Consistency and reproducibility in atomic layer deposition

Abstract

Atomic layer deposition (ALD) is a thin film synthesis technique that can provide exquisite accuracy and precision in film thickness and composition even on complex, large area substrates. Based on self-limiting surface chemistry, ALD can be insensitive to process conditions and reactor designs, allowing an ALD process developed in one lab to be easily reproduced in other labs. In practice, however, ALD is sometimes difficult to reproduce or replicate, and the results can vary substantially between ALD reactors and between labs. This is exemplified by large deviations in reports on the growth of, e.g., Al2O3, FeOx, and TiO2 given the same precursors under similar conditions. Furthermore, the problem of irreproducibility seems to be growing as ALD is adopted by more researchers and integrated into new applications. In this article, the authors highlight some of the major sources of variations and errors and common misconceptions related to ALD. In particular, the authors focus on issues related to precursors, substrates, and deposition tools. The authors illustrate these problems through examples from the literature, and they present results from numerical simulations that describe how nonidealities would manifest in thickness profiles in a typical cross-flow reactor. They also describe how reproducibility in ALD is linked to consistent experimental practice and reporting between labs. The authors’ hope is that by educating newcomers to ALD and advocating for consistent reporting of deposition conditions, they can minimize irreproducibility and enable ALD practitioners to realize the full potential afforded by self-limiting surface chemistry.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Sønsteby, Henrik H. (ORCID:0000000255971125), Yanguas-Gil, Angel (ORCID:0000000182073825), Elam, Jeffrey W. (ORCID:0000000258612996). 2020-02-06. Consistency and reproducibility in atomic layer deposition. https://doi.org/10.1116/1.5140603

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗