Engineering PapersSearch

DOE OSTI · 2997042

Encapsulant UV Accelerated Aging Experimental Data

Abstract

Chemical and thermal characterization (FTIR-ATR, Soxhlet extraction, DSC) of polymeric encapsulants (EVA, POE, EPE) aged under accelerated aging conditions containing an UV source.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Liu, Kuan [Stanford Univ., CA (United States)], Miller, David [National Renewable Energy Laboratory (NREL), Golden, CO (United States)], Bosco, Nick [National Renewable Energy Laboratory (NREL), Golden, CO (United States)], Newkirk, Jimmy [National Renewable Energy Laboratory (NREL), Golden, CO (United States)], Dauskardt, Reinhold [Stanford Univ., CA (United States)]. 2025-09-30. Encapsulant UV Accelerated Aging Experimental Data. https://doi.org/10.21948/2997042

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Coupons (mini-modules) experimental data

Adhesion testing results on mini-module coupons (cell/encapsulant/glass laminates) that were aged under the different accelerated aging conditions (outlined more in the DataHub URL).

accelerated aging

Investigating the Crosslinking, Degradation, and Adhesion Behavior of Photovoltaic Encapsulants Under Thermal Accelerated Aging

Degradation of photovoltaic (PV) module encapsulant characteristics that lead to mechanical embrittlement and delamination remains a cause of failure in solar installations. A multiscale reliability model connecting the encapsulant mechanical and fracture properties to the degraded molecular structure and interfacial bonding to adjacent solar cell and glass substrates was previously published. The model, developed primarily for poly(ethylene-co-vinyl acetate) acetate (EVA) encapsulants, remains to be experimentally validated. Determining the degradation and crosslinking kinetics of alternative encapsulants, such as polyolefin elastomer (POE) and EVA/POE/EVA composites (EPE), can generalize the model. In this work, we subject fully cured EVA, POE, and EPE encapsulants to accelerated thermal aging to determine how high temperatures impact reaction kinetics. An increase in gel content (crosslinking) and decrease in crystallinity of the encapsulants under hot-aerobic (90 degrees C, 22% RH) and hot-anaerobic (90 degrees C, sealed in N 2 air) aging were observed, even in the absence of UV and crosslinking initiators. Fourier transform infrared spectroscopy (FTIR)-attenuated total reflectance analysis showed insignificant encapsulant degradation, demonstrating the critical role of UV and moisture in accelerating degradation. Adhesion testing performed on coupon-level specimens (cell/encapsulant/glass laminates) showed decreases in adhesion energy, Gc , from 5000 h of hot-dry (90 degrees C, ~1% RH) and hot-humid (90 degrees C, 60% RH) aging. POE coupons demonstrated the best stability, followed by EPE then EVA. For EVA and POE, hot-humid aged coupons experienced a larger decrease in Gc due to enhanced hydrolytic degradation. Hot-dry aging condition demonstrated that thermal degradation of the interface could be significant even if the encapsulant experiences negligible degradation in the absence of UV and elevated humidity.

accelerated aging