Abstract

Hydrogen production via two-step thermochemical water splitting redox cycles using nonstoichiometric redox-active metal oxides has the potential to dramatically increase fuel production rates. At moderate-to-low water splitting temperatures, surface reaction kinetics co-limit the process. In such cases, stable and high surface area microstructures that allow exploitation of the full thermodynamic potential of the materials are essential as is tight thermal integration of the reactor module. This project’s goals were the development of novel nonstoichiometric perovskite oxides with high stability and favorable thermodynamic and kinetic properties, to optimize their microstructure for maximizing the fuel productivity, and to build a prototype reactor train system (RTS) comprising at least one reactor to meet specific performance targets: (1) capable of an in-house solar thermochemical hydrogen (STCH) productivity ≥ 12 mL g -1 for stable continuous operation ≥ 20 cycles; and (2) demonstration of scalable solar fuels production at practical solar reactor level in an industrial-scale concentrated solar tower (CST) using developed perovskites to achieve a hydrogen production rate ≥ 1 g h -1 .

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Qian, Xin [Saint-Gobain Ceramics & Plastics, Inc., Northborough, MA (United States)], Haile, Sossina M. [Northwestern Univ., Evanston, IL (United States)], Ghoniem, Ahmed [Massachusetts Inst. of Technology (MIT), Cambridge, MA (United States)], Pietras, John [Saint-Gobain Ceramics & Plastics, Inc., Northborough, MA (United States)]. 2026-03-19. Scalable Solar Fuels Production in A Reactor Train System by Thermochemical Redox Cycling of Novel Nonstoichiometric Perovskites. https://doi.org/10.2172/3025188

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Elucidating key reducing species beyond ions in hydrogen plasma smelting reduction of iron ore

Hydrogen plasma smelting reduction (HPSR) of iron ore has attracted significant attention over the past decade due to its high-temperature operation, rapid plasma mediated reduction kinetics, and simpler density-based separation of molten iron product, compared to H2-based solid-state reduction. All of these attributes enable processing of low-grade ores for downstream use in electric-arc furnaces, as virgin iron with low gangue content is required for high quality steel and improved furnace operation. While positive ions exist within the plasma arc, this work demonstrates that near the anodic ore surface, hydrogen radicals and vibrationally excited hydrogen species dominate and their densities correlate well with observed reduction rates. Species concentrations in the transferred plasma arc and at the plasma-ore interface are evaluated using coupled thermal plasma and near-wall non-equilibrium plasma models. The thermal plasma model is validated against experimental voltage data and spectroscopic measurements of plasma temperature and density for varying current inputs. Modeling of the near surface thermochemical non-equilibrium and micrometer scale anode sheath layer reveals, in addition to the expected H + , significant concentrations of ArH + and H$^+_3$ ions, typically not observed in thermal plasmas under thermodynamic equilibrium. Our results show that the inverted sheath structure at the anodic ore surface strongly suppresses reactive positive ion fluxes, while non-equilibrium electron-impact processes generate abundant hydrogen radicals and vibrationally excited species. These findings highlight the critical role of non-equilibrium effects in hydrogen arc-driven iron ore reduction and advance understanding beyond prevailing hypotheses centered on hydrogen ion-driven mechanisms.

08 HYDROGEN

SimH 2 : an integrated techno-economic modeling framework for hydrogen pipeline infrastructure and network optimization

Large-scale hydrogen (H 2 ) pipeline transport design and network optimization have seldom been reported due to the lack of a cost model accounting for the relationship between transport cost and hydrogen mass flow rate. Here, this work introduced a system-level cost model for hydrogen pipeline transport at supercritical state and integrated it with an existing CO 2 pipeline network tool, SimCCS, for hydrogen-specific pipeline design and optimization. The Intermountain West (I-West) region of the U.S., historically dependent on fossil fuel-based economies, is chosen to demonstrate the capabilities of our H 2 pipeline cost model and transport network optimization platform called SimH 2 . Two scenarios are examined: one where the pipeline is not allowed to pass through disadvantaged communities and the other where it is permitted. The results highlight that incorporating disadvantaged-community constraints lead to longer pipeline routes and increased transport costs, reflecting the trade-offs involved in equitable infrastructure development. It is demonstrated that the newly developed SimH 2 tool not only enables the efficient design of H 2 transportation pipelines but also optimizes the network by accounting for local terrain and the presence of disadvantaged areas.

08 HYDROGEN

Disordered hydrogen adsorption at the three-fold site of W(110)

Hydrogen often forms disordered phases on metals; however, deciphering the atomic-scale behavior requires experimental and modeling techniques that directly probe the short-range order between neighboring hydrogen adsorbates. Here, to address this challenge, we applied direct recoil spectroscopy (DRS) to investigate hydrogen adsorption on the W(110) surface. We show that the recoiled hydrogen flux measured during DRS is sensitive to the short range order of the adsorbed hydrogen. Ordered hydrogen neighbors are much more efficient at dechanneling incident ions along low-index surface channels, strongly suppressing the recoiled hydrogen flux along these directions. By modeling the DRS measurements with molecular dynamics for ordered and disordered hydrogen phases, we find that at a hydrogen surface coverage of approximately Θ = 0.6, the hydrogen adsorbates are bound to three-fold sites in a disordered phase at room temperature. This finding is consistent with transfer-matrix scaling model calculations that suggest the transition to an ordered hydrogen phase occurs at a greater surface coverage of Θ = 0.83.

08 HYDROGEN