Engineering Papers⌕ Search

DOE OSTI · 3023552

Machine Learning Vacancy Formation Energy in Nickel-Based Superalloys

Abstract

Thermal vacancies play a critical role in high-temperature Ni-based superalloys and influence various properties such as creep resistance, oxidation, etc. This study systematically investigates the impact of commonly used transition metals (Cr, Co, Fe), refractory metals (Nb, Ta, Mo, W) and other elements (Al, Cu, Ti, Mn) on the thermodynamic stability of 36 binary, 20 ternary, 11 quaternary, 9 quinary, and 3 senary FCC Ni-based alloys covering various elemental combinations. Density functional theory-based studies on Ni-X binary alloys show that higher concentrations of Cr, Nb, Ta, Al, and Ti introduce significant lattice distortions and broaden the distribution of vacancy formation energies (standard deviation up to 0.15 eV). These elements partially donate electrons, reducing their self-consistent chemical potentials relative to single-element reference values and lowering vacancy formation energies, while Co, Fe, Mo, and W show lower charge localization. These trends extend from 3-6 element alloys, where Cr, Nb, and Ta-rich compositions have low-energy states (~0.5 eV) that increase vacancy concentrations. Finally, graph neural network models are developed to screen over 5000 virtual alloys. Eleven leading compositions are identified with mean vacancy formation energy higher than 1.75 eV and vacancy concentration ~2 orders of magnitude lower than pure Ni at 1000 K. These results provide valuable guidelines to achieve controlled defect engineering in structural alloys.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Sundar, Aditya [NETL Site Support Contractor, National Energy Technology Laboratory], San, Saro [NETL Site Support Contractor, National Energy Technology Laboratory], Gao, Michael [NETL] (ORCID:000000020515846X). 2026-03-17. Machine Learning Vacancy Formation Energy in Nickel-Based Superalloys. https://doi.org/10.2172/3023552

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Role of Surface Termination in the Structural and Electronic Properties of Sc$_2$CT$_\textrm{x}$ MXene

Graphene-like layered transition metal carbides, nitrides, or carbonitrides, called MXenes, obey the stoichiometric formula of M n+1 X n T x , where M is an early transition metal such as scandium (Sc), n is a natural number, X is C, N, or CN, and T x is a functional group such as –O, –F, or –OH that passivates the surface of the MXene. The electronic structure of bare Sc 2 C and functionalized Sc 2 CT x MXenes are explored by performing first-principles density functional theory (DFT) calculations. The bare Sc 2 C is metallic, but less stable than its passivated structure. The Sc 2 C MXene has an interlayer 2D electron gas not bound to Sc or C atoms but free to move, making it an electride. DFT calculations show that functionalization can open an energy gap in Sc 2 CT x MXenes. The size and type (direct versus indirect) of the bandgap vary with the functional groups, which provides a means for opening and tuning of the band gap.

DFT↗

Achieving high tensile strength and ductility in refractory alloys by tuning electronic structure

The energy efficiency of heat engines (gas and steam turbines) for electricity production and propulsion is determined by the Carnot cycle and scales with operating temperature. Commercial nickel- and cobalt-based superalloys melt near 1,500 °C and rapidly lose mechanical strength beyond 1,000 °C. Refractory metals melt well above 2,000 °C but have inherent manufacturability challenges that are barriers to adoption, such as high ductile-to-brittle transition temperatures. Using density functional theory-guided design, we demonstrate tailored local lattice distortions that promote phase-stable, non-equiatomic refractory concentrated solid solutions with both high ductility and strength. Here, we exemplify this for single-phase, body-centred cubic Nb 4 Ta 4 V 3 Ti that exhibits castability, excellent room-temperature tensile yield strength (∼1 GPa) and ductility (approaching 20% uniform strain), and exceptional high-temperature tensile strength (500 MPa at 1,000 °C). These findings illustrate a path for designing materials that hold great potential for advancing next-generation technologies such as Generation IV fission reactors, first-generation fusion-plasma reactors, and more efficient gas turbines for electricity generation and propulsion.

DFT↗

Kohn anomalies and phonon anharmonicity in iridium

Elemental iridium presents surprising challenges for both inelastic neutron scattering (INS) and theoretical thermal transport calculations due to its high neutron absorption cross-section and strong electron-phonon interactions, respectively. Here, in this study, we overcome these challenges to measure temperature-dependent phonon dispersion curves, compare these with calculations based on density functional theory (DFT), and ultimately examine the electron-phonon limited transport behaviors of this material. Our DFT calculations demonstrate Kohn anomalies, near the 𝐾 point of the iridium Brillouin zone, indicating coupling between electrons and phonons. Strong electron-phonon coupling can compete with anharmonic effects to determine electrical and thermal transport behaviors and make the Kohn anomalies challenging to observe. Nonetheless, our INS measurements map these anomalies and other dispersion features over the Brillouin zone from 100 to 700 K. These measurements also uncover unexpectedly large mode specific Grüneisen parameters obtained from the temperature-dependent phonon energies, highlighting strong anharmonicity in iridium. DFT-based Boltzmann transport calculations demonstrate how anharmonicity and electron-phonon couplings determine electronic and lattice transport behaviors. Furthermore, we correlate the Kohn anomalies with calculated electron-phonon nesting functions, Fermi surfaces, and DFT-derived coupling strengths. This study provides detailed insights into the temperature-dependent mode-resolved lattice dynamics and anharmonicity, transport behavior, and electron-phonon interactions.

DFT↗