The Feasibility of Atomic Layer Deposition of Aluminum Oxide on TATB

Abstract

The source did not provide an abstract. Follow the original record for more information.

Explore related subjects

Keep this discovery

BibTeXRIS

Miller, John [Lawrence Livermore National Laboratory], Li, Tian [Lawrence Livermore National Laboratory], Reeves, Rob [Lawrence Livermore National Laboratory]. 2026-08-31. The Feasibility of Atomic Layer Deposition of Aluminum Oxide on TATB. https://doi.org/10.1002/prep.70263

Cite the original work for its findings. Save a collection to share your selection of sources.

Discover connections

Connections use source metadata and explicit phrase matches, not verified experimental comparisons.

KEEP EXPLORING

Related reports

The effect of dogbone sample size in the tensile testing of TATB-based plastic‑bonded explosive materials

Mechanical properties are of interest for many plastic‑bonded explosive (PBX) materials with tensile properties being of particular interest. Direct tensile measurements using dogbone-shaped samples are considered the gold standard, but they are fairly large, making testing more costly and less desirable from a safety perspective. We investigated whether the measured tensile strength depends on the dogbone specimen size, which to our knowledge, has not been reported in the literature for PBX materials. Understanding this should inform the feasibility of employing smaller samples and how sample size should be considered when comparing PBX dogbone values in the literature. The TATB-based PBX dogbone sample size was varied by (a) scaling all dimensions proportionally and (b) varying only the length of the samples. It was observed that the measured tensile peak stress (strength) was a function of the sample size, and was more dependent on the diameter (cross-sectional area) than the length of the samples. Since peak stress is calculated as peak force normalized to the diameter of the sample, one might not expect an explicit diameter dependence for the peak stress. Therefore, these results suggest there may be an additional strengthening effect as the sample diameter is increased.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH

Synthesis and investigation into explosive sensitivity for a series of new picramide explosives

Tailoring the molecular properties that govern energetic material sensitivity is essential to improve safety and help develop new energetic materials. Despite this need, understanding the complex chemistry and physics of explosive initiation and propagation is still a challenge. Recent work by our group has reinforced the view that explosive sensitivity under sub-shock conditions is connected to the strength of the weakest covalent bond in the molecule, that is, its “trigger linkage.” These correlations have been observed with different classes of energetic molecules and indicate that “trigger linkage” bond breaking, and heat of explosion are good indicators for the sensitivity trends. Herein we report the synthesis of aliphatic energetic materials with ethane, propane and neopentane backbones. Experimental and computational studies show that the trigger linkage model, based on results from quantum molecular dynamics simulations, correctly predicts trends observed in the impact sensitivity of the molecules. However, while the model predicts the impact sensitivities of the ethane series, the neopentane series has higher impact sensitivities than predicted, which is presumably influenced by crystal packing effects.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH