DOE OSTI · 2349491
Improved Creep Testing Approach for Bentonite EBS
Abstract
In the United States, the nuclear reactor contributes 18.7 percent of the nation’s total electricity generation and produces a significant amount of spent nuclear fuel (SNF) and high-level waste. Because SNF is being stored for longer periods than initially envisioned, the U.S. Department of Energy Office of Nuclear Energy, Office of Spent Fuel and Waste Science and Technology is assessing the technical performance of the SNF storage systems after extended durations. The concept of a sustainable geologic repository for SNF disposal relies heavily on the safety provided by multiple barriers, such as repository host rock, overlying rock formation, and human-made engineered barrier systems (EBS). One of the major components of EBS is bentonite-based buffer materials that isolate the nuclear-waste canisters from the host rock and fill the void left in the horizontally drilled boreholes. The resaturated bentonite has a swelling characteristic, which is useful for self-sealing the microcracks in the host rock and supporting the canister’s heavy weight. However, factors such as nonuniformity in the saturation, swelling pressure of bentonite, and the high temperature at the canister-bentonite interface may lead to instability of the waste canister inside the borehole. Therefore, evaluating the long-term deformation of bentonite-based material is necessary. RESPEC Company, LLC recently completed a preliminary study for the U.S. Department of Energy (DE SC0022804) that is attempting to understand the time-dependent deformation in the consolidated sand/bentonite (SB) specimens through triaxial creep experiments and improve the understanding of EBS performance under anticipated repository conditions. The project included developing a standard testing procedure for preparing the consolidated core specimen from a mixture of sand and bentonite in a 50:50 ratio by weight, fabricating a new pressure vessel in-house, modifying existing creep equipment to perform triaxial creep experiments on consolidated SB specimens, and performing six long-term triaxial creep experiments under low-deviatoric stress at two different temperature conditions, which is representative of hypothetical conditions that might be encountered in a geologic repository within a reasonable rate of success in completing creep experiments. The consolidated SB specimen was prepared using the novel specimen preparation procedure and had physical characteristics (e.g., moisture content and bulk density) reasonably comparable with the properties of bentonite-based buffer, which is proposed to be used in the EBS in the Swedish KBS-3H design and the Swiss design of SNF disposal in the horizontal drifts. The newly fabricated pressure vessel could withstand the confining pressure of up to 15 megapascals (MPa) while maintaining the test temperature of up to 90 degrees Celsius (°C) for long-term creep experiments. The preliminary results from the triaxial creep experiments suggested that the consolidated SB specimen may experience time-dependent deformation at a low-deviatoric stress state and room temperature condition. Based on the deformation recorded in the SB specimen from axial and radial linear variable differential transformers (LVDTs) and physical characteristic changes, it is apparent that the time-dependent deformation is a combination of consolidation and creep, which is influenced by the level of deviatoric stresses and temperature. The systematic creep testing of bentonite-based specimens helped develop a standard testing procedure applicable for analyzing the similar characteristics of shale or clay-like materials in different geologic conditions outside repository science, including in civil engineering and infrastructure projects, underground and open pit mining, and deep drilling.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Gupta, Neel, Keffeler, Evan R., Hladysz, Jakub P., Buchholz, Stuart A., Vining, Cody A., Hardin, Ernest L.. 2024-05-14. Improved Creep Testing Approach for Bentonite EBS. https://doi.org/10.2172/2349491
Cite the original work for its findings. Save a collection to share your selection of sources.