An automatic multi-precursor flow-type atomic layer deposition system

Abstract

Designs for two automated atomic layer deposition (ALD) flow reactors are presented, and their capabilities for coating additively manufactured (AM) metal prints are described. One instrument allows the coating of several AM parts in batches, while the other is useful for single part experiments. To demonstrate reactor capabilities, alumina (Al 2 O 3 ) was deposited onto AM 316L stainless steel by dosing with water (H 2 O) vapor and trimethylaluminum (TMA) and purging with nitrogen gas (N 2 ). Both instruments are controlled by custom-programmed LabVIEW software that enables in situ logging of temperature, total pressure, and film thickness using a quartz crystal microbalance. An initial result shows that 150 ALD cycles led to a film thickness of ~55 nm, which was verified with Rutherford backscattering spectroscopy. This indicates that the reactors were indeed depositing single atomic layers of Al 2 O 3 per ALD cycle, as intended.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Rodriguez, Daniel Jorge, Her, Mai Ar, Usov, Igor Olegovich, Safarik, Douglas Joseph, Jones, Rommel, Heidlage, Michael Gregory, Gorey, Timothy John. 2024-11-18. An automatic multi-precursor flow-type atomic layer deposition system. https://doi.org/10.1063/5.0222271

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

High Multiplicity Trigger for long-lived particles in CMS detector

Searches for long-lived particles (LLPs) at the CMS experiment often involve unconventional event topologies that are difficult to efficiently select using standard trigger strategies. To improve sensitivity to such signatures during LHC Run 3 operation, a dedicated High Multiplicity Trigger (HMT) has been developed and deployed in the CMS trigger system. The trigger targets events containing unusually large numbers of hits in the CMS cathode strip chamber (CSC) muon detectors, a characteristic signature of several LLP scenarios involving displaced decays in the muon system. The HMT implementation, trigger logic, rate dependence with pileup, and operational stability are described. Optimized hit multiplicity thresholds are used to maintain acceptable trigger rates under high-luminosity and high-pileup conditions while preserving high efficiency across a broad range of LLP lifetimes and kinematic regimes. The trigger performance is evaluated using both simulated event samples and proton-proton collision data collected during Run 3 of the LHC. The HMT substantially extends the CMS sensitivity to non-standard signatures associated with LLP decays and provides a flexible platform for future searches for physics beyond the Standard Model.

47 OTHER INSTRUMENTATION↗