Tailoring Nitinol for elastocaloric application
Abstract
This study focuses on tailoring commercial Nitinol, the most commonly used elastocaloric material, for near-room-temperature cooling applications. Short heat treatments near 500 °C were used to fine-tune the material’s transition temperature, resulting in austenite finish temperatures ranging from 6.0 to 25.5°C and altered superelastic and elastocaloric properties. Plateau stresses decreased while temperature changes rose from 21.5°C up to 27.9°C at 6% strain. Significant variability in the Nitinol response when testing below its austenite finish temperature was observed. In conclusion, the effect of mechanical cycling on transition temperatures was also evaluated, demonstrating an increase for all the samples.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Czernuszewicz, Agata [Ames Lab., and Iowa State Univ., Ames, IA (United States)] (ORCID:0000000233992515), Pelton, Alan R. [G.RAU, Inc., Scotts Valley, CA (United States); Stanford Univ., CA (United States)], Carl, Matthew [ATI Specialty Alloys and Components, Albany, OR (United States)], Slaughter, Julie [Ames Lab., and Iowa State Univ., Ames, IA (United States)]. 2025-10-24. Tailoring Nitinol for elastocaloric application. https://doi.org/10.1557/s43579-025-00855-1
Cite the original work for its findings. Save a collection to share your selection of sources.