent fabrication and testing efforts performed at INL. DOESCs are sealed by two sequential gas tungsten arc welds, both of which are performed by remotely operated and semiautomatic welding systems. The first weld is a circumferential pipe weld that completes the assembly of the canister body and lid assembly. The second and final closure weld attaches the vent plug to the vent socket via a butt joint. After the second weld is performed, the welds are helium leak tested using an evacuated envelope technique. The LTA was designed for both remote and manual operation. This report describes the fabrication and performance testing associated with the evacuated envelope technique. INL staff designed, fabricated, and tested the LTA at INL facilities. This testing included establishing technique and system sensitivities in accordance with ASME and American National Standards Institute N14.5 requirements. Forthcoming work will cover such areas as design optimization, process and personnel qualification, and implementation in Road-Ready Demonstration operations.

42 ENGINEERING↗