DOE OSTI · 965599

Interconnects

Abstract

The identification and fabrication of suitable interconnect materials is a major challenge in the development of SOFCs [1,2]. The primary function of the interconnect is to carry electrical current from the electrochemical cell to the external circuit, so the inteconnect material must have good electrical conductivity. In addition, the interconnect must be chemically and mechanically stable for operation at high temperatures for long periods of time. This is especially challenging, since the interconnect is exposed to both oxidizing conditions at the cathode and reducing conditions at the anode. Thus, interconnect materials should not undergo significant dimensional changes with changes in either temperature or oxygen partial pressure. One such change is thermal expansion, which must be matched with the expansion of other fuel cell components to avoid the generation of thermal stresses during heating or cooling. Similarly, some materials undergo expansion or contraction with changes in oxygen partial pressure, which can also lead to stresses in the fuel cell. Thus, although the interconnect is not always a load-bearing component, moderate mechanical strength of the interconnect material is required to avoid fracture when stresses are generated during operation. Even higher strength is required in some planar designs were the interconnect provides structural support. In such designs, the interconnect also separates the fuel from air, so oxygen and hydrogen permeability should be low. The interconnect material must also be chemically stable with other fuel cell components. This includes not only stability during fuel cell operation, but also during fabrication, which typically involves higher temperatures. Finally, ease of fabrication and cost are important so that application of the fuel cell is economically feasible.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Yang, Zhenguo, Fergus, Jeff. 2008-09-10. Interconnects. https://engineeringpapers.com/record/osti%3A965599/interconnects

Citations retain the original authors and DOI and include this site’s record URL. If this discovery service contributed to your research, you can also cite Engineering Papers by Indiciae: BibTeX · RIS.

KEEP EXPLORING

Related reports

Elucidating key reducing species beyond ions in hydrogen plasma smelting reduction of iron ore

Hydrogen plasma smelting reduction (HPSR) of iron ore has attracted significant attention over the past decade due to its high-temperature operation, rapid plasma mediated reduction kinetics, and simpler density-based separation of molten iron product, compared to H2-based solid-state reduction. All of these attributes enable processing of low-grade ores for downstream use in electric-arc furnaces, as virgin iron with low gangue content is required for high quality steel and improved furnace operation. While positive ions exist within the plasma arc, this work demonstrates that near the anodic ore surface, hydrogen radicals and vibrationally excited hydrogen species dominate and their densities correlate well with observed reduction rates. Species concentrations in the transferred plasma arc and at the plasma-ore interface are evaluated using coupled thermal plasma and near-wall non-equilibrium plasma models. The thermal plasma model is validated against experimental voltage data and spectroscopic measurements of plasma temperature and density for varying current inputs. Modeling of the near surface thermochemical non-equilibrium and micrometer scale anode sheath layer reveals, in addition to the expected H + , significant concentrations of ArH + and H$^+_3$ ions, typically not observed in thermal plasmas under thermodynamic equilibrium. Our results show that the inverted sheath structure at the anodic ore surface strongly suppresses reactive positive ion fluxes, while non-equilibrium electron-impact processes generate abundant hydrogen radicals and vibrationally excited species. These findings highlight the critical role of non-equilibrium effects in hydrogen arc-driven iron ore reduction and advance understanding beyond prevailing hypotheses centered on hydrogen ion-driven mechanisms.

08 HYDROGEN↗

SimH 2 : an integrated techno-economic modeling framework for hydrogen pipeline infrastructure and network optimization

Large-scale hydrogen (H 2 ) pipeline transport design and network optimization have seldom been reported due to the lack of a cost model accounting for the relationship between transport cost and hydrogen mass flow rate. Here, this work introduced a system-level cost model for hydrogen pipeline transport at supercritical state and integrated it with an existing CO 2 pipeline network tool, SimCCS, for hydrogen-specific pipeline design and optimization. The Intermountain West (I-West) region of the U.S., historically dependent on fossil fuel-based economies, is chosen to demonstrate the capabilities of our H 2 pipeline cost model and transport network optimization platform called SimH 2 . Two scenarios are examined: one where the pipeline is not allowed to pass through disadvantaged communities and the other where it is permitted. The results highlight that incorporating disadvantaged-community constraints lead to longer pipeline routes and increased transport costs, reflecting the trade-offs involved in equitable infrastructure development. It is demonstrated that the newly developed SimH 2 tool not only enables the efficient design of H 2 transportation pipelines but also optimizes the network by accounting for local terrain and the presence of disadvantaged areas.

08 HYDROGEN↗

Disordered hydrogen adsorption at the three-fold site of W(110)

Hydrogen often forms disordered phases on metals; however, deciphering the atomic-scale behavior requires experimental and modeling techniques that directly probe the short-range order between neighboring hydrogen adsorbates. Here, to address this challenge, we applied direct recoil spectroscopy (DRS) to investigate hydrogen adsorption on the W(110) surface. We show that the recoiled hydrogen flux measured during DRS is sensitive to the short range order of the adsorbed hydrogen. Ordered hydrogen neighbors are much more efficient at dechanneling incident ions along low-index surface channels, strongly suppressing the recoiled hydrogen flux along these directions. By modeling the DRS measurements with molecular dynamics for ordered and disordered hydrogen phases, we find that at a hydrogen surface coverage of approximately Θ = 0.6, the hydrogen adsorbates are bound to three-fold sites in a disordered phase at room temperature. This finding is consistent with transfer-matrix scaling model calculations that suggest the transition to an ordered hydrogen phase occurs at a greater surface coverage of Θ = 0.83.

08 HYDROGEN↗