Engineering Papers⌕ Search

DOE OSTI · 3010667

Modeling diffusion and depletion in high-aspect-ratio atomic layer deposition processes: Process parameters and manufacturing impacts

Abstract

Atomic layer deposition (ALD) is a powerful technique for modifying the surface chemistry and properties of substrates with complex and nonplanar topologies. However, achieving uniform and conformal deposition on ultrahigh-aspect-ratio substrates remains challenging, typically requiring large quantities of precursors and long exposure times. Furthermore, process optimization is often performed empirically and involves substantial trial and error. In this work, we perform a combined experimental and computational study of ALD Al 2 O 3 infiltration into silica aerogel monoliths (aspect ratio >10 5 ). A reaction-diffusion model is used to explore the effects of key processing parameters, namely, exposure time per dose, precursor source temperature, number of aerogels in the reactor, and reactor volume. The model is based on quasi-static mode ALD, where the dosed precursor is held in the chamber for a fixed period of time before purging. We analyze the trade-offs between process throughput and precursor utilization for each of these parameters. Furthermore, we investigate the co-optimization and interactions between multiple process parameters, demonstrating the potential for further improvements. Furthermore, this physics-based model can be used to identify a set of process parameters for high-aspect-ratio ALD that meet specific manufacturing objective functions, including throughput, cost, and sustainability.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Vogt, Victor A. [University of Michigan, Ann Arbor, MI (United States)] (ORCID:0000000292988401), Gayle, Andrew J. [University of Michigan, Ann Arbor, MI (United States)] (ORCID:0000000348022439), Mañón, Andrés Miranda [University of Michigan, Ann Arbor, MI (United States)] (ORCID:0009000471085539), Lenert, Andrej [University of Michigan, Ann Arbor, MI (United States)] (ORCID:0000000211426627), Dasgupta, Neil P. [University of Michigan, Ann Arbor, MI (United States)] (ORCID:0000000251804063). 2025-09-17. Modeling diffusion and depletion in high-aspect-ratio atomic layer deposition processes: Process parameters and manufacturing impacts. https://doi.org/10.1116/6.0004702

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Breaking the Linear Scaling Relations for the Oxygen Reduction Reaction with a Dual‐Atom Catalyst Composed of a MnFe‐Porphyrrole Aerogel

Bimetallic catalysts offer enhanced catalytic performance through synergistic interactions between the two metals, allowing them to break the linear scaling relations and reach high electrocatalytic activity. This study presents bimetallic aerogel-based catalyst synthesized as a covalent, three-dimensional framework containing neighboring iron and manganese sites. The aerogel structure provides a high surface area and porosity, facilitating an ultra-high active site density and efficient mass transport. The MnFe porphyrrole's unique structure is obtained by alternately linking Mn-porphyrin and Fe-corrole complexes. It exhibited outstanding performance with an onset potential of 0.99 V RHE . Comparative studies with a free-base Fe porphyrrole catalyst (E onset 0.97 V RHE ) revealed that while Mn incorporation led to only a slight improvement in half-cell performance, it resulted in significantly enhanced performance in anion exchange membrane fuel cell. The MnFe catalyst achieved an OCV of 0.97 V and a peak power density of 0.27 W cm −2 , outperforming the free-base Fe counterpart. Using density functional theory calculations, we show that the higher ORR activity of MnFe-porphyrrole is due to charge transfer between Mn and Fe atoms, which is absent in the reference free-base Fe-porphyrrole. These findings underscore the advantages of bimetallic catalysts in improving ORR activity and fuel cell efficiency by leveraging synergistic effects.

Aerogel↗

Synthesis and Properties of Cross-Linked Polyamide Aerogels

We report the first synthesis of cross-linked polyamide aerogels through step growth polymerization using a combination of diamines, diacid chloride and triacid chloride. Polyamide oligomers endcapped with amines are prepared as stable solutions in N-methylpyrrolidinone from several different diamine precursors and 1,3-benzenedicarbonyl dichloride. Addition of 1,3,5-benzenetricarbonyl trichloride yields gels which form in under five minutes according to the scheme shown. Solvent exchange of the gels into ethanol, followed by drying using supercritical CO2 extraction gives colorless aerogels with densities around 0.1 to 0.2 gcm3. Thicker monolithes of the polyamide aerogels are stiff and strong, while thin films of certain formulations are highly flexible, durable, and even translucent. These materials may have use as insulation for deployable space structures, rovers, habitats or extravehicular activity suits as well as in many terrestrial applications. Strucure property relationships of the aerogels, including surface area, mechanical properties, and thermal conductivity will be discussed.

Aerogel↗