Site-specific surface reactivity on SnO 2 : Evaluating selective atomic layer deposition processes

Abstract

Area selective atomic layer deposition (AS-ALD) is a bottom-up synthesis approach with potential for deposition with molecular level precision. Here, the site-specific hydration of metal oxide substrates, combined with surface H 2 O-selective ALD processes, provides a potentially powerful path to targeted synthesis. Density functional theory (DFT) calculations are used to predict the thermodynamics of ALD precursor reactivity and hydration for (001), (101), (110), and (100) rutile SnO 2 facets as a function of temperature. Trimethylaluminum (TMA) and dimethyl aluminum isopropoxide (DMAI) dimers are predicted to react with both dehydrated and hydrated SnO 2 (001), (101), and (110) facets at ALD-relevant temperatures, while the SnO 2 (100) facet is predicted to be uniquely unreactive with TMA and DMAI monomers as well as dehydrate near 177 °C making this facet more amenable to targeted ALD. In situ ellipsometric studies of Al 2 O 3 ALD on polycrystalline SnO 2 at 150 °C are consistent with the computational predictions of rapid and unselective nucleation, in stark contrast to inhibited and selective ALD on isostructural rutile TiO 2 .

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Xu, Jiayi [Argonne National Laboratory (ANL), Argonne, IL (United States)] (ORCID:0000000317636251), Muir, Mark [Argonne National Laboratory (ANL), Argonne, IL (United States)] (ORCID:0000000318900579), Kamphaus, Ethan Philip [Argonne National Laboratory (ANL), Argonne, IL (United States)] (ORCID:0000000158212223), Jones, Jessica Catharine [Argonne National Laboratory (ANL), Argonne, IL (United States)] (ORCID:0000000174754620), Martinson, Alex B. F. [Argonne National Laboratory (ANL), Argonne, IL (United States)] (ORCID:0000000339161672), Liu, Cong [Argonne National Laboratory (ANL), Argonne, IL (United States)] (ORCID:0000000221455034). 2025-03-14. Site-specific surface reactivity on SnO 2 : Evaluating selective atomic layer deposition processes. https://doi.org/10.1016/j.apsusc.2025.162966

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Probing the Effects of the First Atomic Layer on the Dynamic Behavior of Sub-2 nm MgO/Al 2 O 3 Memristors

As electronic devices continue to scale down from the current sub-5 nm range, atomic-scale control of defects becomes increasingly crucial to suppressing their impact on the physical properties of the devices. Memristors present an excellent example as a nonlinear and dynamic device with high speed and endurance required for electronic applications ranging from neuromorphic computing to nonvolatile memories. Herein we investigate the impact of atomic defects in sub-2 nm thick MgO/Al 2 O 3 atomic layer stack (ALS) memristors that use an M1 (switching layer)/M2 (oxygen vacancy reservoir layer) bilayer structure grown using in vacuo atomic layer deposition (iALD). Intriguingly, we revealed a direct correlation of the atomic defects in the M2 layer with the memristor dynamic behavior using a combined analysis of in situ scanning tunneling spectroscopy (iSTS) on the M2 layer and ex situ characterization on the memristors. Specifically, incomplete coverage of the 1st ALD atomic layer of M2 on the electrode yields defects at the M2/electrode interface. Despite the monotonic increase of ALD coverage, by almost three-fold from ~30% to >90%, at completion of the M2 layer of ~ 0.7 nm in thickness, the impact of the defects on the M2/electrode interface has been found detrimental to both memristor switching speed and endurance. Guided by atomistic simulation, we addressed the issue of interface defects via tuning of the Al surface hydroxylation to increase the first atomic layer ALD coverage to ~75%, leading to improved memristor switching speed and endurance by several orders of magnitude. In conclusion, these findings shed light on the correlation between the atomic defects and the dynamic behavior of sub-2 nm memristors and the importance of minimizing the atomic defects in memristors for future electronic applications.

Atomic Layer Deposition↗